1. Technical Field
The present disclosure relates to a method for manufacturing a shell with a textured appearance.
2. Description of Related Art
With the development of surface treatment technology, it is feasible to decorate the shells for portable electronic devices, such as by texturing the shells. A textured appearance can be achieved by an implementing of an extra surface treatment, such as with a laser to etch a previous molded shell. However, the extra surface treatment usually costs time and money.
Therefore, there is room for improvement within the art.
Many aspects of the new method for manufacturing a shell with a textured appearance can be better understood with reference to the following drawings. The components in the drawings are not necessarily drawn to scale, the emphasis instead being placed upon clearly illustrating the principles of the method for manufacturing a shell with a textured appearance. Moreover, in the drawings, like reference numerals designate corresponding parts throughout the several views.
An exemplary manufacturing method is provided for manufacturing a shell 10 (shown in
Referring further to
A plastic film 12 is provided and made of a material selected from a group consisting of polycarbonate (PC), polyethylene terephthalate (PET), polymethyl methacrylate (PMMA) or other plastic materials that may be transparent to a degree. The surface of the plastic film 12 has a decorative layer 124 formed thereon for example, the decorative layer 124 can include a colorful pattern or product logo. The decorative layer 124 can be an ink layer fabricated by a typical screen printing.
The plastic film 12 is trimmed into a predetermined two-dimensional shape. The trimmed plastic film 12 is then hot formed into a predetermined three-dimensional shape corresponding to the shell 10.
Referring to
The male mold 24 and the female mold 22 is closed and a molten plastic material 246 is injected through the flow passage 244 into the mold cavity 222. The plastic material 246 is selected from a group consisting of Polyethylene (PE), polyamide (PA), polycarbonate (PC), acrylonitrile-butadiene-styrene (ABS), polymethyl methacrylate (PMMA) and polyethylene terephthalate (PET). The injected molten plastic material 246 fills the mold cavity 222 and pushes the opposite surface of the plastic film 12 further into the textured mold portion 224. Thus, the textured shell portion 122 of the shell 10 is physically achieved.
After cooling, the base shell 14 attached to the surface of the film 12 with the decorative layer 124 is formed. The shell 10 can then be taken out by opening the male mold 24 and the female mold 22.
It is to be understood, however, that even through numerous characteristics and advantages of the exemplary invention have been set forth in the foregoing description, together with details of the structure and function of the invention, the disclosure is illustrative only, and changes may be made in detail, especially in matters of shape, size, and arrangement of parts within the principles of the invention to the full extent indicated by the broad general meaning of the terms in which the appended claims are expressed.
Number | Date | Country | Kind |
---|---|---|---|
200810302680.7 | Jul 2008 | CN | national |