This application claims priority to China Application Serial Number 201810251026.1, filed Mar. 26, 2018, which is herein incorporated by reference.
The present invention relates to a resistor. More particularly, the present invention relates to a method for manufacturing a shunt resistor having a modular structure.
In manufacturing a shunt resistor, an E-beam welding technique, a seam welding technique or a laser beam welding technique is typically used to combine a highly electrically-conductive electrode material with a resistance alloy material to form a resistance composite material. Then, the resistance composite material is divided and punched to form a preliminary model for plural shunt resistors. Next, resistance of the preliminary model of the shunt resistor is trimmed and adjusted by using a resistance trimming apparatus, so as to achieve an accuracy of the resistance of the shunt resistor.
However, an E-beam welding operation has to be performed in vacuum for the whole process, thus increasing welding cost. In addition, during the E-beam welding operation, materials are likely to be spattered, thus not only affecting a main body of the resistance alloy material that results in a bad control on the resistance of the shunt resistor, but also forming holes and/or spattered protrusions on a surface of the shunt resistor that results in a poor appearance of the shunt resistor. Furthermore, if the depth of the E-beam is not appropriately adjusted during welding, obvious weld beads are formed, and the resistance of the shunt resistor is also hard to be controlled. Moreover, when punching is performed, the stress in the resistance composite material is changed, thus causing the resistance of the shunt resistor to be changed. Accordingly, it needs a lot time to trim the resistance of the shunt resistor that is formed by using the E-beam welding technique. A remnant of the resistance composite material after being punched is a composite material of the electrode material and the resistance alloy material, and thus is difficult to be recycled.
When being aligned and emitted toward top and bottom sides of the resistance composite material for welding the resistance composite material, the laser beams are often too large or too small, thus resulting in weld beads with poor appearance, and poor control of the resistance of the shunt resistor. In addition, the laser beam welding technique also has disadvantages including of difficultly recycling remnants of the material and requiring a lot time of trimming the resistance.
One objective of the present invention is to provide a method for manufacturing a shunt resistor, in which a highly electrically-conductive electrode material and a resistance alloy material are respectively used to form the first electrode plate and the second electrode plate, and the resistor plate, and then rivets are used to combine the first electrode and the second electrode plate with the resistor plate located on the first electrode and the second electrode. Thus, utilization of the electrode material and the resistance material is increased, remnants of the electrode material and the resistance material are easy to be recycled, and the shunt resistors may be in various shapes according to the practical requirements.
Another objective of the present invention is to provide a method for manufacturing a shunt resistor, in which a first rivet and a second rivet are used to pre-position the resistor plate on the first electrode plate and the second electrode plate, and pressure and current are directly applied to the first rivet and the second rivet, such that the current is mainly centered on the first rivet and the second rivet. Thus, heat generated by applying current is also centered on the first rivet and the second rivet, such that an outer edge of the first rivet, the first electrode plate, and the resistor plate are welded, and an outer edge of the second rivet, the second electrode plate, and the resistor plate are welded. Accordingly, with the application of the method, productivity is effectively enhanced, and energy consumption of welding the resistor module is greatly decreased, thereby reducing production cost of the shunt resistor. Furthermore, a combination method that uses the rivets to weld the electrode plates and the resistor plate can strengthen the structure of the shunt resistor, thereby enhancing stability of the shunt resistor.
Still another objective of the present invention is to provide a method for manufacturing a shunt resistor, in which the resistance of the resistor plate can be firstly and accurately calculated in forming the resistor plate, such that the accuracy of the resistance of the shunt resistor is enhanced, and time for trimming the resistance of the shunt resistor is greatly reduced, thereby effectively increasing productivity.
Yet another objective of the present invention is to provide a method for manufacturing a shunt resistor, in which various resistor modules are arranged on a conveyer in sequence, the resistor modules are pressed in sequence as the conveying of the conveyer by simultaneously pressing two sides of each of the resistor modules, and pressure and current are directly applied to the rivets by using conductive modules. Thus, the shunt resistors can be continuously manufactured, thereby effectively enhancing production efficiency.
According to the aforementioned objectives, the present invention provides a method for manufacturing a shunt resistor. In this method, a first electrode plate and a second electrode plate are provided, in which the first electrode plate includes a first carrying portion, the second electrode plate includes a second carrying portion, the first carrying portion has at least one first hole, and the second carrying portion at least one second hole. A resistor plate is placed between the first electrode plate and the second electrode plate on the first carrying portion and the second carrying portion, in which the resistor plate has at least one first through hole and at least one second through hole, the first through hole is correspondingly located on the first hole, and the second through hole is correspondingly located on the second hole. At least one first rivet is pressed and placed into the first through hole and the first hole, and at least one second rivet is pressed and placed into the second through hole and the second hole. A current is applied to the first rivet and the second rivet to weld the first rivet, the first electrode plate, and the resistor plate, and to weld the second rivet, the second electrode plate, and the resistor plate.
According to the aforementioned objectives, the present invention further provides a method for manufacturing a shunt resistor. In this method, various resistor modules are placed on a conveyer. Each of the resistor modules includes a first electrode plate, a second electrode plate, and a resistor plate. The first electrode plate includes a first carrying portion, and the first carrying portion has at least one first hole. The second electrode plate includes a second carrying portion, and the second carrying portion has at least one second hole. The resistor plate is disposed between the first electrode plate and the second electrode plate and is located on the first carrying portion and the second carrying portion, in which the resistor plate has a first side surface and a second side surface opposite to the first side surface, the resistor plate has at least one first through hole and at least one second through hole, the first through hole is correspondingly located on the first hole, and the second through hole is correspondingly located on the second hole. The first electrode plate and the second electrode plate of each of the resistor modules are pressed onto the first side surface and the second side surface of the resistor plate respectively. At least one first rivet and at least one second rivet are pressed and placed into the first through hole and the first hole, and the second through hole and the second hole of each of the resistor modules respectively. A current is applied to the first rivets and the second rivets in the resistor modules in sequence to weld the first rivet, the first electrode plate, and the resistor plate of each of the resistor modules, and to weld the second rivet, the second electrode plate, and the resistor plate of each of the resistor modules.
The invention can be more fully understood by reading the following detailed description of the embodiment, with reference made to the accompanying drawings as follows:
Referring to
Next, a step 210 is performed to provide a resistor plate 120 and to place the resistor plate 120 on the first carrying portion 102 of the first electrode plate 100 and the second carrying portion 112 of the second electrode plate 110, in which the resistor plate is placed between the first electrode plate 100 and the second electrode plate 110. The resistor plate 120, the first electrode plate 100, and the second electrode plate 110 form a resistor module 130 together. The resistor plate 120 has at least one first through hole 122 and at least one second through hole 124, in which the first through hole 122 and the second through hole 124 are respectively located in two opposite sides and both pass through the resistor plate 120. In placing the resistor plate 120, the first through hole 122 of the resistor plate 120 is correspondingly located on the first hole 104 of the first carrying portion 102 of the first electrode plate 100, the second through hole 124 of the resistor plate 120 is correspondingly located on the second hole 114 of the second carrying portion 112 of the second electrode plate 110, and the first through hole 122 and the second through hole 124 are respectively aligned to the first hole 104 and the second hole 114. The resistor plate 120 may be formed by punching a resistance alloy material, so as to form the resistor plate 120 with a desired shape and resistance. A material of the resistor plate 120 includes, but is not limited to, a MnCuSn alloy, a MnCuNi alloy, a MnCu alloy, a NiCrAl alloy, a NiCrAlSi alloy, or a FeCrAl alloy.
In the present embodiment, the resistor plate 120 shown in
Referring to
Next, a pressure 150 is applied to a bottom surface of the first carrying portion 102 of the first electrode plate 100 and the first rivet 140, and a pressure 150a is applied to a bottom surface of the second carrying portion 112 of the second electrode plate 110 and the second rivet 142, so as to closely connect the first rivet 140 with the first electrode plate 100 and the resistor plate 120, and to closely connect the second rivet 142 with the second electrode plate 110 and the resistor plate 120. In some examples, a first conductive element 152 and a second conductive element 154 that are high-temperature resistant may be used to apply the pressure 150 to the first rivet 140 and the bottom surface of the first carrying portion 102 of the first electrode plate 100 respectively, and a third conductive element 156 and a fourth conductive element 158 that are high-temperature resistant may be used to apply the pressure 150a to the second rivet 142 and the bottom surface of the second carrying portion 112 of the second electrode plate 110 respectively. In other embodiments, the first conductive element 152 and the third conductive element 156 may be integrated into one conductive element to simultaneously apply the pressure to the first rivet 140 and the second rivet 142; and the second conductive element 154 and the fourth conductive element 158 may also be integrated into one conductive element to simultaneously apply the pressure to the bottom surface of the first carrying portion 102 of the first electrode plate 100 and the bottom surface of the second carrying portion 112 of the second electrode plate 110. Materials of the first conductive element 152, the second conductive element 154, the third conductive element 156, and the fourth conductive element 158 of high-temperature resistant preferably use conductive materials with melting points exceeding 3000 degrees Celsius, such as carbon plates or tungsten plates.
In some examples, a step 230 may be optionally performed to apply a pressure 160 to the first electrode plate 100 and the second electrode plate 110, thereby respectively pressing the first electrode plate 100 and the second electrode plate 110 onto the first side surface 126 and the second side surface 128 of the resistor plate 120 from a first side end 132 and a second side end 134 of the resistor module 130, in which the first side end 132 is opposite to the second side end 134. The step 230 may be performed before the step 220. For example, the pressure 160 may preferably range from about 0.1 MPa to about 10 MPa depending on a current applied to the resistor module 130. With the pressing step, the side surface 100s of the first electrode plate 100 is closely adhered to the first side surface 126 of the resistor plate 120, and the side surface 110s of the second electrode plate 110 is closely adhered to the second side surface 128 of the resistor plate 120. A connection surface formed between the first electrode plate 100 and the resistor plate 120, and a connection surface formed between the second electrode plate 110 and the resistor plate 120 both are hetero-junctions. In some examples, a first pressing element 162 and a second pressing element 164 may be used to press the first electrode plate 100 and the second electrode plate 110 respectively, in which the first pressing element 162 and the second pressing element 164 are high-temperature resistant. Materials of the first pressing element 162 and the second pressing element 164 may use high-temperature resistant materials, such as carbon plates or tungsten plates.
Subsequently, a step 240 is performed to apply a current to the first rivet 140 through the first electrode plate 100 and the first rivet 140, and to apply a current to the second rivet 142 through the second electrode plate 110 and the second rivet 142 by using a power supply 170. The power supply 170 may be a direct current (DC) power supply or an alternating current (AC) power supply. In some examples, the power supply 170 may apply the current through the first conductive element 152, the second conductive element 154, the third conductive element 156, and the fourth conductive element 158 that are high-temperature resistant. The first conductive element 152 presses the first rivet 140, the second conductive element 154 presses the bottom surface of the first carrying portion 102 of the first electrode plate 100, the third conductive element 156 presses the second rivet 142, and the fourth conductive element 158 presses the bottom surface of the second carrying portion 112 of the second electrode plate 110. The power supply 170 preferably applies high current to the first rivet 140 and the second rivet 142. For example, the current applied by the power supply 170 may range from about 700 A to about 800 A, or higher. In some examples, two electrodes of the power supply 170 are connected to the first conductive element 152 and the third conductive element 156, and the second conductive element 154 and the fourth conductive element 158 respectively via a first wire 172 and a second wire 174. The power supply 170 applies the current to the first rivet 140 and the second rivet 142 from the first rivet 140, the second rivet 142, the first electrode plate 100, and the second electrode plate 110 through the first wire 172 and the second wire 174.
The current is mainly centered on the first rivet 140 and the second rivet 142, and the heat generated by applying the current is also centered on the first rivet 140 and the second rivet 142, such that an outer edge of the first rivet 140, and edges of the first electrode plate 100 and the resistor plate 120 that are close to the first rivet 140 are heated and melt firstly; and an outer edge of the second rivet 142, and edges of the second electrode plate 110 and the resistor plate 120 that are close to the second rivet 142 are heated and melt firstly. With the pressures 150, 150a, and 160, materials of the first rivet 140, the first electrode plate 100, and the resistor plate 120 diffuse and exchange with each other by thermal melt, and materials of the second rivet 142, and the second electrode plate 110, and the resistor plate 120 diffuse and exchange with each other by thermal melt, thus welding together to form a shunt resistor. Accordingly, the first rivet 140 and the second rivet 142 can combine the resistor plate 120 with the first electrode plate 100 and the second electrode plate 110.
In some examples, when the current is applied to the first rivet 140 and the second rivet 142, an inert gas 180, such as nitrogen or argon, may be simultaneously introduced, such that the welding of the resistor module 130 is performed in an inert gas environment to protect the welded portions from being oxidized. In addition, when the current is applied to the first rivet 140 and the second rivet 142, the first electrode plate 100 may be placed on a first heat conductive base 190, and the second electrode plate 110 may be placed on a second heat conductive base 192. In some exemplary examples, the first heat conductive base 190 is closer to the first pressing element 162 and is farther away the first rivet 140, such that the heat of the first electrode plate 100 is conducted by the first heat conductive base 190, thereby centering the heat on the first rivet 140. In addition, the second heat conductive base 192 is closer to the second pressing element 164 and is farther away the second rivet 142, such that the heat of the second electrode plate 110 is conducted by the second heat conductive base 192, thereby centering the heat on the second rivet 142.
In this method, the electrode material and the resistance alloy material are respectively used to form the first electrode plate 100 and the second electrode plate 110, and the resistor plate 120, and then the first rivet 140 is used to combine the first electrode plate 100 with the resistor plate 120 located on the first carrying portion 102 of the first electrode plate 100, and the second rivet 142 is used to combine the second electrode plate 110 with the resistor plate 120 located on the second carrying portion 112 of the second electrode plate 110. Thus, utilization of the electrode material and the resistance material is increased, remnants of the electrode material and the resistance material are easy to be recycled, and the shunt resistors may be in various shapes according to the practical requirements. In addition, the first rivet 140 and the second rivet 142 can pre-position the resistor plate 120 on the first electrode plate 100 and the second electrode plate 110, and a rate of welding the first rivet 140, the first electrode plate 100, and the resistor plate 120 and a rate of welding the second rivet 142, the second electrode plate 110, and the resistor plate 120 are increased by directly applying the pressures 150 and 160 and the current to the first rivet 140, and directly applying the pressures 150a and 160 and the current to the second rivet 142. Accordingly, with the application of the method, productivity is effectively enhanced, and energy consumption of welding the resistor module 130 is greatly decreased, thereby reducing production cost of the shunt resistor. Furthermore, a combination method that uses the first rivet 140 to weld the first electrode plate 100 and the resistor plate 120, and uses the second rivet 142 to weld the second electrode plate 110 and the resistor plate 120 can strengthen the structure of the shunt resistor, thus enhancing stability of the shunt resistor. Moreover, the resistance of the resistor plate 120 can be firstly and accurately calculated in forming the resistor plate 120, such that the accuracy of the resistance of the shunt resistor is enhanced, and time for trimming the resistance of the shunt resistor is greatly reduced, thereby effectively increasing productivity.
Referring to
Next, a step 410 is performed to apply a pressure 330 to the first electrode plate 100 and the second electrode plate 110, thereby pressing the first electrode plate 100 onto the first side surface 126 of the resistor plate 120 from the first side end 132 of the resistor module 130, and pressing the second electrode plate 110 onto the second side surface 128 of the resistor plate 120 from the second side end 134 of the resistor module 130. Thus, the side surface 100s of the first electrode plate 100 is closely adhered to the first side surface 126 of the resistor plate 120, and the side surface 110s of the second electrode plate 110 is closely adhered to the second side surface 128 of the resistor plate 120. For example, the pressure 330 preferably ranges from about 0.1 MPa to about 10 MPa depending on a current applied to the resistor module 130. A connection surface formed between the first electrode plate 100 and the resistor plate 120, and a connection surface formed between the second electrode plate 110 and the resistor plate 120 both are hetero-junctions. In some examples, a first pressing element 332 and a second pressing element 334 may be used to press the first electrode plate 100 and the second electrode plate 110 respectively, in which the first pressing element 332 and the second pressing element 334 are high-temperature resistant. Materials of the first pressing element 332 and the second pressing element 334 may use high-temperature resistant materials, such as carbon plates or tungsten plates.
Next, referring to
Then, the pressure 150 is sequentially applied to the bottom surfaces 100b of the first electrode plates 100 and the first rivets 140 in the resistor modules 130, and the pressure 150a is sequentially applied to the bottom surfaces 110b of the second electrode plates 110 and the second rivets 142 in the resistor modules 130 at an outlet 304 of the conveyer 300, thereby more closely connecting the first rivets 140 with the first electrode plates 100 and the resistor plates 120, and more closely connecting the second rivets 142 with the second electrode plates 110 and the resistor plates 120. In some examples, a first conductive element 320 and a second conductive element 322 that are high-temperature resistant may be used to apply the pressure to the first rivet 140 and the bottom surface of the first carrying portion 102 of the first electrode plate 100 respectively, and a third conductive element 324 and a fourth conductive element 326 that are high-temperature resistant may be used to apply the pressure to the second rivet 142 and the bottom surface of the second carrying portion 112 of the second electrode plate 110 respectively. Materials of the first conductive element 320, the second conductive element 322, the third conductive element 324, and the fourth conductive element 326 of high-temperature resistant may use conductive materials with melting points exceeding 3000 degrees Celsius, such as carbon plates or tungsten plates.
Subsequently, a step 430 is performed to apply a current to the first rivet 140 and the second rivet 142 respectively through the first electrode plate 100 of the resistor module 130 and the first rivet 140, and through the second electrode plate 110 and the second rivet 142 by using a power supply 340. The power supply 340 may be a direct current power supply or an alternating current power supply. In some examples, the power supply 340 may apply the current through the first conductive element 320, the second conductive element 322, the third conductive element 324, and the fourth conductive element 326 that are high-temperature resistant, in which the first conductive element 320, the second conductive element 322, the third conductive element 324, and the fourth conductive element 326 are near the outlet 304 of the conveyer 300. The first conductive element 320 and the third conductive element 324 respectively press the first rivet 140 on the first electrode plate 100 and the second rivet 142 on the second electrode plate 110, and the second conductive element 322 and the fourth conductive element 326 respectively press the bottom surface of the first carrying portion 102 of the first electrode plate 100 and the bottom surface of the second carrying portion 112 of the second electrode plate 110. The power supply 340 preferably applies to the first rivet 140 and the second rivet 142 with high current, such as the current ranging from about 700 A to about 800 A, or higher. In some examples, two electrodes of the power supply 340 are connected to the first conductive element 320 and the third conductive element 324, and the second conductive element 322 and the fourth conductive element 326 respectively via a first wire 342 and a second wire 344. The power supply 340 applies the current to the first rivet 140 and the second rivet 142 from the first electrode plate 100, the second electrode plate 110, the first rivet 140, and the second rivet 142 through the first wire 342 and the second wire 344.
With the applying of the current and the pressures, an outer edge of the first rivet 140, and edges of the first electrode plate 100 and the resistor plate 120 that are close to the first rivet 140 are heated and melt firstly, and an outer edge of the second rivet 142, and edges of the second electrode plate 110 and the resistor plate 120 that are close to the second rivet 142 are heated and melt firstly. Thus, materials of the first rivet 140, the first electrode plate 100, and the resistor plate 120 diffuse and exchange with each other by thermal melt, and materials of the second rivet 142, and the second electrode plate 110, and the resistor plate 120 diffuse and exchange with each other by thermal melt, thereby welding together. Therefore, the first rivet 140 and the second rivet 142 can combine the resistor plate 120 with the first carrying portion 102 of the first electrode plate 100 and the second carrying portion 112 of the second electrode plate 110. In some exemplary examples, the operation of applying the current to the first rivet 140 and the second rivet 142 is performed in an inert gas environment to protect the welded portions from being oxidized, in which the inert gas may be nitrogen or argon. In the present embodiment, the resistor modules 130, and the first rivets 140 and the second rivet 142 on the resistor modules 130 at the outlet 304 of the conveyer 300 are sequentially applied with the pressure and the current as the conveying of the conveyer 300, thereby sequentially welding the resistor modules to form shunt resistors. Accordingly, the application of the method can greatly enhance production efficiency of the shunt resistors.
Although the present invention has been described in considerable detail with reference to certain embodiments thereof, the foregoing embodiments of the present invention are illustrative of the present invention rather than limiting of the present invention. It will be apparent to those having ordinary skill in the art that various modifications and variations can be made to the present invention without departing from the scope or spirit of the invention. Therefore, the spirit and scope of the appended claims should not be limited to the description of the embodiments contained herein.
Number | Date | Country | Kind |
---|---|---|---|
2018 1 0251026 | Mar 2018 | CN | national |
Number | Name | Date | Kind |
---|---|---|---|
4037073 | Becker | Jul 1977 | A |
5382938 | Hansson | Jan 1995 | A |
6304062 | Batson | Oct 2001 | B1 |
10438730 | Kao | Oct 2019 | B2 |
20060193051 | Anthony | Aug 2006 | A1 |
20120154104 | Hetzler | Jun 2012 | A1 |
20120229247 | Yoshioka | Sep 2012 | A1 |
20140097933 | Yoshioka et al. | Apr 2014 | A1 |
20150212115 | Nakamura | Jul 2015 | A1 |
20170125142 | Nakamura | May 2017 | A1 |
Number | Date | Country |
---|---|---|
1545106 | Nov 2004 | CN |
101097232 | Jan 2008 | CN |
100481277 | Apr 2009 | CN |
101483091 | Jul 2012 | CN |
102640233 | Sep 2015 | CN |
205810498 | Dec 2016 | CN |
206639664 | Nov 2017 | CN |
201523653 | Jun 2015 | TW |
2017110354 | Jun 2017 | WO |
Number | Date | Country | |
---|---|---|---|
20190295748 A1 | Sep 2019 | US |