The present invention relates to a method of manufacturing a touch panel, and particular to a method for manufacturing a touch panel with a glass panel layer and a glass substrate. The method can produce multiple touch panels in one manufacturing cycle.
Touch panel is an input device which is often to be arranged to a screen of a Liquid Crystal Display (LCD) or a CRT. A user can press on the panel through a finger tip or a tip of a pen based on the instruction of the display showing through the touch panel so as to access the input of the position. A general structure of a touch panel, such as a resistive touch panel, is formed by two plates of resistive film attached oppositely with a certain gap between. Usually an upper resistive film is arranged on a surface of a panel layer made of a flexible clear film or a thin glass. A lower resistive film is arranged on a surface of a glass substrate. Through the gluing on a periphery of the opposite side of the panel layer, the two plates are attached together tightly as a touch panel. As known in recent years, through the improvement of performance and manufacturing quality and the deduction of the price, touch panel is extensively applied to various electronics. However, in some special application such as a touch panel equipped to a mobile GPS device, the touch panel will be usually exposed to sunlight and it must have the high temperature resistance ability. In such circumstance, a common plastic film is not appropriate for a material of a panel layer, and a heat-proof glass without light polarization will be a better choice. When a glass is used for a panel layer, the thickness should be very small to form a touch sensing ability which is usually thinner than 0.25 mm. Also, with a brittle characteristic of the glass and the low intensity, it can be only used for manufacturing a small area touch panel which is not bigger than 120 mm to 150 mm in length or width. Moreover, the thin glass is easy to break during a cutting process. It is also hard to maintain the flatness during the combination process of the thin plasses, an optical interference is happened such as a Newton Ring. Besides, the stress remained between the plates will reduce the intensity and the durability of the thin glasses. The manufacturing processes of the touch panel equipped to an automobile have a lot of difficulties to overcome as described above.
Accordingly, a primary object of the present invention is to provide a method for manufacturing a touch panel, and particular to a method of manufacturing a touch panel with a glass panel layer and a glass substrate and capable of producing multiple touch panels in one manufacturing cycle so as to improve production efficiency and also save time and labor power. Also, a greater area touch panel with thin glasses can be manufactured without twisting and breaking the glass during the processes so as to raise the quality and the yield of the touch panel product.
The thickness of the panel layer is about 0.15 mm to 0.25 mm, and the etching thickness is about 0.1 mm to 0.3 mm. Moreover, the gluing frame and sealing frame can be arranged to the substrate and to the panel layer, or to both of them. While the sealing frame can make of a petroleum wax, a light curable gluing, or a heat curable gluing. The constancy of the solution of the hydrofluoric acid is 10% to 30%.
Moreover, at least one function film is attached to the panel layer above the positions of each electrode unit after the process of etching and before the process of cutting, the function films are any or the combination of at least two of a polarizing film, filter, and border icon.
In order that those skilled in the art can further understand the present invention, a description will be provided in the following in details. However, these descriptions and the appended drawings are only used to cause those skilled in the art to understand the objects, features, and characteristics of the present invention, but not to be used to confine the scope and spirit of the present invention defined in the appended claims.
The features of the present invention will be further described in an embodiment of manufacturing a resistive touch panel with a glass panel layer with 0.2 mm thickness and a glass substrate with 0.5 mm thickness.
As shown in
A 0.4 mm thickness glass having an area corresponding to that of the substrate 1 is used as a panel layer 2. A lower surface of the panel layer 2 is formed with a plurality of upper electrode units 22 which are arranged corresponding to those of the lower electrode units 12 of the substrate 1. The upper electrode unit 22 also includes a clear transparent resistive film 22A, a bus electrode 22B, and others.
Then, the substrate 1 and the panel layer 2 are overlaid by aligning the targets 17, 27 on edges of the substrate 1 and the panel layer 2 respectively or by other precisely aligning method. By the gluing frames 41 and the sealing frame 42, the substrate 1 and the panel layer 2 are combined together as a combined plate. Therefore, each of the upper electrode units 22 and the corresponding lower electrode unit 12 are combined together by the gluing frame 41 so as to form as an independent touch sensing unit. Referring to the
The following thinning process is performed by etching the combined plate through a solution of hydrofluoric acid with density about 10% to 30%. The outer surfaces of the glasses of the substrate 1 and the panel layer 2 are etched to be removed with a thickness of 0.2 mm so as to form a desired thickness of a finished touch panel. That is, the panel layer 2 is thinned as a glass with 0.2 mm thickness, and the substrate 1 is thinned as a glass with 0.5 mm thickness.
A next process is to attach at least one function film 6 to the surface of the panel layer 2 above each electrode unit, such as a polarizing film, a filter, or a border icon. Thus the touch panel will have functions of polarizing and filtering, and also the intensity of the panel layer 2 will be improved so as to prevent the thin glass from being cracked and broken.
A next process is a cutting process as shown in the
Through the above description, the thicker substrate 1 and the thicker panel layer 2 used in the front manufacturing processes of the electrode unit arrangement, gluing frame attachment, and overlaying of two plates can prevent a crash and break because of a better intensity thereof. After the thinning process, one or more than one function film 6 attached to the panel layer 2 above each electrode unit can also improve the intensity of the panel layer 2 to prevent a crash and break. Therefore, the present invention of the touch panel with a glass panel layer and a glass substrate can produce one or more than one touch panel in one production cycle so as to improve production efficiency and also save time and labor power. Because of the better intensity of the thin glass of the panel layer 2 and the substrate 1 during the processes, a greater area touch panel can be manufactured without twisting and breaking the glass so as to substantially raise the quality and the yield of the touch panel product.
The present invention is thus described, it will be obvious that the same may be varied in many ways. Such variations are not to be regarded as a departure from the spirit and scope of the present invention, and all such modifications as would be obvious to one skilled in the art are intended to be included within the scope of the following claims.
Number | Name | Date | Kind |
---|---|---|---|
20020030769 | Bae | Mar 2002 | A1 |
20030057183 | Cho et al. | Mar 2003 | A1 |
20040263771 | Jeong et al. | Dec 2004 | A1 |
20080042996 | Endo et al. | Feb 2008 | A1 |