The present disclosure relates in general to wind turbine towers, and more particularly to methods of manufacturing wind turbine tower structures for preventing vortex shedding, reducing drag, and/or reinforcing the structures.
Wind power is considered one of the cleanest, most environmentally friendly energy sources presently available, and wind turbines have gained increased attention in this regard. A modern wind turbine typically includes a tower, a generator, a gearbox, a nacelle, and one or more rotor blades. The rotor blades capture kinetic energy of wind using known foil principles. The rotor blades transmit the kinetic energy in the form of rotational energy so as to turn a shaft coupling the rotor blades to a gearbox, or if a gearbox is not used, directly to the generator. The generator then converts the mechanical energy to electrical energy that may be deployed to a utility grid.
The wind turbine tower is generally constructed of steel tubes, prefabricated concrete sections, or combinations thereof. Further, the tubes and/or concrete sections are typically formed off-site, shipped on-site, and then arranged together to erect the tower. For example, one manufacturing method includes forming pre-cast concrete rings, shipping the rings to the site, arranging the rings atop one another, and then securing the rings together. As wind turbines continue to grow in size, however, conventional manufacturing methods are limited by transportation regulations that prohibit shipping of tower sections having a diameter greater than about 4 to 5 meters. Thus, certain tower manufacturing methods include forming a plurality of arc segments and securing the segments together on site to form the diameter of the tower, e.g. via bolting. Such methods, however, require extensive labor and can be time-consuming.
In addition, cylindrical towers can cause vortex shedding, which generally refers to an oscillating flow that takes place when air flows past the bluff (as opposed to streamlined) body at certain velocities, depending on the size and shape of the tower. Thus, in the oscillating flow, vortices are created at the back of the body and detach periodically from either side thereof. Therefore, the fluid flow past the body creates alternating low-pressure vortices on the downstream side of the body. If the bluff body is not mounted rigidly and the frequency of vortex shedding matches the resonance frequency of the tower, then the tower can begin to resonate, vibrating with harmonic oscillations driven by the energy of the flow. In addition, the aerodynamic drag on the tower increases the load on the structure as well as reduces the wind velocity which can have a negative effect on a downwind rotor machine.
In view of the foregoing, the art is continually seeking improved methods for manufacturing wind turbine towers. Accordingly, the present disclosure is directed to methods for manufacturing wind turbine tower structures that address the aforementioned issues.
Aspects and advantages of the invention will be set forth in part in the following description, or may be obvious from the description, or may be learned through practice of the invention.
In one aspect, the present disclosure is directed to a method for manufacturing a tower structure of a wind turbine. The method includes printing, via an additive printing device, the tower structure of the wind turbine of a cementitious material. The method also includes printing, via the additive printing device, one or more additional airflow modifying features on an outer surface the tower structure of the wind turbine so as to reduce and/or prevent vortex shedding, excitation, and/or drag of the tower structure. Further, the method includes curing the cementitious material so as to form the tower structure.
In one embodiment, the additional airflow modifying feature(s) may include strakes, scallops, protrusions, dimples, one or more coils wrapped at least partially around the tower structure, or combinations thereof. In another embodiment, the method may include printing, via the additive printing device, the tower structure of the wind turbine of the cementitious material to have a non-cylindrical shape as to further reduce and/or prevent vortex shedding, excitation, and/or drag of the tower structure.
In additional embodiments, during printing, the method may include embedding one or more reinforcement elements at least partially within the cementitious material at one or more locations of the tower structure. In such embodiments, embedding the one or more reinforcement elements at least partially within the cementitious material at one or more locations may include printing, via the additive printing device, the reinforcement element(s) within the cementitious material at the one or more locations during printing of the tower structure. More specifically, in one embodiment, the reinforcement element(s) may include elongated cables or wires, helical cables or wires, reinforcing bars, metallic or polymeric reinforcing fibers, reinforcing metallic rings couplings, and/or mesh. Such elements can be either statically placed in the tower structure to provide concrete reinforcement or post-tensioned after the cementitious material has cured to put the tower structure into compression.
In several embodiments, the method may include providing one or more molds of the tower structure on a foundation of the wind turbine and printing, via the additive printing device, the tower structure of the wind turbine within the one or more molds. In such embodiments, the method may also include printing, via the additive printing device, the one or more molds of the tower structure.
In another aspect, the present disclosure is directed to a method for manufacturing a tower structure of a wind turbine. The method includes printing, via an additive printing device, the tower structure of the wind turbine of a cementitious material on a foundation of the tower structure. Further, the method includes curing the cementitious material so as to form the tower structure. In addition, the method includes providing one or more reinforcement cables on an outer surface of the tower structure. Moreover, the method include printing, via the additive printing device, one or more additional airflow modifying features on the outer surface the tower structure of the wind turbine so as to reduce and/or prevent vortex shedding, excitation, and/or drag of the tower structure during installation, idling, service, or operation of the wind turbine.
In one embodiment, providing the reinforcement cable(s) on the outer surface of the tower structure may include wrapping the reinforcement cable(s) in the same direction around the tower structure with variable spacing between wraps and tensioning the reinforcement cable(s) on the outer surface of the tower structure to provide a varied compression level to the tower structure. Alternatively, providing the reinforcement cable(s) on the outer surface of the tower structure may include wrapping a plurality of reinforcement cables in opposing directions around the tower structure with constant spacing between wraps and tensioning the reinforcement cable(s) on the outer surface of the tower structure to provide a uniform compression level to the tower structure. This compression acts in both the axial (i.e. height) direction as well as the horizontal (i.e. hoop) direction, allowing the cementitious material of the tower structure to be optimized, thereby reducing the amount of cementitious material required in the tower structure as compared to conventional methods.
In another embodiment, providing the one or more reinforcement cables on the outer surface of the tower structure may include pre-tensioning the reinforcement cable(s) before providing the reinforcement cable(s) on the outer surface of the tower structure and releasing the one or more pre-tensioned reinforcement cable(s) after curing the cementitious material.
In further embodiments, providing the reinforcement cable(s) on the outer surface of the tower structure may include printing, via the additive printing device, the reinforcement cable(s) on the outer surface of the tower structure. In several embodiments, the reinforcement cable(s) may include, for example, solid reinforcing bars, hollow reinforcing bars, pultruded reinforcing bars, and/or mesh. It should be further understood that the method may further include any of the additional features and/or steps as described herein.
In yet another aspect, the present disclosure is directed to a tower structure for a wind turbine. The tower structure includes a tower wall formed, at least in part, of a cementitious material and one or more additional airflow modifying features additively printed onto an outer surface of the tower wall of the wind turbine so as to reduce and/or prevent vortex shedding, excitation, and/or drag of the tower structure during installation, idling, service, or operation of the wind turbine. It should be understood that the tower structure may further include any of the additional features as described herein.
These and other features, aspects and advantages of the present invention will become better understood with reference to the following description and appended claims. The accompanying drawings, which are incorporated in and constitute a part of this specification, illustrate embodiments of the invention and, together with the description, serve to explain the principles of the invention.
A full and enabling disclosure of the present invention, including the best mode thereof, directed to one of ordinary skill in the art, is set forth in the specification, which makes reference to the appended figures, in which:
Reference now will be made in detail to embodiments of the invention, one or more examples of which are illustrated in the drawings. Each example is provided by way of explanation of the invention, not limitation of the invention. In fact, it will be apparent to those skilled in the art that various modifications and variations can be made in the present invention without departing from the scope or spirit of the invention. For instance, features illustrated or described as part of one embodiment can be used with another embodiment to yield a still further embodiment. Thus, it is intended that the present invention covers such modifications and variations as come within the scope of the appended claims and their equivalents.
Generally, the present disclosure is directed to methods for manufacturing wind turbine towers using automated deposition of cementitious materials via technologies such as additive manufacturing, 3-D Printing, spray deposition, extrusion additive manufacturing, concrete printing, automated fiber deposition, as well as other techniques that utilize computer numeric control and multiple degrees of freedom to deposit material. More specifically, methods of the present disclosure include printing features or alternate geometry in concrete wind turbine towers to eliminate the potential of vortex shedding. For example, in certain embodiments, the printed features/geometry may include printed-in strakes or a predetermined outside profile (e.g. a scalloped edge, dimples, etc.).
Referring now to the drawings,
Referring now to
Referring now to
Referring now to
Referring particularly to
As shown at (102), the method 100 may include printing, via an additive printing device 32, the tower structure 12 of the wind turbine 10 of the cementitious material 28. For example, as shown in
Still referring to
Suitable polymer materials may include, for example, a thermoset material, a thermoplastic material, a biodegradable polymer (such as a corn-based polymer system, fungal-like additive material, or an algae-based polymer system) that is configured to degrade/dissolve over time, or combinations thereof. As such, in one embodiment, the outer polymer mold may be biodegradable over time, whereas the inner polymer mold remains intact. In alternative embodiments, the outer and inner molds may be constructed of the same material.
In such embodiments, as shown, the additive printing device 32 may be configured to fill the mold(s) 38 of the tower structure 12 with the cementitious material 28. More specifically, as shown, one or more of the nozzles 34 may be configured to print the cementitious material 28 into the molds 38. In alternative embodiments, rather than printing the cementitious material 28, the injector 36 of the additive printing device 32 may simply inject or fill the mold(s) 38 with the cementitious material 28, e.g. by injecting the cementitious material 28 from the top of the molds 38 or by injecting the cementitious material 28 through openings in the mold.
In additional embodiments, during printing, the method 100 may include embedding one or more of the reinforcement elements 30 at least partially within the cementitious material 28 at one or more locations of the tower structure 12. In such embodiments, the additive printing device 32 may be configured to print the reinforcement element(s) 30 within the cementitious material 28 at the one or more locations during printing of the tower structure 12.
In further embodiments, the additive printing device 32 is configured to print the cementitious material 28 in a manner that accounts for the cure rate thereof such that the tower structure 12, as it is being formed, can bond to itself. In addition, the additive printing device 32 is configured to print the tower structure 12 in a manner such that it can withstand the weight of the wall 20 as the additively-formed cementitious material 28 can be weak during printing. In certain embodiments, the method 100 may include printing, via the additive printing device 32, the tower structure 12 to have a non-cylindrical or alternative shape as to further reduce and/or prevent vortex shedding, excitation, and/or drag of the tower structure 12.
Referring back to
Referring particularly to
As shown at (202), the method 200 may include printing, via the additive printing device 32, the tower structure 12 of the wind turbine 10 of the cementitious material 28 on a foundation of the tower structure 12, such as the foundation 15 of the wind turbine 10. For example, as mentioned, the additive printing device 32 may be configured to print the tower structure 12 of the cementitious material 28 and/or may fill one or more molds 38 with the cementitious material 28 as described herein. As shown at (204), the method 200 may include curing the cementitious material 28 so as to form the tower structure 12.
As shown at (206), the method 200 may include providing one or more reinforcement cables 30 on the outer surface 22 of the tower structure 12. For example, in one embodiment, the additive printing device 32 may be configured to print the reinforcement cable(s) 30 on the outer surface 22 of the tower structure 12. In several embodiments, the reinforcement cable(s) 30 may include, for example, solid reinforcing bars, hollow reinforcing bars, pultruded reinforcing bars, and/or mesh. In addition, the reinforcement cable(s) 30 may be constructed of any suitable material, including for example, a metal or metal alloy (such as steel), a composite material, basalt, or similar.
Further, in certain embodiments, as shown in
Referring back to
Referring now to
As used herein, the term “processor” refers not only to integrated circuits referred to in the art as being included in a computer, but also refers to a controller, a microcontroller, a microcomputer, a programmable logic controller (PLC), an application specific integrated circuit, and other programmable circuits. The processor 46 is also configured to compute advanced control algorithms and communicate to a variety of Ethernet or serial-based protocols (Modbus, OPC, CAN, etc.). Additionally, the memory device(s) 48 may generally comprise memory element(s) including, but not limited to, computer readable medium (e.g., random access memory (RAM)), computer readable non-volatile medium (e.g., a flash memory), a floppy disk, a compact disc-read only memory (CD-ROM), a magneto-optical disk (MOD), a digital versatile disc (DVD) and/or other suitable memory elements. Such memory device(s) 48 may generally be configured to store suitable computer-readable instructions that, when implemented by the processor(s) 46, configure the controller 44 to perform the various functions as described herein.
This written description uses examples to disclose the invention, including the best mode, and also to enable any person skilled in the art to practice the invention, including making and using any devices or systems and performing any incorporated methods. The patentable scope of the invention is defined by the claims, and may include other examples that occur to those skilled in the art. Such other examples are intended to be within the scope of the claims if they include structural elements that do not differ from the literal language of the claims, or if they include equivalent structural elements with insubstantial differences from the literal languages of the claims.
Filing Document | Filing Date | Country | Kind |
---|---|---|---|