Claims
- 1. In a process for permanent shaping of hair comprising the steps of bringing the hair into a desired shape, treating the hair with a hair shaping agent, rinsing with water, subjecting the hair to an oxidative aftertreatment with an oxidizing agent selected from the group consisting of alkali bromates, sodium perborate, hydrogen peroxide and urea peroxide, setting the hair to form a permanent wave and drying, the improvement wherein the hair shaping agent consists essentially of an aqueous hair shaping composition having a pH from 6 to 8.5, said aqueous hair shaping composition containing 0.1 to 30 percent by weight of at least one Bunte-salt and 0.5 to 30 percent by weight of at least one member selected from the group consisting of sulfites and hydrogen sulfites and wherein said subjecting said hair to an oxidative aftertreatment includes treating said hair with an aqueous oxidative aftertreatment composition containing from 0.5 to 10 percent of said oxidizing agent, and
- wherein said a least one Bunts-salt is selected from the group consisting of 2-S-thiosulfatocarboxylic acids of the formula (I):
- M.sup.+- OOC--(CH.sub.2).sub.n --S.sub.2 O.sub.3.sup.- M.sup.+(I);
- wherein n is an integer from 1 to 6 and M.sup.+ is an alkali metal or ammonium cation;
- 2-S-thiosulfatoethylamine of the following formula (II):
- H.sub.2 N--CH.sub.2 --CH.sub.2 --S.sub.2 O.sub.3.sup.- M.sup.+(II),
- wherein M.sup.+ is an alkali metal or ammonium cation;
- polyamide-epichlorohydrin-Bunte-salt of the formula (III):
- P--N--CH.sub.2 --CH(OH)--CH.sub.2 --S.sub.2 O.sub.3.sup.- M.sup.+(III),
- wherein M.sup.+ is an alkali metal or ammonium cation and P is a polymer chain;
- polyoxyalkylene-Bunte-salts of the formula (IV) or (v):
- [(O-alkylene).sub.m OH].sub.q R[(O-alkylene).sub.m O--X--S.sub.2 O.sub.3 Y].sub.p (IV),
- YO.sub.3 S.sub.2 --X--(O-alkylene).sub.m --X--S.sub.2 O.sub.3 Y(V),
- wherein
- p=2, 3, 4, 5 or 6;
- q=0, 1, 2, 3 or 4;
- (p+q)=3, 4, 5 or 6;
- m.gtoreq.a whole number<1;
- R is a group obtained by cleavage of hydroxyl groups from an aliphatic alcohol having at least two carbon atoms;
- X is a divalent substituted or unsubstituted aliphatic group having one to 10 carbon atoms; and
- Y is a hydrogen atom, a salt-forming ion or a salt-forming group;
- (3-S-thiosulfato-2-hydroxypropyl)-N,N-dimethylamine of the formula (VI):
- (CH.sub.3).sub.2 N--CH.sub.2 --CH(OH)--CH.sub.2 --S.sub.2 O.sub.3(VI);
- keratin-Bunte salts obtained by reaction of keratin hydrolysates with sodium thiosulfate; and
- polysiloxane-Bunte-salts of the formula (VII):
- R.sup.1.sub.a --Si(R.sup.2.sub.b)--O.sub.{( 4--a--b)/2} (VII)
- wherein from 90 to 100% of the R.sup.1 groups are methyl, and from 0 to 10% of the R.sup.1 groups are phenyl; and R.sup.2 =R.sup.3 and/or R.sup.4,
- wherein
- R.sup.3 =--(C.sub.n H.sub.2n)--O--(C.sub.m H.sub.2m O).sub.p --R.sup.5 q--CH.sub.2 CH(R.sup.7)CH.sub.2 R.sup.6
- R.sub.5 =--CH(CH.sub.2 W)--CH.sub.2 O-- or --CH.sub.2 --CH(CH.sub.2 W)--O--
- wherein W=halogen,
- R.sup.6, R.sup.7 include an --OH group and a member selected from the group consisting of --S.sub.2 O.sub.3 Me wherein Me=a substituted ammonium cation or an alkali metal cation,
- n=3 to 6,
- m=2 to 3,
- p=0 to 100,
- q=0 to 5,
- and R.sup.4 =--(C.sub.x H.sub.2x)--O--(C.sub.y H.sub.2y O).sub.z R.sup.8
- wherein R.sup.8 =hydrogen, an alkyl group with one to four carbon atoms or an acetyl group,
- x=3 to 6,
- y=2 to 3,
- z=1 to 100, with the proviso that at least one R.sup.2 group is an R.sup.3 group, and, when p=0 in the R.sup.3 group, at least one
- R.sup.4 group is present, wherein a=1 to 2.33,
- b=0.02 to 1 and
- .ltoreq. (a+b).ltoreq.3.
- 2. The improvement as defined in claim 1, wherein said keratin hydrolysates are a mixture of soluble keratin proteins having an average molecular weight of about 100,000 Daltons, said soluble keratin proteins having an amino acid composition comprising 4.9% by weight isoleucine, 10.6% by weight leucine, 5.5% by weight lysine, 1.5% by weight methionine, 2.0% by weight cystsine, 3.9% by weight phenylalanine, 4.8% by weight threonine, 1.4% by weight tyrosine, 5.2% by weight valine, 7.6% by weight arginine, 3.8% by weight histidine, 4.2% by weight alanine, 9.1% by weight aspartic acid, 11.4% by weight glutamic acid, 3.3% by weight glycine, 2.4% by weight proline and 8.3% by weight sering.
- 3. The improvement as defined in claim 1, wherein the drying is performed prior to the oxidative aftertreatment with the oxidizing agent.
- 4. The improvement as defined in claim 1, wherein the sulfites are selected from the group consisting of alkali metal sulfites and ammonium sulfites and the hydrogen sulfites are selected from the group consisting of alkali metal hydrogen sulfites, ammonium hydrogen sulfites and alkanolamine salts of sulfurous acid.
- 5. The improvement as defined in claim 1, wherein the aqueous hair shaping composition is allowed to act on the hair for from 10 to 60 minutes.
- 6. The improvement as defined in claim 1, wherein in the treating of the hair with the hair shaping agent, the aqueous hair shaping composition is applied to the hair in an amount of from 80 to 120 grams.
- 7. The improvement as defined in claim 1, wherein said oxidizing agent is allowed to act on the hair during said subjecting for from 1 to 20 minutes.
Priority Claims (1)
Number |
Date |
Country |
Kind |
40 41 164.8 |
Dec 1990 |
DEX |
|
Parent Case Info
This is a continuation of application Ser. No. 806,882, filed Dec. 12, 1991, now abandoned.
US Referenced Citations (3)
Foreign Referenced Citations (2)
Number |
Date |
Country |
0346151 |
Dec 1989 |
EPX |
1423342 |
Feb 1976 |
GBX |
Continuations (1)
|
Number |
Date |
Country |
Parent |
806882 |
Dec 1991 |
|