The invention relates to a method for producing a heterogeneous, in particular multicolored, sheet-like structure, for example a decorative skin for an interior trim part of a vehicle, and to molds suitable for this purpose and to sheet-like structures produced thereby.
Patent application DE 102 11 663 A1 discloses a method for producing a heterogeneous, but one-piece, molded part, which consists in certain regions of a hard, thermoplastic material, for example polypropylene (PP) or a PP compound, and an elastically deformable material, for example an olefin-based thermoplastic elastomer. The first and second segments of the molded part are produced in separate molds and subsequently joined to form a unit by molding on a connecting segment.
This method is suitable for producing small molded parts of complex geometry and high-value appearance, but is less suitable for producing large, sheet-like structural members, in particular decorative skins for interior trim parts, on account of the awkward handling of the extended segments of the structural member.
The invention is based on the problem of providing a method for producing high-value and heterogeneous, in particular at least two-colored, sheet-like structures.
The problem is solved according to the invention in the case of this method by at least a first cavity and a second cavity of a mold being filled with at least a first and a second polymer material which are free-flowing and after removal form a one-piece sheet-like structure, a sealing element being arranged in the mold, at least during the filling of one cavity, and extends along the parting plane in relation to the neighboring cavity.
The sealing element achieves the effect of reliable segmentation of the surface of the one-piece molded skin in the case of an extended and possibly complexly shaped longitudinal extent of the parting plane. In particular in the case of multicolored sheet-like structures, a distinct separation is created between the adjacent, differently colored surface regions, so that the molded skin is suitable for use in particularly demanding application areas of automobile construction.
A suitable mold for carrying out the method has at least a first mold part and a second mold part, which can be displaced with respect to said first part, which mold parts form at least a first cavity and a neighboring second cavity, which can be filled with at least a first and a second free-flowing polymer material, after the closing of the mold. According to the invention, a sealing element is arranged along the parting plane between the first cavity and the second cavity.
The following developments of the method can be used with particular advantage when reactively curing polymer materials are used, injected into the cavities by means of an injection-molding process (Reaction Injection Molding (RIM)). These polymers have a particularly low viscosity in the free-flowing state, so that the sealing between the cavities assumes special significance.
According to a first embodiment of the method according to the invention, the sealing element is firmly connected to one mold part, in particular the upper mold, and can be pressed against another mold part, in particular the lower mold. The sealing element is preferably expandable under fluid pressure (“inflatable seal”) and can be pressed against a protruding projection of the other mold part, in particular the lower mold.
After the filling of the first cavity with the first polymer material, the sealing element can be lifted off the other mold part and the second cavity filled with the second polymer material, the first and second polymer materials bonding with each other in such a way that they fuse together but appear distinctly separate. The lifting off of the seal preferably takes place by reducing the fluid pressure inside the tube-like seal, it also being possible to set a fluid pressure that lies below the ambient pressure. This creates a lifting-off force which exceeds the elastic recovery of the sealing element.
In the case of a mold that can be used here, the sealing element is preferably firmly arranged in one mold part, in particular the upper mold, and can be pressed against the other mold part, in particular the lower mold, in an expandable manner under fluid pressure.
According to another embodiment of the invention, before the filling of the cavities, the sealing element is loosely placed into one mold part, in particular the upper mold, in the region of the parting plane, and, during the closing of the mold, is made to bear in a sealing manner against the other mold part, in particular the lower mold.
The sealing element can advantageously be pressed against a protruding projection of the other mold part, in particular the lower mold, and, during the filling of the cavities, bonds with the first polymer material on the one hand and the second polymer material on the other hand in such a way that they fuse together. The sealing element is therefore lost in the production of the molded skin and must be replaced by a new sealing element before renewed filling of the cavities.
In the case of a suitable mold, the sealing element can be loosely placed into one mold part, in particular the upper mold, and can be pressed against the other mold part, in particular the lower mold.
The figures present various embodiments of the invention schematically and by way of example.
a-e show how a first method according to the invention is carried out using a first mold suitable for this purpose,
a-e shows a mold and a method according to another development of the invention.
The mold 1 shown in
The upper mold 3 is provided along the parting plane 6 between the neighboring cavities 5, 5′ with a tubular sealing element 7, the hollow space 8 of which can be filled with a compressed gas after the closing of the mold parts 2, 2′. The sealing element 7 is firmly connected to the mold upper part 3 by means of a securing means 10, which can be fixed by screws 9. As a result of the positive pressure, the sealing element 7, the longitudinal extent of which may likewise have a complex profile, expands elastically and comes to lie in a sealing manner against a projection 11 protruding from the lower mold 4. Subsequently, as can be seen from
Subsequently, the hollow space 8 of the sealing element 7 is subjected to negative pressure, so that the sealing element 7 lifts off from the projection 11 (
The mold as shown in
After the closing of the mold 1 (
As shown in
Number | Date | Country | Kind |
---|---|---|---|
10 2004 059 066.4 | Dec 2004 | DE | national |
The present invention claims priority as a national stage application of International Patent Application Serial No. PCT/EP 05/012623 filed on Nov. 25, 2005; and German Patent Application Serial No. DE 102004059066.4 filed on Dec. 7, 2004, which are both hereby incorporated herein by reference in their entirety.
Filing Document | Filing Date | Country | Kind | 371c Date |
---|---|---|---|---|
PCT/EP05/12623 | 11/25/2005 | WO | 00 | 5/13/2009 |