The present invention relates to a method for producing an electrical storage device, and an electrical storage device.
In recent years, a lithium-ion capacitor that utilizes the electrical storage principle of a lithium-ion secondary battery and the electrical storage principle of an electrical double-layer capacitor has attracted attention as an electrical storage device that may be used for applications that require high energy density and high output characteristics. The lithium-ion capacitor is configured so that the energy density can be significantly increased by causing the negative electrode to occlude (store) and support lithium ions (hereinafter may be referred to as “doping”) using an electrochemical method or the like to lower the potential of the negative electrode.
For example, WO2010/073930 discloses a technique that forms a wound element by winding a positive electrode, a negative electrode, and a lithium ion source (wherein the positive electrode and the negative electrode are situated on either side of a separator), and dopes the negative electrode with lithium ions through electrochemical contact between the negative electrode and the lithium ion source. In WO2010/073930, the wound element is placed in a casing having a circular cross-sectional shape, and has an approximately circular cross-sectional shape.
The wound element may have a cross-sectional shape other than a circular cross-sectional shape corresponding to the shape of the casing in which the wound element is placed. In such a case, it may be difficult to uniformly dope the negative electrode with lithium ions released from the lithium ion source. For example, if the negative electrode is excessively doped with lithium ions, lithium dendrites may precipitate during repeated charge and discharge, and pass through the separator to short-circuit the positive electrode and the negative electrode. This may decrease the lifetime of the electrical storage device, and impair the reliability of the electrical storage device.
An object of several aspects of the invention is to provide a method for producing an electrical storage device that makes it possible to uniformly dope the negative electrode with lithium ions. Another object of several aspects of the invention is to provide an electrical storage device in which the negative electrode is uniformly doped with lithium ions.
The invention was conceived in order to solve the above problem.
According to one aspect of the invention, a method for producing an electrical storage device includes:
winding a positive electrode, a negative electrode, and a lithium ion source to form a wound element that has a flat part and a curved part, the lithium ion source including a plurality of parts that are arranged in a winding direction through a gap,
the wound element being formed so that the gap is situated in the curved part.
In the method for producing an electrical storage device according to Application Example 1,
at least part of the lithium ion source may be situated on the outer side of the positive electrode and the negative electrode.
In the method for producing an electrical storage device according to Application Example 1 or 2,
a length S of the gap, and a length L of a part of the lithium ion source situated in the curved part in which the gap is formed, may satisfy the relationship “3/10≦S/(S+L)≦7/10” in a state in which the wound element is extended.
According to another aspect of the invention, a method for producing an electrical storage device includes:
winding a positive electrode, a negative electrode, and a lithium ion source to form a wound element that has a flat part and a curved part, the lithium ion source including a thin part and a thick part that are arranged in a winding direction,
the wound element being formed so that the thin part is situated in the curved part.
In the method for producing an electrical storage device according to Application Example 4,
at least part of the lithium ion source may be situated on the outer side of the positive electrode and the negative electrode.
In the method for producing an electrical storage device according to Application Example 4 or 5,
a thickness T1 of the thin part and a thickness T2 of the thick part may satisfy the relationship “3/10≦T1/T2≦7/10”.
The method for producing an electrical storage device according to any one of Application Examples 1 to 6 may further include placing the wound element in a casing.
The method for producing an electrical storage device according to any one of Application Examples 1 to 7 may further include doping the negative electrode with lithium ions released from the lithium ion source.
In the method for producing an electrical storage device according to any one of Application Examples 1 to 8, a separator may be placed between the positive electrode and the negative electrode when forming the wound element.
The method for producing an electrical storage device according to any one of Application Examples 1 to 9 may produce a lithium-ion capacitor as the electrical storage device.
According to another aspect of the invention, an electrical storage device includes:
a wound element that is formed by winding a positive electrode, a negative electrode, and a metal foil, the metal foil including a plurality of parts that are arranged in a winding direction through a gap,
the wound element having a flat part and a curved part, and
the gap being situated in the curved part.
In the electrical storage device according to Application Example 11, at least part of the metal foil may be situated on the outer side of the positive electrode and the negative electrode.
The method for producing an electrical storage device according to the aspects of the invention can suppress a situation in which the part of the negative electrode situated in the curved part of the wound element is excessively doped with lithium ions, and ensures that the negative electrode is uniformly doped with lithium ions.
Exemplary embodiments of the invention are described below with reference to the drawings. Note that the invention is not limited to the following exemplary embodiments. It is intended that the invention includes various modifications that may be practiced without departing from the scope of the invention.
An electrical storage device according to a first embodiment of the invention is described below with reference to the drawings. The electrical storage device according to the first embodiment is formed by doping (pre-doping) a negative electrode 50 with lithium ions released from a lithium ion source. More specifically, the electrical storage device according to the first embodiment is formed by placing a wound element in a casing, and injecting an electrolyte solution into the casing to effect pre-doping. A state (hereinafter may be referred to as “cell”) before pre-doping is performed (i.e., before the electrolyte solution is injected) will be described first, and the electrical storage device will be described thereafter.
Note that
As illustrated in
As illustrated in
The wound element 20 is placed inside the casing 10. The wound element 20 has a shape that corresponds to the shape of the casing 10. Specifically, the wound element 20 has a flat part 22 and a curved part 24.
The flat part 22 of the wound element 20 is situated between two flat surfaces 12 of the casing 10. The flat part 22 is a part in which the surface of a lithium ion source 30 included in the wound element 20 is flat, for example. In the example illustrated in
The curved part 24 of the wound element 20 is a part in which the surface of the lithium ion source 30 included in the wound element 20 is curved (i.e., a part having a curvature), for example. The wound element 20 has two curved parts 24. In the example illustrated in
The wound element 20 is formed by winding the lithium ion source 30, a positive electrode 40, the negative electrode 50, the first separator 60, and the second separator 62. More specifically, the wound element 20 is formed by sequentially stacking the first separator 60 to which the lithium ion source 30 is compression-bonded, the positive electrode 40, the second separator 62, and the negative electrode 50 to form a laminate 21, and winding the laminate 21 from a winding start side 2 of the laminate 21 (see
The lithium ion source 30 is situated between the first separator 60 and the second separator 62. The lithium ion source 30 is compression-bonded or bonded to the first separator 60, for example. The lithium ion source 30 is situated apart from the positive electrode 40 and the negative electrode 50. The lithium ion source 30 is situated closer to a winding end side (i.e., the side in the +X-axis direction in the example illustrated in the drawings) 4 of the laminate 21 than the winding start side (i.e., the side in the −X-axis direction in the example illustrated in the drawings) 2 of the laminate 21 in a state in which the wound element 20 is extended (see
The lithium ion source 30 includes a plurality of parts that are arranged in the winding direction (i.e., a direction R illustrated in
The first part 32 and the second part 34 included in the lithium ion source 30 have a rectangular planar shape (i.e., a shape observed in the Z-axis direction in the example illustrated in the drawings) (see
In the example illustrated in
The first part 32 included in the lithium ion source 30 has a first end face 32a that is situated on the winding start side 2, and a second end face 32b that is situated on the winding end side 4. The second part 34 included in the lithium ion source 30 has a third end face 34a that is situated on the winding start side 2, and a fourth end face 34b that is situated on the winding end side 4.
In the example illustrated in
Likewise, the angle θ3 formed by an imaginary straight line Q1 that passes through the first end face 32a and a point Ob, and an imaginary straight line β that passes through the point Ob and is parallel to the X-axis, is 45°. The angle θ4 formed by an imaginary straight line Q2 that passes through the fourth end face 34b and the point Ob, and the imaginary straight line β, is 45°. Note that the point Ob is a point that is situated on a boundary line δ between the flat part 22 and the curved part 24b, and situated in the −Z-axis direction with respect to the point Oa due to the asymmetrical shape of the curved part 24b.
Note that the angles θ1 to θ4 are not limited to 45°. The angles θ1 to θ4 may be an arbitrary angle that is larger than 0° and smaller than 90°.
The gap 36 between the first part 32 and the second part 34 included in the lithium ion source 30 in the winding direction is the gap between the second end face 32b and the third end face 34a. As illustrated in
As illustrated in
The metal foil 38 included in the lithium ion source 30 has an independent part 39 to which the lithium foil 37 is not compression-bonded. As illustrated in
The lithium ion source 30 functions as a source that supplies lithium ions. Specifically, when the wound element 20 illustrated in
The size of the lithium ion source 30 (i.e., the size of the lithium foil 37) is appropriately determined taking account of the amount of lithium ions with which the negative electrode 50 is pre-doped. The thickness of the lithium foil 37 is not particularly limited. For example, the thickness of the lithium foil 37 is 50 to 300 micrometers. A porous metal foil is used as the metal foil 38. Specifically, the negative electrode 50 is doped with the lithium ions that have passed through the metal foil 38. The metal foil 38 is formed of copper or stainless steel, for example. The thickness of the metal foil 38 is not particularly limited. For example, the thickness of the metal foil 38 is 10 to 200 micrometers.
As illustrated in
The positive electrode active material layer 42 is provided on the positive electrode current collector 44. In the example illustrated in
A porous metal foil is used as the positive electrode current collector 44. Specifically, the negative electrode active material layer 52 is doped with the lithium ions that have passed through the positive electrode current collector 44 when the wound element 20 illustrated in
The positive electrode current collector 44 has the uncoated part 46 on which the positive electrode active material layer 42 is not provided. As illustrated in
As illustrated in
The negative electrode active material layer 52 is provided on the negative electrode current collector 54. In the example illustrated in
A porous metal foil is used as the negative electrode current collector 54. Specifically, the negative electrode active material layer 52 is doped with the lithium ions that have passed through the negative electrode current collector 54 when the wound element 20 illustrated in
The negative electrode current collector 54 has an uncoated part 56 on which the negative electrode active material layer 52 is not provided. As illustrated in
The first separator 60 and the second separator 62 are formed in the shape of a strip. A porous material that exhibits durability with respect to the electrolyte solution and the active material layers 42 and 52 is used as a material for forming the separators 60 and 62. More specifically, a nonwoven fabric formed of cellulose, polyethylene, polypropylene, an aramid resin, an amide-imide, polyphenylene sulfide, a polyimide, or the like, a porous film, or the like is used as the separators 60 and 62. The thickness of the separators 60 and 62 is not particularly limited. For example, the thickness of the separators 60 and 62 is 15 to 50 micrometers. The separators 60 and 62 are situated between the positive electrode 40 and the negative electrode 50, and isolate the positive electrode 40 and the negative electrode 50 when the wound element 20 illustrated in
The electrical storage device 100 is described below with reference to the drawings.
Specifically, the electrical storage device 100 is formed by immersing the wound element 20 in the electrolyte solution within the cell 101 so that the lithium foil 37 included in the lithium ion source 30 is dissolved in the electrolyte solution to produce lithium ions, with which the negative electrode 50 is pre-doped.
As illustrated in
The metal foil 38 included in the electrical storage device 100 includes a plurality of parts (first part 38a and second part 38b) that are arranged in the winding direction through a gap 136 in the same manner as the lithium ion source 30. The gap 136 is situated in the curved part 24a of the wound element 20. Specifically, an end (edge) 138 of the metal foil 38 is situated in the curved part 24a, and is not situated in the flat part 22 of the wound element 20.
The casing 10 included in the electrical storage device 100 holds the electrolyte solution (not illustrated in the drawings). A non-aqueous electrolyte solution is used as the electrolyte solution. Examples of the solvent used to prepare the electrolyte solution include ethylene carbonate, propylene carbonate, dimethyl carbonate, diethyl carbonate, γ-butyrolactone, acetonitrile, dimethoxyethane, tetrahydrofuran, dioxolane, methylene chloride, sulfolane, and the like. These solvents may be used either alone or in combination.
A lithium salt may be used as the electrolyte used to prepare the electrolyte solution. Specific examples of the electrolyte include LiClO4, LiAsF6, LiBF4, LiPF6, Li(C2F5SO2)2N, and the like. The concentration of the electrolyte in the electrolyte solution is 0.5 to 1.5 mol/L, for example.
The electrical storage device 100 has the following features, for example.
The negative electrode 50 is uniformly doped with lithium ions. The details thereof are described later.
The end (edge) 138 of the metal foil is situated in the curved part 24 of the wound element 20. Therefore, a local pressure is not applied to the wound element 20 even if pressure is applied to the electrical storage device 100 in the widthwise direction (Z-axis direction) during use. This makes occurrence of precipitation of dendrites difficult, and the lifetime of the electrical storage device 100 is increased.
For example, since the cell size of the electrical storage device 100 may change due to repeated charge and discharge, the electrical storage device 100 is normally used in a state in which pressure is applied to the electrical storage device 100 in the widthwise direction (Z-axis direction) in order to maintain the cell size. If the end (edge) of the metal foil is situated in the flat part of the wound element, a local decrease in resistance may occur at the position of the end (edge) of the metal foil. In this case, the transfer of lithium ions may locally increase at the position of the end (edge) of the metal foil, and precipitation of dendrites may easily occur.
Although an example in which the electrical storage device 100 is a lithium-ion capacitor has been described above, the electrical storage device 100 may be a lithium-ion secondary battery.
A method for producing the electrical storage device according to the first embodiment is described below with reference to the drawings.
As illustrated in
As illustrated in
More specifically, the first separator 60 to which the lithium ion source 30 is compression-bonded, the positive electrode 40, the second separator 62, and the negative electrode 50 are sequentially stacked to form the laminate 21 (see
The wound element having an approximately circular cross-sectional shape is deformed to have the flat part 22 and the curved part 24 (see
Note that the wound element 20 that has the flat part 22 and the curved part 24 may be formed by winding the laminate 21 using the core rod 70 having the desired shape (e.g., cylindrical shape having a flat part) (not illustrated in the drawings).
The wound element 20 is then placed in the casing 10 (S2). The wound element 20 is placed in the casing 10 using a known method, for example. The cell 100a is thus formed.
The negative electrode 50 is then doped with lithium ions released from the lithium ion source 30 (S3). More specifically, the electrolyte solution is injected into the casing 10 to immerse the wound element 20 in the electrolyte solution. Lithium ions are thus released from the lithium foil 37 included in the lithium ion source 30, and the negative electrode active material layer 52 is doped with the lithium ions. Note that the wound element 20 may be immersed in the electrolyte solution by placing the wound element 20 in the casing 10 that holds the electrolyte solution.
The casing 10 is then sealed.
Note that the positive electrode 40 and the negative electrode 50 are formed by providing (applying) the active material layers 42 and 52 to each side of the collectors 44 and 54, respectively. The active material layers 42 and 52 may be formed as follows. Specifically, an active material powder (e.g., activated carbon or graphite) and a binder are dispersed in an aqueous medium or an organic solvent to prepare a slurry. A conductive powder may optionally be mixed into the slurry. The slurry is applied to the surface of the collectors 44 and 54, and dried. The active material layers 42 and 52 can thus be obtained.
Examples of the binder used to prepare the slurry include a rubber binder (e.g., styrene-butadiene rubber (SBR)), a fluororesin (e.g., polytetrafluoroethylene and polyvinylidene fluoride), a thermoplastic resin (e.g., polypropylene and polyethylene), and the like. Examples of the conductive powder that may optionally be mixed into the slurry include acetylene black, graphite, a metal powder, and the like.
The electrical storage device 100 illustrated in
The method for producing the electrical storage device 100 has the following features, for example.
The method for producing the electrical storage device 100 forms the wound element 20 so that the gap 36 is situated in the curved part 24. This makes it possible to suppress a situation in which the part of the negative electrode 50 situated in the curved part 24 is excessively doped with lithium ions, and ensure that the negative electrode 50 is uniformly doped with lithium ions. Therefore, it is possible to suppress a situation in which lithium dendrites precipitate within the curved part 24 of the wound element 20, and pass through the separators 60 and 62 to short-circuit the positive electrode 40 and the negative electrode 50. This makes it possible to increase the lifetime of the electrical storage device 100, and improve the reliability of the electrical storage device 100.
As illustrated in
The part of the lithium ion source 1030 situated in the curved part 1024a produces lithium ions with which the part of the negative electrode 1050 situated in the curved part 1024a is doped. The area (i.e., the cross-sectional area illustrated in
Accordingly, the lithium ion doping amount (per unit length) of the part of the negative electrode 1050 situated in the curved part 1024a is twice the lithium ion doping amount (per unit length) of the part of the negative electrode 1050 situated in the flat part 1022. Specifically, the cell 1000a (electrical storage device 1000) has a problem in which the part of the negative electrode 1050 situated in the curved part 1024a is excessively doped with lithium ions (i.e., the negative electrode 1050 cannot be uniformly doped with lithium ions).
The method for producing the electrical storage device 100 according to the first embodiment can prevent occurrence of the problem. Specifically, the method for producing the electrical storage device 100 according to the first embodiment can suppress a situation in which the part of the negative electrode 50 situated in the curved part 24 is excessively doped with lithium ions, and ensures that the negative electrode 50 is uniformly doped with lithium ions.
According to the method for producing the electrical storage device 100, the length S of the gap 36, and the length L of the part of the lithium ion source 30 situated in the curved part 24a in which the gap 36 is formed, satisfy the relationship “3/10≦S/(S+L)≦7/10”, preferably satisfy the relationship “2/5≦S/(S+L)≦3/5”, and more preferably satisfy the relationship “S/(S+L)=1/2”, in a state in which the wound element 20 is extended. This ensures that the negative electrode 50 is more uniformly doped with lithium ions.
An electrical storage device according to a first modification of the first embodiment, and an electrical storage device according to a second modification of the first embodiment are described below with reference to the drawings. The electrical storage device according to the first modification of the first embodiment is formed in the same manner as the electrical storage device 100 by doping the negative electrode 50 with the lithium ions released from the lithium ion source 30 within a cell according to the first modification of the first embodiment. The electrical storage device according to the second modification of the first embodiment is formed in the same manner as the electrical storage device 100 by doping the negative electrode 50 with the lithium ions released from the lithium ion source 30 within a cell according to the second modification of the first embodiment.
In
The cell 100a has a structure in which the lithium ion source 30 includes the first part 32 and the second part 34 that are arranged in the winding direction through the gap 36 (see
As illustrated in
The second part 34 and the fourth part 234 included in the lithium ion source 30 are situated in the flat part 22 of the wound element 20. In the examples illustrated in
The third part 232 included in the lithium ion source 30 is situated in the curved part 24a of the wound element 20. The third part 232 has a length of πC/2 (C is the dimension of the curved part 24a in the X-axis direction) in the winding direction, for example. The third part 232 is disposed symmetrically with respect to the imaginary straight line α.
A gap 36 formed between the first part 32 and the second part 34 in the winding direction is situated in the curved part 24b. Specifically, the positive electrode 40 and the negative electrode 50 situated in the curved part 24b have an area that is not covered by the lithium ion source 30 due to the presence of the gap 36. The positive electrode 40 and the negative electrode 50 situated in the curved part 24b have an area that is not covered by the lithium ion source 30 since the first part 32 is situated apart from the fourth part 234.
A gap 236 formed between the second part 34 and the third part 232 in the winding direction is situated in the curved part 24a. A gap 237 formed between the third part 232 and the fourth part 234 in the winding direction is situated in the curved part 24a. Specifically, the positive electrode 40 and the negative electrode 50 situated in the curved part 24b have an area that is not covered by the lithium ion source 30 due to the presence of the gaps 236 and 237.
The angle θ5 formed by an imaginary straight line U1 that passes through a first end face 32a of the first part 32 on the winding start side 2 and the point Ob, and the boundary line δ, is 45°. The angle θ6 formed by an imaginary straight line U2 that passes through a second end face 32b of the first part 32 on the winding end side 4 and the point Ob, and the boundary line δ, is 45°. The angle θ7 formed by an imaginary straight line V1 that passes through a fifth end face 232a of the third part 232 on the winding start side 2 and the point Oa, and the boundary line γ, is 45°. The angle θ8 formed by an imaginary straight line V2 that passes through a sixth end face 232b of the third part 232 on the winding end side 4 and the point Oa, and the boundary line γ, is 45°.
Note that the length of the first part 32, the second part 34, the third part 232, and the fourth part 234 in the winding direction is not particularly limited as long as the first part 32, the second part 34, the third part 232, and the fourth part are situated apart from each other. The angles θ5 to θ8 are not limited to 45°. The angles θ5 to θ8 may be an arbitrary angle that is larger than 0° and smaller than 90°.
The electrical storage device 100 has a structure in which the first end face 32a of the first part 32 included in the lithium ion source 30 is situated along the imaginary straight line Q1 that forms an angle of 45° with the imaginary straight line β, and the second end face 32b of the first part 32 included in the lithium ion source 30 is situated along the imaginary straight line P1 that forms an angle of 45° with the imaginary straight line α (see
As illustrated in
The third end face 34a of the second part 34 is situated along the imaginary straight line α, and the fourth end face 34b of the second part 34 is situated along the imaginary straight line δ. The second part 34 situated in the curved part 24b has a length of πC/2 (C is the dimension of the curved part 24a in the X-axis direction) in the winding direction, for example.
The angle θ9 formed by the boundary line γ that passes through the second end face 32b of the first part 32 on the winding end side 4 and the point Oa, and the imaginary straight line α that passes through the third end face 34a of the second part 34 on the winding start side 2 and the point Oa, is 90°. The angle θ10 formed by the imaginary straight line β that passes through the first end face 32a of the first part 32 on the winding start side 2 and the point Ob, and the boundary line δ that passes through the fourth end face 34b of the second part 34 on the winding end side 4 and the point Ob, is 90°.
2.1. Electrical Storage Device
An electrical storage device according to a second embodiment of the invention is described below with reference to the drawings. The electrical storage device according to the second embodiment is formed in the same manner as the electrical storage device 100 by doping the negative electrode 50 with the lithium ions released from the lithium ion source 30 within a cell according to the second embodiment.
In
The cell 100a has a structure in which the lithium ion source 30 includes the first part 32 and the second part 34 that are arranged in the winding direction through the gap 36 (see
The thin part 432 has a thickness smaller than that of the thick part 434. The thin part 432 is situated in the curved part 24. In the example illustrated in
The thickness T1 of the thin part 432 and the thickness T2 of the thick part 434 satisfy the relationship “3/10≦T1/T2≦7/10”. The thickness T1 and the thickness T2 preferably satisfy the relationship “2/5≦T1/T2≦3/5”. The thickness T1 and the thickness T2 more preferably satisfy the relationship “T1/T2=1/2”.
A method for producing the electrical storage device according to the second embodiment is described below. The method for producing the electrical storage device 400 according to the second embodiment is basically the same as the method for producing the electrical storage device 100 according to the first embodiment, except that the positive electrode 40, the negative electrode 50, and the lithium ion source 30 that includes the thin part 432 and the thick part 434 that are arranged in the winding direction, are wound to form the wound element 20 so that the thin part 432 is situated in the curved part 24. Therefore, detailed description of thereof is omitted.
Note that the lithium ion source 30 that includes the thin part 432 and the thick part 434 may be formed by providing a lithium ion source having a given thickness, and etching the part of the lithium ion source that corresponds to the thin part, or may be formed by bonding lithium ion sources that differ in thickness.
The method for producing the electrical storage device 400 ensures that the negative electrode 50 is uniformly doped with lithium ions in the same manner as the method for producing the electrical storage device 100.
The method for producing the electrical storage device 400 ensures that the negative electrode 50 is more uniformly doped with lithium ions when the thickness T1 of the thin part 432 and the thickness T2 of the thick part 434 satisfy the above relationship.
The invention is not limited to the above embodiments, and various modifications and variations may be made of the above embodiments. The embodiments and the modifications thereof may be appropriately combined.
The invention is not limited to the above embodiments, and various modifications and variations may be made. The invention includes various other configurations substantially the same as the configurations described in connection with the above embodiments (such as a configuration having the same function, method, and results, or a configuration having the same objective and results). The invention also includes configurations in which an unsubstantial part described in connection with the above embodiments is replaced with another part. The invention also includes a configuration having the same effects as those of the configurations described in connection with the above embodiments, or a configuration capable of achieving the same objective as that of the configurations described in connection with the above embodiments. The invention further includes a configuration in which a known technique is added to the configurations described in connection with the above embodiments.
2: winding start side, 4: winding end side, 10: casing, 12: flat surface, 14: curved surface, 20: wound element, 21: laminate, 22: flat part, 24: curved part, 30: lithium ion source, 32: first part, 32a: first end face, 32b: second end face, 33: part included in curved part, 34: second part, 34a: third end face, 34b: fourth end face, 35: part included in curved part, 36: gap, 37: lithium foil, 38: metal foil, 39: independent part, 40: positive electrode, 42: positive electrode active material layer, 44: positive electrode current collector, 46: uncoated part, 50: negative electrode, 52: negative electrode active material layer, 54: negative electrode current collector, 56: uncoated part, 60: first separator, 62: second separator, 70: core rod, 100: electrical storage device, 100a: cell, 136: gap, 138: end, 200a: cell, 232: third section, 232a: fifth end face, 232b: sixth end face, 234: fourth part, 236: gap, 237: gap, 300a: cell, 400: electrical storage device, 400a: cell, 432: thin part, 434: thick part, 1000a: cell, 1010: casing, 1020: wound element, 1022: flat part, 1024: curved part, 1030: lithium ion source, 1040: positive electrode, 1050: negative electrode
Number | Date | Country | Kind |
---|---|---|---|
2012-272636 | Dec 2012 | JP | national |
Filing Document | Filing Date | Country | Kind |
---|---|---|---|
PCT/JP2013/082330 | 12/2/2013 | WO | 00 |