Claims
- 1. A method for recovering vanadium from vanadium-containing ores comprising the steps of roasting a vanadium containing ore with a sodium source to form a roasted product containing sodium vanadate; piling the roasted product to form at least one heap in a manner to provide multiple sections; passing an aqueous leaching solution successively through different sections of the at least one heap until a desired vanadium concentration in the leaching solution is obtained; and then withdrawing the leaching solution from the at least one heap.
- 2. The method as defined in claim 1 wherein concentration of vanadium in the leaching solution when it is withdrawn from the at least one heap is at a level reasonably close to the saturation level for said roasted product and below the level at which precipitation will occur.
- 3. The method as defined in claim 1 wherein the leaching solution comprises water and sodium carbonate in an amount sufficient to enhance the recovery of sodium vanadate.
- 4. A method as defined in claim 3 wherein the leaching solution consists of water and 5 to 20 grams of sodium carbonate per liter prior to being passed to the at least one heap.
- 5. The method as defined in claim 1 wherein sodium carbonate is mixed into the roasted product before it is piled into a heap.
- 6. The method of claim 1 wherein the roasted product exhibits an initial pH of between about 9.0 and 11.0.
- 7. The method of claim 6 wherein the sodium salt for the roasting comprises sodium carbonate.
- 8. The method of claim 7 wherein the pH of the leaching solution passing between sections of the at least one heap provided at 9.0 to 11.0.
- 9. The method of claim 7 wherein the leaching solution passes through a section of the heap for at least 10 hours.
- 10. The method of claim 7 wherein the concentration of the vanadium (V.sub.2 O.sub.5) in the leaching solution withdrawn from the at least one heap is at least 180 grams per liter.
- 11. The method of claim 6 wherein the sodium source for roasting comprises sodium hydroxide, sodium chloride, sodium carbonate or sodium sulfate or mixtures thereof to provide a roasted product exhibiting an initial pH of between about 9.0 and 10.2.
- 12. The method of claim 11 wherein sufficient sodium source is provided for roasting to enable recovery of at least about 75 percent of the sodium vanadate from the ore.
- 13. The method of claim 6 wherein a mixture of sodium sources are used for roasting such that the roasted product exhibits an initial pH of between about 9.0 and 10.2.
- 14. The method of claim 13 wherein sufficient sodium source is provided for roasting to enable recovery of at least about 75 percent of the contained vanadium in the ore.
Parent Case Info
This is a continuation-in-part of application Ser. No. 724,557, filed Apr. 18, 1985, herein incorporated by reference, now abandoned.
US Referenced Citations (3)
Non-Patent Literature Citations (1)