This application claims the benefit of German patent application 102018102034.1, filed on Jan. 30, 2018, which application is hereby incorporated herein by reference.
The present disclosure relates to a method for testing a multitude of sensor devices. Specifically, the present disclosure relates to a method for testing a multitude of sensor devices, wherein each sensor device comprises a sensor element configured to sense an ambient condition and a heating element to heat the sensor element. The sensor devices are each equipped with connection terminals for supply voltage and sense signal. The present disclosure also relates to a panel that can be used in the method. This disclosure also relates to a sensor component that is achieved by performing the method.
Sensor devices may include heated metal oxide layers that are designed to measure the presence or the concentration of a specific target gas. The gas performs a chemical reaction such as an oxidation on the surface of the heated metal oxide layer. The electrodes generated or required by the chemical reaction cause a change of the impedance of the metal oxide layer that can be determined and evaluated to produce an output signal that is indicative of the concentration of the target gas.
At the end of the production process of the sensor device the sensor should undergo calibration and functional test procedures to meet the expected specifications and accuracy ranges. However, the metal oxide sense elements within the sensor devices may have adsorbates on their surface or may still be covered with substances resulting from the production process. For example, the sensor elements may be covered with water molecules that are always present in ambient air and solvents that originate from the production process of the metal oxide layers or with other contaminants.
While it usually takes a short time to heat up the sensor elements, it requires a considerably longer time for the adsorbates and the solvents to evaporate from the heated sensor elements. In order to obtain a good calibration result, the sensor element should have achieved the equilibrium state at elevated temperature before the calibration procedure begins. For a typical metal oxide gas sensor, the heating time may be in the range of about 1 second (typically 20 milliseconds to 1 second), whereas the time to achieve the equilibrium may last from about 1 to 30 minutes. In a common tester that tests one sensor device after the other, it is commercially almost impossible to wait for the sensor to achieve the equilibrium state because the throughput would be drastically low and the calibration process would be rather expensive. Present sensor devices that operate with a metal oxide sensor element at elevated temperature are only purely calibrated or are even sold uncalibrated.
Embodiments provide a method for testing and calibrating sensor devices that employ the principle of heated metal oxide sensor layers that has a high throughput rate and achieves a good calibration result.
Embodiments provide a method for testing a multitude of sensor devices that has a high throughput rate and provides a good calibration result.
Embodiments provide an equipment with which a multitude of sensor devices can be tested at a high throughput rate and to ensure a good calibration result.
Embodiments provide a sensor device that is treated by the multi-testing procedure.
In an embodiment of the present disclosure, a method for testing a multitude of sensor devices comprises: providing a multitude of sensor devices, each sensor device comprising a sensor element configured to sense an ambient condition, a heating element to heat the sensor element, connection terminals for a supply voltage and at least one connection terminal for a sense signal indicative of the state of the sensor element; providing a panel, the panel comprising a multitude of groups of connection pads, the connection pads of each one of the groups configured to be connected to the connection terminals of one of the sensor devices; mounting the sensor devices to the groups of connection pads; applying a supply voltage to the sensor devices and concurrently heating the heating elements of the sensor devices to an elevated temperature; calibrating the sensor devices at least one after another.
In an embodiment the disclosed method is directed to sensor devices that have a heated sensor element, wherein the sensor element is configured to sense an ambient condition such as a concentration of a specific gas or humidity in various environments. Typical fields of application include industry, high temperature processing, automotive, air conditioning, mobile and the medical sector. The heating of the gas sensor is achieved by a resistive heating element that is biased by a heating current. For test and calibration, the multitude of sensor devices is placed on a panel that is suitably equipped with connection pads and wires so that a supply voltage can simultaneously be supplied to the multitude of sensor devices so that the devices can concurrently heat up to the elevated temperature and wait concurrently until the equilibrium state is achieved. Then, the tester can proceed and calibrate one sensor device after the other or a subgroup of sensor devices after the other. The time-consuming process of heating and achieving the equilibrium state is performed in parallel and simultaneously for the multitude of sensor devices, while the subsequent calibration process is relatively fast and can be performed individually. The throughput is increased in that the time-consuming part of the testing procedure is performed concurrently for a great number of sensor devices.
In embodiments, during the application of the supply voltage and the parallel heating of the sensor devices, a test gas atmosphere is inserted into the closed chamber of the tester. The test gas atmosphere has a well-defined concentration. The test gas atmosphere comprises that target gas for the measurement of which the sensor is dedicated.
In order to achieve the equilibrium state, the elevated temperature of the sensor element causes the contaminants to disappear such as adsorbed water vapor and/or solvents that are left over from the manufacturing process of the heating element. In the equilibrium state, the solvents disappeared and the water vapor has achieved an equilibrium of desorption and adsorption.
The testing procedure may then proceed with the calibration of the sensor devices, wherein usually one sensor device is calibrated after the other, which is acceptable because the calibration procedure is relatively fast. For calibration, the tester may receive a signal from the sensor element and compare it with a predetermined value that represents the concentration of the test gas in the test gas atmosphere. The comparison will deliver at least one correction value that is required to correct the sensing characteristic of the sensor element so that the combination of correction value and sense signal indicates the proper test gas concentration.
The correction value may be stored in an application-specific integrated circuit (ASIC) that is incorporated in the package of the sensor device. Such an ASIC may be responsible for generating the adequate heating current from the supply voltage, perform a measurement at the sensor device and perform suitable evaluations to provide an output signal that is indicative of the result of the measurement such as the concentration of the target gas in the ambient atmosphere. The measurement may be a resistance measurement detecting the change of the resistance of the metal oxide layer in response to the test gas atmosphere. Other measurements are also possible that generate an output signal in response to changes of resistance, current and/or voltage at the sensor element.
The ASIC may be configured such that it determines that a supply voltage is applied for the first time to the sensor device. This is an indicator for the fact that the test and calibration procedure starts so that the sensor device automatically goes into the heating mode and heats the heating element automatically. The first time application event may be determined by the status of the on-chip memory in that the circuit realizes that it is still empty and includes no correction value yet.
While the calibration process may be performed on panel level, the panel may be diced after finishing the calibration process to form individualized sensor components. The diced components are compositions of the sensor device attached to the diced panel piece.
A final functional test may then be performed on the separated compositions to validate the electrical and functional performance of the completed sensor components. The functional test is also performed on an individual basis of one component after the other or of a small group of components after the other. As explained above, the rather time-consuming step of heating the sensor devices and waiting to achieve the equilibrium state is, instead, parallel and simultaneous for a great number of sensor devices.
The sensor devices may be configured to sense the presence or the concentration of a specific target gas, humidity conditions or a medical gas component. Furthermore, sensors can be combinations of gas sensors with other sensors such as pressure sensors. Specifically, the sensor elements of these sensor devices are made of a metal oxide, wherein the metal oxide may be one of tin oxide, indium oxide, gallium oxide or ruthenium oxide, wherein sensor elements made of tin oxide may provide the broadest range of applications. The sensors concerned in the present disclosure may have in common that they need a relatively long time to find the equilibrium state.
The heating elements may be resistive heating wires that may be disposed beneath the sensor elements isolated from the sensor elements by an insulation layer. The heating elements may cover a reasonable area that can be achieved by a meander shape of the heating wire. Specifically, the heating element may be made of a metal from one of tungsten and platinum. The heating element being made of palladium is also possible.
Embodiments provide a panel arrangement for use in the above described method that comprises: a substrate; a multitude of groups of connection pads, the connection pads configured to be connected to corresponding connection terminals of a sensor device; a wire for a supply potential, said wire connected to a respective connection pad in each one of the groups of connection pads; another wire for a ground potential, said other wire connected to another respective connection pad in each one of the groups of connection pads.
The panel arrangement comprises a substrate on which a multitude of sensor devices can be mounted. Connection pads are provided for each of the sensor devices. The ones of the connection pads that are configured to provide the positive supply potential to the sensor devices are connected together to a first wire. The ones of the connection pads that are configured to apply the ground potential to the sensor devices are all connected to another wire. The multitude of sensor devices and the multitude of connection pads may be organized in rows so that two or more rows are disposed on the panel arrangement in parallel fashion. The wires for the supply voltage and for the ground potential may be disposed in one or more layers of the multilayer structure of the panel. The panel may be made of a ceramic material in which multiple metal layers are disposed to supply the supply and ground potentials. In general, the sensor devices that may be disposed on the panel arrangement can be organized in several rows or areas and their connection pads for the supply potential and the ground potential are connected together using the different metal layers within the ceramic substrate of the panel. In one embodiment, all the connection pads for the supply potential may be connected together by the first wire and all the connection pads for the ground potential may be connected together by the second wire so that all sensor elements disposed on the panel arrangement in a calibration process can be heated simultaneously.
After calibration, as explained above, the panel may be diced in order to individualize compositions of sensor device plus the diced panel piece. The dicing process cuts the wires for the supply potential and the ground potential and thereby generates diced sidewall portions of the panel pieces that include the cut surfaces of the wires for the supply and ground potentials. In one embodiment, the cut wires for supply and ground potentials may be included in diced sidewall portions of the panel that are located on opposite sides of the rectangular form of the diced panel piece.
It is to be understood that both the foregoing general description and the following detailed description are merely exemplary, and are intended to provide an overview or framework to understand the nature and character of the claims. The accompanying drawings are included to provide a further understanding and are incorporated in, and constitute a part of, this description. The drawings illustrate one or more embodiments, and together with the description serve to explain principles and operation of the various embodiments. The same elements in different figures of the drawings are denoted by the same reference signs.
In the drawings:
The present disclosure will now be described more fully hereinafter with the reference to the accompanying drawings showing embodiments of the disclosure. The disclosure may, however, be embodied in many different forms and should not be construed as limited to the embodiments set forth herein. Rather, these embodiments are provided so that the disclosure will fully convey the scope of the disclosure to those skilled in the art. The drawings are not necessarily drawn to scale but are configured to clearly illustrate the disclosure.
The sensing element 111 may be made of a metal oxide such as tin oxide. Other oxides are also useful such as indium oxide, gallium oxide or ruthenium oxide. The heating element 114 may be made of a metal such as tungsten. Other metals are also useful such as platinum or palladium. In operation, the reactive gas interacts with the heated surface of the metal oxide sensor element 111 and may be oxidized. The electrons used in the oxidization process cause a resistance change at terminals 112, 113. The resistance state of the sensor element 111 is evaluated in the ASIC 120 and output to terminals 123a, 123b.
At the end of the fabrication process of sensor device 100, the sensor must be calibrated to meet the expected specifications. However, the metal oxide sensor element 111 may still be contaminated with substances from the manufacturing processes such as solvents that are used to provide the metal oxide particles. Furthermore, water vapor molecules (H2O) may adhere to the sensing element 111 as water vapor is almost everywhere in the ambient gas atmosphere.
The heating up of the sensing element 111 is achieved in a rather fast way in the range of about 20 ms to about 1 s, whereas it takes much longer time to remove the residual solvents and the water steam from the sensing element 111. This process may last for several minutes, up to about 30 minutes. Calibration is only useful when the contaminants have disappeared from the sensing element 111 and the water vapor achieves an equilibrium of adsorption and resorption.
After the fabrication of a sensor device and before shipping to the customer, the sensor device should be calibrated so that the output signal VSENSE provides a proper signal that is indicative of the sensed ambient condition such as the gas concentration of a specific reactive gas. The calibration and testing process is depicted in
Each one of the sensor devices is mounted on the panel and the connection terminals of the sensor devices are matched and connected to corresponding groups of connection pads of the panel 200 (step 502).
The panel 200 equipped with the multitude of sensor devices is inserted into the tester machine. The pins for supplying positive supply potential VIN and ground potential GND are connected to the wires 221 and 222 (step 504).
The multitude of sensor devices is then provided with electrical power so that the ASIC 120 can generate the respective currents to heat the heating elements 114 of each sensor device. Heating is performed concurrently and simultaneously for all the sensor devices in parallel (step 505).
A test gas atmosphere with defined gas concentration is inserted. The test gas atmosphere comprises that gas for which the sensor is to be calibrated and for the measurement of which the sensor is dedicated and configured. The tester has a closed chamber in which the panel is positioned and in which the gas is inserted (step 506).
The process will now wait for a sufficient amount of time so that the contaminants disappear from the metal oxide sensing element 111. Contaminants may be solvents left over from the production of the sensing element 111. Furthermore, water vapor may adhere to the metal oxide sensing element 111 and it takes quite a long time so that surplus water vapor disappears and the sensing element 111 achieves an equilibrium state of adsorption and resorption (step 507). While the heating up of heating element 114 and sensing element 111 may be achieved in a rather short time of several seconds or even about 1 second, the waiting period until the equilibrium state is achieved will last considerably longer. This may require up to several minutes. In the worst case, this can last until expiry of about 30 minutes. Heating and waiting for the equilibrium state is performed in parallel for all of the sensor devices mounted on the panel substrate.
Turning now to step 508, the sensor devices are calibrated. The calibration process can be made for one sensor device after the other in that the probe needles from the tester contact the terminals of the sensor devices and perform the calibration process for that sensor device. If a tester has more probe needles and channels, more than one sensor device can be tested in parallel. Usually, the tester may have only few probe needles and channels so that only a small subset of the multitude of sensor devices on the panel or even one single sensor device can be tested at a time. During the calibration process, the tester evaluates the sense output signal VSENSE in response to the known gas concentration supplied to the chamber of the tester. A correction value is calculated so that the combination of sense value and correction value is a measure for and is indicative of the measured concentration of the test gas. The correction value is applied to the characteristics of the sensor device. The correction value is stored in the ASIC of the chip such as in one time programmable memory 124 (step 508).
After the calibration process has been completed for all of the sensor devices on the panel, the panel will be diced through dicing lines that separate the panel into a multitude of panel pieces comprising the diced portion of the panel combined with the sensor device attached thereto. The sensor component comprising a sensor device plus panel piece can be placed into a package (step 509).
The individual sensor component will then be subjected to a functional test which validates the electrical and logical function of the sensor circuit (step 510).
An advantage of the present disclosure is that the time-consuming portions of the test and calibration procedures are performed in parallel for a multitude of sensor devices so that the average time spent per device is low. On the other hand, the specific calibration and test procedures will be performed for one individual device one after the other, or at best a small group of individual devices one after the other group depending on the capabilities of the tester machine. During the initial steps, the application of supply power, the heating up of the devices, the inserting of the gas atmosphere and the waiting for the equilibrium state are performed in parallel for all devices on the panel. Depending on the field of application of the sensor, the specific test gas atmosphere and the specific temperature to which the sensing element is to be heated may vary.
In an embodiment, the ASIC 120 of the sensor device 100 may be formed such that the ASIC determines that the device is still uncalibrated, for example, in that the programmable memory 124 is empty. In that case the ASIC may go immediately into the heating mode when it realizes that the supply voltage VIN, GND is supplied.
It will be apparent to those skilled in the art that various modifications and variations can be made without departing from the spirit or scope of the disclosure as laid down in the appended claims. Since modifications, combinations, sub-combinations and variations of the disclosed embodiments incorporating the spirit and substance of the disclosure may occur to the persons skilled in the art, the disclosure should be construed to include everything within the scope of the appended claims.
Number | Date | Country | Kind |
---|---|---|---|
10 2018 102 034.1 | Jan 2018 | DE | national |
Number | Name | Date | Kind |
---|---|---|---|
9818656 | Schlarmann et al. | Nov 2017 | B1 |
20030037590 | Stark | Feb 2003 | A1 |
20130311108 | Stetter | Nov 2013 | A1 |
20180003660 | Tayebi | Jan 2018 | A1 |
20180038825 | Ratto | Feb 2018 | A1 |
20190346406 | Gerber | Nov 2019 | A1 |
20210015399 | Gouma | Jan 2021 | A1 |
Number | Date | Country |
---|---|---|
19845112 | Dec 2000 | DE |
3124962 | Feb 2017 | EP |
Entry |
---|
Ams datasheet “AS-MLV-P2 Air Quality Sensor” [v1-01] Oct. 12, 2015, 24 pages. |
Number | Date | Country | |
---|---|---|---|
20190234919 A1 | Aug 2019 | US |