Claims
- 1. A method for electroless nickel plating a relatively long body having a longitudinal axis, comprisimg the steps of:
- (a) completely immersing said long body in a bath of an electroless nickel plating solution within a deep plating tank, and positioning said long body so that the longitudinal axis of said long body is substantially vertical,
- (b) heating said electroless nickel solution to a predetermined, substantially uniform temperature,
- (c) immersing a fluid conduit having a plurality of vertically spaced sparger outlets in said bath and spaced from said long body,
- (d) directing said sparger outlets generally toward said long body,
- (e) forcing said electroless nickel solution through said fluid conduit to discharge said solution through said sparger outlets in streams flowing against said long body throughout its vertical length.
- 2. The method according to claim 1 further comprising the step of filtering said plating solution prior to the discharge of said solution through said sparger outlets.
- 3. The method according to claim 1 in which the streams of solution discharged through said sparger outlets increase in size from the top to the bottom of said bath.
- 4. The method according to claim 3 in which said sparger outlets are uniformly vertically spaced within said tank, and in which the size of said sparger outlets increases uniformly from the top to the bottom of said fluid conduit.
- 5. The method according to claim 1 further comprising the step of arranging said sparger outlets in a plurality of laterally spaced vertical rows so that said forcing step discharges substantially horizontal streams of solution from said sparger outlets, said streams from one vertical row of sparger outlets discharging in horizontal directions different from the horizontal directions of the streams discharging from the sparger outlets in any other vertical row.
- 6. The method according to claim 1 further comprising the step of maintaining the electroless nickel solution within said plating tank at a substantially uniform temperature, concentration and pH.
- 7. The method according to claim 1 in which the length of said long body immersed in said bath is at least approximately 34 feet.
- 8. The method according to claim 1 in which the length of said body immersed in said bath is long enough to extend to a depth in the bath where the fluid pressure is at least approximately one atmosphere.
CROSS REFERENCE TO RELATED APPLICATION
This is a division of application Ser. No. 919,211 filed June 26, 1978, now abandoned.
US Referenced Citations (16)
Divisions (1)
|
Number |
Date |
Country |
Parent |
919211 |
Jun 1978 |
|