Claims
- 1. A method for the biaxial molecular orientation of a plastic material having at least one layer of polyester, comprising the steps of:
- sealing together overlapping edge zones of a sheet of the plastic material to form a tube;
- continuously introducing the tube of plastic material into a first heated liquid thereby heating said tube;
- introducing a second heated liquid into the interior of said tube, the first and second liquids each having a temperature of 70.degree.-100.degree. C.;
- maintaining said first liquid at a lower pressure than said second liquid thereby controllably expanding the material by the internal pressure prevailing in said tube to orient the plastic material in a transverse direction;
- controllably stretching the expanded material longitudinally concurrently with the expansion in the transverse direction while the material is entirely within the first liquid to orient the plastic material in a longitudinal direction; and
- subsequently introducing said tube into a third liquid, said third liquid being maintained at a temperature below that of said first heated liquid for cooling said molecular oriented tube.
- 2. The method of claim 1, wherein as the tube is longitudinally stretched the tube is also flattened and compressed.
- 3. The method of claim 1, wherein the heated first liquid and the heated and pressurized second liquid are both water.
Priority Claims (1)
Number |
Date |
Country |
Kind |
1740/81 |
Mar 1981 |
CHX |
|
Parent Case Info
This application is a continuation of application Ser. No. 357,642, filed Mar. 12, 1982 abandoned.
US Referenced Citations (11)
Foreign Referenced Citations (2)
Number |
Date |
Country |
67799 |
May 1969 |
DEX |
55-100118 |
Jul 1980 |
JPX |
Continuations (1)
|
Number |
Date |
Country |
Parent |
357642 |
Mar 1982 |
|