Claims
- 1. A method for lining or relining an existing engineering structure to rehabilitate, reinforce, and protect the engineering structure, said method comprising:
- a. preparing the surface of the engineering structure to be lined or relined by cleaning the brick, tile, concrete block, concrete, mortar, or foreign material from the surface;
- b. spraying a liquid primer on the surface of the engineering structure, said primer adapted to promote adhesion of an elastomeric material to said engineering structure;
- c. applying a polyurea elastomeric material to the prepared surface of the engineering structure to be lined or relined by spraying the elastomeric material onto the prepared surface whereby a monolithic, continuous polyurea elastomeric coating is formed on the prepared surface, wherein the fast-curing polyurea elastomeric material is prepared by rapidly mixing and initiating the reaction of an isocyanate-terminated compound having reactive isocyanate groups with an amine-terminated compound having reactive amine groups immediately before spraying the elastomeric material onto the prepared surface; and
- d. allowing the fast-curing polyurea elastomeric coating to cure, whereby an elastomeric polyurea liner is formed on the prepared surface to rehabilitate, reinforce, and protect the engineering structure.
- 2. The method as defined in claim 1, wherein said method includes spraying an aqueous solution of a silane primer.
- 3. The method as defined in claim 2, wherein said method includes spraying an aqueous solution of said silane primer having at least 5% of aminoethyl aminopropyl trimethoxysilane.
- 4. A method for lining or relining the interior surface of a manhole to rehabilitate, reinforce and protect the structure of said manhole, said method comprising:
- a. preparing said interior surface of said manhole to be lined or relined by cleaning the brick, tile, concrete block, concrete, mortar, or metal forming said interior surface and removing loose particles of brick, tile, concrete block, concrete, mortar, or foreign material from said surface;
- b. spraying a liquid primer on said interior manhole surface, said primer promoting adhesion of a polyurea elastomeric material which is the reaction product of an isocyanate-terminated compound and an amine-terminated compound;
- c. applying a polyurea elastomeric material to said prepared interior manhole surface to be lined or relined by spraying a fast-curing polyurea elastomeric material onto said prepared surface, whereby a monolithic, continuous polyurea elastomeric coating is formed on said prepared surface, wherein said fast-curing polyurea elastomeric materials is prepared by rapidly mixing and initiating the reaction of an isocyanate-terminated compound and an amine-terminated compound immediately before spraying the fast-curing polyurea material onto said prepared surface; and
- d. allowing said fast-curing polyurea elastomeric coating to cure, whereby an elastomeric polyurea liner is formed on said prepared surface to rehabilitate, reinforce and protect said manhole interior surface.
- 5. The method as defined in claim 4, wherein said method includes spraying an aqueous solution of silane primer on said manhole interior surface and allowing said primer to dry before applying said polyurean elastomeric material.
- 6. The method as defined in claim 5, wherein said method includes spraying an aqueous solution of said silane primer on said manhole interior surface having at least 10% of an aminoethyl aminopropyl trimethyloxysilane.
- 7. A method as defined in claim 4, wherein said isocyanate-terminated compound is a monomeric or polymeric methylene diphenyl diisocyanate or a mixture of monomeric or polymeric methylene diphenyl diisocyanates of the general formula ##STR7## where n is an integer from 0 to about 10 and wherein said method includes rapidly mixing said isocyanate-terminated compound with amine-terminated compound, then spraying said interior surface of said manhole with said polyurea elastomeric material.
- 8. A method as defined in claim 4, wherein the isocyanate-terminated compound is a quasi-prepolymer or mixture of quasi-prepolymers of general formula ##STR8## or of general formula ##STR9## where m is equal to 2 or 3, R' is a hydrogen or an aliphatic radical, and R is an aliphatic polyether, said method including rapidly mixing said isocyanate-terminated compound with said amine-terminated compound, then immediately spraying said manhole interior surface with said polyurea elastomeric material.
- 9. The method as defined in claim 4, wherein the method includes spraying a primer on said repaired manhole interior surface containing 10% to 30% silane.
RELATED APPLICATION
This application is a continuation-in-part application of U.S. patent application, Ser. No. 07/878,943, filed May 5, 1992, now U.S. Pat. No. 5,405,218.
US Referenced Citations (7)
Continuation in Parts (1)
|
Number |
Date |
Country |
Parent |
878943 |
May 1992 |
|