Claims
- 1. A method of welding mitered surfaces of frame sections made of plastic material and having incorporated therein a seal of weldable material extending along the frame sections and including an attachment foot and at least a sealing lip, for use in windows or doors; comprising the steps of:
- heating mitered surfaces of adjoining frame section zones by means of a heated mirror to a welding temperature;
- removing the heated mirror from the area of the mitered surfaces;
- moving at least one form-part that is positioned in and neighboring the miter plane and has a contour which substantially complements the inner contour of the seal formed by the sealing lip and the attachment foot adjacent to the seal so that the contour of the form part bears against the inner contour of the seal which is substantially covered thereby;
- pressing the mitered surfaces together; and
- retracting the form-part from the inner seal after welding.
- 2. The method of claim 1, and further comprising the step of so covering during the heating step an outer contour of the seal adjacent the miter plane by form-parts as to leave in the miter plane a gap for escape of a welding bead, and removing the form-parts and the welding bead formed externally on the seal after welding of the frame sections and seals.
- 3. The method of claim 1 wherein the seal is made of thermoplastic material.
Priority Claims (1)
Number |
Date |
Country |
Kind |
196 44 183 |
Oct 1996 |
DEX |
|
Parent Case Info
This is a continuation of patent application Ser. No. 08/955,212, filed Oct. 21, 1997 now U.S. Pat. No. 5,938,888.
US Referenced Citations (6)
Foreign Referenced Citations (1)
Number |
Date |
Country |
6-015746 |
Jan 1994 |
JPX |
Continuations (1)
|
Number |
Date |
Country |
Parent |
955212 |
Oct 1997 |
|