Claims
- 1. A method of beneficiating a phosphate ore comprising apatite and including dolomite impurities, said method consisting essentially of the steps of:
- (a) reagentizing a sample of said ore having a particle size in the range of from about 75 microns to 420 microns, with an aqueous solution having a pH of from about 4.0 to about 7.0 and containing from about 0.05% to about 0.2%, by weight of the ore, of cationic collector and from about 0.04% to about 0.12%, by weight of the aqueous solution, of sodium chloride,
- (b) subjecting said reagentized ore sample to flotation to float said apatite fraction, and
- (c) recovering, as the float fraction, an apatite concentrate.
- 2. The method of claim 1 including the step of washing and sizing said phosphate ore to said particle size prior to said reagentizing step.
- 3. The method of claim 1 including the step of recovering, as the sink fraction, said dolomite impurities.
- 4. The method of claim 1 wherein said cationic collector is an amine collector.
Parent Case Info
This is a divisional of application Ser. No. 147,307, filed Jan. 22, 1988--which was a continuation of No. 147,307, filed Jan. 22, 1988--which was a continuation of Ser. No. 833,070, filed Feb. 26, 1986, now abandoned.
US Referenced Citations (6)
Divisions (1)
|
Number |
Date |
Country |
Parent |
147307 |
Jan 1988 |
|
Continuation in Parts (1)
|
Number |
Date |
Country |
Parent |
833070 |
Feb 1986 |
|