Method of fabrication of a container for bulk material

Information

  • Patent Grant
  • 5186775
  • Patent Number
    5,186,775
  • Date Filed
    Monday, February 4, 1991
    33 years ago
  • Date Issued
    Tuesday, February 16, 1993
    31 years ago
Abstract
A method of attaching a membrane across an opening of an annular deformable wall including the steps of placing a disc across the opening with the disc extending outwardly beyond the wall, and deforming the outer edge of the disc and the wall simultaneously by applying heat and pressure thereto to fuse the outer edge of the disc onto the wall.
Description

BACKGROUND OF THE INVENTION
The present invention relates to an improved container for bulk material such as a desiccant, adsorbent or absorbent or the like and to a method of fabrication thereof.
By way of background, various types of containers for desiccants, adsorbents and absorbents are known. Such containers are placed within a closed environment, such as a pill bottle, for removing moisture or gases therefrom, and certain types of such containers are affixed to a screw cap of the bottle.
SUMMARY OF THE INVENTION
It is one object of the present invention to provide an improved container for desiccants, adsorbents or absorbents or the like which has an unique construction and which is fabricated in an unique manner. Other objects and attendant advantages of the present invention will readily be perceived hereafter.
The present invention relates to a container for material such as a desiccant, adsorbent, absorbent, or the like, comprising a plastic shell having a wall with an inner surface and an outer surface, an opening extending transversely to said wall, an end portion on said wall proximate said opening, a first edge portion on said outer surface of said wall proximate said end portion, a permeable membrane extending transversely to said wall, a second edge portion on said permeable membrane extending onto said first edge portion and sealed thereto, and material within said inner surface of said shell on one side of said membrane for treating the environment on the other side of said membrane.
The present invention also relates to a method of attaching a membrane across an opening comprising the steps of providing a deformable wall having an outer surface and an end and a first edge portion on said outer surface proximate said end and extending transversely thereto, an opening within said end, providing a membrane of larger size than said opening, a second edge portion on said membrane, placing said membrane across said end with said second edge portion lying outwardly beyond said end, and applying a sealing die with a tapered opening to said first and second edge portions to simultaneously deform and seal together said first and second edge portions into a shape which is complementary to said tapered opening of said die.
The various aspects of the present invention will be more fully understood when the following portions of the specification are read in conjunction with the accompanying drawings wherein:





BRIEF DESCRIPTION OF THE DRAWINGS
FIG. 1 is a side elevational view, partially broken away, of the improved container of the present invention;
FIG. 2 is a bottom plan view taken substantially in the direction of arrows 2--2 of FIG. 1;
FIG. 3 is a cross sectional view taken substantially along line 3--3 of FIG. 1;
FIG. 4 is a cross sectional view similar to FIG. 3 but showing only the plastic shell before it is filled with bulk material and before it has the permeable membrane secured thereto;
FIG. 5 is an enlarged fragmentary cross sectional view of the portion of FIG. 4 which is designated by the rectangular area which is designated FIG. 5;
FIG. 6 is a plan view of the permeable membrane which is secured to the shell of FIG. 4;
FIG. 7 is a view of the permeable membrane taken substantially in the direction of arrows 7--7 of FIG. 6;
FIG. 8 is an exploded cross sectional view of one of the early steps of the method of assembly showing the shell mounted in a die base with the permeable membrane located above it and the sealing die in position to effect a sealing operation;
FIG. 9 is a view of a subsequent step in the process showing the permeable membrane sealed to the shell after the action of the die of FIG. 8 and showing a trimming die in position to trim the membrane flash off of the shell;
FIG. 10 is a view showing the die of FIG. 9 trimming the flash;
FIG. 11 is an exploded fragmentary view, partially in cross section, showing the container of FIG. 1 mounted in the cap of a bottle;
FIG. 12 is a view similar to FIG. 11 but showing the cap of FIG. 11 with the container mounted therein screwed onto the neck of the bottle;
FIG. 13 is an exploded fragmentary cross sectional view of one of the early steps in a method of assembly of a modified embodiment of the present invention;
FIG. 14 is a fragmentary enlarged cross sectional view of the outer end of the shell;
FIG. 15 is a fragmentary exploded cross sectional view of the permeable membrane secured to the outer end of the shell by the equipment of FIG. 13 and also showing the configuration of the trimming die;
FIG. 16 is a fragmentary enlarged cross sectional view of the portion of FIG. 15;
FIG. 17 is a fragmentary cross sectional view showing the blending die in position for sealing the overhanging portions of the permeable membrane to the outer edge portions of the shell; and
FIG. 18 is a fragmentary enlarged cross sectional view of the sealed portion of the membrane on the outer edge portion of the shell.





DESCRIPTION OF THE PREFERRED EMBODIMENTS
The improved container 10 comprises a one-piece molded high density polyethylene shell 11 (FIG. 4) having an end wall 12 with a cylindrical side wall 13 formed integrally therewith. An annular rim 14 is essentially a continuation of end wall 12 and extends outwardly beyond cylindrical side wall 13. A thickened annular portion 15 is located at the junction of side wall 13 and end wall 12. The end 17 of wall 13 (FIG. 5) has a narrowed annular portion 19 formed thereon which terminates at a relatively narrow annular end 20.
Container 11 has bulk material 21 therein which may be a suitable desiccant adsorbent or absorbent, and without limitation, may comprise silica gel, metal alumino silicate, alumina, calcium sulfate, activated charcoal, molecular sieve, or any other compound in bead, pellet or grannular form.
Shell 11 is impermeable and a permeable membrane 22 extends across end 17 and is affixed to the outer edge 26 at end portion 23 of wall 13. As can be seen from a comparison of FIGS. 3 and 4, the end portion 23 proximate shell opening 24 is deformed from the condition of FIG. 4 to the condition of FIG. 3 during the application of the permeable membrane 22 thereto, as will be described hereafter. However, since the polyethylene material of wall 13 has a memory, the end portion 23 will have a tendency to expand outwardly from the position of FIG. 3 to the position of FIG. 4 to thus tension permeable membrane 22. This produces extreme tightness of membrane 22 to cause it to lie flat. In addition, the tension provides hoop strength to end portion 23. The annular outer edge portion 25 of permeable disc 22 is sealed to outer edge portion 26 in any suitable manner, as will be described hereafter, which may include ultrasonic welding or impulse welding or it may be effected by any other process which will provide good sealing therebetween.
The method of fabricating container 10 is depicted in FIGS. 8-10. More specifically, shell 11, which is preferably a high density polyethylene, but which may be of any other suitable plastic, is placed in die base 27, as shown, and bulk material 21 is placed therein. A circular permeable disc 22 which is preferably a spun-bonded polyolefin known under the trademark TYVEK is placed on the upper rim of shell 11 resting on reduced annular end 20. The plastic shell 11 and disc 22 have melting temperatures which are sufficiently close to each other so that when they are subjected to heat, their contacting portions will fuse. A sealing die or horn 29 includes an internal frustoconical surface 30 which is brought down onto disc 22. Since the outer annular portion 25 of disc 22 is lying on narrow end portion 20, the ultrasonic or impulse energy will be concentrated at this narrow area of contact to provide a good seal therewith on end 17. In addition, as the die 29 is moved downwardly, the annular end 23 will be deformed from the condition of FIG. 8 to the condition of FIG. 9, as will the outer annular edge 25 of disc 22. Furthermore, the application of pressure and generation of heat will cause a fusion between the contacting portions 26 and 25. Additionally, since the polyethylene shell 11 has a memory, annular end 23 will tend to somewhat return to its original condition of FIG. 4, and thus will tension disc 22 which in turn provides hoop strength to end portion 23. The heat and pressure experienced during the sealing operation will also cause the outer edge 25 of disc 22 to lie smoothly on shell edge 26.
After the foregoing attachment has taken place, a trimming die 31 is moved from the position of FIG. 9 to the position of FIG. 10. Its frustoconical inner surface 32 is of a steeper slope than frustoconical surface 30 and it will trim the flash 33 from the extreme outer portions of outer edge 25 so that there will be a neat junction 34 (FIG. 3) between the extreme outer edge 35 of disc 22 and the adjacent outer surface 26 of wall 13. More specifically, frustoconical surface 30 may be at about a 60.degree. angle, and frustoconical surface 32 may be at about a 26.degree. angle. The exact angularity would depend on a number of factors and must be calculated so that trimming horn 31 merely trims the flash 33. By way of example and not limitation, the disc 22 may be fabricated of a material known under the trademark TYVEK 107B and its melting temperature may be approximately 275.degree. F. The melting temperature of the high density polyethylene shell is approximately 275.degree. F. The thickness of wall 13 is approximately 0.060 inches before it has been deformed.
In use, the container 10 is intended to be held within a cap 37 having an internal screw thread 39 which threads onto external thread 40 on neck 41 of bottle 42 which may contain material such as pills, capsules or any other item which has to be in an atmosphere within the container from which moisture or other gases are removed. The outer flange 14 of container 10 is trapped behind ledge 43 within cap 37 and is thus retained therein. The flange or annular rim 14 can be placed in the position of FIGS. 11 and 12 because rim 14 is flexible and thus can be pushed into this position.
If desired, narrowed annular portion 19 may be eliminated, in which event end 17 would extend straight across to outer edge 26.
In FIGS. 13-18 a modified method and container 50 are shown. In this method, after shell 53 has been filled with the material 21 of the type described above, the permeable circular membrane 51 is first sealed to the extreme outer annular end portion 52 of shell 53 before the overhanging annular portion 54 is sealed to the outer annular edge portion 55. In this respect, the shell 53, which may be identical to shell 11 described above or which has an annular triangular ridge 56 for concentrating heat and pressure during sealing, is placed into a die base 57. A sealing die 59 is provided on which membrane 51 is held by applying suction to conduit 60 which is in communication with bore 61. Membrane 51 is substantially identical to membrane or disc 22 described above. After die 59 has pressed and sealed the outer edge portion 62 to end surface 52 by heat and pressure (FIG. 16), die 59 is withdrawn. There will be an annular overhang 54 which extends outwardly beyond the outer surface of wall 53. Thereafter, a blending horn 63, which has a frustoconical internal surface 64 is brought downwardly as shown in FIG. 17 to seal the overhang 54 by heat and pressure about edge portion 55 which is also slightly deformed to the frustoconical condition shown at 65 in FIG. 18. The outer annular portion 54 of membrane 51 is not trimmed; it is merely blended into the outer annular portion 55 of shell 53 which is deformed to the condition shown in FIG. 18. Thus, the central portion 67 of membrane 51 is not tensioned, as in FIGS. 1-12, but there is a double seal at two positions, namely, at 62 and at surface 65. Furthermore, there is a substantially flush edge at 69.
It can thus be seen that the improved container and method are manifestly capable of achieving the objects of the present invention, and while preferred embodiments have been disclosed, it will be appreciated that the present invention is not limited thereto but may be otherwise embodied within the scope of the following claims.
Claims
  • 1. A method of attaching a membrane across an opening comprising the steps of providing a member with an annular deformable wall having an outer surface and an end surface and a first edge portion on said outer surface proximate said end surface and extending transversely thereto, an opening within said end surface, providing a membrane of larger size than said opening and said end surface, a second edge portion on said membrane, placing said membrane across said end surface with an outer portion of said second edge portion lying outwardly beyond said end surface, applying a sealing die with a tapered opening to said first edge portion and said outer portion of said second edge portion to simultaneously deform and seal together said first edge portion and said outer portion of said second edge portion into a shape which is complementary to said tapered opening of said die, and applying a second die with a tapered opening of lesser slope to said outer portion of said second edge portion to trim off any flash existing on said second edge portion after the application of said sealing die.
  • 2. A method as set forth in claim 1 wherein said first edge portion has a memory, and wherein said memory places said membrane in tension after said sealing die is removed.
  • 3. A method as set forth in claim 2 wherein said first and second edge portions are fabricated of plastic which have melting temperatures which permit them to fuse on the application of heat and pressure, and wherein said sealing die applies sufficient heat and pressure to said first and second edge portions to effect said sealing thereof.
  • 4. A method as set forth in claim 1 wherein said wall is part of a container, and wherein said container is filled with material before said membrane is sealed across said opening.
  • 5. A method as set forth in claim 1 wherein said membrane is permeable.
  • 6. A method as set forth in claim 4 wherein said membrane is permeable.
  • 7. A method as set forth in claim 2 wherein said membrane is permeable.
  • 8. A method as set forth in claim 3 wherein said membrane is permeable.
  • 9. A method of attaching a membrane across an opening comprising the steps of providing a member with an annular deformable wall having an outer surface and an end surface and a first edge portion on said outer surface proximate said end surface and extending transversely thereto, an opening within said end surface, providing a membrane of larger size than said opening and said end surface, said membrane having a second edge portion, placing said membrane across said end surface with an outer portion of said second edge portion lying outwardly beyond said end surface, applying a first sealing die to said second edge portion to seal said second edge portion to said end surface while permitting said outer portion of said second edge portion to extend outwardly beyond said end surface, and applying a second die to said outer portion to seal said outer portion to said first edge portion which lies transversely to said end surface.
  • 10. A method as set forth in claim 9 wherein said second die includes a tapered opening to deform said first edge portion to a shape complementary therewith.
  • 11. A method as set forth in claim 10 wherein said first and second edge portions are fabricated of plastic which have melting temperatures which permit them to fuse on the application of heat and pressure, and wherein said first and second dies apply sufficient heat and pressure to said first and second edge portions to effect said sealing thereof.
  • 12. A method as set forth in claim 10 including the step of dimensioning said outer portion of said membrane so that the extreme outer portion of said second edge portion blends into said first edge portion.
CROSS REFERENCE TO RELATED APPLICATION

This is a division of application Ser. No. 366,128, filed Jun. 14, 1989, now U.S. Pat. No. 5,005,763, which is a continuation-in-part of application Ser. No. 253,553, filed Oct. 5, 1988, now abandoned.

US Referenced Citations (17)
Number Name Date Kind
2105551 Purdy Jan 1938
3356552 Pearl Dec 1967
3558055 Storchheim Jan 1971
3808074 Smith et al. Apr 1974
3849972 Pepmeier et al. Nov 1974
4157787 Schwartz Jun 1979
4161283 Hyman Jul 1979
4171236 Winchell et al. Oct 1979
4184310 Shelby Jan 1980
4282699 Embro, Jr. Aug 1981
4625498 Parsons Dec 1986
4640777 Lemonnier Feb 1987
4663206 Bouyoucos et al. May 1987
4769095 Sager Sep 1988
4809912 Santini Mar 1989
4913307 Takata et al. Apr 1990
4992219 Meunier Feb 1991
Foreign Referenced Citations (1)
Number Date Country
47-46197 Dec 1967 JPX
Divisions (1)
Number Date Country
Parent 366128 Jun 1989
Continuation in Parts (1)
Number Date Country
Parent 253553 Oct 1988