Claims
- 1. A method of field welding head-hardened rails, comprising the steps of:
- a. clamping and pressing together in abutting relation two rails to be welded together, with a portable welder device;
- b. gas heating the two rails with the portable welder device where the two rails abut while pressed together by the portable welder device, so as to pressure weld the rails together to form a pressure welded portion of the two rails where the two rails abut;
- c. punching excess metal formed on the pressure welded portion with the portable welder device so as to remove the excess metal on the pressure welded portion, immediately following said step of gas heating;
- d. positioning a pair of metal jigs, having respective fitting portions each defined by a respective top contact portion and side contact portions, over the respective ones the two rails on opposite sides of the welded portion with the top contact portions in contact with the top surface of the respective rails and the side contact portions in contact with the respective side surfaces of the rail;
- e. straddling the rails after said punching step with a truck of a heater device on a foot of the two rails;
- f. after said straddling step and said positioning step, reciprocating a gas heater over the welded portion with a reciprocator attached to frames on the truck so as to heat treat the portion of the two rails, including the welded portion, between the pair of metal jigs; and
- g. immediately after said reciprocating step, cooling the welded portion with an air blowing type cooler by disposing the cooler over the welded portion so as to have an injection portion of the cooler over the top surface of the welded portion and air jetting portions opposing the sides of the welded portion, blowing cooling air onto the top surface through the injection portion and jetting the air through the jetting portions.
- 2. A method as in claim 1, wherein said step of punching comprises the step of shearing the excess metal from the welded portion with punching blades of the portable welder device.
- 3. A method as in claim 1, wherein said step of gas heating is performed at a maximum heating temperature in the range from about 1200.degree. C. to about 1300.degree. C., and said step of reciprocating a gas heater is initiated when the temperature of the welded portion is in a range of from 600.degree. C. to 650.degree. C. and continued until the temperature of the welded portion has a temperature value in the range 1000.degree. C. to 1050.degree. C., said step of punching being performed while the welded portion is red hot.
- 4. A method as in claim 3, wherein said step of punching comprises the step of shearing the excess metal from the welded portion with punching blades of the portable welder device.
- 5. A method as in claim 1, further comprising the step of unclamping the portable welding device from the two rails after said step of punching.
- 6. A method as in claim 1, wherein said step of positioning is performed after said step of punching.
Priority Claims (1)
Number |
Date |
Country |
Kind |
57-214418 |
Dec 1982 |
JPX |
|
Parent Case Info
This application is a division of now abandoned application Ser. No. 511,291 filed July 6, 1983.
US Referenced Citations (6)
Divisions (1)
|
Number |
Date |
Country |
Parent |
511291 |
Jul 1983 |
|