Claims
- 1. A method of making a foamed polymer comprising the steps of:
- a. immersing a solid polymer in an immersant solution consisting essentially of (1) a compatible (with said polymer) carrier solvent, and (2) an infusant solution of an anti-emulsion agent and an incompatible (with said polymer) liquid blowing agent, chosen from the group consisting of isopropyl alcohol and water, in said compatible carrier solvent; for a time sufficient for said immersant solution to infuse into said polymer;
- b. selectively extracting said carrier solvent from said polymer so as to leave behind said infusant solution with said blowing agent entrapped in said polymer; and
- c. subsequently heating said polymer to a temperature sufficiently high to volatilize said blowing agent entrapped in said polymeric material and thereby expand said polymer into a foamed state.
- 2. The method defined in claim 1 wherein said carrier solvent is selectively extracted from said polymer by gradually diluting said immersant solution with said infusant solution.
- 3. The method defined in claim 1 wherein said polymer is an acrylic polymer, said carrier solvent is acetone, and said infusant solution consists essentially of water.
- 4. The method defined in claim 3 wherein said infusant solution consists essentially of a solution of water and polyethylene glycol having a molecular weight of approximately 4,000.
- 5. The method defined in claim 3 wherein said infusant solution consists essentially of a solution of water and hydroxypropylcellulose.
- 6. The method defined in claim 1 wherein said polymer is unmodified polystyrene, said carrier solvent consists essentially of methylene chloride, and said infusant solution comprises isopropyl alcohol.
- 7. The method defined in claim 6 wherein said infusant solution consists essentially of a solution of isopropyl alcohol and propylene glycol.
- 8. The method defined in claim 6 wherein said infusant solution consists essentially of a solution of isopropyl alcohol and polypropylene glycol having an approximate molecular weight of 1,200.
- 9. The method defined in claim 6 wherein said infusant solution consists essentially of a solution of isopropyl alcohol and polyvinyl pyrrolidone having a molecular weight of approximately 10,000.
BACKGROUND OF INVENTION
The invention disclosed herein is generally related to foamed polymeric materials and methods of making such materials. This invention is the result of a contract with the Department of Energy (Contract No. W-7405-ENG-36).
US Referenced Citations (5)