1. Field of the Invention
The present invention relates generally to methods and apparatuses for imparting fiber twist, and more particularly, to methods and apparatuses for imparting mechanical twist in optical fiber to reduce polarization mode dispersion (PMD) and to ensure optical fiber quality.
2. Technical Background
Light traveling in an optical fiber has two polarization modes. For optical fibers that are perfectly circularly symmetric in both geometry and internal and applied stress, operation at a wavelength or in a wavelength range which is regarded as “single-moded” actually supports two orthogonal polarization modes, wherein the two polarization modes are degenerate, propagate with the same group velocity and have no time delay after traveling the same distance in the fiber. However, in practice, optical fibers are not perfectly circularly symmetric. For example, imperfections such as geometric and form deformation and stress asymmetry break the degeneracy of the two modes. As a result, the two polarization modes propagate with different propagation constants. The difference between the propagation constants is called birefringence. Polarization mode dispersion (PMD) occurs in an optical fiber as a result of small birefringence induced by deviations of the fiber's core from a perfectly cylindrical shape, asymmetric stresses or strains, and random external forces acting upon the fiber. PMD is well known to severely impair transmission of optical signals at relatively high bit rates.
Various attempts to reduce PMD have been made and involve imparting a spin rotation into the fiber during manufacturing. One prior art method of reducing PMD involves spinning the preform during the fiber drawing process. Another method of combating PMD is to deliberately spin the fiber as it is drawn from the preform, so that a mechanical spin becomes “frozen” into the fiber as it cools. The resulting rotation of the birefringence axis in the fiber produces continual mode-coupling between the orthogonal polarization modes of a carried signal, thereby inhibiting the accumulation of a significant phase lag between the two modes, and consequently causing a significant reduction in the fiber's PMD.
A method as specified in the opening paragraph is known from United States Patent U.S. Pat. No. 6,324,872, wherein the drawn fiber is caused to pass over a roller whose rotational axis can be canted, so that the pulley can be caused to rock back and forth about an axis perpendicular to its rotational axis. The rocking motion of the roller produces a spin in the fiber along a substantial portion of its length. In particular, portions of warm fiber which are spun in this manner will become endowed with a permanent spin as their constituent material subsequently cools. This “spin” travels up the fiber to where the fiber is essentially in a malleable state, thereby solidifying the spin in the fiber as the fiber cools.
In addition to “spin”, another metric regarding optical fibers that is measured during the manufacture is “twist”. The spin and twist metrics are related, and some may use such terms interchangeably. However, as used herein, spin refers to the rotation introduced into the molten optical fiber, whereas twist refers to the rotational twist which is imparted to the cooled optical fiber. As discussed above, spin imparted into the molten fiber is permanently fixed when the fiber is cooled. Twist refers to the mechanical rotational force imposed on the optical fiber after it has cooled. Twist introduces torsional stresses on the fiber, and extreme amounts can cause microscopic cracks, and ultimately physical destruction of the fiber. Twist can be removed from the fiber by untwisting the fiber or allowing the fiber to relax, e.g. by hanging a very long length of fiber and allowing the fiber twist to “untwist” itself.
The present invention relates to methods for producing low PMD fiber via imparting a twist to the optical fiber. In one aspect of the present invention, a glass fiber is pulled or drawn from an optical fiber preform, for example by a tractor device which pulls the optical fiber from the preform. At some point after the tractor has pulled the optical fiber from the preform, and the fiber has cooled to the point where it is essentially non-malleable, the optical fiber is twisted about its axis to increase the magnitude of twist which is imparted to the fiber. Thereafter, the fiber is wound onto an optical fiber storage spool such that at least a portion of the twist which was imparted to the optical fiber is retained while said fiber is wound on the spool. Preferably, the optical fiber is coated prior to contact with the tractor wheel.
The twisting of the optical fiber may be performed prior to the fiber being cut from the continuous length of optical fiber which is being pulled from the optical fiber perform. In other words, such twist can be imparted to the fiber during the optical fiber draw process, before the optical fiber is stored onto a storage spool. Alternatively, the twisting step can occur offline. For example, the optical fiber may be drawn and stored on a fiber optical fiber storage spool and then taken offline and the twist imparted to the optical fiber prior to being stored on a second storage spool, where the twist is maintained on the second storage spool.
In one embodiment for applying mechanical twist to an optical fiber offline (i.e. not in the course of the fiber draw process) a fiber is stored on a central section of a first fiber storage spool having at least one flange end. The fiber is pulled from the first spool, and a torque is applied to the fiber via contact with a torque increasing device, said torque causing the fiber to undergo rotation around the longitudinal axis of the fiber such that the twist is impressed on the fiber. Thereafter the fiber is stored on a second fiber storage spool such that at least a portion of the twist imparted to said optical fiber is retained while said fiber is wound and stored on the second spool. Preferably, the torque is alternately applied in a clockwise and counterclockwise direction, such that the twist impressed on the fiber is alternately clockwise and counterclockwise.
The preferred torque increasing device for this embodiment includes at least one roller. Preferably, the fiber is engaged with a first roller disposed on a first side of the fiber at a first location along the length of the fiber, the first roller having a first roller axis transverse to the length of the fiber. The fiber is also engaged with at least one second roller disposed on a second (preferably opposite that of the first roller) side of the fiber at locations upstream and/or downstream from said first location so that the first roller is longitudinally aligned with a gap between the second roller(s), the second roller(s) having second roller axes transverse to the longitudinal direction. The fiber is maintained under tension so that the fiber bears on the first and second rollers. The rollers rotate about said roller axes; and the first roller rocks relative to said frame of reference about a rocking axis transverse to the length of the fiber and transverse to the first roller axis so that the first roller axis tilts from perpendicular to the longitudinal direction, whereby said rotation of the rollers will twist the fiber. In other words, the first roller axis is tilted alternately in opposite directions from perpendicular to the longitudinal direction.
Preferably, during the twist imparting process, the fiber is removed without having to remove the fiber from the first storage spool by pulling the fiber over the flange of the spool. In other words, preferably the twist is imparted to said fiber while pulling the fiber between the two flange ends of the first spool, such that in order to remove fiber from the first fiber spool, the first fiber spool has to rotate and the fiber is pulled therefrom.
In any of the methods disclosed herein, the twist may be unidirectional or bidirectional. Preferably the twist is bidirectional, and more preferably, the twist profile is sinusoidal. Preferably the twist magnitude applied to the fiber via any of the methods disclosed herein is at least one turn per meter, more preferably at least 2 turns/meter and most preferably at least 3 turns/meter, and the twist period or twist repeat distance is at least 10 meters, more preferably at least 20 meters, and most preferably at least 50 meters. The twist magnitude is also preferably less than 10 turns/m, more preferably less than 6 turns/m.
Applying twist to the optical fiber in this manner has the effect of reducing the measured PMD in the fiber. Any of the methods for applying twist to the fiber as disclosed herein can be used to reduce the PMD in either spun (i.e., a fiber to which has been spun in a manner in which the spin imparted into the molten fiber is permanently fixed when the fiber is cooled) or unspun fiber. In one preferred embodiment, the twist is applied to unspun fiber. In another embodiment, the twist is imparted to a fiber which has already received a spinning treatment to reduce PMD (and therefore has been spun in a manner in which the spin imparted into the molten fiber is permanently fixed when the fiber is cooled).
Additional features and advantages of the invention will be set forth in the detailed description which follows, and in part will be readily apparent to those skilled in the art from that description or recognized by practicing the invention as described herein, including the detailed description which follows, the claims, as well as the appended drawings.
It is to be understood that both the foregoing general description and the following detailed description present embodiments of the invention, and are intended to provide an overview or framework for understanding the nature and character of the invention as it is claimed. The accompanying drawings are included to provide a further understanding of the invention, and are incorporated into and constitute a part of this specification. The drawings illustrate various embodiments of the invention, and together with the description serve to explain the principles and operations of the invention.
Whenever possible, the same reference numerals will be used throughout the drawings to refer to the same or like parts. One exemplary apparatus for carrying out the methods of the present invention is illustrated in
In a melt zone adjacent the upstream end of the fiber path, i.e., at the point where the fiber is being drawn from the perform 12, the fiber is substantially molten. However, as the fiber moves downstream, it is cooled and solidified so that when the fiber reaches a point considerably downstream from draw furnace, the fiber has cooled to a substantially solid state. Cooling devices may be provided between the melt zone and the coaters to facilitate cooling of the fiber to a solid state. Desirably, the cooling device provides non-contact cooling of the fiber, such that no solid object touches the surface of the fiber while it cools.
The coating device 14 is typically adapted to apply a polymeric coating on the outside of the fiber. Preferably, the coating device is also a non-contact device. That is, the fiber passes through coater 14 without contacting or engaging any other solid object. Suitable non-contact coaters are disclosed, for example, in U.S. Pat. No. 4,792,347. The apparatus may further include additional guide rollers (not shown), for diverting the fiber and hence the fiber path from a straight line or for further constraining the fiber in the path. Other conventional elements such as quality testing equipment and the like may also be included.
Any apparatus which is capable of imparting a twist to the fiber may be used to carry out the methods of the present invention.
Twist assembly 42 further includes a cylindrical first roller 60 mounted to yoke 50 for rotation about a first element axis 62. Roller 60 has a circumferential surface 64 encircling first element axis 62 and coaxial therewith. The frame of a motor 68 is mounted to carriage 46. A crank 66 is supported on the shaft of motor 68 so that the motor can turn crank 66 around an axis 70 parallel to the rocking axis 56. A connecting rod 72 has one end pivotally connected to crank 66 remote from its axis 70 and has the opposite end pivotally connected to yoke 50 remote from rocking axis 56. Thus, rotation of crank 66 about crank axis 70 will drive yoke 50 in a rocking motion about rocking axis 56 between a first extreme position in which the roller axis or first element axis 62 is tilted to the position indicated in broken lines at 62′ in
The spin-imparting assembly 42 further includes a second element incorporating an upstream roller 76 and a downstream roller 78. Roller 76 is mounted to frame 24 for rotation about an axis 80 perpendicular to the longitudinal direction of the fiber path and upstream from first element 60 whereas roller 78 is mounted to frame 24 downstream from first element 60 for rotation about an axis 82 parallel to axis 80 and also perpendicular to the longitudinal direction of the fiber path. Upstream roller 76 has a circumferential surface in the form of a surface of revolution about axis 80. The circumferential surface includes a generally V-shaped groove 84 aligned with the fiber path, so that the fiber is received in the groove. Downstream roller 78 has a similar groove 86, also aligned with the fiber.
As best seen in
Such spinning devices are further described in U.S. Pat. Nos. 6,550,283 and 6,324,872, the specifications of which is hereby incorporated by reference. Apparatus other than that shown in
Additional mechanisms for practicing the methods of the invention will be evident to persons skilled in the art from the disclosure herein, e.g., mechanisms for sinusoidal or non-sinusoidal spinning of a preform, when such preform spinning is used alone or in combination with applying a spinning force to a fiber.
Preferably, the twist is imparted to the optical fiber so that the twist period is at least 10 meters, more preferably at least 20 meters, and even more preferably at least 50 meters, although applicants believe that the upper limit to the period in which the twist can take place is not limited, and thus, the twist period could be as long as 100 meters or more. In order to facilitate retaining of the twist on the fiber after the twisting device 22 has twisted the fiber, the fiber free length, which is the distance between the twisting device and the storage spool, is preferably less than 10, more preferably less than 5 and most preferably less than 3 meters. To illustrate, reference is made to
The twist profiles employed herein to impart the twist to the fiber can be unidirectional or alternatively can be of any periodic shape. Preferably, the twist profile employed is of a periodic shape wherein the fiber is twisted first clockwise and then counter-clockwise. The periodic twist profile is also preferably a symmetric twist profile, wherein the magnitude of the maximum twist rate in the counter-clockwise direction is at least substantially equal to the magnitude of the twist rate of the fiber when twisted in the clockwise direction. The shape of the periodic twist profile could be any shape, including but not limited to sinusoidal, non-sinusoidal, triangular, trapezoidal or other periodic twist functions with similar or longer twist periods. The most preferred twist profile employed herein is a sinusoidal twist profile which is symmetric in the magnitude of the twist rate of the clockwise and counter-clockwise directions.
It will be apparent to those skilled in the art that various modifications and variations can be made to the present invention without departing from the spirit and scope of the invention. Thus it is intended that the present invention cover the modifications and variations of this invention provided they come within the scope of the appended claims and their equivalents. For example, while some of the examples set forth above are for unspun optical fiber, these examples would also work on spun optical fiber.