Method of insert molding auto and truck bumper, rocker panel and chin spoiler parts

Abstract
A paint film laminate is co-molded over a desired plastic substrate to produce an automobile bumper member, chin spoiler or rocker panel part. Along a desired surface of the part, such as, for example, a border between a part surface having one segment covered by paint film and a second segment comprising the exposed substrate, the edge of the paint film is embedded in the plastic substrate along a surface discontinuity such as a recess or ridge so that an aesthetically pleasing sight edge having a desired contour exists along this surface portion. The sight edge is formed during the co-molding process via the provision of an incline or ramp along a desired mold cavity surface. When the co-molded part is installed in its intended application, the paint film edge is substantially hidden from view by the surface discontinuity.
Description




FIELD OF THE INVENTION




The present invention pertains to an improved method of insert molding of a laminated film or the like over a plastic substrate to produce a part such as a bumper, chin spoiler or rocker panel for an automobile or truck.




BACKGROUND OF THE INVENTION




A variety of injection molded parts have been made and used for auto or truck body and trim parts. For example, bumpers, body panels, doors, filler panels, wheel covers, dashboards, arm rests and other parts have been made via injection molding techniques. Additionally, with regard to automobile exteriors, body side moldings, beltline moldings, roof moldings and window moldings are made via injection molding of thermoplastic olefin (“TPO”) or acrylonitrile-butadiene-styrene copolymer (“ABS”) or from other thermoplastic materials.




In order to provide a painted surface for these parts, film lamination techniques have been successfully employed. In accordance with these processes a paint film laminate is insert molded with the desired thermoplastic to fuse the film over the injection molded part. The resulting injection molded part is ready for assembly without subsequent painting.




The paint film laminate used in these insert molding techniques may comprise a backing sheet of about 0.020″ in thickness to which paint layers are adhered. Typically, the backing sheet comprises an extruded thermoplastic sheet.




In such paint film laminates, a paint film, comprising a cast dried continuous paint coating, is provided over the backing sheet. The paint film may consist of a monocoat, a clear coat over a base coat or a clear coat and a base coat with interposed print or design. The paint film, including base coat, clear coat and print or design, if desired, may range from about 0.5-4 mil. in thickness.




The laminated paint films are available, for example, from Avery Dennison, Decorative Films Division, Schererville, Ind., or Rexham Decorative Products, Charlotte, N.C. The films are typically provided in a roll, unwound, then trimmed to a proper “preform” size and shape, ready for insertion into the injection mold. The preform is usually placed along the cavity side of the mold with the painted side thereof facing the mold cavity surface. In some instances, the preform may be placed along the core side of the mold. The mold is then clamped and the desired molten resin is injected into the mold cavity. Heat and pressure conditions in the mold partially melt the backing sheet and a melt bonding or fusion of the injected resin and film occurs. Injection molds used for these processes are rear or edge gated so that the molten resin is directed along the backside of the film. The process leads to a finished plastic part with the paint film fused over the underlying plastic substrate. The painted or decorative side of the paint film laminate is exposed over the surface of the substrate to exhibit the desired aesthetic appearance.




It has become increasingly popular to insert or co-mold bumper, rocker panel, and chin spoiler parts for autos and trucks. Conventionally employed co-molding techniques however often result in the unsightly disposition of one of the paint film laminate edges over the substrate plastic in such manner that the laminate edge is exposed on the surface of the part and presents an uneven or non-uniform border with the plastic substrate material. This not only detracts from the physical appearance of the edge, but the exposed edge then serves as a site for peeling back and eventual separation of the film laminate from the underlying substrate.




Furthermore, the border between the film laminate and plastic substrate may have a wavy or uneven appearance. This may be caused by non-uniform dimensions or shrinkage of the paint film laminate during molding.




Accordingly, there is a need for a method for co-molding bumper, rocker panel, and chin spoiler parts wherein a uniform border is provided between the film laminate and plastic substrate. There is a more specific need for a method in which the paint film edge is located in a recess or relief area so that it can not be readily peeled back from the underlying substrate. Additionally, there is a need for a manufacturing process that will place the laminate-plastic border on the far or remote side of a raised area of the plastic part so that it will be hidden from sight and not normally seen from the vantage point of an ordinary observer.




SUMMARY OF THE INVENTION




These and other objects of the invention are met by the instant methods and fused film-plastic parts made thereby.




Briefly, improvement in traditional insert molding techniques is provided so as to provide for bumper, chin spoiler or rocker panel-type parts having Class A show surfaces. A specifically configured mold cavity structure is provided to facilitate formation of a uniform sight edge in the paint film laminate adjacent the boundary between the paint film laminate edge portion and the underlying plastic substrate. This results from provision of a surface discontinuity in the mold and corresponding part.




In one form of the invention, this discontinuity comprises a ramped or inclined concave cavity surface portion along a mold cavity surface for which the formation of the uniform sight edge is provided. The film edge is positioned along the ramp, short of the nadir of the concavity. Upon molding, the film edge is positioned in the recessed part portion formed, in the mold, adjacent the concavity.




In a preferred form of the invention, the film laminate edge is positioned over the apex of a convex ramp formed in the mold cavity. Upon molding, the film edge is formed in the part adjacent the convex ramp of the mold cavity. The paint film edge is positioned over the apex of the ramp remote from the viewer's vantage point. In this way, the viewer will see only the film covered ramp side facing him or her.




The invention will be further described in conjunction with the appended drawings and detailed description.











BRIEF DESCRIPTION OF THE DRAWINGS





FIG. 1

is a front end elevational view of an automobile having a chin spoiler paint film covered plastic part made in accordance with the invention;





FIG. 1A

is a partial side elevational view of an automobile having a rocker panel paint film covered plastic part made in accordance with the invention;





FIG. 2

is a transverse cross-sectional view of a mold cavity utilized to practice the instant invention;





FIG. 2A

is a magnified cross-sectional view of the circled area of the mold cavity shown in

FIG. 2

;





FIG. 3

is a sectional view of the chin spoiler shown in

FIG. 1

, taken along the lines and arrows


3





3


of

FIG. 1

;





FIG. 4

is a sectional view of the chin spoiler shown in

FIG. 1

taken along the lines and arrows


4





4


of

FIG. 3

;





FIG. 5

is a transverse cross-sectional view of a mold cavity utilized to practice a second embodiment of the instant invention;





FIG. 5A

is a magnified view of the circled area of the mold cavity shown in

FIG. 5

;





FIG. 6

is a sectional view of a part produced using the mold cavity of

FIG. 5

used as a chin spoiler and shown in combination with a car body panel; and





FIG. 7

is a sectional view of the part shown in

FIG. 6

taken along the lines and arrows


7





7


of FIG.


6


.











DETAILED DESCRIPTION OF THE INVENTION




Turning now to

FIG. 1

, there is shown an automobile


2


having disposed across its front body portion thereof continuous bumper member


4


. Continuous with and underneath the bumper member is a chin spoiler


6


made in accordance with the invention. The bumper member


4


and the chin spoiler


6


, together, present a continuous surface. Often, such chin spoilers, such as those depicted in

FIG. 1

, are used to improve the aerodynamic drag of the vehicle and/or to guard against body scratches and dents which could otherwise occur via the action of road debris or the like.




Turning now to

FIG. 1A

, the same automobile


2


has disposed along its side body portion a rocker panel


7


, which basically serves the same purposes as the chin spoiler


6


as well as providing support to passengers entering and leaving a passenger compartment (not shown) of the automobile


2


.




Turning now to

FIG. 3

, there is shown a part


8


in accordance with the invention. The part


8


, shown in cross-section in

FIG. 2

, may be either a chin spoiler


6


(

FIG. 1

) or a rocker panel


7


(FIG.


1


A). While not shown in

FIG. 3

, the part


8


would include mounting structure such as clip houses (not shown) positioned along its length to facilitate mounting of the part


8


on the exterior of the automobile


2


.




The part


8


comprises an outer layer composed of a paint film laminate. The paint film laminate comprises a show face front surface


9


, a top horizontally disposed edge


10


and a bottom edge


12


parallel to edge


10


. The paint film laminate is superposed over and provides a show surface over the plastic substrate


14


. In many cases, it is desirable to match colors between the front surface


9


of the paint film and the resin


14


.




The entire surface of bottom edge


12


is embedded within the plastic


14


in groove


51


so that this edge is recessed from the bottom surface


60


of the chin spoiler. Accordingly, when viewed from this bottom, an aesthetically pleasing part is shown that does not exhibit an abrupt or unsightly transition between the edge


12


and the bottom surface


60


of the part due to the tucking and ultimate fusing of the surface of edge


12


within the plastic matrix at groove


51


. Additionally since the edge


12


is totally recessed and attached to the matrix at this point, the paint film laminate is more securely anchored at this location than in other co-molded parts wherein the edge is merely superposed over but not embedded in the plastic. Accordingly, edge


12


will be less likely to peel back than in ordinary moldings where the boundary between the film edge and the plastic substrate is disposed along a relatively planar contour of the part.




Turning now to

FIG. 2

, there is shown a male mold member


16


and female mold member


18


which are configured so that they may be used in accordance with the instant process to form the part


8


shown in FIG.


3


. Again, with reference to

FIG. 2

, a cavity


20


is defined between the male and female mold members


16


,


18


. The cavity comprises a front surface


22


, top surface


24


and bottom surface


26


. Sprue


40


serves as an entry port for admission of thermoplastic or thermoset resin such as polypropylene or TPO into the cavity


20


.




In accordance with the invention, the paint film laminate is positioned in the mold cavity adjacent the front surface


22


of the cavity. The show or decorative side of the paint film laminate is contiguous with the front surface


22


of the mold cavity. As best viewed in

FIG. 2A

, a convex ramp or incline


42


is provided having an apex


43


and two sloping sides


45


,


47


respectively along the bottom surface of the mold cavity


26


. Here, the edge


12


of the film is positioned in the mold so that it is positioned along ramp side


45


short of the apex


47


. The molten plastic is injected into the mold along the rear side of the paint film laminate. The paint film is thereby pressed into the cavity surface by the action of the molten plastic thereon. At the location of inclined surface


45


, a border is provided between the bottom edge


12


of the paint film and the plastic that, during the molding process, will be disposed within the ridge or relief area


51


(see FIG.


3


).




Although the provision of one ramp


42


is shown along the bottom side


26


of mold cavity


20


, it is to be appreciated that a similar ramp could also be provided along the top side


24


of the mold cavity to provide the desired border between the otherwise free edge of the film laminate and the plastic matrix at this location as well.




After injection of a proper amount of plastic into the mold, the plastic is allowed to set and the mold cavities are separated to thereby result in the formation of the desired plastic part, either a bumper, a chin-spoiler or a rocker panel.




As to the plastic that may be utilized for the injection molding process, thermoplastic resins or thermoset resins may both be mentioned. Additionally, thermoplastic elastomer components may also be used. At present, it is preferred to utilize TPO as the resin component.




In accordance with the above process an insert molded plastic article is provided wherein the film laminate or the like covers the intended face surface of the part and wherein the bottom or top edge of the film laminate and the contiguous plastic surface provide a uniform border area.




The invention is therefore broadly directed toward improved methods in which a bi-component surface such as surface


60


may be provided. Turning specifically now to

FIG. 4

, the surface


60


is substantially smooth and planar and has a first segment


21


that is covered by the paint film laminate and a second segment


23


that includes the exposed substrate. The border


25


between the first and second segments is substantially linear and disposed longitudinally along the length of the part. The border is defined by the upturned portion of the paint film laminate proximate edge


12


(

FIG. 3

) into the groove


51


. The edge


12


is positioned within the groove


51


, however.




Turning now to

FIG. 5

there is shown another embodiment quite similar to that shown in

FIG. 2

save for the provision of a concave ramp formed in the mold along the parting line formed by the male and female mold members


16


,


18


. This type of ramp and the ensuing method are used to provide a borderline between paint film and contiguous plastic substrate that will be hidden from sight when positioned adjacent to the requisite structural part such as an auto or truck body part.




More specifically,

FIG. 5

discloses mold cavity


20


defined between male mold member


16


and female mold member


18


. Sprue


40


is provided and functions to provide an entrance way into the cavity


20


for the pressurized molten plastic. Similar to

FIG. 2

, the paint film laminate


11


is positioned in the mold cavity adjacent the front surface


22


of the cavity. The show or decorative side of the paint film is contiguous with the front surface


22


of the cavity.




As best shown in

FIG. 5A

, the paint film laminate


11


comprises a top longitudinal edge


15


. A concave ramp


152


is provided on the mold surface between the male mold member and female mold member along part line


151


of the mold. The concave ramp includes upwardly and downwardly sloped surfaces


153


,


155


respectively which are acutely angled from vertex


157


. Edge


15


of the laminate is positioned in the mold so that it extends past the vertex and terminates along downwardly sloped surface


155


. This is important since the part made in this mold cavity


20


(

FIG. 5

) will be positioned so that the edge


15


will be disposed closely adjacent a frame or body panel so that the viewer will only see the front


8


and top


10


show side of the film without being able to view the edge


15


.




Turning now to

FIG. 6

, there is shown a paint film covered part


70


made in the mold cavity of

FIG. 5

for use as a chin spoiler, rocker panel or the like on an automobile or truck. Here, the part comprises show side front


9


and top


10


surfaces with the paint film fused over the plastic substrate


14


. The part is positioned closely adjacent body or truck member


201


such that the edge


15


will not be viewed by the observer's eyes. This helps to ensure that the part presents an aesthetically pleasing show surface with regard to all visible surfaces thereof.




Stated differently, and with regard to

FIGS. 6 and 7

, the part


70


is an elongated film laminate covered plastic part wherein a front show face


9


is provided and a top show surface


10


provided over plastic substrate


14


along the length of the part. The top show surface comprises a longitudinally extending ridge or convexity having apex


77


and upwardly and downwardly sloping surfaces,


79


and


81


, respectively. The paint film completely covers the upwardly disposed ridge surface


79


and apex


77


with its longitudinal end


15


thereof terminating along the downwardly sloped surface


81


. This downwardly sloped surface


81


is positioned in close spatial proximity to the auto or truck


201


.




It is apparent then that film laminate covered parts are made in accordance with the invention wherein a film laminate end forms a longitudinally extending border with the underlying plastic substrate. The border is disposed with a surface irregularity that interrupts the normally smooth contour of the surface.




This surface irregularity may comprise either an elongated recess or ridge like member with the end of the film laminate disposed in the recess or on the ridge spaced downwardly from the apex of the ridge. In either case, the edge is better protected since it is not disposed on the normally smooth contour.




Having described the invention in detail and by reference to preferred embodiments thereof, it will be apparent that modifications and variations are possible without departing from the scope of the invention defined in the appended claims.



Claims
  • 1. Method of making a part for a motor vehicle, said part selected from the group consisting of a bumper member, a spoiler and a rocker panel, said part having a bi-component surface including a plastic substrate and a paint film laminate overlying a portion of said plastic substrate and having an end forming a border area of said part adjacent said plastic substrate, said method comprising:(a) providing a mold cavity defining a mold cavity surface portion for forming said bi-component surface, (b) providing a surface discontinuity in said mold cavity surface portion, said discontinuity having a pair of oppositely sloping surfaces and an intermediate region located between and connecting said sloping surfaces, (c) placing said film laminate along said mold cavity surface portion, and positioning said end of said film laminate along one of said sloping surfaces, (d) injecting molten plastic into said mold cavity and along said mold cavity surface portion and said film laminate; and (e) allowing said molten plastic to set thereby forming the part.
  • 2. Method as recited in claim 1 wherein in said step (b) said surface discontinuity comprises an elongated concavity.
  • 3. Method as recited in claim 1 wherein said surface discontinuity comprises an elongated convexity.
  • 4. Method as recited in claim 1 wherein said surface discontinuity is a convexity and said intermediate region is the apex of said convexity.
  • 5. Method as recited in claim 1 wherein said surface discontinuity is a concavity and said intermediate region is the nadir of said concavity.
US Referenced Citations (73)
Number Name Date Kind
3289253 Buonaiuto Dec 1966
3290082 Fritsch Dec 1966
3357056 Reyburn Dec 1967
3359030 Newman Dec 1967
3388523 Evans Jun 1968
3444275 Willett May 1969
3451709 Swauger Jun 1969
3493257 Fitzgerald et al. Feb 1970
3506294 Newman Apr 1970
3715138 Finkle Feb 1973
3843475 Kent Oct 1974
3897967 Barenyi Aug 1975
3914482 Sawa et al. Oct 1975
3959538 Loew May 1976
4015760 Bott Apr 1977
4066285 Hall et al. Jan 1978
4083592 Rubin et al. Apr 1978
4154893 Goldman May 1979
4160052 Krysiak et al. Jul 1979
4174986 Jennings Nov 1979
4197688 Mauer Apr 1980
4216184 Thomas Aug 1980
4298324 Soulier Nov 1981
4334700 Adell Jun 1982
4334706 Seki Jun 1982
4358482 Jubelt Nov 1982
4364789 Moran Dec 1982
4401232 Constable et al. Aug 1983
4408432 Carter et al. Oct 1983
4414731 Riemer Nov 1983
4489019 Takeda et al. Dec 1984
4546021 Mears Oct 1985
4579755 Takeda et al. Apr 1986
4587761 Adell May 1986
4587762 Adell May 1986
4597755 Samson et al. Jul 1986
4613178 Fujita Sep 1986
4617209 Ives Oct 1986
4619847 Jackson Oct 1986
4634565 Irrgang Jan 1987
4671974 Murachi Jun 1987
4710338 Bagnall et al. Dec 1987
4715648 Hensel Dec 1987
4719067 Thiel Jan 1988
4721642 Yoshimi et al. Jan 1988
4722818 Zoller Feb 1988
4724585 Whitman Feb 1988
4726614 Myers et al. Feb 1988
4734147 Moore Mar 1988
4767040 Miller et al. Aug 1988
4778550 Barton et al. Oct 1988
4786094 Barton et al. Nov 1988
4797244 Sauer Jan 1989
4808450 Guy Feb 1989
4833741 Mizuno et al. May 1989
4906421 Plamthottam et al. Mar 1990
4940557 Kimura Jul 1990
4968474 Ito Nov 1990
5000902 Adams Mar 1991
5023033 Cakmakci Jun 1991
5063014 Cakmakci Nov 1991
5087488 Cakmakci Feb 1992
5100728 Plamthottam et al. Mar 1992
5108681 Cakmakci Apr 1992
5178708 Hara et al. Jan 1993
5193711 Hirata et al. Mar 1993
5203941 Spain et al. Apr 1993
5240751 Cakmakci Aug 1993
5242650 Rackovan et al. Sep 1993
5372491 Fritsch et al. Dec 1994
5599608 Yamamoto et al. Feb 1997
5746962 Yamamoto May 1998
5972279 Harris et al. Oct 1999
Non-Patent Literature Citations (1)
Entry
SAE International®, SAE Technical Paper Series 902231, “Paint Film Laminate Technology Provides Painted Thermoplastic Parts Without VOC Issues,” Charles H. Fridley, Nov. 1, 1990.