Claims
- 1. A method of making a plastic knuckle pin for a coupler on a railway car, wherein the pin includes a shaft with fluting along its length to increase the surface area of the pin and a head at one end, said method comprising the steps of
- (a) melting a suitable plastic raw material;
- (b) injecting said melted plastic material into a mold;
- (c) forming a knuckle pin having fluting from said plastic material in said mold;
- (d) removing said knuckle pin from said mold;
- (e) placing said knuckle pin in a hot water bath;
- (f) removing said knuckle pin from said hot water bath and allowing said knuckle pin to be cooled therein;
- (g) allowing said knuckle pin to be cooled in air, wherein said fluting increases the surface area of the pin being cooled to enhance cooling, thereby reducing stresses and resulting in a plastic knuckle pin having a substantially uniform matrix.
- 2. The method of making a knuckle pin of claim 1, wherein the material is heated to a temperature of approximately 450 degrees fahrenheit in step (a).
- 3. The method of making a knuckle pin of claim 1, wherein the mold is maintained at a temperature of approximately 180 degrees fahrenheit.
- 4. The method of making a knuckle pin of claim 3, wherein the mold is heated by circulating high-temperature fluid in the mold.
- 5. The method of making a knuckle pin of claim 1, wherein said plastic material is in said mold for approximately two minutes.
- 6. The method of making a knuckle pin of claim 1, wherein the hot water bath is maintained at a temperature of approximately 180 degrees fahrenheit.
- 7. The method of making a knuckle pin of claim 1, wherein the plastic knuckle pin is placed in the hot water bath for approximately 20 minutes.
- 8. The method of making a knuckle pin of claim 1, wherein the plastic knuckle pin is cooled in air for approximately ten minutes.
- 9. A method of making a knuckle pin for a coupler on a railway car, wherein the pin includes a shaft with fluting along its length to increase the surface area of the pin and a head at one end, said fluting including longitudinally extending and circumferentially arranged slots, said method comprising the steps of
- (a) melting a suitable plastic raw material to a temperature of approximately 450 degrees fahrenheit;
- (b) injecting said melted plastic material into a tool maintained at a temperature of approximately 180 degrees fahrenheit;
- (c) forming a knuckle pin having fluting from said plastic material in said tool, maintaining said material in said tool for approximately two minutes;
- (d) removing said knuckle pin from said tool;
- (e) placing said knuckle pin in a hot water bath maintained at a temperature of approximately 180 degrees fahrenheit for approximately 20 minutes and allowing said knuckle pin to be cooled therein;
- (f) removing said knuckle pin from said hot water bath;
- (g) allowing said knuckle pin to be cooled in air for approximately ten minutes, wherein said fluting increases the surface area of the pin being cooled to enhance cooling thereby reducing stresses and forming a plastic knuckle pin having a substantially uniform matrix.
Parent Case Info
This application is a division of application Ser. No. 08/622,961, filed Mar. 27, 1996, now U.S. Pat. No. 5,630,519.
US Referenced Citations (13)
Divisions (1)
|
Number |
Date |
Country |
Parent |
622961 |
Mar 1996 |
|