Claims
- 1. A method for the manufacture of a heater for an indirectly heated cathode of an electron tube which comprises:
- (a) oxidizing the surface of a heater wire in the presence of an oxidizing gas to form an oxidized exposed surface on said wire, said wire being composed of a refractory metal selected from the group consisting of tungsten and molybdenum; and
- (b) reducing the exposed oxidized surface of the wire formed by step (a) to the metallic state of the refractory metal to form a rough, black surface on the wire, step (b) being the final step for forming the heater for the indirectly heated cathode.
- 2. A method for the manufacture of a heater for an indirectly heated cathode of an electron tube which comprises the steps of:
- (a) oxidizing the surface of a heater wire by heating the wire in the presence of an oxidizing gas to form an exposed oxidized surface on said wire, said wire being composed of a refractory metal selected from the group consisting of tungsten and molybdenum;
- (b) coating the exposed oxidized surface of the wire with alumina;
- (c) heating the coated wire in the presence of hydrogen to reduce the refractory oxides on the surface of the wire and to sinter the alumina to the wire to form a resulting wire;
- (d) coating the resulting wire with a soluble salt of a refractory metal; and
- (e) heating the wire formed by step (d) in a reducing atmosphere to form a rough, black surface on the wire.
- 3. The method of claim 2 wherein the soluble salt is ammonium tungstate.
- 4. The method of claim 2 wherein the wire is composed of tungsten.
- 5. The method of claim 2 wherein the refractory metal of the salt and wire are the same.
- 6. A method for the manufacture of a heater for an indirectly heated cathode of an electron tube which comprises:
- (a) oxidizing the surface of a heater wire by heating the wire in the presence of an oxidizing gas to form an exposed oxidized surface on said wire, said wire being composed of a refractory metal selected from the group consisting of tungsten and molybdenum;
- (b) coating the exposed oxidized wire with a soluble salt of a refractory metal; and
- (c) reducing the coating and the oxidized surface of the wire in the presence of hydrogen to their metallic states to form a rough, black surface on the wire.
- 7. The method of claim 6 wherein the soluble salt is ammonium tungstate.
- 8. The method of claim 7 wherein, following step (a), the oxidized wire is coated with alumina and wherein, during step (c), the coated oxidized wire is heated sufficiently to sinter the alumina coating to the wire as well as to reduce the oxidized wire and ammonium tungstate to their metallic states.
BACKGROUND OF THE INVENTION
The present application is a continuation of my abandoned application Ser. No. 380,013, which is a continuation of Ser. No. 41,720, now abandoned, which is a continuation of abandoned Ser. No. 621,194, respectively filed July 17, 1973, May 27, 1970, and Mar. 7, 1967.