Claims
- 1. A method for manufacturing a modified fast fade drive axle housing comprising:
- providing a flat blank of sheet steel of generally rectangular shape having two top node portions, two bottom node portions, a right arm portion, a left arm portion and a nodal portion and internodal portion therebetween in which said two top node portions are aligned opposite said two bottom node portions, the right arm portion and left arm portions having a combined length from about 50% of the total length of the blank to a length which is less than the sum of said nodal portion and said internodal portion and the right and left arm portion having a uniform width while the internodal portion and nodal portion have a width which varies, the right arm and left arm portions of uniform width being about 70% of the total width of the blank, the remaining upwardly tapered nodal portions and internodal portions having relatively shallow tapers, inner nodal slopes being substantially steeper than outer nodal slopes and the center of the blank having a single notch;
- heating said blank to a temperature range of at least 1350.degree. up to 1650.degree. F. to bring the blank to a uniform temperature prior to bending;
- and bending said blank in two stages within said temperature range;
- said bending in the first stage being at a first temperature which forms the central bowl portion and pushes in by bending the sides of the bowl portion to achieve the semispherical configuration of the bowl portion having bent in sides while the top and bottom nodal portions and the right and left arm portions are left flat;
- said bending in said second stage being at a second temperature in said range which bends the two top nodes inwardly and the two bottom nodes inwardly while simultaneously bending the left and right arm portions inwardly, and bending the internodal portions inwardly to thereby align the top nodes opposite the bottom node, the internodal portions, top and bottom opposite each other and the bent in portions at the right and left arms opposite each other to thereby bend the right and left arm portions in the form of U-shaped rectangular cross-sections with the differential receiving portion lying in the internodal span and a transition zone intermediate the beam arms and the differential portion, and form a half differential housing;
- said bending operation in said second stage further deforming the outer circular cylindrical area of said bowl to form a narrow stoved in U-shaped section with simultaneous narrowing of the corner where the metal is squeezed inwardly in a short transition zone in the fast fade bend at the boundary of the bowl and arms to provide a substantially greater amount of bending than required in a longer transition zone between the stoved transition zone and the arms, and
- said U-shape rectangular cross section half differential housing being adapted to be welded along the top edges of the beam arm portion to a like half differential housing to provide a complete modified fast fade drive axle housing.
- 2. A method as claimed in claim 1 wherein the upwardly tapered nodel portions of the blank, the nodes and the internodal portions constitute in length from 50-52% of the total length of the blank.
- 3. A method as claimed in claim 2 wherein the left arm portion is shorter in length than the right arm portion.
- 4. A method as claimed in claim 2 wherein the left arm portion is about equal in length to the right arm portion.
- 5. A method as claimed in claim 2 wherein the left arm portion is longer than the right arm portion.
Parent Case Info
This is a continuation of application Ser. No. 845,109, filed Mar. 27, 1986, now abandoned.
US Referenced Citations (7)
Non-Patent Literature Citations (1)
Entry |
Caruz Howard, "Modern Welding Technology", Feb. 13, 1980, p. 514. |
Continuations (1)
|
Number |
Date |
Country |
Parent |
845109 |
Mar 1986 |
|