Claims
- 1. A method for manufacturing a deodorizing filter, comprising the steps of
- preparing a slurry comprising a reducing agent, cuprous oxide, a binder, and water;
- impregnating a paper of a ceramic fiber with said slurry; drying said paper; and
- forming said paper into a honeycomb structure.
- 2. The method of claim 1 wherein a porous powder is added to said slurry.
- 3. The method of claim 2 wherein the reducing agent is selected from the group consisting of erythorbic acid, erythorbic acid sodium, ascorbic acid, ascorbic acid sodium, and oxalic acid.
- 4. The method of claim 1 wherein the reducing agent is selected from the group consisting of erythorbic acid, erythorbic acid sodium, ascorbic acid, ascorbic acid sodium, and oxalic acid.
- 5. A method for manufacturing a deodorizing filter, comprising the steps of
- preparing a slurry comprising a reducing agent, cuprous oxide, a binder, a solid acid, and water;
- impregnating a paper of a ceramic fiber with said slurry; drying said paper; and
- forming said paper into a honeycomb structure.
- 6. The method of claim 5 wherein the reducing agent is selected from the group consisting of erythorbic acid, erythorbic acid sodium, ascorbic acid, ascorbic acid sodium, and oxalic acid.
- 7. A method for manufacturing a deodorizing filter, comprising the steps of
- forming a paper made of ceramic fiber and a binder into a honeycomb structure;
- preparing a slurry comprising a reducing agent, cuprous oxide, a binder and water;
- soaking the paper in the slurry; and
- drying said paper.
- 8. The method of claim 7 wherein a porous powder is added to said slurry.
- 9. The method of claim 8 wherein the reducing agent is selected from the group consisting of erythorbic acid, erythorbic acid sodium, ascorbic acid, ascorbic acid sodium, and oxalic acid.
- 10. The method of claim 7 wherein the reducing agent is selected from the group consisting of erythorbic acid, erythorbic acid sodium, ascorbic acid, ascorbic acid sodium, and oxalic acid.
- 11. A method for manufacturing a deodorizing filter, comprising the steps of forming a paper made of ceramic fiber and a binder into a honeycomb structure;
- preparing a slurry comprising a reducing agent, cuprous oxide, a binder, a solid acid and water;
- soaking the paper in the slurry; and
- drying said paper.
- 12. The method of claim 11 wherein the reducing agent is selected from the group consisting of erythorbic acid, erythorbic acid sodium, ascorbic acid, ascorbic acid sodium, and oxalic acid.
- 13. A method for manufacturing a deodorizing filter wherein ceramic fibrous paper is soaked in a slurry of a mixture of an aqueous solution of a reducing agent with cuprous oxide, solid acid and binder, and then dried; and then the dried ceramic fibrous paper is formed into a honeycomb filter.
- 14. The method of claim 13 wherein the reducing agent is selected from the group consisting of erythorbic acid, erythorbic acid sodium, ascorbic acid, ascorbic acid sodium, and oxalic acid.
- 15. A method for manufacturing a deodorizing filter wherein ceramic fibrous paper with a binder added is formed into a honeycomb filter which is then soaked in a slurry of a mixture of an aqueous solution of a reducing agent with cuprous oxide, solid acid and a binder, and the soaked filter is dried to make the deodorizing filter.
- 16. The method of claim 15 wherein the reducing agent is selected from the group consisting of erythorbic acid, erythorbic acid sodium, ascorbic acid, ascorbic acid sodium, and oxalic acid.
Parent Case Info
This is a division of application Ser. No. 07/554,128, filed Jul. 17, 1990, now U.S. Pat. No. 5,372,788.
US Referenced Citations (2)
Number |
Name |
Date |
Kind |
3112184 |
Hollenbach |
Nov 1963 |
|
3857732 |
Yoshino |
Dec 1974 |
|
Divisions (1)
|
Number |
Date |
Country |
Parent |
554128 |
Jul 1990 |
|