Claims
- 1. A method for reprocessing used printed paper, the method comprising the steps of:
- a) dissolving the paper into pulp;
- b) initially cleaning the pulp;
- c) one of floating and washing the pulp after the step of initially cleaning;
- d) a first step of disintegrating and defibering the pulp using a disk disintegrator;
- e) a second step of disintegrating and defibering the pulp by treating the pulp with a strong kneading action using a single-shaft disintegrator, the second step of disintegrating and defibering occurring after the first step of disintegrating and defibering.
- 2. The method of claim 1, further comprising the step of bleaching the pulp after the second step of disintegrating and defibering.
- 3. The method of claim 2, further comprising the steps of fine cleaning the pulp and one of sorting and screening the pulp between the first and second steps of disintegrating and defibering.
- 4. The method of claim 3, further comprising the step of floating the pulp before the step of fine cleaning and after the first step of disintegrating and defibering.
- 5. The method of claim 2, further comprising the step of floating the pulp after the first step of disintegrating and defibering and before the second step of disintegrating and defibering.
- 6. The process of claim 3, wherein the temperature at the second disintegrating and defibering step is in the range between 38.degree. and 65.degree. C.
- 7. The method of claim 3, wherein the operational consumption at the second disintegrating and defibering step is between 30 and 80 kilowatt hours per ton oven-dried pulp.
- 8. The method of claim 1, wherein the kneading action is performed by kneading elements on a stator or on a rotor, the method comprising rotating the rotor with respect to the stator for causing the kneading elements to knead the pulp.
- 9. The method of claim 8, wherein the first step of disintegrating and defibering is performed at a consistency of at least 20% and the second step of disintegrating and defibering is performed at temperatures in a range between 20.degree. and 140.degree. C. and at an operational consumption of between 30 and 100 kilowatt hours per ton of oven-dried pulp.
- 10. The method of claim 1, wherein the first and second steps of disintegrating and defibering occur successively without any additional pulp floating step occurring therebetween.
- 11. The method of claim 1, wherein the second disintegrating and defibering step additionally comprises a dispersing step.
- 12. The method of claim 1, further comprising the step of floating the pulp following the first and second steps of disintegrating and defibering.
Priority Claims (2)
Number |
Date |
Country |
Kind |
41 31 308.9 |
Sep 1991 |
DEX |
|
41 33 683.6 |
Oct 1991 |
DEX |
|
Parent Case Info
This is a Continuation of application Ser. No. 08/050,474 filed on May 18, 1993, now abandoned.
US Referenced Citations (4)
Foreign Referenced Citations (8)
Number |
Date |
Country |
0092124 |
Oct 1983 |
EPX |
0354307 |
Feb 1990 |
EPX |
0398846 |
Nov 1990 |
EPX |
2517713 |
Jun 1983 |
FRX |
2413278 |
Sep 1975 |
DEX |
0904279 |
Aug 1962 |
GBX |
1429626 |
Mar 1976 |
GBX |
2033784 |
May 1980 |
GBX |
Non-Patent Literature Citations (1)
Entry |
Das Papier; J. Bruckner "dispergierung"; vol. 42, No. 10, Oct. 1988, pp. 547-550. |
Continuations (1)
|
Number |
Date |
Country |
Parent |
50474 |
May 1993 |
|