Claims
- 1. A method of producing a fine titanium-free powder of an element selected from the group consisting of Mo, Re, Cu, Ag, Au, Zn, Cd, In, Sn, Pb, Sb, As, Bi, Te, Se, S, Ni, Ru, Rh, Pd, Pt, Os, Ir and mixtures thereof which comprises preparing a reaction mixture by combining a reducing amount of titanium trichloride with an aqueous solution of a water soluble compound or complex of said element at a temperature below the boiling point of the aqueous solution, and thereafter recovering the titanium-free fine powder produced by the reducing action of the titanium trichloride from the reaction mixture.
- 2. A method of producing a fine powder in accordance with claim 1, additionally comprising the step of preparing said aqueous solution by combining titanium trichloride and water.
- 3. A method of producing a fine powder in accordance with claim 2, in which the aqueous solution is of a water soluble complex of said element.
- 4. A method of producing a fine powder in accordance with claim 2, in which the temperature of the aqueous solution is 60.degree. to 80.degree. C.
- 5. A method of producing a fine powder in accordance with claim 2, in which the element is lead.
- 6. A method of producing a fine powder in accordance with claim 2, in which the element is antimony.
- 7. A method of producing a fine powder in accordance with claim 2, in which the element is iridium.
- 8. A method of producing a fine powder in accordance with claim 2, in which the element is cadmium.
- 9. A method of producing a fine powder in accordance with claim 2, in which the element is nickel.
- 10. A method of producing a fine powder in accordance with claim 2, in which the element is a mixture of tin and lead.
- 11. A method of producing a fine powder in accordance with claim 2, in which the element is rhenium.
- 12. A method of producing a fine powder in accordance with claim 2, in which the element is molybdenum.
- 13. A method of producing a fine powder in accordance with claim 2, in which the element is selenium.
- 14. A method of producing a fine powder in accordance with claim 2, in which the element is tellurium.
- 15. A method of producing a fine powder in accordance with claim 2, in which the element is copper.
- 16. A method of producing a fine powder in accordance with claim 2, in which the element is a mixture of cadmium and sulfur.
- 17. A method of producing a fine powder in accordance with claim 2, in which the element is a mixture of indium and antimony.
- 18. A method of producing a fine powder in accordance with claim 1, wherein a reaction between the aqueous solution and the titanium trichloride takes place under atmospheric pressure or under high pressure.
Priority Claims (1)
Number |
Date |
Country |
Kind |
3-270162 |
Sep 1991 |
JPX |
|
Parent Case Info
This is a continuation-in-part of application Ser. No. 07/949,046 filed Sep. 21, 1992, now abandoned.
US Referenced Citations (3)
Number |
Name |
Date |
Kind |
4217152 |
Aonuma et al. |
Aug 1980 |
|
4445931 |
Worthington |
May 1984 |
|
4803291 |
Rousset et al. |
Feb 1984 |
|
Continuation in Parts (1)
|
Number |
Date |
Country |
Parent |
949046 |
Sep 1992 |
|