Claims
- 1. In a method of producing gas concrete in which a mass comprising water, lime, rising agent, cement, and sand, said mass being suitable for production of gas concrete, is cast into a mold where it is permitted to rise and harden into a mass capable of being cut into a desired shape and wherein the hardened material is hydrothermally cured with steam in an autoclave to form a gas concrete product, the improvement wherein said castable mass is prepared by the steps of:
- providing water in a mixing vessel, adding lime, cement, and sand to the water in the mixing vessel while stirring and mixing for 40 to 80 seconds, said lime and cement together forming a binding agent in which the lime is predominant;
- mixing a calcium sulphate-containing component with said homogeneous pre-mixture for 30 to 35 seconds to form a homogeneous calcium sulphate-containing mixture, said calcium sulphate-containing component being selected from the group consisting of calcium sulphate anhydrite and gypsum and being present in an amount of 6-12% by weight SO.sub.3 based on the weight of CaO in said lime;
- mixing a rising agent with said homogeneous calcium sulphate-containing mixture for 20 to 40 seconds to form said castable mass; and
- after mixing is completed, retaining the castable mass in the mixing vessel until rising starts.
- 2. A method according to claim 1 wherein the castable mass is retained in the mixing vessel for 8 to 14 seconds.
- 3. In a method of producing gas concrete in which a mass comprising water, lime, rising agent, cement, and sand, said mass being suitable for production of gas concrete, is cast into a mold where it is permitted to rise and harden into a mass capable of being cut into a desired shape and wherein the hardened material is hydrothermally cured with steam in an autoclave to form a gas concrete product, the improvement wherein said castable mass is prepared by the steps of:
- pre-mixing water, lime, cement, and sand to form a homogeneous pre-mixture, said lime and cement together forming a binding agent in which the lime is predominant;
- mixing a calcium sulphate-containing component with said homogeneous pre-mixture to form a homogeneous calcium sulphate-containing mixture, said calcium sulphate-containing component being selected from the group consisting of calcium sulphate anhydrite and gypsum and being present in an amount of 6-12% by weight SO.sub.3 based on the weight of CaO in said lime;
- mixing a rising agent with said homogeneous calcium sulphate-containing mixture to form said castable mass; and
- retaining the castable mass in the mixing vessel for 8 to 14 seconds.
Priority Claims (1)
Number |
Date |
Country |
Kind |
2739181 |
Aug 1977 |
DEX |
|
Parent Case Info
This is a continuation of the application Ser. No. 937,749 filed Aug. 29, 1978 now abandoned.
US Referenced Citations (6)
Foreign Referenced Citations (1)
Number |
Date |
Country |
54-97622 |
Aug 1979 |
JPX |
Continuations (1)
|
Number |
Date |
Country |
Parent |
937749 |
Aug 1978 |
|