Claims
- 1. A method of manufacturing an amorphous metal sheet having a thickness of less than 30 .mu.m which comprises extruding a molten metal from an orifice of a slot defined by a pair of side walls and a pair of lips and making a stream of the molten metal from the orifice onto a moving chill surface to rapidly cool and solidify the metal thereby forming said amorphous metal sheet, wherein the stream of the molten metal is extruded to be advanced toward the moving direction of the chill surface and the upper surface of the stream of the molten metal extends beyond a front lip of the pair of lips arranged downstream of the slot in the direction of metal movement and sweeps the front lip under the following conditions; said orifice being a rectangular slit, said front lip being flat and a back lip of the pair of lips arranged upstream of the slot in the direction of metal movement being flat; said chill surface moving at a speed of 10m/sec to 50m/sec and being spaced from the front lip by a gap length of from 100 .mu.m to 600 .mu.m and the width W.sub.F of the front lip measured in the direction of movement of the chill surface being represented by the relationship W.sub.F /W.ltoreq.0.8 wherein W, representing the width of a slot in the nozzle, has a value of 0.3 mm to 0.9 mm, the slot formed in the nozzle is inclined to make an angle such that the molten metal is extruded in the same direction as the moving direction of the chill surface, and the gap length G between the chill surface and the tip of the front lip satisfies an inequality:
- 3 g.ltoreq.G.ltoreq.20 g
- where g represents a thickness of the formed metal sheet.
- 2. A method according to claim 1, wherein the surface vector of the slot which is normal to the slot surface makes an angle of about 20 degrees with the moving direction vector of the chill surface.
- 3. A method according to claim 1, wherein W.sub.F satisfies an inequality:
- 0.1 W.ltoreq.W.sub.F .ltoreq.0.5 W.
- 4. A method according to claim 1, wherein the width W.sub.B of the back lip satisfies an inequality:
- 0.1 W.ltoreq.W.sub.B .ltoreq.0.8W.
- 5. A method according to claim 1, wherein the back lip is substantially free of contact with the stream of the molten metal and the front lip contacts a minor portion of the upper surface of the stream; a major portion of the upper surface being free from the front lip.
Priority Claims (1)
Number |
Date |
Country |
Kind |
60-279856 |
Dec 1985 |
JPX |
|
Parent Case Info
This is a continuation of application Ser. No. 807,685, filed Dec. 11, 1985, and now abandoned.
US Referenced Citations (3)
Number |
Name |
Date |
Kind |
4221257 |
Narasimhan |
Sep 1980 |
|
4386648 |
Hilzinger et al. |
Jun 1983 |
|
4479528 |
Maringer |
Oct 1984 |
|
Continuations (1)
|
Number |
Date |
Country |
Parent |
807685 |
Dec 1985 |
|