Claims
- 1. A method of depolymerizing a fibrous thermoplastic resin, comprising
- A. compressing a fibrous thermoplastic resin mass by extrusion and, while compressing and during extrusion, melting only the surface portion of the mass,
- B. cooling the mass to solidify the molten surface portion, thereby forming a shaped article having a specific gravity greater than 1/2 of the true specific gravity of the resin, said shaped article consisting of the fibrous thermoplastic resin mass having on its surface a crusty thin resin layer bonded to the resin mass,
- C. cutting the shaped article into sections, and
- D. introducing the resulting cut shaped article into a depolymerization chamber, wherein said article is subjected to heat depolymerization.
- 2. A method according to claim 1 wherein said crusty thin resin layer is formed by melting the surface portion of the fibrous thermoplastic resin by friction heat generated during extrusion.
- 3. A method according to claim 1 wherein said crusty thin layer has a Shore hardness of from 15 to 60 and a breaking strength of at least 10 g/mm.sup.2.
- 4. A method according to claim 1 wherein the fibrous thermoplastic resin is a polyester fiber.
- 5. A method according to claim 1 wherein the fibrous thermoplastic resin is a polyamide fiber.
- 6. A method according to claim 4 wherein the polyester fiber is a polyester yarn scrap and prior to the shaping, it is cut into short fibers and is then washed with a detergent, water-washed, dehydrated and dried.
- 7. A method according to claim 1 wherein said crusty thin resin layer has a thickness of 0.05 to 3 mm.
- 8. A method of depolymerizing a fibrous thermoplastic resin, comprising
- A. compressing a fibrous thermoplastic resin mass by extrusion and, while compressing and during extrusion, elevating only the surface portion of the mass to a temperature above the glass transition point,
- B. cooling the mass to solidify the softened surface portion, thereby forming a shaped article having a specific gravity greaer than 1/2 of the true specific gravity of the resin, said shaped article consisting of the fibrous thermoplastic resin mas having on its surface a crusty thin resin layer bonded to the resin mass,
- C. cutting the shaped article into sections, and
- D. introducing the resulting cut shaped article into a depolymerization chamber, wherein said article is subjected to heat depolymerization.
- 9. The method according to claim 8 wherein the temperature is elevated by friction heat generated during extrusion.
Priority Claims (1)
Number |
Date |
Country |
Kind |
47-36243 |
Apr 1972 |
JA |
|
Parent Case Info
This application is a continuation application of Ser. No. 349,462, filed Apr. 9, 1973, now abandoned.
US Referenced Citations (6)
Continuations (1)
|
Number |
Date |
Country |
Parent |
349462 |
Apr 1973 |
|