Claims
- 1. A method of reducing the volume of a radioactive waste mixture of filter fibers and a powder-form ion-exchange resin, which comprises:
- dissolving filter fibers in a radioactive waste mixture comprising filter fibers and a powder-form ion-exchange resin by adding a solvent to the radioactive waste mixture forming a resultant mixture; and
- first drying and then additionally heat treating the resultant mixture.
- 2. The method according to claim 1, which comprises carrying out the dissolving step by adding a solvent selected from the group consisting of dimethylformamide, dimethylacetamide, dimethyl sulfoxide, ethylene carbonate and a solution of zinc chloride to dissolve polyacrylonitrile filter fibers.
- 3. The method according to claim 1, which comprises carrying out the additional heat treatment step by adding between 10 and 50% by weight of a substance selected from the group consisting of sodium hydroxide, potassium carbonate, calcium oxide, calcium hydroxide, borate salts and phosphorus pentoxide to the dried, solvent-treated mixture in a temperature range between 120.degree. C. and 220.degree. C.
- 4. The method according to claim 1, which comprises carrying out the additional heat treatment step by adding between 10 and 50% by weight of a substance selected from the group consisting of sodium hydroxide, potassium carbonate, calcium oxide, calcium hydroxide, borate and phosphorus pentoxide to the dried, solvent-treated mixture in a temperature range between 130.degree. C. and 190.degree. C.
- 5. The method according to claim 1, which comprises mixing acidic mixtures with calcium oxide or magnesium oxide until a neutral to slightly basic pH is established, to avoid package corrosion.
- 6. The method according to claim 1, which comprises mixing alkaline mixtures with boric acid or acidic phosphate until an at least approximately neutral pH is established.
- 7. A method of reducing the volume of a radioactive waste mixture of filter fibers and a powder-form ion-exchange resin, which comprises:
- dissolving filter fibers in a radioactive waste mixture comprising filter fibers and a powder-form ion-exchange resin by adding a zinc chloride solution to the radioactive waste mixture forming a resultant mixture; and
- first drying and then additionally heat treating the resultant mixture.
- 8. A method of reducing the volume of a radioactive waste mixture of filter fibers, water and a powder-form ion-exchange resin, which comprises:
- dissolving filter fibers in a radioactive waste mixture comprising filter fibers, water, and a powder-form ion-exchange resin by mixing a zinc chloride solid with the water of the radioactive waste mixture forming a resultant mixture; and
- first drying and then additionally heat treating the resultant mixture.
Priority Claims (1)
Number |
Date |
Country |
Kind |
44 20 658.5 |
Jun 1994 |
DEX |
|
CROSS-REFERENCE TO RELATED APPLICATIONS
This application is a Continuation of International Application Ser. No. PCT/DE95/00724, filed Jun. 2, 1995.
US Referenced Citations (5)
Foreign Referenced Citations (2)
Number |
Date |
Country |
0 182 172 B1 |
May 1986 |
EPX |
0 262 823 A2 |
Apr 1988 |
EPX |
Non-Patent Literature Citations (1)
Entry |
Japanese Patent Abstract No. 86-065767. |