Claims
- 1. A method for manufacturing a porous sintered stainless steel body comprising the steps of:
- (a) forming a mixture comprising stainless steel powder, Ni-Mn powder and Ni-Cr powder, wherein the particles of the Ni-Mn powder and the Ni-Cr powder are smaller than the particles of said stainless steel powder;
- (b) pouring the resulting powder mixture of step (a) into a heat-proof vessel without applying any pressure to said mixture;
- (c) sintering said mixture poured into said heat-proof vessel of step (b) under a non-oxidizing atmosphere without applying any pressure to said mixture such that said sintering is started at about at least 1000.degree. C. with the temperature gradually being raised and said sintering is finished at 1200.degree. C. to 1350.degree. C.
Parent Case Info
This is a continuation of application Ser. No. 212,462, filed Dec. 3, 1980, now abandoned.
US Referenced Citations (8)
Foreign Referenced Citations (1)
Number |
Date |
Country |
779949 |
Jul 1957 |
GBX |
Continuations (1)
|
Number |
Date |
Country |
Parent |
212462 |
Dec 1980 |
|