Claims
- 1. A method of using a bipolar electrode element, which element comprises a laminated substrate including a first layer comprising a particulate conductive metal oxide dispersed in a resin binder, and a second layer comprising particulate carbon material dispersed in a resin binder, the metal oxide being selected from the group consisting of barium metaplumbate and the conductive oxides of titanium, tungsten, vanadium, niobium and molybdenum, a negative electrode material applied to the first layer, and a positive electrode material applied to the second layer, which method comprises:
- employing the first layer at the negative side of a bipolar electrical element;
- employing the second layer at the positive side of the bipolar electrical element.
- 2. The method of claim 1, wherein the thickness of the first layer is between about 0.005-0.1 inch.
- 3. The method of claim 1, wherein the thickness of the second layer is between about 0.001-0.02 inch.
- 4. The method of claim 2, wherein the thickness of the second layer is between about 0.001-0.02 inch.
- 5. The method of claim 1, wherein the conductive metal oxide consists essentially of barium metaplumbate.
- 6. The method of claim 1, wherein the resin binder is a polyolefin.
- 7. The method of claim 1, wherein the particle size of the conductive metal oxide is in the range of 0.1 to 300 microns.
- 8. The method of claim 7, wherein the particle size of the conductive metal oxide is in the range of 0.1 to 40 microns.
- 9. The method of claim 1, wherein the first layer comprises 10-95 parts by volume of the conductive oxide and 90-5 parts by volume of the binder.
- 10. The method of claim 1, wherein the second layer comprises 10-95 parts by volume of the conductive oxide and 90-5 parts by volume of the binder.
- 11. The method of claim 1, wherein the particle size of the carbon is in the range of 0.1 to 300 microns.
- 12. The method of claim 11, wherein the carbon has an average particle size in the range of 0.1 to 40 microns.
- 13. The method of claim 1, wherein the second layer is thinner than the first layer.
- 14. The method of claim 13, wherein the electrode element is formed by coating the conductive oxide layer with a liquid or paste containing the binder and the particulate carbon.
- 15. The method of claim 14, wherein the second layer binder comprises a synthetic rubber.
- 16. The method of claim 1, wherein the electrode element is formed by coating the conductive oxide layer with a liquid or paste containing the binder and the particulate carbon.
- 17. The method of claim 16, wherein the second layer binder comprises a synthetic rubber.
- 18. The method of claim 1, wherein the electrode element is a double-layered capacitor.
- 19. The method of claim 1, wherein the electrode element is a bipolar lead-acid battery electrode.
Parent Case Info
This is a continuation of Application Ser. No. 08/341,023 filed Nov. 17, 1994, abandoned.
US Referenced Citations (7)
Foreign Referenced Citations (2)
Number |
Date |
Country |
62-115666 |
May 1987 |
JPX |
63-314760 |
Dec 1988 |
JPX |
Continuations (1)
|
Number |
Date |
Country |
Parent |
341023 |
Nov 1994 |
|