1. Field of the Invention
A method to control the pretilt angle of a liquid crystal device (LCD) is disclosed, more particular, the method utilizes a particle beam with plasma or ions to treat the surface of the vertical alignment layers of the LCD before the alignment process, so as to adjust the pretilt angle of the liquid crystal (LC) molecules.
2. Description of Related Art
Liquid crystal is often used for display screens since it has intrinsic photoelectric characteristics. Generally, productive flat-panel LCDs are TN (Twisted Nematic) types.
The basic structure of a TN LCD includes upper and lower conductive glass substrates, with a Nematic liquid crystal injected therebetween. Moreover, two polarized plates with orthogonal-polarization are disposed on the outside of each substrate. Next, an alignment film is coated on each conductive substrate and rubbed with rubbing clothes, so that the liquid crystal molecules are aligned in the rubbing direction. Under conditions in which an electric field isn't being used, the polarized direction of the ray will change as torsion occurs to the liquid crystal molecules after entering the LCD, thereby causing a bright state. Conversely, the liquid crystal molecules will be homeotropic, namely vertical to the direction of the alignment film, when an electric field is used, so as to form a dark state since the ray cannot pass through the second polarizer.
LCD is well-developed, but there are still several problems existing such as the viewing angle, contrast, and display uniformity. Particularly, the above-mentioned alignment film is relevant to implementing high-density and large-sized LCDs, as well as faster response times. Liquid crystal molecules of the LCD are used in displayers since the direction of the polarization of ray can be changed by an external electric field. Shutting off the electric field recovers the original arrangement via the recovering force, i.e. the anchoring force. Therefore, whether the ray passes through the device determines either a bright state or a dark state of the LCD.
There are three kinds of liquid crystal arrangements—homogeneous alignment, vertical alignment, and tilted-angle alignment. Reference is made to
Conventional liquid crystal alignment method is rubbing. Reference is made to
In the field of non-contact alignment, such as photo-alignment, a polarized UV ray is used to perform surface anisotropy on alignment film. Reference is made to U.S. Pat. No. 5,711,999 illustrating a method of applying light to produce surface anisotropy of a photosensitive alignment film. U.S. Pat. No. 5,711,999 has disclosed the range of light wavelength and the quantity of radiation, which react with the chemical components of the film. The characteristics of the alignment film are changed by controlling the intensity of exposure and the wavelength of the light. The pretilt angles of the LC molecules are changed thereby. Moreover, U.S. Pat. No. 5,623,354 has disclosed that an ultraviolet light can change the pretilt angle of the liquid crystal molecules on the alignment layer of the LCD. A display device with a multi-domain liquid crystal layer is thereby manufactured.
U.S. Pat. No. 6,852,374 has disclosed a LCD, an optical element, a method of fabricating the LCD, and a method of making an optical element. This patent relates to the structural design and a manufacturing method of a liquid crystal panel with optical compensation birefringence (OCB) mode.
For implementing the OCB structure mentioned above, the control of the pretilt angle (i.e. generally, larger than 5 degree but less than 85 degree) of the LC molecules is necessary. For controlling the pretilt angle, the above-mentioned patent uses the wavelength and the quantity of the light source to treat the surface on the alignment film. Since a particular material is used for the alignment film, only specific side-chain of the alignment film will be broken under a specific light wavelength, so as to change the pretilt angle of liquid crystal.
Reference is made to
In a displaying mode with the optical compensation birefringence (OCB), a high pretilt angle of the liquid crystal molecules is required so that a step of converting a splay state into a bend state of the liquid crystal molecules by stressing an external high voltage can be ignored. However, in view of other conventional arts, if the step of alignment is solely achieved by rubbing, an ionic beam, light beams or plasma beams individually, the high pretilt angle required by OCB will not be reached.
Alternatively, although combining the vertical and horizontal polyimides of the conventional art allows the high pretilt angle to be reached, it requires particular solution mixture and the evaporation process to control the surface fraction of vertical and horizontal polyimides. Moreover, the step of treating the surface by a light or a heat source with assistance of the step of rubbing to produce high pretilt angle will cause a high residual DC voltage or a bad thermal stability.
Consequentially, the technology of the conventional art using light to treat the surface cannot generate the required characteristics of the alignment film precisely because the quantity of light is not easily controlled, so the surface of the alignment film is damaged after exposure. Specially designed alignment film cannot achieve a stable high pretilt angle and is not cost effective as well.
In view of the drawbacks of the prior arts, the present invention provides a method of feasible control the high pretilt angle of liquid crystal molecules. The method uses a step of coating the vertical alignment film, and a step of treating the surface with particle beam and a rubbing step afterward to achieve a high pretilt angle of the LC molecules. The exchange for the sequence of surface treating step and the rubbing step can also produce the high LC pretilt angle. Since the pretilt angle of the LC molecules is relative to the side chains density of the alignment film's surface, the present invention uses the particle beam generated by plasma or ions to process the surface treatment of the alignment film of the LCD, so as to adjust the density of the side chains and to change the pretilt angle of the LC molecules.
The present invention differs from the prior art in that the prior art requires a blend of the vertical and horizontal alignment films to achieve a higher pretilt angle under specific conditions. The present invention merely requires a vertical alignment film and a surface treatment to control the density of the side chains of the alignment film's surface.
A preferred embodiment of the method of controlling the pretilt angle of the LC molecule is adopted on a liquid crystal panel with an optical compensation birefringence (OCB) mode. The steps thereof comprise: preparing a vertical alignment film on a substrate, such as the step of roller coating, scraper coating spin coating or inkjet printing, so as to form a vertical alignment film. Moreover, an inorganic vertical alignment film, such as fluorinated diamond-like carbon (F-DLC), can be made by the step of sputtering or plasma enhanced chemical vapor deposition (PECVD). Next, a particle beam generated by the plasma or ion beam performs a surface treatment on the surface of the vertical alignment film, and performs an alignment treatment thereon consequently. In conclusion, the side chain of the above vertical alignment film is changed by the particle beam generated by the plasma or ionic beam, so as to control the pretilt angle of the molecules.
The preferred embodiment of the aforementioned particle beam is generated by the ions or plasma. By means of controlling the energy, quantity, incident angle, or even the types of the particle beam, the density and distribution of the side chains of the vertical alignment film are changed, thereby controlling the pretilt angle of the LC molecules.
The present invention will be readily understood by the following detailed description in conjunction with accompanying drawings, in which:
To understand the technology, means and functions adopted in the present invention further, reference is made to the following detailed description and attached drawings. The invention shall be readily understood deeply and concretely from the purpose, characteristics and specifications. Nevertheless, the present invention is not limited to the attached drawings and embodiments in the following description.
The present invention relates to a manufacturing method of a liquid crystal device, and the method for controlling a pretilt angle of the liquid crystal molecules thereof. In view of the connection between the LC pretilt angle and the density of the alignment film side chains thereof, an ionic beam generated by plasma or ions is used to treat the surface on the alignment film of the LCD, so as to adjust the density of the side chains. Thereby, the pretilt angle of the LC molecules can be changed. The present invention differs from the conventional art requiring a special combination of the vertical and horizontal alignment films to implement higher pretilt angle. In the present invention only the vertical alignment film including the material and solution thereof is used for the present invention. Furthermore a surface treatment and an alignment step are performed to implement the required density of the side chains and the surface anisotropy of the alignment film.
Reference is made to
The preferred embodiment of the present invention uses a single alignment film, such as a vertical alignment layer, sandwiched between the top substrate and the bottom substrate, adjusting the density of the side chains by a surface treating step for generating a stable alignment film of the liquid crystal molecules with a high pretilt angle. The vertical alignment layer processes the surface treatment via the particle beam using ions or plasma. After the step of orientating the alignment direction, the liquid crystal device is fabricated to implement a fast response LCD, i.e OCB. The scheme using the particle beam mentioned above can precisely control the energy, quantity, incident angle, or even the types of the beam. Thereby the density and proportion of the side chains of the alignment film can be changed to affect the pretilt angle of the LC molecules. Specifically, the present invention can obtain a pretilt angle from 5 to about 85 degree, depends on the extent of the surface treating step.
For achieving a specific pretilt angle needless of an external voltage for splay to bend transformation as in the conventional art, the particle beam using plasma or ions is used to treat the surface of the alignment film to reach the high pretilt angle of the LC molecules of the present invention. The above-mentioned scheme not only eliminates the step of converting LC molecules from the splay state to the bend state, but also causes the LC molecules to have a stable bend state for increasing the response of the LCD.
Next, the vertical alignment film is treated with an alignment step for producing surface anisotropy after the surface treatment. In the preferred embodiment, after the surface treatment of the vertical alignment film, a polar alignment is accomplished. Next, a step of roller rubbing is used for the alignment in an azimuthal direction.
The step of treating the surface is performed before the step of alignment mentioned above. The step of the alignment can be performed before the step of treating the surface in another embodiment. The proportion of the vertical alignment and the horizontal alignment of the LC molecules are determined by the above-mentioned surface treatment of the vertical alignment film, so as to control the pretilt angle of the LC molecules.
Consequently, the top substrate and the bottom substrate are assembled together, and the liquid crystal is injected for fabricating the LCD. The preferred embodiment of the present invention provides the OCB liquid crystal panel (step S509).
The aforementioned particle beam performs the surface treatment to control the density of the side chains by controlling some particle beam parameters. The pretilt angle of the LC molecules is then controlled. The particle beam can be used to control the surface energy of the alignment film precisely, and the incident angle thereof can be a vertical or an oblique angle. Since the particles generated from the ionic beam or the plasma beam only reach the surface of the alignment film, the effective depth of the surface treatment of the present invention is shallower than the depth of the surface treatment using light of the conventional art. Therefore, it s not easy to have unstable electric or thermal problems.
The particle beam of the preferred embodiment ranges between 50 eV and 3000 eV, and the compound of the particles is one of hydrogen ion, nitrogen ion, oxygen ion, fluorine ion, and argon ion, or a combination of hydrogen ion, nitrogen ion, oxygen ion, fluorine ion or argon ion. However, the compound of the particle beam is not limited to the above mention. The material of the substrate includes glass, plastic, flexible material and metal. The implementation is not limited in this embodiment.
To sum up, the method for controlling the pretilt angle of the LC molecules of the present invention uses a particle beam, such as an ionic beam or a plasma beam, to treat the surface of the alignment film by impacting the film and side chains. After the surface treatment, the density of the side chains is changed in response to the conditions of the particle beam or gas therein, so as to change the density and distribution. Therefore, the pretilt angle of the LC molecules in the surface of alignment film is determined.
The many features and advantages of the present invention are apparent from the written description above and it is intended by the appended claims to cover all. Furthermore, since numerous modifications and changes will readily occur to those skilled in the art, it is not desired to limit the invention to the exact construction and operation as illustrated and described. Hence, all suitable modifications and equivalents may be resorted to as falling within the scope of the invention.
Number | Date | Country | Kind |
---|---|---|---|
95117020 A | May 2006 | TW | national |
Number | Name | Date | Kind |
---|---|---|---|
5579141 | Suzuki et al. | Nov 1996 | A |
5604615 | Iwagoe et al. | Feb 1997 | A |
5623354 | Lien et al. | Apr 1997 | A |
5629056 | Koike et al. | May 1997 | A |
5697192 | Inoue et al. | Dec 1997 | A |
5710608 | Nakabayashi et al. | Jan 1998 | A |
5711999 | Yamada et al. | Jan 1998 | A |
5764326 | Hasegawa et al. | Jun 1998 | A |
5855968 | Hirata et al. | Jan 1999 | A |
6067141 | Yamada et al. | May 2000 | A |
6115098 | Kume et al. | Sep 2000 | A |
6124914 | Chaudhari et al. | Sep 2000 | A |
6246458 | Koma et al. | Jun 2001 | B1 |
6519018 | Samant et al. | Feb 2003 | B1 |
6630975 | Terashita | Oct 2003 | B1 |
6724449 | Andry et al. | Apr 2004 | B1 |
6852374 | Mizusaki et al. | Feb 2005 | B2 |
7227606 | Takeda et al. | Jun 2007 | B2 |
20040119924 | Takeda et al. | Jun 2004 | A1 |
Number | Date | Country | |
---|---|---|---|
20070263151 A1 | Nov 2007 | US |