Claims
- 1. A method of controlling uniformity of temperature and peak temperature of an exterior surface of a rapidly heated substrate comprising coating a thin layer of an essentially homogenous slurry of a selected mass of a solid fuel, which comprises an metal-containing oxidizing agent and a reducing agent in a defined ratio, on a portion of an interior surface of the substrate to be heated.
- 2. The method of claim 1, wherein said coating is a dip coating, spray coating, roller coating, gravure coating, reverse roll coating, gap coating, metering rod coating, slot die coating, curtain coating, and air knife coating.
- 3. The method of claim 2, wherein said gap coating is done with a wire wound coating rod.
- 4. The method of claim 1, wherein the peak temperature of the substrate upon heating is controlled by selecting and coating a mass of solid fuel determined to give that peak temperature.
- 5. The method of claim 1, wherein the substrate is selected from a metal, an alloy, and a ceramic.
- 6. The method claim 5, wherein the substrate is a metal foil.
- 7. The method of claim 6, wherein the metal foil exhibits a thickness ranging from 0.001 inches to 0.010 inches.
- 8. The method of claim 1, wherein the thin layer of solid fuel exhibits a thickness ranging from 0.001 inches to 0.030 inches.
- 9. The method of claim 1, wherein the thin layer of solid fuel exhibits a thickness ranging from 0.001 inches to 0.005 inches.
- 10. The method of claim 1, wherein the metal containing oxidizing agent is selected from at least one of the following MoO3, KClO4, KClO3, and Fe2O3.
- 11. The method of claim 1, wherein the metal reducing agent is selected form at least one of the following: aluminum, zirconium, iron, and titanium.
- 12. The heating unit of claim 1, wherein the amount of metal reducing agent ranges from 60% by weight to 90% by weight of the total dry weight of the solid fuel.
- 13. The heating unit of claim 1, wherein the amount of metal-containing oxidizing agent ranges from 10% by weight to 40% by weight of the total dry weight of the solid fuel.
- 14. The heating unit of claim 1, wherein the solid fuel comprises at least one additive material.
- 15. The method of claim 14, wherein said additive material is an inorganic material.
- 16. The method of claim 15, wherein the inorganic material is selected from the group consisting of clays, metal alkoxides, sodium silicates, potassium silicates, aluminum silicates, alumina, silica based sol and inorganic sol-gel material.
- 17. The method of claim 16, wherein the clay is selected from the group consisting of: Laponite, Montmorillonite, and Cloisite.
- 18. A method for providing an essentially homogenous and uniform coating of dry solid fuel on a surface of a substrate comprising:
a. mixing a solid fuel, comprising at least one oxidizing agent and at least one reducing agent, with an additive material in a solvent to form a homogenous slurry; b. coating a thin layer of the slurry at a set thickness on an surface of a substrate; and c. drying the coated slurry to form a dry solid fuel on the substrate.
- 19. The method of claim 18, wherein said coating is dip coating, spray coating, roller coating, gravure coating, reverse roll coating, gap coating, metering rod coating, slot die coating, curtain coating, and air knife coating.
- 20. The method of claim 19, wherein said gap coating is done with a wire wound coating rod in a bar coater.
- 21. The method of claim 18, wherein prior to coating a mask is positioned on a portion of the surface of the substrate to prevent deposition of the solid fuel on said portion.
- 22. The method claim 18, wherein the substrate is a metal foil.
- 23. The method of claim 22, wherein the metal foil exhibits a thickness ranging from 0.001 inches to 0.010 inches.
- 24. The method of claim 18, wherein the thin layer of solid fuel exhibits a thickness ranging from 0.001 inches to 0.030 inches.
- 25. The method of claim 18, wherein the thin layer of solid fuel exhibits a thickness ranging from 0.001 inches to 0.005 inches.
- 26. The method of claim 18, wherein the metal containing oxidizing agent is selected from at least one of the following MoO3, KClO4, KClO3, and Fe2O3.
- 27. The method of claim 18, wherein the metal reducing agent is selected from at least one of the following: aluminum, zirconium, iron, and titanium.
- 28. The method of claim 18, wherein said additive material is an inorganic material.
- 29. The method of claim 18, wherein the additive material is Laponite.
- 30. The method of claim 18, wherein said drying is in an oven for at least two hours.
- 31. A heating unit that upon firing rapidly heats a defined area of an exterior surface of a substrate to an essentially uniform temperature and a set peak temperature comprising:
a. an enclosure comprising at least one substrate having an exterior surface and an interior surface, b. an essentially homogenous and thin layer of solid fuel coated on the interior surface of the substrate corresponding to the defined area of the exterior surface of the substrate to be heated; and c. an igniter disposed within the enclosure for igniting the solid fuel.
- 32. The heating unit of claim 31, wherein the peak temperature is set by the mass of solid fuel coated on the interior surface of the substrate.
- 33. The method of claim 31, wherein the thin layer of solid fuel exhibits a thickness ranging from 0.001 inches to 0.030 inches.
- 34. The method of claim 31, wherein the thin layer of solid fuel exhibits a thickness ranging from 0.001 inches to 0.005 inches.
- 35. The method of claim 31, wherein the enclosure comprises more than one substrate.
- 36. The method of claim 31, wherein the substrate is a metal foil.
- 37. The method of claim 31, wherein the metal containing oxidizing agent is selected from at least one of the following MoO3, KClO4, KClO3, and Fe2O3.
- 38. The method of claim 31, wherein the metal reducing agent is selected from at least one of the following: aluminum, zirconium, iron, and titanium.
- 39. The method of claim 31, wherein the solid fuel comprises at least one additive material.
- 40. The method of claim 39, wherein the additive material is Laponite.
REFERENCE TO RELATED APPLICATIONS
[0001] This application is a continuation-in-part and claims priority to U.S. provisional application Ser. No. 60/472,697 entitled “Self-Contained Heating Unit and Drug-Supply Unit Employing Same,” filed May 21, 2003, Hale et al., the entire disclosure of which is hereby incorporated by reference.
Provisional Applications (1)
|
Number |
Date |
Country |
|
60472697 |
May 2003 |
US |