The disclosure relates generally to superalloy parts, and more particularly, to methods of forming a desired geometry on a superalloy part.
High performance industrial parts are oftentimes made of superalloys. Where damage or wear occur to these parts that creates voids, such as in turbine blades, it is desirable to repair the parts to a desired geometry matching the originally manufactured part. Currently, brazing is the main approach to repair superalloy parts. In brazing, a molten material is formed in the repair location, and the material is allowed to cool. Brazing poses a number of challenges. Brazing is ideally carried out on a repair location that is horizontal so the flow of molten material can be controlled to not overflow the repair location. However, many repair locations are not position-able in a perfectly horizontal orientation, such as vertical or curved surfaces. As a result, multiple brazing processes that are time consuming and complicated are performed to address these types of repairs. Another challenge is that many superalloy parts are manufactured to very precise dimensions, for example, using computer controlled additive manufacturing techniques. Using brazing techniques to repair a superalloy part does not allow for the same level of precision as the original manufacturing, resulting in parts that do not meet original dimensional specifications for the part.
A first aspect of the disclosure provides a method of forming a desired geometry at a location on a superalloy part, the method comprising: directing particles of a powder mixture including a low melt temperature superalloy powder and a high melt temperature superalloy powder to the location on the superalloy part at a velocity sufficient to cause the superalloy powders to deform and to form a mechanical bond but not metallurgical bond to the superalloy part; continuing the directing of particles until the desired geometry is formed; and applying heat to the superalloy part including the powder mixture, the heat causing the low melt temperature superalloy powder to melt, creating a metallurgical bond with the superalloy part, wherein the low melt temperature superalloy powder has a melt temperature less than 1287° Celsius (° C.), and the high melt temperature superalloy powder has a melt temperature greater than 1287° C.
A second aspect of the disclosure provides a method, including: creating a preform by directing particles of a powder mixture including a low melt temperature superalloy powder and a high melt temperature superalloy powder onto a build plate at a velocity sufficient to cause the superalloy powders to deform and to form a mechanical bond but not a metallurgical bond to the build plate; and applying heat to the preform after having the preform: removed from the build plate, shaped into a desired geometry for a location of a superalloy part, and positioned in the location of the superalloy part, wherein the heat applying causes the low melt temperature superalloy powder to melt and form a metallurgical bond with the superalloy part, wherein the low melt temperature superalloy powder has a melt temperature less than 1287° Celsius (° C.), and the high melt temperature superalloy powder has a melt temperature greater than 1287° C.
A third aspect of the disclosure includes a method, including: creating a preform by directing particles of a powder mixture including a low melt temperature superalloy powder and a high melt temperature superalloy powder onto a build plate at a velocity sufficient to cause the superalloy powders to deform and to form a mechanical bond but not a metallurgical bond to the build plate; and removing the preform from the build plate allowing subsequent shaping into a desired geometry for a location on a superalloy part, wherein the low melt temperature superalloy powder has a melt temperature less than 1287° Celsius (° C.), and the high melt temperature superalloy powder has a melt temperature greater than 1287° C.
The illustrative aspects of the present disclosure are designed to solve the problems herein described and/or other problems not discussed.
These and other features of this disclosure will be more readily understood from the following detailed description of the various aspects of the disclosure taken in conjunction with the accompanying drawings that depict various embodiments of the disclosure, in which:
It is noted that the drawings of the disclosure are not necessarily to scale. The drawings are intended to depict only typical aspects of the disclosure and therefore should not be considered as limiting the scope of the disclosure. In the drawings, like numbering represents like elements between the drawings.
As an initial matter, in order to clearly describe the subject matter of the current disclosure, it will become necessary to select certain terminology. To the extent possible, common industry terminology will be used and employed in a manner consistent with its accepted meaning. Unless otherwise stated, such terminology should be given a broad interpretation consistent with the context of the present application and the scope of the appended claims. Those of ordinary skill in the art will appreciate that often a particular component may be referred to using several different or overlapping terms. What may be described herein as being a single part may include and be referenced in another context as consisting of multiple components. Alternatively, what may be described herein as including multiple components may be referred to elsewhere as a single part.
In addition, several descriptive terms may be used regularly herein, as described below. The terms “first,” “second,” and “third” may be used interchangeably to distinguish one component from another and are not intended to signify location or importance of the individual components.
The terminology used herein is for the purpose of describing particular embodiments only and is not intended to be limiting of the disclosure. As used herein, the singular forms “a,” “an” and “the” are intended to include the plural forms as well, unless the context clearly indicates otherwise. It will be further understood that the terms “comprises” and/or “comprising,” when used in this specification, specify the presence of stated features, integers, steps, operations, elements, and/or components but do not preclude the presence or addition of one or more other features, integers, steps, operations, elements, components, and/or groups thereof. “Optional” or “optionally” means that the subsequently described event or circumstance may or may not occur or that the subsequently describe component or element may or may not be present, and that the description includes instances where the event occurs or the component is present and instances where it does not or is not present.
Where an element or layer is referred to as being “on,” “engaged to,” “connected to” or “coupled to” another element or layer, it may be directly on, engaged to, connected to, or coupled to the other element or layer, or intervening elements or layers may be present. In contrast, when an element is referred to as being “directly on,” “directly engaged to,” “directly connected to” or “directly coupled to” another element or layer, there may be no intervening elements or layers present. Other words used to describe the relationship between elements should be interpreted in a like fashion (e.g., “between” versus “directly between,” “adjacent” versus “directly adjacent,” etc.). As used herein, the term “and/or” includes any and all combinations of one or more of the associated listed items.
As indicated above, the disclosure provides methods of forming a desired geometry at a location on a superalloy part. The methods may include directing particles of a powder mixture including a low melt temperature superalloy powder and a high melt temperature superalloy powder to the location on the superalloy part at a velocity sufficient to cause the superalloy powders to deform and to form a mechanical bond but not metallurgical bond to the superalloy part. The low melt temperature superalloy powder has a melt temperature less than 1287° Celsius (° C.), and the high melt temperature superalloy powder has a melt temperature greater than 1287° C. The particle directing can continue until the desired geometry is formed on the superalloy part. The methods may also include applying heat to the superalloy part and the powder mixture on the repair location. The heat is sufficient to cause the low melt temperature superalloy powder to melt, creating a metallurgical bond at the location. The methods may also include forming a preform on a build plate using the particle directing. The preform may be removed from the build plate, shaped to a desired geometry, and positioned in a location on a superalloy part. Applying heat then melts the low melt temperature superalloy powder (brazes) in place on the superalloy part, forming a metallurgical bond therewith. Any minor machining necessary to bring the repaired superalloy part to match desired dimensional specifications can be carried out thereafter.
Superalloy part 100 may include a repair location 102 in which a repair is desired. In one example, superalloy part 100 may have been originally manufactured, for example, using computer controlled additive manufacturing techniques. In another example, superalloy part 100 may have been manufactured by casting.
As shown in
As shown in
The directing of particles of powder mixture 110 can continue, as shown in
Once hardened, any minor machining of location 102 can be performed, e.g., polishing, etc. As understood in the art, any variety of additional protective coatings, e.g., bond coatings, thermal barrier coatings, etc., can then be applied.
Referring to
Once in position, as shown in
Each of the steps of forming of preform 166, removing preform 166 from build plate 162, shaping preform 166 into preform 172, and positioning preform 172 may be carried out at different locations, and by different actors. Consequently, this embodiment of the method allows for flexibility in repair. For example, the process allows an original equipment manufacturer (OEM) to provide preform 166 (with or without build plate 162) to a service location for superalloy parts 100, and either the OEM or another service provider may remove build plate 162 (where still provided), shape preform 172 as necessary, and carry out the actual repair by positioning preform 172 and applying the heat to preform 172 and superalloy part 100. Preform 172 can be additionally customized, e.g., shaped, or dimensioned, on location where the part is being repaired. Hence, another embodiment of a method according to embodiments of the disclosure may only include the preform 166 creating, and removing preform 166 from build plate 162 allowing subsequent shaping into a desired geometry for location 102 on superalloy part 100. It will also be recognized that an OEM may provide preform 172 already shaped for use.
Embodiments of the disclosure provide methods of repairing superalloy parts, such as precisely dimensioned additively manufactured parts, via a cold spray and brazing process. The powder mixture is composed of low melt and high melt temperature superalloy powders. The powder mixture can be automatically controlled to deposit uniformly on the to-be coated surface by using the cold spray system. Alternatively, the process can be used to create a preform for a repair location. The embodiments described herein provide an effective method to repair hard-to-weld superalloy parts, such as superalloy additively manufactured parts. That said, the methods described herein can also be used to repair cast, forged, and/or welded parts. The repair location has a near net shape after brazing, i.e., it is at or near the desired geometry. In addition, the repair can have a uniform thickness after coat spray buildup and the braze thermal cycle. The methods allow brazing multiple locations (flat or vertical, or overhead) in one braze cycle. The process is easier to implement, and can be controlled to remove human errors. The resulting repair can include dense material, e.g., up to 99%.
The foregoing drawings show some of the processing associated according to several embodiments of this disclosure. In this regard, each drawing may represent a step associated with embodiments of the methods described. It should also be noted that in some alternative implementations, the acts noted in the drawings may occur out of the order noted in the figure or, for example, may in fact be executed substantially concurrently or in the reverse order, depending upon the act involved. Also, one of ordinary skill in the art will recognize that additional steps that describe the processing may be added.
Approximating language, as used herein throughout the specification and claims, may be applied to modify any quantitative representation that could permissibly vary without resulting in a change in the basic function to which it is related. Accordingly, a value modified by a term or terms, such as “about,” “approximately” and “substantially,” are not to be limited to the precise value specified. In at least some instances, the approximating language may correspond to the precision of an instrument for measuring the value. Here and throughout the specification and claims, range limitations may be combined and/or interchanged; such ranges are identified and include all the sub-ranges contained therein unless context or language indicates otherwise. “Approximately,” as applied to a particular value of a range, applies to both end values and, unless otherwise dependent on the precision of the instrument measuring the value, may indicate +/−10% of the stated value(s).
The corresponding structures, materials, acts, and equivalents of all means or step plus function elements in the claims below are intended to include any structure, material, or act for performing the function in combination with other claimed elements as specifically claimed. The description of the present disclosure has been presented for purposes of illustration and description but is not intended to be exhaustive or limited to the disclosure in the form disclosed. Many modifications and variations will be apparent to those of ordinary skill in the art without departing from the scope and spirit of the disclosure. The embodiment was chosen and described in order to best explain the principles of the disclosure and the practical application and to enable others of ordinary skill in the art to understand the disclosure for various embodiments with various modifications as are suited to the particular use contemplated.
This application is a Divisional Application of U.S. patent application Ser. No. 17/079,829, filed Oct. 26, 2020, the entire contents of which are fully incorporated herein.
| Number | Date | Country | |
|---|---|---|---|
| Parent | 17079829 | Oct 2020 | US |
| Child | 17816472 | US |