Conventionally, some portable electronic devices use glass as a part of their devices, either internal or external. Externally, a glass part can be provided as part of a housing, such a glass part is often referred to as a cover glass. The transparent and scratch-resistance characteristics of glass make it well suited for such applications. Internally, glass parts can be provided to support display technology. More particularly, for supporting a display, a portable electronic device can provide a display technology layer beneath an outer cover glass. A sensing arrangement can also be provided with or adjacent the display technology layer. By way of example, the display technology layer may include or pertain to a Liquid Crystal Display (LCD) that includes a Liquid Crystal Module (LCM). The LCM generally includes an upper glass sheet and a lower glass sheet that sandwich a liquid crystal layer therebetween. The sensing arrangement may be a touch sensing arrangement such as those used to create a touch screen. For example, a capacitive sensing touch screen can include substantially transparent sensing points or nodes dispersed about a sheet of glass or plastic.
Unfortunately, however, use of glass with portable electronic devices requires that the glass be relatively thin. Generally speaking, the thinner the glass the more susceptible the glass is to damage when the portable electronic device is stressed or placed under a significant force. Chemically strengthening has been used to strengthen glass. While chemically strengthening is effective, there is a continuing need to provide improved ways to provide cover glass that is thin and sufficiently strong to resist breakage.
The invention relates to transparent structures for portions of electronic device housings. The transparent structures are formed from multiple layers of transparent (optically clear) materials. The multiple layers can include at least an outer glass layer and one or more other transparent layers that can be either glass or polymer layers. The multiple layers can be bonded together with one or more lamination layers. Accordingly, multi-layer transparent structures that are formed from multiple layers bonded together are able to be not only thin but also sufficiently strong and resistant to damage. The multi-layer transparent structures are well suited for use in consumer products, such as consumer electronic devices (e.g., portable electronic devices).
The invention can be implemented in numerous ways, including as a method, system, device, or apparatus. Several embodiments of the invention are discussed below.
As an electronic device, one embodiment can, for example, include at least an outer housing for the electronic device, and a plurality of electrical components provided within the outer housing. At least a portion of the outer housing can include at least a multi-layer housing structure. The multi-layer housing structure can include a first layer, a lamination layer, and a second layer. The first layer and second layer can be laminated together via the lamination layer.
As a consumer electronic product, one embodiment can, for example, include at least: a housing having a front surface, a back surface and side surfaces; electrical components provided at least partially internal to the housing, the electrical components including at least a controller, a memory, and a display, the display being provided at or adjacent the front surface of the housing; and a multi-layer cover structure provided at, over or in the front surface of the housing such that it is provided over the display. The multi-layer cover structure can include a first layer, a lamination layer and a second layer, and the first layer and second layer can be laminated together via the lamination layer.
As a method for forming a laminated glass structure, one embodiment can, for example, include at least the acts of: obtaining an outer glass layer, chemically strengthening the outer glass layer, obtaining a transparent layer, obtaining a lamination layer, and laminating the transparent layer to the outer glass layer via the lamination layer to form the laminated glass structure.
As a method for forming a laminated glass structure, one embodiment can, for example, include at least the acts of: obtaining a first glass layer, chemically strengthening the first glass layer, obtaining a second glass layer, chemically strengthening the second glass layer, obtaining a lamination layer, and forming the lamination glass structure from the first glass layer, the lamination layer and the second glass layer.
Other aspects and advantages of the invention will become apparent from the following detailed description taken in conjunction with the accompanying drawings which illustrate, by way of example, the principles of the invention.
The invention will be readily understood by the following detailed description in conjunction with the accompanying drawings, wherein like reference numerals designate like structural elements, and in which:
The invention relates to transparent structures for portions of electronic device housings. The transparent structures are formed from multiple layers of transparent (optically clear) materials. The multiple layers can include at least an outer glass layer and one or more other transparent layers that can be either glass or polymer layers. The multiple layers can be bonded together with one or more lamination layers. Accordingly, multi-layer transparent structures that are formed from multiple layers bonded together are able to be not only thin but also sufficiently strong and resistant to damage. Since the transparent structures include at least one glass layer, the transparent structures can also be referred to as glass articles (or multi-layer glass articles). The multi-layer transparent structures are well suited for use in consumer products, such as consumer electronic devices (e.g., portable electronic devices).
Embodiments of the invention can relate to apparatus, systems and methods for improving strength of a glass article for a consumer product, such as a consumer electronic device. In one embodiment, the glass article may be an outer surface of a consumer electronic device. For example, the glass article may, for example, correspond to a glass cover that helps form part of a display area of the electronic device (i.e., situated in front of a display either as a separate part or integrated within the display). As another example, the glass article may form a part of a housing for the consumer electronic device (e.g., may form an outer surface other than in the display area). In another embodiment, the glass article may be an inner component of a consumer electronic device. For example, the glass article can be a component glass piece of a LCD display provided internal to the housing of the consumer electronic device.
The apparatus, systems and methods for improving strength of thin glass articles are especially suitable for glass covers or displays (e.g., LCD displays), particularly those assembled in small form factor electronic devices such as handheld electronic devices (e.g., mobile phones, media players, personal digital assistants, remote controls, etc.). The glass articles can be thin in these small form factor embodiments, such as less than 3 mm, or more particularly between 0.3 and 2.5 mm. The apparatus, systems and methods can also be used for glass covers or displays for other devices including, but not limited to, relatively larger form factor electronic devices (e.g., portable computers, tablet computers, displays, monitors, televisions, etc.). The glass articles can also be thin in these larger form factor embodiments, such as less than 5 mm, or more particularly between 0.3 and 3 mm.
Embodiments of the invention are discussed below with reference to
The multi-layer housing structure 100 has a multi-layer structure. In particular, the multi-layer housing structure 100 includes a glass layer 102 that provides an outer surface for the multi-layer housing structure 100, and thus also for at least a portion of the outer housing for the electronic device. The multi-layer housing structure 100 also includes a lamination layer 104 as well as a transparent layer 106. The lamination layer 104 serves to bond together the glass layer 102 and the transparent layer 106. The bonding together of the glass layer 102 and the transparent layer 106 via the lamination layer 104 can be denoted as a lamination, whereby the multi-layer housing structure 100 is formed from the lamination of the transparent layer 106 to the glass layer 102 using the lamination layer 104.
Typically, the multi-layer housing structure 100 is to be optically clear or transparent. The glass layer 102 and the transparent layer 106 are inherently optically clear or transparent. The lamination layer 104 is also optically clear or transparent. Although it is desired that the distinct layers of the multi-layer housing structure 100 be optically clear or transparent, it is understood that certain materials may not be completely optically clear or transparent, thus, it is sufficient that these layers be substantially optically clear when formed into the multi-layer housing structure 100. Also, in some embodiments, the lamination layer 104 might be initially opaque before being activated to bond with other layers of the multi-layer housing structure 100; however, once the lamination layer 104 is activated, the lamination layer 104 turns clear or transparent (at least substantially so).
The transparent layer 106 is typically an internal layer that does not form an outer user surface for the housing for the electronic device. As a result, the transparent layer 106 can use different materials depending upon its particular product application. As an example, the transparent layer 106 can correspond to a glass layer or can correspond to a polymer-based layer.
In one embodiment, the lamination layer 104 can be referred to as a lamination film. The lamination layer 104 can pertain to any material that is suitable for lamination of the glass layer 102 with the transparent layer 106. One example of a lamination material is polyvinyl butyral (PVB). PVB is a resin that provides strong binding, optical clarity, adhesion to many surfaces, toughness and flexibility. Other examples of lamination materials include thermoplastic polyurethane (TPU).
In
Although the widths of the glass layer 102, the lamination layer 104 in the transparent layer 106 illustrated in
The lamination process 300 initially obtains 302 an outer glass layer. The outer glass layer can serve as one side of the laminated structure can be formed or assembled. The outer glass layer can then be chemically strengthened 304. By chemically strengthening the outer glass layer, the outer glass layer is better able to resist damage (such as breakage), such as when subjected to an impact event.
In addition, a transparent layer is obtained 306. The transparent layer can serve as an inner layer or an intermediate layer for the multi-layer structure. The transparent layer can be formed of glass or can be formed of a polymer. A lamination layer can also be obtained 308. The lamination layer is a thin layer of a material that can serve to laminate together the outer glass layer to the transparent layer. Hence, the lamination process 300 then operates to laminate 310 the transparent layer with the outer glass layer via the lamination layer, thereby forming a laminated structure. For example, the lamination layer can be between the outer glass layer and the transparent layer, and then lamination can cause the lamination layer to bond to adjacent surfaces of the outer glass layer and the transparent layer.
To laminate 310 the transparent layer with the outer glass layer, the lamination layer typically needs to be activated, such as by heating the lamination layer or inducing energy (e.g., RF energy) into the lamination layer. The lamination serves to strongly bond, e.g., fuse, together the outer glass layer and the transparent layer. Following the lamination 310, the lamination process 300 is complete and can therefore end.
The lamination process 400 can obtain 402 a first glass layer. The first glass layer can then be chemically strengthened 404. By chemically strengthening the first glass layer, the first glass layer is better able to resist damage (such as breakage), such as when subjected to an impact event.
In addition, as second glass layer can be obtained 406. Similarly, the second glass layer can be chemically strengthened 408. By chemically strengthening the second class layer, the second glass layer is better able to resist damage (such as breakage), such as when subjected to an impact event. In one embodiment, the chemical strengthening 404 applied to the first glass layer is performed to a different level, degree or state than is the chemical strengthening applied to the second class layer. In other words, it may be desirable to chemically strengthen the different glass layers of the multi-layer housing structure in different ways. Specifically, in one example, the outer glass layer could be chemically strengthened to provide a relatively deep depth of layer, whereas an inner layer or the second glass layer can have a smaller depth of layer but a higher compressive stress.
Still further, the lamination process 400 obtains 410 a lamination layer. The lamination layer can be used to form 412 the laminated glass structure from the first glass layer and the second glass layer after the laminated glass structure has been formed 412, the lamination process 400 can and.
The electronic device housing 700 includes a housing 702. The housing 702 include a side member 704 and a bottom member 706. A multi-layer translucent member 708 can be provided as a top surface for the electronic device housing 700. For example, the multi-layer translucent member 708 can be a multi-layer structure, often referred to as a cover glass, which can include at least one glass layer (glass member) and may also include at least one polymer-based layer (polymer-based member). For example, the polymer-based layer(s), if provided, can be formed of plastic. In different embodiment, the multi-layer translucent member 708 can be implemented as shown in
The electronic device housing 700 can include a display screen assembly 710. The display screen assembly 710 can be secured to a bottom surface of the translucent member 708 by a layer of adhesive 812 (e.g., translucent adhesive). The display screen assembly 710 can include one or a plurality of distinct technology components that can be laminated together. In one implementation, the technology components can, for example, include a sensing layer (e.g., touch sensors), a display technology layer (e.g., LCD panel) and/or a backlight layer. In another implementation, the technology components can, for example, include an organic light emitting diode (OLED) panel with or without a sensing layer (e.g., touch sensors).
In addition, however, the electronic device housing 700 depicts one embodiment of the display screen assembly 710 has having at least three (3) distinct technology layers, namely, a Liquid Crystal Display (LCD) panel layer 710a (e.g., TFT LCD), a touch sensing layer 710b and a backlight layer 710c. These layers themselves can include multiple layers or additional layers can also be present, such as polarizers, color filters, etc.
An internal space 718 is provided internal to the electronic device housing 700 whereby various electrical components (e.g., including processor, memory, battery and circuit board) can be attached, affixed or placed so as to provide electronic operations for the electronic device.
In general, the various members, parts or assemblies of the electronic device housing 700 can be formed of any of a variety of materials, e.g., glass, polymers or metal. In one embodiment, the multi-layer translucent member 708 is at least partially formed of glass, and the housing 702 is formed from glass, polymer (e.g., plastic) or metal.
Additionally, it should be understood that one or more of the layers of the display screen assembly 710 could be integrated with the multi-layer translucent member 708. In one example, the LCD panel layer 710a could be integrated with the multi-layer translucent member 708 such as by being bonded (e.g., laminated) to the bottom surface of the multi-layer translucent member 708. In another example, the LCD panel layer 710a and the touch sensing layer 710b could be integrated with the multi-layer translucent member 708 such as by being successively bonded (e.g., laminated) to the bottom surface of the multi-layer translucent member 708. In still another example, the LCD panel layer 710a, the touch sensing layer 710b and the backlight layer 710c could be integrated with the multi-layer translucent member 708 such as by being successively bonded (e.g., laminated) to the bottom surface of the multi-layer translucent member 708. An adhesive layer can be used to secure any of the remaining layers of the display screen assembly 710 not integrated to the multi-layer translucent member 708 through lamination.
The housing 802 may have any suitable shape, including, for example, one or more elements that may be combined to form a rectangular structure. The housing 802 may at least partially enclose an inner volume in which electronic device components may be assembled and retained. The shape of the housing 802 may substantially define boundaries of the inner volume, and may be determined based upon the size and type of components placed within the inner volume.
The housing 802 may have any suitable size, and the size may be determined based on any suitable criteria. Suitable criteria may include, but are not limited to including, aesthetics or industrial design, structural considerations, components required for a desired functionality, and/or product design. The housing 802 may have any suitable cross-section, including for example a variable cross-section or a constant cross-section. In some embodiments, the cross-section may be selected based on desired structural properties for the housing 802. For example, the cross-section of housing 802 may be substantially rectangular, such that the height of the housing 802 is substantially larger than the width of the housing 802. Such a cross-sectional shape may provide structural stiffness in compression and tension, as well as in bending. In some embodiments, the dimensions of the housing 802 cross-section may be determined relative to the dimensions of the components contained by housing 802.
In some embodiments, the housing 802 may include features 810. The features 810 may generally include one or more openings, knobs, extensions, flanges, chamfers, or other features for receiving components or elements of the device. The features 810 of the housing 802 extend from any surface of housing 802, including for example from internal surfaces, e.g., to retain internal components or component layers, or from external surfaces. In particular, the housing 802 may include a slot or opening (not shown) for receiving a card or tray within the handheld electronic device 800. The housing 802 may also include a connector opening (not shown), e.g., for a 30-pin connector, through which a connector may engage one or more conductive pins of the handheld electronic device 800. Other features 810 included on the housing 802 may include, but are not limited to, an opening for providing audio to a user, an opening for receiving audio from a user, an opening for a connector (e.g., audio connector or power supply connector), and/or features for retaining and enabling a button such as a volume control or silencing switch.
As noted above, the electronic device can be a handheld electronic device or a portable electronic device. The invention can serve to enable a glass cover to be not only thin but also adequately strong. Since handheld electronic devices and portable electronic devices are mobile, they are potentially subjected to various different impact events and stresses that stationary devices are not subjected to. As such, the invention is well suited for implementation of glass surfaces for handheld electronic device or a portable electronic device that are designed to be thin.
The strengthened glass, e.g., glass covers or cover windows, is particularly useful for thin glass applications. For example, the thickness of a glass cover being strengthened can be between about 0.5-2.5 mm. In other embodiments, the strengthening is suitable for glass products whose thickness is less than about 2 mm, or even thinner than about 1 mm, or still even thinner than about 0.6 mm.
In one embodiment, the size of the glass cover depends on the size of the associated electronic device. For example, with handheld electronic devices, the size of the glass cover is often not more than five (5) inches (about 12.7 cm diagonal. As another example, for portable electronic devices, such as smaller portable computers or tablet computers, the size of the glass cover is often between four (4) (about 10.2 cm) to twelve (12) inches (about 30.5 cm) diagonal. As still another example, for portable electronic devices, such as full size portable computers, displays (including televisions) or monitors, the size of the glass cover is often between ten (10) (about 25.4 cm) to twenty (20) inches (about 50.8 cm) diagonal or even larger.
However, it should be appreciated that with larger screen sizes, the thickness of the glass layers may need to be greater. The thickness of the glass layers may need to be increased to maintain planarity of the larger glass layers. While the displays can still remain relatively thin, the minimum thickness can increase with increasing screen size. For example, the minimum thickness of the glass cover can correspond to about 0.3 mm for small handheld electronic devices, about 0.5 mm for smaller portable computers or tablet computers, about 1.0 mm or more for full size portable computers, displays or monitors, again depending on the size of the screen. However, more generally, the thickness of the glass cover can depend on the application and/or the size of electronic device.
As discussed above, glass cover or, more generally, a glass piece may be chemically treated such that surfaces of the glass are effectively strengthened. Through such strengthening, glass pieces can be made stronger so that thinner glass pieces can be used with consumer electronic device. Thinner glass with sufficient strength allows for consumer electronic device to become thinner.
The techniques describe herein may be applied to glass surfaces used by any of a variety of electronic devices including but not limited handheld electronic devices, portable electronic devices and substantially stationary electronic devices. Examples of these include any known consumer electronic device that includes a display. By way of example, and not by way of limitation, the electronic device may correspond to media players, mobile phones (e.g., cellular phones), PDAs, remote controls, notebooks, tablet PCs, monitors, all in one computers and the like.
In general, the steps associated with the methods described herein may vary widely. Steps may be added, removed, altered, combined, and reordered without departing from the spirit or the scope of the invention.
The various aspects, features, embodiments or implementations of the invention described above can be used alone or in various combinations.
Additional details on strengthening edges of glass articles and/or different chemical baths can be found in: (i) U.S. Provisional Patent Application No. 61/156,803, filed Mar. 2, 2009 and entitled “TECHNIQUES FOR STRENGTHENING GLASS COVERS FOR PORTABLE ELECTRONIC DEVICES”, which is herein incorporated by reference; (ii) International Patent Application No. PCT/US2010/025979, filed Mar. 2, 2010 and entitled “Techniques for Strengthening Glass Covers for Portable Electronic Devices”, which is herein incorporated by reference; (iii) U.S. Provisional Patent Application No. 61/374,988, filed Aug. 18, 2010, and entitled “ENHANCED STRENGTHENING OF GLASS”, which is hereby incorporated herein by reference; (iv) U.S. patent application Ser. No. 12/895,823, filed Sep. 30, 2010 and entitled “ENHANCED STRENGTHENING OF GLASS”; (v) U.S. patent application Ser. No. 12/895,372, filed Sep. 30, 2010 and entitled “TECHNIQUES FOR STRENGTHENING GLASS COVERS FOR PORTABLE ELECTRONIC DEVICES”, which is herein incorporated by reference; (vi) U.S. patent application Ser. No. 12/895,393, filed Sep. 30, 2010 and entitled “TECHNIQUES FOR STRENGTHENING GLASS COVERS FOR PORTABLE ELECTRONIC DEVICES”, which is herein incorporated by reference; (vii) Provisional Patent Application No. 61/301,585, filed Feb. 4, 2010 and entitled “TECHNIQUES FOR STRENGTHENING GLASS COVERS FOR PORTABLE ELECTRONIC DEVICES,” which is hereby incorporated herein by reference; (viii) U.S. Provisional Patent Application No. 61/410,290, filed Nov. 4, 2010, and entitled “ENHANCED STRENGTHENING OF GLASS”, which is hereby incorporated herein by reference; (ix) PCT International Application No. PCT/US2011/023499, filed Feb. 2, 2011, and entitled “ENHANCED CHEMICAL STRENGTHENING GLASS OF COVERS FOR PORTABLE ELECTRONIC DEVICES”, which is hereby incorporated herein by reference; (x) U.S. patent application Ser. No. 12/847,926, filed Jul. 30, 2010, and entitled “ELECTRONIC DEVICE HAVING SELECTIVELY STRENGTHENING GLASS COVER GLASS”, which is hereby incorporated herein by reference; (xi) U.S. Provisional Patent Application No. 61/453,404, filed Mar. 16, 2011, and entitled “ELECTRONIC DEVICE HAVING SELECTIVELY STRENGTHENED GLASS”, which is hereby incorporated herein by reference; and (xii) U.S. patent application Ser. No. 13/235,090, filed Sep. 16, 2011, and entitled “ELECTRONIC DEVICE HAVING SELECTIVELY STRENGTHENED GLASS”, which is hereby incorporated herein by reference.
Additional details on compact housing configurations for portable electronic device can be found in: (i) U.S. patent application Ser. No. 13/246,707, filed Sep. 27, 2011, and entitled “HOUSING FOR PORTABLE ELECTRONIC DEVICE WITH REDUCED BORDER REGION”, which is herein incorporated by reference; and (ii) U.S. patent application Ser. No. 13/246,697, filed Sep. 27, 2011, and entitled “HOUSING FOR PORTABLE ELECTRONIC DEVICE WITH REDUCED BORDER REGION”, which is herein incorporated by reference.
Although only a few embodiments of the invention have been described, it should be understood that the invention may be embodied in many other specific forms without departing from the spirit or the scope of the present invention. By way of example, the steps associated with the methods of the invention may vary widely. Steps may be added, removed, altered, combined, and reordered without departing from the spirit of the scope of the invention. Similarly, while operations are depicted in the drawings in a particular order, this should not be understood as requiring that such operations be performed in the particular order shown or in sequential order, or that all illustrated operations be performed, to achieve desirable results.
While this specification contains many specifics, these should not be construed as limitations on the scope of the disclosure or of what may be claimed, but rather as descriptions of features specific to particular embodiment of the disclosure. Certain features that are described in the context of separate embodiments can also be implemented in combination. Conversely, various features that are described in the context of a single embodiment can also be implemented in multiple embodiments separately or in any suitable subcombination. Moreover, although features may be described above as acting in certain combinations, one or more features from a claimed combination can in some cases be excised from the combination, and the claimed combination may be directed to a subcombination or variation of a subcombination.
While this invention has been described in terms of several embodiments, there are alterations, permutations, and equivalents, which fall within the scope of this invention. It should also be noted that there are many alternative ways of implementing the methods and apparatuses of the present invention. It is therefore intended that the following appended claims be interpreted as including all such alterations, permutations, and equivalents as fall within the true spirit and scope of the present invention.
This application is a continuation patent application of U.S. patent application Ser. No. 16/429,583, filed Jun. 3, 2019 and titled “Multi-Layer Transparent Structures for Electronic Device Housings,” which is a continuation patent application of U.S. patent application Ser. No. 15/338,157, filed Oct. 28, 2016 and titled “Multi-layer Transparent Structures for Electronic Device Housings,” now U.S. Pat. No. 10,320,959, which is a continuation patent application of U.S. patent application Ser. No. 13/249,038, filed Sep. 29, 2011 and titled “Multi-layer Transparent Structures for Electronic Device Housings,” now U.S. Pat. No. 9,516,149, the disclosures of which are hereby incorporated herein by reference in their entireties.
Number | Date | Country | |
---|---|---|---|
Parent | 16429583 | Jun 2019 | US |
Child | 16740522 | US | |
Parent | 15338157 | Oct 2016 | US |
Child | 16429583 | US | |
Parent | 13249038 | Sep 2011 | US |
Child | 15338157 | US |