Claims
- 1. A catalytic cracking process undertaken in at least two risers, said two risers being in communication with each other via a catalyst regeneration zone, which process comprises,
- providing a first catalyst component as particles which have a first settling rate and
- providing a second catalyst component as particles which have a second settling rate, which second catalyst component comprises a medium pore zeolite,
- wherein said first settling rate is different from said second settling rate, wherein settling rate is a function of a physical property selected from the group consisting of density, particle size and shape;
- cracking a feed which is a gas oil or a resid in a first of said two risers, in the presence of particles of said first catalyst component selected from the group consisting of an amorphous cracking catalyst and a large pore crystalline cracking catalyst at 980.degree. to 1050.degree. F.; and separating products of cracking from catalyst in a stripper;
- thermally and catalytically cracking C.sub.3 -C.sub.6 paraffin rich charge material introduced to a second riser of said two risers in a lower region of said second riser to produce a product mixture comprising propylene, butylene, ethylene and hydrogen; wherein the heat for thermally and catalytically cracking said charge material is provided by regenerated catalyst from the regenerator which is conveyed to the lower region of said second riser;
- passing, from the stripper, particles of said second catalyst component, to downstream of said lower region and
- passing said product mixture downstream of said lower region of said second riser wherein said product mixture downstream of said lower region is contacted with particles of said medium pore zeolite, to reduce temperature in an upper zone of said second riser,
- contacting said product mixture with the medium pore zeolite in said upper zone of said second riser to convert said product mixture to high octane gasoline comprising aligomers of said ethylene, propylene and butylene;
- separating said high octane gasoline from said medium pore zeolite;
- separating particles of said medium pore zeolite from particles of said first catalyst component in said stripper,
- wherein a difference between said first settling rate and said second settling rate allows said separating said medium pore zeolite from said first catalyst component; and
- passing the separated medium pore zeolite from said stripper to said downstream of said lower region and passing separated particles of first catalyst component to the regenerator; and
- passing from the regenerator regenerated catalyst to the lower region of said second riser.
- 2. The process of claim 1, wherein in the first riser, the zeolite concentration of the medium pore zeolite represents from about 0.1 to about 10 weight percent of the total catalyst mixture, the catalyst to oil ratio is from about 3:1 to about 20:1 and the catalyst contact time is from about 0.5 to about 30 seconds.
- 3. The process of claim 1, wherein in the first riser, the medium pore zeolite concentration represents from about 0.2 to about 5.0 weight percent of the total catalyst mixture, the temperature is within the range of from about 925.degree. to about 1050.degree. F., the catalyst to feed ratio is from about 4:1 to about 10:1 and the catalyst contact time is from about 1 to about 15 seconds.
- 4. The process of claim 1, wherein the first riser, the medium pore zeolite concentration can comprise from about 1 to about 25 weight percent of the catalyst mixture, the catalyst to feed ratio is from about 3:1 to about 20:1 and the catalyst contact time is from about 0.5 to about 30 seconds.
- 5. The process of claim 4, wherein in the first riser, the medium pore zeolite concentration can comprise from about 2 to about 10 weight percent of the total catalyst mixture.
- 6. The process of claim 1 wherein in the lower region of the second riser, the temperature is within the range of from about 1110.degree. to about 1500.degree. F., the catalyst to feed ratio is from about 50:1 to about 200:1 and the catalyst contact time is from about 10 to about 50 seconds.
- 7. The process of claim 1, wherein in the lower region of the second riser, the temperature is within the range of from about 1250.degree. to about 1350.degree. F., the catalyst to feed ratio is from about 100:1 to about 150:1 and the catalyst contact time is from about 15 to about 35 seconds.
- 8. The process of claim 1, wherein in the upper region of the second riser, the temperature is within the range of from about 400.degree. to about 1000.degree. F., the second catalyst component to hydrocarbon ratio is from about 5:1 to about 40:1 and the catalyst contact time is from about 5 to about 45 seconds.
- 9. The process of claim 1, wherein in the upper region of the second riser, the temperature is within the range of from about 650.degree. to about 800.degree. F., the second catalyst component to hydrocarbon ratio is from about 20:1 to about 30:1 and the catalyst contact time is from about 25 to about 35 seconds.
- 10. The process of claim 1, wherein the heavy hydrocarbon charge material is subjected to hydrotreatment prior to its introduction in the first riser.
- 11. The process of claim 10, wherein the hydrotreatment utilizes hydrogen recovered from the catalytic cracking process.
- 12. The process of claim 1, wherein products of cracking said gas oil or resid comprises C.sub.3 -C.sub.6 paraffin rich charge material.
Parent Case Info
This is a continuation of copending application Ser. No. 144,788, filed on Jan 21, 1988, now abandoned which is a continuation of copending application Ser. No. 903,161, filed on Sept. 3, 1986, now abandoned.
US Referenced Citations (28)
Foreign Referenced Citations (3)
Number |
Date |
Country |
0074501 |
Mar 1983 |
EPX |
0101553 |
Feb 1984 |
EPX |
0171460 |
Feb 1986 |
EPX |
Continuations (2)
|
Number |
Date |
Country |
Parent |
144788 |
Jan 1988 |
|
Parent |
903161 |
Sep 1986 |
|