The present invention generally relates to nickel-base alloy compositions, and more particularly to nickel-base superalloys suitable for components requiring a polycrystalline microstructure and high temperature dwell capability, for example, turbine disks of gas turbine engines.
The turbine section of a gas turbine engine is located downstream of a combustor section and contains a rotor shaft and one or more turbine stages, each having a turbine disk (rotor) mounted or otherwise carried by the shaft and turbine blades mounted to and radially extending from the periphery of the disk. Components within the combustor and turbine sections are often formed of superalloy materials in order to achieve acceptable mechanical properties while at elevated temperatures resulting from the hot combustion gases. Higher compressor exit temperatures in modem high pressure ratio gas turbine engines can also necessitate the use of high performance nickel superalloys for compressor disks, blisks, and other components. Suitable alloy compositions and microstructures for a given component are dependent on the particular temperatures, stresses, and other conditions to which the component is subjected. For example, airfoil components such as blades and vanes are often formed of equiaxed, directionally solidified (DS), or single crystal (SX) superalloys, whereas turbine disks are typically formed of superalloys that must undergo carefully controlled forging, heat treatments, and surface treatments such as peening to produce a polycrystalline microstructure having a controlled grain structure and desirable mechanical properties.
Turbine disks are often formed of gamma prime (γ′) precipitation-strengthened nickel-base superalloys (hereinafter, gamma prime nickel-base superalloys) containing chromium, tungsten, molybdenum, rhenium and/or cobalt as principal elements that combine with nickel to form the gamma (γ) matrix, and contain aluminum, titanium, tantalum, niobium, and/or vanadium as principal elements that combine with nickel to form the desirable gamma prime precipitate strengthening phase, principally Ni3(Al,Ti). Particularly notable gamma prime nickel-base superalloys include René 88DT (R88DT; U.S. Pat. No. 4,957,567) and René 104 (R104; U.S. Pat. No. 6,521,175), as well as certain nickel-base superalloys commercially available under the trademarks Inconel®, Nimonic®, and Udimet®. R88DT has a composition of, by weight, about 15.0-17.0% chromium, about 12.0-14.0% cobalt, about 3.5-4.5% molybdenum, about 3.5-4.5% tungsten, about 1.5-2.5% aluminum, about 3.2-4.2% titanium, about 0.5.0-1.0% niobium, about 0.010-0.060% carbon, about 0.010-0.060% zirconium, about 0.010-0.040% boron, about 0.0-0.3% hafnium, about 0.0-0.01 vanadium, and about 0.0-0.01 yttrium, the balance nickel and incidental impurities. R104 has a nominal composition of, by weight, about 16.0-22.4% cobalt, about 6.6-14.3% chromium, about 2.6-4.8% aluminum, about 2.4-4.6% titanium, about 1.4-3.5% tantalum, about 0.9-3.0% niobium, about 1.9-4.0% tungsten, about 1.9-3.9% molybdenum, about 0.0-2.5% rhenium, about 0.02-0.10% carbon, about 0.02-0.10% boron, about 0.03-0.10% zirconium, the balance nickel and incidental impurities.
Disks and other critical gas turbine engine components are often forged from billets produced by powder metallurgy (P/M), conventional cast and wrought processing, and spraycast or nucleated casting forming techniques. Gamma prime nickel-base superalloys formed by powder metallurgy are particularly capable of providing a good balance of creep, tensile, and fatigue crack growth properties to meet the performance requirements of turbine disks and certain other gas turbine engine components. In a typical powder metallurgy process, a powder ofthe desired superalloy undergoes consolidation, such as by hot isostatic pressing (HIP) and/or extrusion consolidation. The resulting billet is then isothermally forged at temperatures slightly below the gamma prime solvus temperature of the alloy to approach superplastic forming conditions, which allows the filling ofthe die cavity through the accumulation of high geometric strains without the accumulation of significant metallurgical strains. These processing steps are designed to retain the fine grain size originally within the billet (for example, ASTM 10 to 13 or finer), achieve high plasticity to fill near-net-shape forging dies, avoid fracture during forging, and maintain relatively low forging and die stresses. In order to improve fatigue crack growth resistance and mechanical properties at elevated temperatures, these alloys are then heat treated above their gamma prime solvus temperature (generally referred to as supersolvus heat treatment) to cause significant, uniform coarsening of the grains.
Though alloys such as R88DT and R104 have provided significant advances in high temperature capabilities of superalloys, further improvements are continuously being sought. For example, high temperature dwell capability has emerged as an important factor for the high temperatures and stresses associated with more advanced military and commercial engine applications. As higher temperatures and more advanced engines are developed, creep and crack growth characteristics of current alloys tend to fall short of the required capability to meet mission/life targets and requirements of advanced disk applications. It has become apparent that a particular aspect of meeting this challenge is to develop compositions that exhibit desired and balanced improvements in creep and hold time (dwell) fatigue crack growth rate characteristics at temperatures of 1200° F. (about 650° C.) and higher, while also having good producibility and thermal stability. However, complicating this challenge is the fact that creep and crack growth characteristics are difficult to improve simultaneously, and can be significantly influenced by the presence or absence of certain alloying constituents as well as relatively small changes in the levels of the alloying constituents present in a superalloy.
The present invention provides a gamma prime nickel-base superalloy and components formed therefrom that exhibit improved high-temperature dwell capabilities, including creep and hold time fatigue crack growth behavior.
According to a first aspect of the invention, the gamma-prime nickel-base superalloy contains, by weight, 16.0 to 30.0% cobalt, 11.5 to 15.0% chromium, 4.0 to 6.0% tantalum, 2.0 to 4.0% aluminum, 1.5 to 6.0% titanium, 1.0 to 5.0% tungsten, 1.0 to 5.0% molybdenum, up to 3.5% niobium, up to 1.0% hafnium, 0.02 to 0.20% carbon, 0.01 to 0.05% boron, 0.02 to 0.10% zirconium, the balance essentially nickel and impurities, wherein the titanium:aluminum weight ratio is 0.5 to 2.0.
Another aspect of the invention are components that can be formed from the alloy described above, particular examples of which include turbine disks and compressor disks and blisks of gas turbine engines.
A significant advantage of the invention is that the nickel-base superalloy described above provides the potential for balanced improvements in high temperature dwell properties, including improvements in both creep and hold time fatigue crack growth rate (HTFCGR) characteristics at temperatures of 1200° F. (about 650° C.) and higher, while also having good producibility and good thermal stability. Improvements in other properties are also believed possible, particularly if appropriately processed using powder metallurgy, hot working, and heat treatment techniques.
Other aspects and advantages of this invention will be better appreciated from the following detailed description.
The present invention is directed to gamma prime nickel-base superalloys, and particular those suitable for components produced by a hot working (e.g., forging) operation to have a polycrystalline microstructure. A particular example represented in
Disks of the type shown in
Superalloy compositions of this invention were developed through the use of a proprietary analytical prediction process directed at identifying alloying constituents and levels capable of exhibiting better high temperature dwell capabilities than existing nickel-base superalloys. More particularly, the analysis and predictions made use of proprietary research involving the definition of elemental transfer functions for tensile, creep, hold time (dwell) crack growth rate, density, and other important or desired mechanical properties for turbine disks produced in the manner described above. Through simultaneously solving of these transfer functions, evaluations of compositions were performed to identify those compositions that appear to have the desired mechanical property characteristics for meeting advanced turbine engine needs, including creep and hold time fatigue crack growth rate (HTFCGR). The analytical investigations also made use of commercially-available software packages along with proprietary databases to predict phase volume fractions based on composition, allowing for the further definition of compositions that approach or in some cases slightly exceed undesirable equilibrium phase stability boundaries. Finally, solution temperatures and preferred amounts of gamma prime and carbides were defined to identify compositions with desirable combinations of mechanical properties, phase compositions and gamma prime volume fractions, while avoiding undesirable phases that could reduce in-service capability if equilibrium phases sufficiently form due to in-service environment characteristics. In the investigations, regression equations or transfer functions were developed based on selected data obtained from historical disk alloy development work. The investigations also relied on qualitative and quantitative data of the aforementioned nickel-base superalloys R88DT and R104.
Particular criteria utilized to identify potential alloy compositions included the desire for a volume percentage of gamma prime ((Ni,Co)3(Al, Ti, Nb, Ta)) greater than that of R88DT, with the intent to promote strength at temperatures of 1400° F. (about 760° C.) and higher over extended periods of time. A gamma prime solvus temperature of not more than 2200° F. (about 1200° C.) was also identified as desirable for ease of manufacture during heat treatment and quench. In addition, certain compositional parameters were identified as starting points for the compositions, including the inclusion of hafnium for high temperature strength, chromium levels of 10 weight percent or more for corrosion resistance, aluminum levels greater than the nominal R88DT level to maintain gamma prime (Ni3(Al, Ti, Nb, Ta)) stability, and cobalt levels of greater than 18 weight percent to aid in minimizing stacking fault energy (desirable for good cyclic behavior) and controlling the gamma prime solvus temperature. The regression equations and prior experience further indicated that relatively high levels of refractory elements were desirable to improve high temperature properties, and selective balancing of titanium, tungsten, niobium and molybdenum levels were employed to optimize creep and hold time fatigue crack growth behavior. Finally, regression factors relating to specific mechanical properties were utilized to narrowly identify potential alloy compositions that might be capable of exhibiting superior high temperature hold time (dwell) behavior, and would not be otherwise identifiable without extensive experimentation with a very large number of alloys. Such properties included ultimate tensile strength (UTS) at 1200° F. (about 650° C.), yield strength (YS), elongation (EL), reduction of area (RA), creep (time to 0.2% creep at 1200° F. and 115 ksi (about 650° C. at about 790 MPa), hold time (dwell) fatigue crack growth rate (HTFCGR; da/dt) at 1300° F. (about 700° C.) and a maximum stress intensity of 25 ksi√m (about 27.5 MPa√m), fatigue crack growth rate (FCGR), gamma prime volume percent (GAMMA′ %) and gamma prime solvus temperature (SOLVUS), all of which were evaluated on a regression basis. Units for these properties reported herein are ksi for UTS and YS, percent for EL, RA and gamma prime volume percent, hours for creep, in/sec for crack growth rates (HTFCGR and FCGR), and ° F. for gamma prime solvus temperature. Thermodynamic calculations were also performed to assess alloy characteristics such as phase volume fraction, stability and solvii for gamma prime, carbides, borides and topologically close packed (TCP) phases.
The process described above was performed iteratively utilizing expert opinion and guidance to define preferred compositions for manufacture and evaluation. From this process, a first series of alloy compositions were defined (by weight percent) as set forth in the table of
Although the thermodynamic calculations of TCP phases were believed to have some uncertainty, the desire to avoid undesirable levels of formation of TCP phases provided the basis for defining a second series of alloy compositions, designated as alloys HL-06 through HL-15, whose compositions (in weight percent) are summarized in the table of
Regression-based property predictions for the second series of alloys are summarized in the table of
On the basis of the above predictions, nine alloys (Alloys A through I) were prepared with compositions based on the ten alloys of the second series. The actual chemistries (in weight percent) of the prepared alloys are summarized in the table of
The titanium:aluminum weight ratio is believed to be important for the alloys of Tables II and III on the basis that higher titanium levels are generally beneficial for most mechanical properties, though higher aluminum levels promote alloy stability necessary for use at high temperatures. In addition, the molybdenum:molybdenum+tungsten weight ratio is also believed to be important for the alloys of Table II as this ratio indicates the refractory content for high temperature response and balances the refractory content of the gamma and the gamma prime phases. As such, these ratios are also included in Tables II and III where applicable. In addition to the elements listed in Tables II and III, it is believed that minor amounts of other alloying constituents could be present without resulting in undesirable properties. Such constituents and their amounts (by weight) include up to 2.5% rhenium, up to 2% vanadium, up to 2% iron, and up to 0.1% magnesium.
Though the alloy compositions identified in
While the invention has been described in terms of particular embodiments, including particular compositions and properties of nickel-base superalloys, the scope of the invention is not so limited. Instead, the scope of the invention is to be limited only by the following claims.
| Number | Name | Date | Kind |
|---|---|---|---|
| 3576681 | Barker et al. | Apr 1971 | A |
| 3655458 | Reichman | Apr 1972 | A |
| 3748192 | Boesch | Jul 1973 | A |
| 3890816 | Allen et al. | Jun 1975 | A |
| 4121950 | Guimier et al. | Oct 1978 | A |
| 4207098 | Shaw | Jun 1980 | A |
| 4388124 | Henry | Jun 1983 | A |
| 4685977 | Chang | Aug 1987 | A |
| 4769087 | Genereux et al. | Sep 1988 | A |
| 4814023 | Chang | Mar 1989 | A |
| 4820353 | Chang | Apr 1989 | A |
| 4867812 | Henry | Sep 1989 | A |
| 4888064 | Chang | Dec 1989 | A |
| 4894089 | Henry | Jan 1990 | A |
| 4957567 | Krueger et al. | Sep 1990 | A |
| 4981644 | Chang | Jan 1991 | A |
| 4983233 | Henry | Jan 1991 | A |
| 5037495 | Henry | Aug 1991 | A |
| 5055147 | Henry | Oct 1991 | A |
| 5061324 | Chang | Oct 1991 | A |
| 5080734 | Krueger et al. | Jan 1992 | A |
| 5087305 | Chang | Feb 1992 | A |
| 5104614 | Ducrocq et al. | Apr 1992 | A |
| 5124123 | Henry | Jun 1992 | A |
| 5129968 | Henry | Jul 1992 | A |
| 5129969 | Henry | Jul 1992 | A |
| 5129970 | Henry | Jul 1992 | A |
| 5129971 | Henry | Jul 1992 | A |
| 5130086 | Henry | Jul 1992 | A |
| 5130087 | Henry | Jul 1992 | A |
| 5130088 | Henry | Jul 1992 | A |
| 5130089 | Henry | Jul 1992 | A |
| 5143563 | Krueger et al. | Sep 1992 | A |
| 5156808 | Henry | Oct 1992 | A |
| 5171380 | Henry | Dec 1992 | A |
| 5393483 | Chang | Feb 1995 | A |
| 5476555 | Erickson | Dec 1995 | A |
| 5662749 | Chang | Sep 1997 | A |
| 5891272 | Raymond et al. | Apr 1999 | A |
| 5897718 | Hessell et al. | Apr 1999 | A |
| 6132527 | Hessell et al. | Oct 2000 | A |
| 6468368 | Merrick et al. | Oct 2002 | B1 |
| 6521175 | Mourer et al. | Feb 2003 | B1 |
| 6866727 | Hieber et al. | Mar 2005 | B1 |
| 6890370 | Merrick et al. | May 2005 | B2 |
| 6969431 | Hieber et al. | Nov 2005 | B2 |
| 6974508 | Gabb et al. | Dec 2005 | B1 |
| 7208116 | Manning et al. | Apr 2007 | B2 |
| 20050142023 | Voice et al. | Jun 2005 | A1 |
| 20070160476 | Cheng et al. | Jul 2007 | A1 |
| 20100303665 | Bain et al. | Dec 2010 | A1 |
| 20110203707 | Mourer et al. | Aug 2011 | A1 |
| Number | Date | Country |
|---|---|---|
| 0248757 | Mar 1990 | EP |
| 0924309 | Jun 1999 | EP |
| 1195446 | Oct 2002 | EP |
| 1710322 | Nov 2006 | EP |
| Entry |
|---|
| ASM International, Materials Park, Ohio, ASM Specialty Handbook: Nickel, Cobalt, and Their Alloys, “Metallography and Microstructures of Heat Resistant Alloys”, Dec. 2000, pp. 302-304. |
| EP 10163817.9, Search Report and Written Opinion, Aug. 27, 2010. |
| EP 10163821.1, Search Report and Written Opinion, Aug. 30, 2010. |
| Non-Final Rejection towards corresponding U.S. Appl. No. 12/474,651 dated Jun. 23, 2014. |
| PCT Search Report and Written Opinion issued in connection with corresponding Application No. PCT/US2014/017336 on Nov. 11, 2014. |
| Number | Date | Country | |
|---|---|---|---|
| 20100303665 A1 | Dec 2010 | US |