The present invention relates to an optical waveguide element, and more particularly, an optical waveguide element including a substrate having an electro-optic effect, an optical waveguide formed on the substrate, and a control electrode provided on the substrate and controlling a light wave propagating through the optical waveguide.
Optical waveguide elements such as optical modulators are widely used in an optical communication field or an optical measurement field. The optical waveguide element includes a substrate having an electro-optic effect such as lithium niobate, an optical waveguide formed on the substrate, and a control electrode provided on the substrate and controlling a light wave propagating through the optical waveguide.
In the related art, gold (Au) has been widely used as a material for the control electrode from the viewpoints of chemical stability of a material and easiness of manufacturing such as wire bonding. On the other hand, from the viewpoint of light modulation operation, it is desirable that conductivity is higher and a conductor loss is smaller. As a material other than gold, for example, it has been proposed to use silver (Ag) as in Patent Literature No. 1 or copper (Cu) or copper alloy as in Patent Literature No. 2. Since these materials have higher conductivity than gold, good high-frequency characteristics can be obtained.
However, when using materials other than gold, corrosion due to oxidation should be considered. As described in Patent Literature No. 3, in a transmission circuit of a high-frequency signal, even in a case where an insulator covers a surface of a metal film, it is known that a skin effect is exhibited by using a portion where a signal current has a low resistance (non-oxidized portion), so that deterioration of high-frequency characteristics is suppressed.
However, generally, in a case where the electrical connection is performed from the peripheral components, which are made of gold, to a pad of a signal electrode or a ground electrode by wire bonding or the like, the connection becomes difficult and the easiness of manufacturing deteriorates when the electrode is oxidized. In Patent Literature No. 1, gold is formed as an anti-oxidation film on an entire surface of the electrode, since this film is formed even on an unnecessary part, it causes deterioration of high-frequency characteristics and cost increase.
In addition, in a case where the gold film is partially disposed on the signal electrode that constitutes the control electrode or the ground electrode that is disposed to face the signal electrode, the following problems occur. For example, on the surface of the signal electrode or the like, a portion where the gold film exists and a portion where the gold film does not exist and becomes an insulator due to oxidation are formed, and the electric resistance of the surface of the electrode becomes uneven. Moreover, the distribution of electric resistance in a depth direction from the electrode surface also differs depending on the location of the electrode. Disturbance of the electric resistance on the electrode surface or in the vicinity thereof further increases the propagation loss of the high-frequency signal.
[Patent Literature No. 1] Japanese Patent No. 3179408
[Patent Literature No. 2] Japanese Patent Application No. 2017-069820 (filed on Mar. 31, 2017)
[Patent Literature No. 3] Japanese Patent No. 6110581
An object of the present invention is to solve the above-described problem and to provide an optical waveguide element capable of connection such as wire bonding, suppressing usage of gold, and suppressing deterioration of a conductor loss.
In order to solve the above problem, the optical waveguide element of the present invention has the following technical features.
(1) In an optical waveguide element including a substrate having an electro-optic effect, an optical waveguide formed on the substrate, and a control electrode provided on the substrate and controlling a light wave propagating through the optical waveguide, the control electrode is made of a material other than gold, and the gold is disposed on at least a wire bonding portion of the control electrode.
(2) In the optical waveguide element according to (1) , the control electrode includes a signal electrode and a ground electrode, and at least in an action portion where an electric field of the control electrode acts on the optical waveguide, the gold is not disposed on a surface of the signal electrode and a surface, on a side facing the signal electrode, of the ground electrode.
(3) In the optical waveguide element according to (1) or (2), a portion on which the gold is disposed is only the wire bonding portion.
(4) In the optical waveguide element according to any one of (1) to (3), the material other than gold has an electric resistivity of 2.44×10−8 Ωm or less.
(5) In the optical waveguide element according to any one of (1) to (4), the control electrode is a plating electrode and a height of the plating electrode is 10 μm or higher.
(6) In the optical waveguide element according to any one of (1) to (5), a ratio of a height of the gold portion to a height of the control electrode is less than 10%.
The present invention provides an optical waveguide element including a substrate having an electro-optic effect, an optical waveguide formed on the substrate, and a control electrode provided on the substrate and controlling a light wave propagating through the optical waveguide. The control electrode is made of a material other than gold, and the gold is disposed on at least a wire bonding portion of the control electrode. Therefore, connection such as wire bonding is possible and the easiness of manufacturing is improved. In addition, the usage of gold can be suppressed and an increase in cost can be suppressed. Furthermore, since gold is not disposed on most parts of the surface of the control electrode, deterioration of a conductor loss can be suppressed.
Hereinafter, the optical waveguide element of the present invention will be described in detail with reference to suitable examples. As shown in
As the substrate having the electro-optic effect used in the present invention, various substrates known in the related art such as lithium niobate can be used.
The optical waveguide 2 can be easily formed by locally increasing a refractive index by thermal diffusion of Ti or the like. In addition, if necessary, it is possible to form a ridge on the substrate 1 to enhance a light confinement effect.
The control electrode used in the present invention is made of a material other than gold (Au), and the material preferably has an electric resistivity of 2.44×10−8 Ωm or less. Specifically, silver (Ag) disclosed in Patent Literature No. 1 or copper (Cu) and copper alloys (Al—Cu alloy, Ni—Cu alloy, Be—Cu alloy, Sn—Cu alloy, or the like) disclosed in Patent Literature No. 2 can be used. Particularly, copper or copper alloy is preferable from the viewpoint of manufacturing cost.
A height H of the control electrode is preferably 10 μm or higherin consideration of impedance for propagating a high-frequency signal. In addition, depending on a depth of oxidation from the surface of the electrode, it is preferable that the height and width have thickness of at least 5 μm or higherin consideration of conversion to an insulator due to oxidation.
A feature of the present invention is that, in order to easily and surely perform wire bonding for electrical connection using metal wires such as a gold wire or a gold ribbon or the like on the surface of the control electrode, gold (Au) or platinum (Pt) is disposed on the surface of the control electrode at the location where the wire bonding is performed. Considering the bonding stability with the gold wire, gold (Au) is more preferable.
In addition, in order to suppress the propagation loss of the high-frequency signal, it is necessary to make a state of a resistance value of the electrode surface (a distribution state of the electric resistance) uniform in the signal electrode and the ground electrode located in an action portion of the control electrode. Therefore, at least the gold (Au) is not disposed on a surface of a signal electrode 30 of the action portion. The gold (Au) is not disposed on a surface, on a side facing the signal electrode, of the ground electrode 31. In addition, as shown in
As shown in
As shown in
Although the X-cut type substrate 1 has been described with reference to
A base layer 5 under the control electrode in
As described above, according to the present invention, it is possible to provide an optical waveguide element capable of connection such as wire bonding, suppressing usage of gold, and suppressing deterioration of the conductor loss.
Number | Date | Country | Kind |
---|---|---|---|
2018-067802 | Mar 2018 | JP | national |
Filing Document | Filing Date | Country | Kind |
---|---|---|---|
PCT/JP2019/002190 | 1/24/2019 | WO | 00 |