This application is a U.S. National Stage under 35 U.S.C. § 371 of International Application No. PCT/CN2017/079321, filed on Apr. 1, 2017, which claims priority to and the benefit of Chinese patent application No. 201620526575.1 filed on May 27, 2016 and entitled “ORGANIC ELECTROLUMINESCENT DISPLAY BACKPANEL, COVER AND DEVICE”, the disclosure of which is hereby incorporated by reference in its entirety.
The present disclosure relates to the technical field of display, and particularly to an organic electroluminescent display backpanel, cover and device.
The current organic light emitting diode (OLED) display device is a device for graphical display by use of a reversible discoloration phenomenon produced by an organic semiconductor material driven by current. OLED display device has advantages such as ultralight, ultrathin, high brightness, large view angle, low voltage, low power consumption, fast response, high definition, antiknock, flexibility, low cost, simple process, less use of raw materials, high luminous efficiency and wide temperature range, and is considered as the most promising next-generation display technology.
OLED device generally includes a cathode, an anode and an organic light-emitting layer sandwiched between the cathode and the anode. Under the externally applied voltage, electrons are injected from the cathode into the organic light-emitting layer and holes are injected from the anode into organic light-emitting layer, and in organic light-emitting layer, the electrons and the holes meet and recombine to produce excitons, i.e., radiating light. In a process of manufacturing OLED devices, especially large size OLED devices, the organic light-emitting layer may be mixed with foreign matters, and due to the small distance between the cathode and the anode, say about 0.3 μm, in the vacuum lamination process, the foreign matters are likely to pierce the membrane of the cathode or the anode under high pressure, which causes a short circuit between the cathode and the anode. Therefore, the whole pixel cannot be lit, dark spot occurs, and the display quality is severely affected.
At present, it is comparatively difficult to limit the size of the foreign matters to below 0.3 μm by means of in-process quality control, so it is hard to reduce dark spots produced by the foreign matters.
The present disclosure provides an organic electroluminescent display backpanel, cover and display device.
According to a first aspect, the present disclosure provides an organic electroluminescent display backpanel comprises a backpanel body and a plurality of supporting columns, the backpanel body comprising a substrate and an array of organic electroluminescent elements formed on the substrate and the supporting column is disposed at a side of the array of organic electroluminescent elements away from the substrate.
Alternatively, each of the supporting columns is located in an interval region between adjacent pixels.
Alternatively, the backpanel further comprises a buffer layer disposed between the array of organic electroluminescent elements and the supporting columns.
Alternatively, a material of the buffer layer comprises a water-absorbing material.
Alternatively, the backpanel further comprises a fill layer disposed between the buffer layer and the supporting columns.
Alternatively, the supporting columns adjoin the fill layer, and a hardness of the supporting columns is higher than that of the fill layer.
Alternatively, a material of the fill layer comprises a water-absorbing material.
Alternatively, the material of the supporting columns is the same with the material of the fill layer.
According to a second aspect, the present disclosure provides an organic electroluminescent display cover comprising a cover body and a plurality of supporting columns disposed at a first side of the cover body, wherein the first side is a side of the cover body that faces a backpanel adapted to the cover.
Alternatively, each of the supporting columns is in an interval region between adjacent pixels.
Alternatively, a material of the supporting columns comprises a water-absorbing material.
According to a third aspect, the present disclosure provides an organic electroluminescent display device comprising any of the aforementioned backpanel or any of the aforementioned cover.
Feature information and advantages of the present disclosure will be understood more clearly by referring to the accompanying drawings, and the accompanying drawings are illustrative and should not be construed as any limitation to the present disclosure. In the drawings:
100—organic electroluminescent display backpanel in the prior art, 100′—organic electroluminescent display backpanel in the present disclosure; 101—substrate, 102—array of organic electroluminescent elements; 1021—first electrode layer; 1022—organic light emitting layer; 1023—second electrode layer; 103—buffer layer, 104—fill layer, 105a, 105b, 105—supporting columns in the backpanel; 106—foreign matters; 200—organic electroluminescent display cover in the prior art; 200′—organic electroluminescent display cover in the present disclosure; 201—cover body; 202—supporting columns in the cover.
In order to understand the above objectives, features and advantages of the present disclosure more clearly, the present disclosure will be further described in detail below in combination with the drawings and the embodiments. It should be noted that, the embodiments of the present application and the features in the embodiments can be combined with each other without conflict.
Unless otherwise defined, the technical terms or scientific terms used herein should have normal meanings as understood by those skilled in the art. The words “first”, “second”, or the like used in the description and claims of the patent application in the present disclosure do not represent any order, number or importance, but are merely used to distinguish between different composite parts. Likewise, the word “one”, or “a”, or the like does not represent a restriction to number, but the existence of at least one. The word “connect” or “connected” or the like is not limited to a physical or mechanical connection, but can comprise an electrical connection, either directly or indirectly. “Up”, “down”, “left”, “right” and the like are used to only represent relative position relations, and after an absolute position of the described object changes, the relative position relations change accordingly.
Unless otherwise explicitly specified in the context, a word used in the description and the claims, though in a singular form, includes its plural form, and vice versa. Thus, when mentioning a singular form of a term, usually a plural form of the corresponding term is included. Similarly, the words “include” and “comprise” are interpreted as inclusive but not exclusive. Likewise, the terms “comprise” and “or” should be interpreted as inclusive, unless such interpretations are explicitly prohibited in this document. For the term “instance” used in this document, especially following a set of terms, the “instance” is merely exemplary and illustrative, and should not be considered exclusive or extensive.
Many concrete details are described below for sufficient understanding of the present disclosure, but the present disclosure can be implemented in other ways than those described herein, so the scope of protection of the present disclosure is not restricted by the embodiments disclosed below.
According to a first aspect, one embodiment of the present disclosure provides an organic electroluminescent display backpanel 100′, as shown in
In the organic electroluminescent display backpanel 100′ provided in the present embodiment, due to the provision of a plurality of supporting columns 105, in the time of vacuum lamination, pressures mainly act on the supporting columns 105. That is to way, the array of organic electroluminescent elements 102 receives greater pressures at the positions corresponding to the locations of the supporting columns 105, but the array of organic electroluminescent elements 102 receives smaller pressures corresponding to the locations where the supporting columns 105 are not provided. In this way, foreign matters in the array of organic electroluminescent elements 102 corresponding to the locations where the supporting columns are not provided are less likely to pierce the membrane in the array of organic electroluminescent elements, thereby achieving the basic objective of reducing dark spots.
For instance, as shown in
In the present embodiment, since a buffer layer 103 is provided between the array of organic electroluminescent elements 102 and the supporting columns 105, during the vacuum lamination, the buffer layer 103 will give a certain buffer against a tremendous pressure applied to the backpanel 100′, thereby preventing the foreign matters in the array of organic electroluminescent elements 102 from piercing the membrane due to a sudden tremendous pressure, which can further reduce dark spots. Furthermore, the buffer layer 103 can be made of a water-absorbing material, to avoid the outside moisture from entering the array of organic electroluminescent elements 102 of the backpanel 100′, thereby extending the lifecycle of the backpanel 100′. Of course, in some alternative embodiments, it is not necessarily to provide a buffer layer 103 between the array of organic electroluminescent elements 102 and the supporting columns 105. Even if the buffer layer 103 is provided, it is not necessarily to manufacture the buffer layer 103 with water-absorbing material. Such a technical solution can also reach the basic objective of reducing dark spots, and thus falls into the scope of protection of the present disclosure.
In the present embodiment, since a fill layer 104 is provided between the buffer layer 103 and the supporting columns 105, and the supporting columns 105 adjoin the fill layer 104, an outside influence to the array of organic electroluminescent elements 102 can be reduced, thereby extending the lifecycle of the backpanel 100′. In practice, during the fabrications, the fill layer 104 can be made of a water-absorbing material, to absorb outside moisture. Of course, in some alternative embodiments, it is not necessarily provided a fill layer 104, and even if the fill layer 104 is provided, it is not necessarily to manufacture the fill layer 104 with water-absorbing material. Such a technical solution can also reach the basic objective of reducing dark spots, and thus falls into the scope of protection of the present disclosure.
In the present embodiment, in order to guarantee the support function of the supporting columns 105, the hardness of the supporting columns 105 is necessarily higher than that of the fill layer 104. In practice, during the fabrications, the supporting columns 105 can be made of a water-absorbing material, and in case where the fill layer 104 is also made of a water-absorbing material, the material of the supporting columns 105 may be selected to be the same with that of the fill layer 104, but it has a fluidity weaker than that of the fill layer 104 and a curing rate faster than the fill layer 104 while being irradiated with ultraviolet light, to make sure that the supporting column 105 has a sufficient hardness for achieving the supporting function. Of course, the supporting columns 105 can also choose a material with a good elasticity and adhesion such as polystyrene resin.
In the present embodiment, the concrete structure of the array of organic electroluminescent elements 102 is not limited and can be set as needed in specific implementations. As shown in
According to a second aspect, an embodiment of the present disclosure provides an organic electroluminescent display cover 200′, as shown in
In the organic electroluminescent display cover 200′ provided in the present embodiment, due to the provision of a plurality of supporting columns 202 at the first side of the cover body 201, when the cover 200′ is fitted to the backpanel 100 after the vacuum lamination is performed, pressures mainly act on the supporting columns 202. That is to way, the backpanel 100 receives greater pressures at the positions corresponding to the locations of the supporting columns 202, but backpanel 100 receives smaller pressures at the positions corresponding to the locations where the supporting columns 202 are not provided. In this way, foreign matters in the backpanel 100 at the positions corresponding to the locations where the supporting columns 202 are not provided are less likely to pierce the membrane, thereby achieving the basic objective of reducing dark spots.
In the present embodiment, the supporting columns 202 can be made of a water-absorbing material, to absorb outside moisture, thereby extending the lifecycle of the backpanel 100 fitted to the cover 200′. Of course, in some alternative embodiments, it is not necessarily to manufacture the supporting column 202 with water-absorbing material. Such a technical solution can also reach the basic objective of reducing dark spots, and thus falls into the scope of protection of the present disclosure.
In the present embodiment, the light exiting direction of the backpanel 100 might be towards the cover 200′, so in order to avoid the supporting columns 202 provided on the cover 200′ from shielding the lights emitted from the backpanel 100, each supporting column 202 is provided in interval regions between adjacent pixels. Moreover, in order to facilitate the fabrication of the supporting columns 202, each supporting column 202 may be uniformly arranged in the interval regions between adjacent pixels.
According to a third aspect, one embodiment of the present disclosure provides an organic electroluminescent display device comprising the backpanel 100′ according to the first aspect or the cover 200′ according to the second aspect.
In specific implementations, the organic electroluminescent display device in the present embodiment may further comprise a cover adapted to the backpanel. The formed display device can be specifically applied to: display panels, e-paper, mobile phones, tablets, televisions, monitors, notebook computers, digital frames, navigators, or any product or member having a display function.
The experiments proved that, as compared with the organic electroluminescent display device in the prior art, in the organic electroluminescent display device according to the present embodiment, dark spots can be reduced by about 75%, that is, the display quality is greatly improved.
Although the embodiments of the present disclosure have been described above in combination with the drawings, those skilled in the art could make various modifications and variations without departing from the spirit and scope of the present disclosure, and such modifications and variations all fall into the scope as defined by the accompanying claims.
Number | Date | Country | Kind |
---|---|---|---|
2016 2 0526575 U | May 2016 | CN | national |
Filing Document | Filing Date | Country | Kind |
---|---|---|---|
PCT/CN2017/079321 | 4/1/2017 | WO | 00 |
Publishing Document | Publishing Date | Country | Kind |
---|---|---|---|
WO2017/202145 | 11/30/2017 | WO | A |
Number | Name | Date | Kind |
---|---|---|---|
20010017372 | Koyama | Aug 2001 | A1 |
20050099123 | Chen et al. | May 2005 | A1 |
20150162386 | Furuie | Jun 2015 | A1 |
20160049443 | Kim | Feb 2016 | A1 |
20160365537 | Qian | Dec 2016 | A1 |
20180059499 | Klement | Mar 2018 | A1 |
Number | Date | Country |
---|---|---|
101740608 | Jun 2010 | CN |
104466031 | Mar 2015 | CN |
104517992 | Apr 2015 | CN |
205645819 | Oct 2016 | CN |
Entry |
---|
International Search Report and Written Opinion for PCT App. No. PCT/CN2017/079321 dated Jul. 7, 2017(with English translation, 17 pages). |
Number | Date | Country | |
---|---|---|---|
20180158874 A1 | Jun 2018 | US |