The disclosure of Japanese Patent Application No. 2006-042275 filed on Feb. 20, 2006 (yyyy/mm/dd) including the claims, the specification, the drawings and the abstract is incorporated herein by reference in its entirety.
1. Field of the Invention
The present invention relates to an organic EL display device, and more particularly to a technique which is effectively applicable to an organic EL display device which can prolong a lifetime thereof and can enhance reliability thereof by suppressing the degradation of an organic EL layer attributed to moisture.
2. Description of the Related Art
As a flat-panel-type display device, a liquid crystal display device (LCD), a plasma display device (PDL), a field emission type display device (FED), an organic EL display device (OLED) and the like have been put into practice or have been studied for future practical use. Among these display devices, the organic EL display device which is a typical example of a thin and light-weighted self-luminous display device is an extremely prospecting display device as a future display device.
The organic EL display device is classified into a so-called bottom-emission-type organic EL display device and a top-emission-type organic EL display device. In the bottom-emission-type organic EL display device, an organic EL element is constituted of a light emitting mechanism which is formed by sequentially stacking a transparent electrode (ITO or the like) which constitutes a first electrode or one electrode, a multi-layered organic film which emits light by applying an electric field thereto (also referred to as a organic light emitting layer), and a metal electrode having reflective property which constitutes a second electrode or another electrode on an insulation substrate which is preferably formed of a glass substrate. A large number of organic EL elements are arranged in a matrix array and another substrate or a sealing film which is referred to as a sealing can and covers the stacked structure is provided to interrupt the above-mentioned light emitting structure from an external atmosphere. Then, for example, by using a transparent electrode as an anode and a metal electrode as a cathode electrode and by applying an electric field between both electrodes, carriers (electrons and holes) are injected into the organic multi-layered film so as to allow the organic multi-layered film to emit light. This emission of light is radiated to the outside from a glass substrate side.
On the other hand, the top-emission-type organic EL display device is configured such that the above-mentioned one electrode is formed of a metal electrode having a reflective property and the above-mentioned another electrode is formed of a transparent electrode made of ITO or the like, an electric field is applied to both electrodes to allow the light emitting layer to emit light, and the light is radiated to another electrode side. In the top-emission-type organic EL display device, a transparent plate which is preferably formed of a glass plate may be used as the sealing can in the bottom-emission-type organic EL display device.
Such an organic EL display device has a drawback that an organic film which constitutes the light emitting layer is easily degraded due to moisture. Conventionally, a desiccant (a drying agent) is arranged in the inside of the sealing can or the sealing film.
With respect to this type of organic EL display device, patent document 1 discloses an organic EL display device which covers an organic light emitting layer with an insulation layer and an oxygen/moisture reaction layer and covers the organic light emitting layer with a resin layer thus sealing the organic light emitting layer. Patent document 2 discloses the organic EL display device by arranging a predetermined gas removing agent along a sealing material. Further, patent document 3 discloses the organic EL display device which seals an element by sandwiching a high moisture-absorbent film with low moisture-absorbent film.
Patent documents 1: JP-A-2000-348859
Patent documents 2: JP-A-2001-307872
Patent documents 3: JP-A-2001-357973
In patent document 1, since a moisture prevention layer is not provided between the oxygen/moisture reaction layer and the organic light emitting layer, the organic light emitting layer is degraded due to a gas which is diffused into the oxygen/moisture reaction layer or is separated from the oxygen/moisture reaction layer. When the desiccant is provided only to the outer periphery of the organic light emitting layer in patent document 2, a position at which the desiccant is arranged is limited and hence, it is not possible to incorporate a sufficient quantity of desiccant in the inside of the sealed space. In patent document 3, as described in
Further, when a flexible organic EL display device is realized by using a resilient substrate which constitutes a thin film transistor substrate and a polymer organic light emitting layer or in realizing or when a hard insulation substrate made of glass or the like is used and a resin film member is used for sealing the insulation substrate, the organic light emitting layer is degraded by the intrusion of a gas from a sealed end, the generation of a gas from a desiccant layer, and the re-discharge of the gas which is absorbed once.
Accordingly, it is an object of the present invention to provide an organic EL display device which can maintain a light emission efficiency thereof and can possess a prolonged lifetime thereof by suppressing the degradation attributed to moisture of a multi-layered organic light emitting layer which includes such sealing structure.
The means of the present invention which can achieve the above-mentioned object can be realized by providing a moisture prevention layer of high gas barrier property between an electrode which is arranged on an uppermost layer of an organic light emitting layer and a moisture absorption layer (desiccant) formed on a sealing film side. To describe specific constitutional examples of the present invention, they are as follows.
An organic EL display element of the present invention includes a first electrode which is formed on a main surface of an insulation substrate, an organic EL layer of the multi-layered structure which is formed on the first electrode, a second electrode which is formed on the organic EL layer, and a sealing member which covers the second electrode and has a peripheral end portion thereof sealed to a peripheral portion of the insulation substrate. An organic light emitting layer is constituted of the first electrode, the organic EL layer of the multi-layered structure and the second electrode.
Further, the organic EL display element is characterized by including a moisture-resistant structural body which covers an upper surface and a side surface of the organic EL layer and is formed by stacking a first moisture prevention layer, a moisture absorption layer and a second moisture prevention layer in this order, wherein the first moisture prevention layer, the moisture absorption layer and the second moisture prevention layer on the side surface of the organic EL layer are bent toward the side surface from the upper surface of the organic EL layer and, further, is bent parallel to a main surface of the insulation substrate from the side surface, and lower surfaces of the respective bent portions are hermetically adhered to the main surface of the substrate.
Further, the present invention is characterized in that an adhesive layer is formed between the moisture absorption layer and the second moisture prevention layer, and the first moisture prevention layer and the moisture absorption layer are fixedly mounted on the main surface of the substrate by the adhesive layer together with the second moisture prevention layer.
Further, the present invention is characterized in that the first moisture prevention layer is made of silicon nitride (SiN), the moisture absorption layer is made of calcium (Ca) and the second moisture prevention layer is made of aluminum (Al) foil.
Further, the present invention is characterized in that a first adhesive layer is formed between the organic EL layer and the first moisture prevention layer, and a second adhesive layer is formed between the first moisture prevention layer and the moisture absorption layer, and
the first moisture prevention layer is fixedly mounted on the main surface of the substrate by the first adhesive layer and, at the same time, the moisture absorption layer and the second moisture prevention layer are fixedly mounted on the main surface of the substrate by the second adhesive layer.
Further, the present invention is characterized in that the first moisture prevention layer is formed of an aluminum foil, the moisture absorption layer is made of zeolite (a product name), and the second moisture prevention layer is formed of an aluminum foil.
Further, the present invention is characterized in that the sealing member is formed of a laminate film made of polyethylene terephthalate.
Further, the present invention is characterized in that a caulking agent is applied to a periphery of the sealing member and a sealing region of the insulation substrate.
Further, the present invention is characterized in that the caulking agent is a silicon-based waterproof caulking agent.
Due to the respective means of the present invention, there is no possibility that a gas which is separated from a desiccant layer or a gas which is diffused in the desiccant layer after intruding from an end portion of a sealing layer reaches the organic light emitting layer thus suppressing the degradation of the organic light emitting layer. Since the material which exhibits high heat resistance and high chemical resistance can be used for forming the moisture prevention layer, the freedom in the selection of the desiccant can be increased. Further, it is possible to seal using the resin film and hence, it is possible to provide the display device which is light-weighted and thin and which exhibits high reliability and a prolonged lifetime.
Hereinafter, the present invention is explained in conjunction with embodiments by reference to drawings showing the embodiment.
The first moisture prevention layer DML1 is made of silicon nitride (SiN), the moisture absorption layer DSC is made of calcium (Ca), and the second moisture prevention layer DML2 is formed of an aluminum foil (Al). In this structure, peripheries of respective layers which constitute the moisture resistant structural body are bent in two steps, bent end surfaces extend along the main surface of the TFT substrate SUB, and extended portions are sealed to the TFT substrate SUB by the adhesive layer SEL. Further, a periphery of the sealing film CEF formed of a resin film, preferably a laminate film of polyethylene terephthalate is bent in two steps and extended portions are sealed by the caulking agent CUL. In this structure, an adhesive area between the moisture-resistant structural body and the sealing film CEF and the TFT substrate SUB is increased and hence, it is possible to effectively interrupt the sealed light emitting layer OLE from the external atmosphere including the elongation of an intrusion path of the moisture.
The first moisture prevention layer DML1 is formed of an aluminum foil (Al), the moisture absorption layer DSC is made of zeolite (product name), and the second moisture prevention layer DML2 is formed of an aluminum foil (Al). Also in this structure, peripheries of respective layers which constitute the moisture resistant structural body are bent in two steps, bent end surfaces extend along the main surface of the TFT substrate SUB, and extended portions are sealed to the TFT substrate SUB by the adhesive layer SEL. Further, a periphery of the sealing film CEF formed of a resin film, preferably a laminate film of polyethylene terephthalate is bent in two steps and extended portions are sealed by the caulking agent CUL. In this structure, an adhesive area between the moisture-resistant structural body and the sealing film CEF and the TFT substrate SUB is increased and hence, it is possible to effectively interrupt the sealed light emitting layer OLE from the external atmosphere including the elongation of an intrusion path of the moisture.
In the inside of the display region AR, data lines DL and gate lines GL which supply drive signals to the respective pixels are arranged in an intersecting manner. A portion of the insulation substrate SUB is larger than the sealing film CEF and projects from the sealing film CEF. A data line drive circuit chip DDR and a gate line drive circuit chip GDR are mounted on such a projecting portion and these chips supply display signals to the drain lines DL.
Number | Date | Country | Kind |
---|---|---|---|
2006-042275 | Feb 2006 | JP | national |
Number | Name | Date | Kind |
---|---|---|---|
5189405 | Yamashita et al. | Feb 1993 | A |
6195142 | Gyotoku et al. | Feb 2001 | B1 |
6891330 | Duggal et al. | May 2005 | B2 |
6992439 | Yamazaki et al. | Jan 2006 | B2 |
7345420 | Kubota | Mar 2008 | B2 |
7728326 | Yamazaki et al. | Jun 2010 | B2 |
20040177577 | Voegele et al. | Sep 2004 | A1 |
20040232833 | Menda et al. | Nov 2004 | A1 |
20060066236 | Tanaka et al. | Mar 2006 | A1 |
20060170341 | Su et al. | Aug 2006 | A1 |
Number | Date | Country |
---|---|---|
2000-348859 | Dec 2000 | JP |
2001-307872 | Nov 2001 | JP |
2001-357973 | Dec 2001 | JP |
10-2004-0098030 | Nov 2004 | KR |
Number | Date | Country | |
---|---|---|---|
20070194711 A1 | Aug 2007 | US |