This application claims the benefit of Korean Patent Application No. 10-2011-0024993, filed on Mar. 21, 2011, in the Korean Intellectual Property Office, the disclosure of which is incorporated herein in its entirety by reference.
1. Field
The present disclosure relates to an organic light-emitting display device, and more particularly, to an organic light-emitting display device that may minimize the reduction in contrast caused by reflection of external light.
2. Description of the Related Art
Organic light-emitting display devices, which are self-emitting display devices, have advantages of wide viewing angles and fast response times. However, the organic light-emitting display devices have disadvantages in that if the organic light-emitting display devices display images in an external light environment, the external light is reflected by metal materials for constituting electrodes and wires in the organic light-emitting display devices, thereby reducing contrast.
In general, in order to minimize the reduction in contrast, a polarization plate, which is expensive, may be used. However, the use of such a polarization plate may increase costs, reduce a transmittance because light emitted from a light-emitting layer is blocked, and reduces brightness.
In order to minimize the reduction in contrast, a black matrix may be formed on electrodes or wires. However, the use of such a black matrix may require an additional masking process to form the black matrix, which makes a manufacturing process complex.
An aspect of the present invention provides an organic light-emitting display device that may improve contrast by modifying the optical properties of surfaces of an electrode unit and a wiring unit.
According to an aspect of the present invention, there is provided an organic light-emitting display device including: a first substrate and a second substrate that face each other; an organic light-emitting device that is disposed between the first and second substrates and includes a pixel electrode separately formed in each pixel, a common electrode facing the pixel electrode, and an organic light-emitting layer disposed between the pixel electrode and the common electrode; and an electrode unit and at least one wiring unit that are disposed between the first substrate and the second substrate, the electrode unit including at least one thin-film transistor configured to transmit a light-emitting signal to the pixel electrode and at least one capacitor, wherein an optical property modification layer having an optical property modified from that of at least one of the electrode unit and the wiring unit is formed on a surface of the at least one of the electrode unit and the wiring unit.
The optical property modification layer may have a reflectance that is lower than a reflectance of each of the electrode unit and the at least one wiring unit.
The optical property modification layer may have a light-absorptance that is higher than a light-absorptance of each of the electrode unit and the at least one wiring unit.
The optical property modification layer may be different from the at least one of the electrode unit and the wiring unit in terms of at least one optical property selected from the group consisting of a transmittance, a refractive index, a diffraction, and a color.
The optical property modification layer may be formed by applying femtosecond-duration laser beam pulses to the surface of the at least one of the electrode unit and the wiring unit at least one time.
An area of the optical property modification layer modified by femtosecond-duration laser beam pulses may have a nanoscale or microscale size.
The at least one thin-film transistor includes a gate electrode, a source electrode, and a drain electrode, and the at least one capacitor includes an electrode.
The at least one wiring unit may include a gate wiring unit, a data wiring unit, and a power wiring unit.
Light emitted from the light-emitting layer may be emitted toward the second substrate, wherein the optical property modification layer is formed on the surface of the at least one of the electrode unit and the wiring unit that faces the second substrate, and wherein the organic light emitting display device comprises a second optical property modification layer having an optical property modified from that of the pixel electrode and formed on a surface of the pixel electrode close to the organic light-emitting layer.
The second optical property modification layer may have a reflectance that is lower than a reflectance of the pixel electrode.
The second optical property modification layer may have a light-absorptance that is higher than a light-absorptance of the pixel electrode.
Light emitted from the organic light-emitting layer may be emitted toward the first substrate, wherein the optical property modification layer is formed on the surface of the at least one of the electrode unit and the wiring unit that faces the first substrate, and wherein the organic light emitting display device comprises a second optical property modification layer having an optical property modified from that of the pixel electrode and formed on a surface of the common electrode close to the organic light-emitting layer.
The second optical property modification layer may have a reflectance that is lower than a reflectance of the common electrode.
The second optical property modification layer may have a light-absorptance that is higher than a light-absorptance of the common electrode.
The second optical property modification layer may be formed only on an area corresponding to the pixel electrode.
At least one of the first substrate and the second substrate may be a transparent substrate, wherein the organic light-emitting display device further includes a transparent interference layer that is disposed on a surface of the transparent substrate on which external light is incident.
The transparent interference layer may have a thickness equal to about ¼ of a wavelength of the external light.
The transparent interference layer may have a refractive index that is lower than a refractive index of the transparent substrate.
The transparent interference layer may include one material selected from the group consisting of magnesium fluoride, silica, a transparent material having a high refractive index, and a combination thereof.
The organic light-emitting display device further comprises a plurality of transparent interference layers disposed on a surface of the transparent substrate on which external light is incident, wherein the at least one transparent interference layer comprises a first transparent interference layer and a second transparent interference layer which is closer to the transparent substrate than the first transparent interference layer and has a refractive index greater than that of the first transparent interference layer.
Each transparent interference layer may have a thickness equal to about ¼ of a wavelength of the external light.
The above and other features and advantages of the present invention will become more apparent by describing in detail embodiments thereof with reference to the attached drawings in which:
Embodiments of the present invention will now be described more fully with reference to the accompanying drawings, in which embodiments of the invention are shown.
Referring to
In order to planarize the first substrate 110 and prevent impurity elements from penetrating into the first substrate 110, a buffer layer 111 formed of SiO.sub.2 and/or SiNx may be disposed on the first substrate 110. A first active layer 211 of the first thin-film transistor 21 and a second active layer 231 of the second thin-film transistor 23 are formed on the buffer layer 111, and a gate insulating film 112 is formed on the first and second active layers 211 and 231. A first gate electrode 212 of the first thin-film transistor 21 and a second gate electrode 232 of the second thin-film transistor 23 are formed on the gate insulating film 112. The first gate electrode 212 is connected to the gate wiring unit 26, and the second gate electrode 232 is connected to a first electrode 221 of the capacitor 22. An interlayer insulating film 113 is formed on the first gate electrode 212, the second gate electrode 232, and the first electrode 221 of the capacitor 22. A first source electrode 213 and a first drain electrode 214 are respectively connected through contact holes to a source region (not shown) and a drain region (not shown) of the first active layer 211. A second source electrode 233 and a second drain electrode 234 are respectively connected to a source region (not shown) and a drain region (not shown) of the second active layer 221. The first source electrode 213 is connected to the data wiring unit 27 to apply a data signal to the first active layer 211, and the first drain electrode 214 is connected to the first electrode 221 of the capacitor 22 to store the data signal in the capacitor 22. The second source electrode 233 is connected to a second electrode 222 of the capacitor 22, and the second drain electrode 234 is connected to the pixel electrode 241 of the organic light-emitting device 24. A passivation layer 114 is formed on the first and second source electrodes 213 and 233, the first and second drain electrodes 214 and 234, and the second electrode 222 of the capacitor 22. The pixel electrode 241 is connected to the second drain electrode 234 through a via-hole in the passivation layer 114. A pixel defining layer 115 is formed over the passivation layer 114 and defines the light-emitting area(s) of the organic light-emitting display device 1.
The organic light-emitting device 24 includes the pixel electrode 241 separately formed for each pixel, the common electrode 243 facing the pixel electrode 241, and the organic light-emitting layer 242 disposed between the pixel electrode 241 and the common electrode 243.
If the organic light-emitting display device 1 is a top-emission type, the pixel electrode 241 may be a reflective electrode and the common electrode 243 may be a transparent electrode. On the contrary, if the organic light-emitting display device is a bottom-emission type, the pixel electrode 241 may be a transparent electrode and the common electrode 243 may be a reflective electrode.
In general, electrodes constituting the first and second thin-film transistors 21 and 23 and the capacitor 22 are formed of metals having a high reflectance, and wires connected to the first and second thin-film transistors 21 and 23 and the capacitor 22 are formed of metals having a high reflectance. Accordingly, external light incident on the organic light-emitting display device 1 from the outside is reflected by the electrodes and the wires disposed over the first substrate 110, and then is emitted together with light emitted from the organic light-emitting layer 242. The light reflected by the electrodes and the wires reduces the contrast of the organic light-emitting display device 1.
An organic light-emitting display device 2 according to an embodiment of the present invention will be explained with reference to
Referring to
In embodiments, optical property modification layers 31, 32, 33, 35, 36, and 37 are obtained by modifying the optical properties of the wiring units 25, 26, and 27, the first and second gate electrodes 212 and 232 of the first and second thin-film transistors 21 and 23, the first and second source electrodes 213 and 233 of the first and second thin-film transistors 21 and 23, and the first and second drain electrodes 214 and 234 of the first and second thin-film transistors 21 and 23. Thus, each of the optical property modification layers 31, 32, 33, 35, 36, and 37 has optical properties modified and different from those of each of the wiring units 25, 26, and 27, the first and second gate electrodes 212 and 232 of the first and second thin-film transistors 21 and 23, the first and second source electrodes 213 and 233 of the first and second thin-film transistors 21 and 23, and the first and second drain electrodes 214 and 234 of the first and second thin-film transistors 21 and 23. Each of the optical property modification layers 31, 32, 33, 35, 36, and 37 is formed by treating a surface of each of the wiring units 25, 26, and 27, the first and second gate electrodes 212 and 232 of the first and second thin-film transistors 21 and 23, the first and second source electrodes 213 and 233 of the first and second thin-film transistors 21 and 23, and the first and second drain electrodes 214 and 234 of the first and second thin-film transistors 21 and 23.
In detail, the optical property modification layers 35, 36, and 37 are formed on the top surfaces of the power wiring unit 25, the gate wiring unit 26, and the data wiring unit 27, respectively. Optical property modification layers 312, 313, and 314 of the optical property modification layer 31 are formed on the top surfaces of the first gate electrode 212, the first source electrode 213, and the first drain electrode 214 of the first thin-film transistor 21, respectively. Optical property modification layers 332, 333, and 334 of the optical property modification layer 33 are formed on the top surfaces of the second gate electrode 232, the second source electrode 233, and the second drain electrode 234 of the second thin-film transistor 23, respectively. Optical property modification layers 321 and 322 of the optical property modification layer 32 are formed on the top surfaces of the first electrode 221 and the second electrode 222 of the capacitor 22, respectively.
The optical property modification layers 31, 32, 33, 35, 36, and 37 are formed on the wiring units 25, 26, and 27 and the top surfaces of the electrodes 212, 213, 214, 232, 233, 234, 221, and 222 of the thin film transistors 21 and 23, and the capacitor 22, and are obtained by modifying optical properties of the wiring units 25, 26, and 27 and the electrodes 212, 213, 214, 232, 233, 234, 221, and 222. For example, the optical property modification layers 31, 32, 33, 35, 36, and 37 may be obtained by modifying at least one optical property from among a reflectance, a light-absorptance, a transmittance, a refractive index, a diffraction, and a color of metal materials for constituting the wiring units 25, 26, and 27 and the electrodes 212, 213, 214, 232, 233, 234, 221, and 222. In
In the organic light-emitting display device 2 that is a top-emission type where an image is formed away from the first substrate 110, external light that enters the organic light-emitting display device 2 may be reflected by surfaces of the electrodes 212, 213, 214, 232, 233, 234, 221, and 222 and the wiring units 25, 26, and 27, thereby reducing the contrast of light emitted from the organic light-emitting layer 242. However, the optical property modification layers 31, 32, 33, 35, 36, and 37 are formed on surfaces of the electrodes 212, 213, 214, 232, 233, 234, 221, and 222 and the wiring units 25, 26, and 27, which face away from the first substrate 10. Thus, the amount of external light reflected by the electrodes 212, 213, 214, 232, 233, 234, 221, and 222 and the wiring units 25, 26, and 27 may be reduced, thereby improving contrast.
In WO 2008/097374 of Chunlei et al., published on Aug. 14, 2008, entitled “Ultra-short duration laser methods for the nanostructuring of materials”, which is incorporated by reference herein, a method of modifying the optical properties of materials is disclosed. According to the above method, the application of femtosecond-duration laser beam pulses to a metal may change the surface structure of the metal such that the modified structure of the metal can have a nanoscale or microscale size, and the optical property of the surface layer of the metal can be modified. In embodiments, the metal can be exposed to femtosecond-duration laser beam pulses at least once to obtain the modified structure change of the metal.
Accordingly, when aluminum is used for the wiring units 25, 26, and 27 and the electrodes 212, 213, 214, 232, 233, 234, 221, and 222 of the organic light-emitting display device 2, such surface treatment is performed by using the afore-described femtosecond laser beam technology on the top surfaces of the wiring units 25, 26, and 27 and the electrodes 212, 213, 214, 232, 233, 234, 221, and 222 can change the optical properties of the top surfaces of the wiring units 25, 26, and 27 and the electrodes 212, 213, 214, 232, 233, 234, 221, and 222. In other words, a treated surface of aluminum having a lower reflectance or a higher light-absorptance than an untreated surface of aluminum forms the optical property modification layers 31, 32, 33, 35, 36, and 37 on the top surfaces of the wiring units 25, 26, and 27 and the electrodes 212, 213, 214, 232, 233, 234, 221, and 222. Thus, the amount of external light reflected by the wiring units 25, 26, and 27 and the electrodes 212, 213, 214, 232, 233, 234, 221, and 222 may be reduced.
Accordingly, without using an expensive polarization plate and without forming a black matrix by performing an additional masking process, contrast may be improved by simply modifying the optical properties of the wiring units 25, 26, and 27 and the electrodes 212, 213, 214, 232, 233, 234, 221, and 222.
Although two thin-film transistors 21 and 23 and one capacitor 22 constitute one pixel in
An organic light-emitting display device 3 that is a top-emission type, according to another embodiment of the present invention, will be explained with reference to
Referring to
The optical property modification layers 31, 32, 33, 35, 36, and 37 obtained by modifying the optical properties of the wiring units 25, 26, and 27, the first and second gate electrodes 212 and 232 of the first and second thin-film transistors 21 and 23, the first and second source electrodes 213 and 233 of the first and second thin-film transistors 21 and 23, and the first and second drain electrodes 214 and 234 of the first and second thin-film transistors 21 and 23 are disposed on top surfaces of the wiring units 25, 26, and 27, the first and second gate electrodes 212 and 232 of the first and second thin-film transistors 21 and 23, the first and second source electrodes 213 and 233 of the first and second thin-film transistors 21 and 23, and the first and second drain electrodes 214 and 234 of the first and second thin-film transistors 21 and 23.
Also, in the illustrated embodiments, an optical property modification layer 34 is disposed on a top surface of the pixel electrode 241.
In the organic light-emitting display device 3 that is a top-emission type, the pixel electrode 241 is a reflective electrode. Accordingly, external light incident on the organic light-emitting display device 3 may be reflected by the top surface of the pixel electrode 241 and then may be emitted along with light emitted from the organic light-emitting layer 242. The external light reflected by the top surface of the pixel electrode 241 may reduce contrast of the organic light-emitting display device 3.
However, in the organic light-emitting display device 3 of
Of course, like in
An organic light-emitting display device 4 that is a top-emission type, according to another embodiment of the present invention, will be explained with reference to
Referring to
The optical property modification layers 31, 32, 33, 34, 35, 36, and 37 obtained by modifying the optical properties of the wiring units 25, 26, and 27, the first and second gate electrodes 212 and 232 of the first and second thin-film transistors 21 and 23, the first and second source electrodes 213 and 233 of the first and second thin-film transistors 21 and 23, the first and second drain electrodes 214 and 234 of the first and second thin-film transistors 21 and 23, and the pixel electrode 241 are disposed on top surfaces of the wiring units 25, 26, and 27, the first and second gate electrodes 212 and 232 of the first and second thin-film transistors 21 and 23, the first and second source electrodes 213 and 233 of the first and second thin-film transistors 21 and 23, the first and second drain electrodes 214 and 234 of the first and second thin-film transistors 21 and 23, and the pixel electrode 241, respectively.
Also, the transparent interference layer 60 is disposed on a surface of a second substrate 50.
The transparent interference layer 60 is disposed on a surface of the second substrate 50, which is a transparent substrate, on which external light is incident. The external light enters the organic light-emitting display device 4 by passing through the second substrate 50, but part of the external light is directly reflected by the surface of the second substrate 50. Accordingly, the light reflected by the surface of the second substrate 50 may enter an observer's eyes along with light emitted from the organic light-emitting layer 242, and may reduce contrast.
However, in the organic light-emitting display device 4 of
Referring to
In this case, the thickness ‘d’ of the transparent interference layer 60 may be determined in various ways, for example, based on a wavelength of external light, by using an arithmetical mean of wavelengths defining a visible spectrum of light, or an arithmetical mean of wavelengths defining a spectrum of external light.
It is preferable that the transparent interference layer 60 has a refractive index n1 between a refractive index n0=1 of air and a refractive index n2 of the second substrate 50. If the second substrate 50 is a general glass having a refractive index n1 of about 1.5, in one embodiment, the refractive index n1 of the transparent interference layer 60 can be about 1.23, but it is difficult to find a material having an appropriate refractive index.
In the present embodiment, the transparent interference layer 60 is formed of magnesium fluoride having a refractive index of about 1.38. Magnesium fluoride has high durability and is easily deposited by physical vapour deposition (PVD). Alternatively, the transparent interference layer 60 may be formed of silica or any of various transparent materials having a high refractive index.
In
Referring to
Part Lr1 of the external light Li is reflected by the first transparent interference layer 61, and part Lr1′ of the light Lt is reflected at a boundary between the second transparent interference layer 62 and the first transparent interference layer 61. In this case, if a thickness d1 of the first transparent interference layer 61 corresponds to ¼ of a wavelength λ of the external light Li, the light Lr1 reflected by the first transparent interference layer 61 and the light Lr1′ reflected at the boundary between the second transparent interference layer 62 and the first transparent interference layer 61 are offset due to interference.
Part Lr2 of the external light Li is reflected by the second transparent interference layer 62, and part Lr2′ of the light Lt is reflected at a boundary between the third transparent interference layer 63 and the second transparent interference layer 62. In this case, if a thickness d2 of the second transparent interference layer 62 corresponds to ¼ of the wavelength λ of the external light Li, the light Lr2 reflected by the second transparent interference layer 62 and the light Lr2′ reflected at the boundary between the third transparent interference layer 63 and the second transparent interference layer 62 are offset due to interference.
Part Lr3 of the external light Li is reflected by the third transparent interference layer 63, and part Lr3′ of the light Lt is reflected at a boundary between the second substrate 50 and the third transparent interference layer 63. In this case, if a thickness d3 of the third transparent interference layer 63 corresponds to ¼ of the wavelength λ of the external light Li the light Lr3 reflected by the third transparent interference layer 63 and the light Lr3′ reflected at the boundary between the second substrate 50 and the third transparent interference layer 63 are offset due to interference. Accordingly, the amount of external light reflected is reduced and thus contrast is improved.
An organic light-emitting display device 5 according to another embodiment of the present invention will be explained with reference to
Referring to
Since the organic light-emitting display device 5 is a bottom-emission type where light is emitted from the organic light-emitting layer 242 toward the first substrate 110, the first substrate 110 is a transparent substrate. The common electrode 243 is a reflective electrode, and the pixel electrode 241 is a transparent electrode.
External light that enters the organic light-emitting display device 5 through the first substrate 110 may be reflected by electrodes and wiring units having a higher reflectance, and then may be emitted along with light emitted from the organic light-emitting layer 242, thereby reducing contrast.
Accordingly, in the organic light-emitting display device 5, since optical property modification layers 41, 42, 43, 45, 46, and 47 obtained by modifying the optical properties of the wiring units 25, 26, and 27, the first and second gate electrodes 212 and 232 of the first and second thin-film transistors 21 and 23, the first and second source electrodes 213 and 233 of the first and second thin-film transistors 21 and 23, and the first and second drain electrodes 214 and 234 of the first and second thin-film transistors 21 and 23 are disposed on bottom surfaces of the wiring units 25, 26, and 27, the first and second gate electrodes 212 and 232 of the first and second thin-film transistors 21 and 23, the first and second source electrodes 213 and 233 of the first and second thin-film transistors 21 and 23, and the first and second drain electrodes 214 and 234 of the first and second thin-film transistors 21 and 23, the amount of external light reflected by the wiring units 25, 26, and 27 and the electrodes 212, 213, 214, 232, 233, and 234 may be reduced.
Also, an optical property modification layer 44 obtained by modifying an optical property of the common electrode 243 is formed on a surface of the common electrode 243, which is a reflective electrode, facing the organic light-emitting layer 242. Accordingly, since the optical property modification layer 44 has a reflectance lower than that of the common electrode 243 or a light-absorptance higher than that of the common electrode 243, the amount of external light reflected by the common electrode 213 that is a reflective electrode may be reduced. Although the optical property modification layer 44 may be formed on an entire area of the common electrode 243, the optical property modification layer 44 may be formed on a part A corresponding to an area where the organic light-emitting layer 242 is to be formed, as shown in
Also, the transparent interference layer 60 is disposed on a surface of the first substrate 110, which is a transparent substrate, on which external light is incident. The transparent interference layer 60 may reduce the amount of external light directly reflected by the surface of the first substrate 110, and improve contrast.
As described above, an organic light-emitting display device according to the one or more embodiments of the present invention has the following effects:
First, since optical property modification layers are formed on surfaces of electrodes and wiring units, the amount of external light reflected by the electrodes and the wiring units may be reduced and contrast may be improved.
Second, since an optical property modification layer is formed on a surface of a reflective electrode, the amount of external light reflected by the reflective electrode may be reduced, and contrast reduction may be minimized.
Third, since a transparent interference layer is formed on a transparent substrate of the organic light-emitting display device, the amount of external light reflected by the transparent substrate may be reduced and contrast may be prevented from being reduced.
While embodiments of the present invention have been particularly shown and described, it will be understood by those of ordinary skill in the art that various changes in form and details may be made therein without departing from the spirit and scope of the present invention as defined by the following claims.
Number | Date | Country | Kind |
---|---|---|---|
10-2011-0024993 | Mar 2011 | KR | national |
Number | Name | Date | Kind |
---|---|---|---|
7282855 | Park et al. | Oct 2007 | B2 |
8212280 | Ikeda et al. | Jul 2012 | B2 |
20030016196 | Lueder et al. | Jan 2003 | A1 |
20030107326 | Park et al. | Jun 2003 | A1 |
20050067378 | Fuerhaupter et al. | Mar 2005 | A1 |
20050263775 | Ikeda et al. | Dec 2005 | A1 |
20080216926 | Guo et al. | Sep 2008 | A1 |
20080218067 | Lee et al. | Sep 2008 | A1 |
20100148204 | Ikeda et al. | Jun 2010 | A1 |
20110204370 | Yoon et al. | Aug 2011 | A1 |
Number | Date | Country |
---|---|---|
2008-071578 | Mar 2008 | JP |
10-2003-0044744 | Jun 2003 | KR |
10-2005-0012958 | Feb 2005 | KR |
10-2005-0119894 | Dec 2005 | KR |
Entry |
---|
O. S. Heavens, Optical properties of thin solid films, 1991, Dover Publications, Inc., pp. 207-219. |
Young. Hugh D. and Freedman Roger A, University Physics; Pierson; 12-th edition; pp. 1223-1224. |
Number | Date | Country | |
---|---|---|---|
20120241775 A1 | Sep 2012 | US |