The present invention relates to methods and compositions for treating subterranean formations, and more specifically, to improved methods and compositions for generating acids for use downhole, for example, to at least partially degrade the acid-soluble portions of filter cakes deposited in subterranean formations.
Filter cakes, e.g., residues deposited on permeable media when servicing fluids contact those media under pressure, are formed in a variety of subterranean operations such as drilling, fracturing, and gravel packing. A filter cake is often desirable, at least temporarily, as it may prevent a fluid from flowing from a desired location to the surrounding subterranean formation. Moreover, the presence of a filter cake may add strength and stability to the formation surfaces on which the filter cake forms.
Filter cakes can form in many subterranean processes. For example, a drill-in fluid in an open hole can form a filter cake. Such filter cakes generally comprise an acid-soluble portion and a polymeric portion. Filter cakes also may be formed during a fracturing operation. As a fracture is created, a portion of the fluid contained in the viscous fracturing fluid may create a filter cake comprising deposited viscosifier and/or fluid loss control additives, inter alia, on the walls of the fracture and/or the formation.
No matter which process forms a filter cake, the filter cake generally acts as a physical barrier to fluid flow that may reduce fluid loss into the producing zone. The filter cake also presents a barrier to flow of liquid from the zone; thus, at some point before the well is put into production, the filter cake generally is removed so that the formation may be placed on production.
While filter cakes may be beneficial, it is generally necessary to remove filter cakes from producing zones once the well is placed into production. For example, to degrade the acid-soluble portion of a drill-in fluid filter cake, a conventional delayed-release acid system usually may be used. A common type of delayed-release acid system comprises esters that slowly hydrolyze to form acids that may ultimately degrade the acid-soluble portion of the filter cake. These delayed-release acid systems, however, can be problematic if they degrade the acid-soluble component of the filter cake too slowly or too quickly. Removal of only 1% to 2% of the bridging solids in the filter cake can result in a significant loss of fluid to the surrounding formation. If a delayed-release acid system is designed not to dissolve more than 1% or 2% of the acid-soluble portion of the filter cake in a chosen period of time (e.g., a 12-hour period), then total removal may take days, if not weeks. This is undesirable. On the other hand, if a delayed-release acid system is designed to totally degrade the acid-soluble portion within an acceptable “total cleanup time” (e.g., 24 to 48 hours), it is likely to cause hole instability and potential fluid loss problems during gravel pack placement. To control such fast-acting delayed-release acid systems, buffers (which are mixtures of weak acids and their conjugate bases) may be considered to achieve a delayed interaction of the acid with the acid-soluble portion of the filter cake for a desired time period. However, such conventional buffer systems have met with little success when used with these delayed-release acid systems, inter alia, because the esters may undergo acid- or base-catalyzed hydrolysis at pHs much below or above 7. Also, conventional buffers may suffer when exposed to components, such as calcium carbonate, in the filter cake and, as a result, the acid component of the buffer may be quickly consumed.
The present invention relates to methods and compositions for treating subterranean formations, and more specifically, to improved methods and compositions for generating acids for use downhole, for example, to at least partially degrade the acid-soluble portions of filter cakes deposited in subterranean formations.
In one embodiment, the present invention provides a method of degrading an acid-soluble portion of a filter cake comprising contacting the acid-soluble portion of the filter cake with an acid generated from an orthoester.
In another embodiment, the present invention provides a method of generating an acid in a subterranean formation comprising the steps of: providing an orthoester composition that comprises an orthoester; placing the orthoester composition in the formation; and allowing the orthoester to generate an acid in the formation.
In another embodiment, the present invention provides a method of degrading an acid-soluble component in a subterranean formation comprising the steps of: providing an orthoester composition that comprises an orthoester; placing the orthoester composition in the formation; allowing the orthoester to generate a generated acid; and allowing the generated acid to at least partially degrade the acid soluble component.
In another embodiment, the present invention provides a method of degrading a filter cake in a subterranean formation comprising the steps of: providing particulates coated or impregnated with an orthoester composition that comprises an orthoester; placing the particulates into the subterranean formation so that they are substantially adjacent to the filter cake; allowing the orthoester to generate a generated acid; and allowing the generated acid to degrade at least a portion of an acid-soluble portion of the filter cake.
In another embodiment, the present invention provides a composition capable of degrading an acid soluble component in a subterranean formation comprising an orthoester that will generate an acid that is capable of degrading at least a portion of the acid soluble component.
The features and advantages of the present invention will be readily apparent to those skilled in the art upon a reading of the description of the preferred embodiments, which follows.
The present invention relates to methods and compositions for treating subterranean formations, and more specifically, to improved methods and compositions for generating acids for use downhole, for example, to at least partially degrade the acid-soluble portions of filter cakes deposited in subterranean formations. One of the desirable features of the compositions and methods of the present invention is that they provide for the delayed release of an acid. The compositions and methods of the present invention are suitable for any application wherein it is desirable to generate an acid downhole that may be useful. Another instance where these compositions and methods may be useful is for reducing the viscosity of a viscosified treatment fluid.
In certain embodiments wherein the compositions and methods of the present invention are used to degrade a filter cake, one of the many benefits offered by the present invention includes the fact that the well does not need to be shut-in for long periods of time to accomplish a substantial, beneficial degradation of the filter cake so as to be able to put the well into production. With the compositions and methods of the present invention, a desirable degradation of a filter cake can be obtained in a highly desirable period of time.
The orthoester compositions of the present invention comprise orthoesters. These orthoesters will generate acids that will degrade the acid-soluble portion of a filter cake. Examples of suitable orthoesters have a structure defined by the formula: RC(OR′)(OR″)(OR′″), wherein R′, R″, and R′″ are not hydrogen, and R′, R″, and R′″ may or may not be the same group. R′, R″, or R′″ may comprise a heteroatom that may affect the solubility of the chosen orthoester in a given application. Suitable heteroatoms could include nitrogen or oxygen. Examples of suitable orthoesters and poly(orthoesters) include, but are not limited to, orthoacetates, such as trimethyl orthoacetate, triethyl orthoacetate, tripropyl orthoacetate, triisopropyl orthoacetate, and poly(orthoacetates); orthoformates, such as trimethyl orthoformate, triethyl orthoformate, tripropyl orthoformate, triisopropyl orthoformate, and poly(orthoformates); and orthopropionates, such as trimethyl orthopropionate, triethyl orthopropionate, tripropyl orthopropionate, triisopropyl orthopropionate, and poly(orthopropionates). Suitable orthoesters also may be orthoesters of polyfunctional alcohols, such as glycerin and/or ethylene glycol. Those skilled in the art with the benefit of this disclosure will recognize suitable orthoesters that may be used in a desired application. In choosing an orthoester, one should be mindful that some orthoesters have low flash points. Therefore, the choice of which particular orthoester to use should be guided by such considerations as environmental factors. The orthoester may comprise less than about 1% to about 100% of the orthoester composition.
To allow the orthoester to hydrolyze to produce an acid, a source of water is needed. The water should be present in an amount from about 2 moles of water for about every 1 mole of orthoester to an excess of water, which may help ensure the solubility of the reaction product of the reaction between the generated acid and the acid-soluble component, e.g., solubility with the acid-soluble portion of a filter cake. One of ordinary skill in the art with the benefit of this disclosure will recognize whether a suitable amount of water is present in either the orthoester composition or in the well bore for a desired application.
The orthoester compositions of the present invention also may comprise an inhibitor, which may delay the generation of the acid from the orthoester of the orthoester composition and also may neutralize the generated acid during the delay period. Suitable inhibitors include bases. Examples of some preferred inhibitors may include sodium hydroxide, potassium hydroxide, amines such as hexamethylenetetramine, sodium carbonate, and combinations thereof. In certain embodiments, a small amount of a strong base as opposed to a large amount of a relatively weak base is preferred to achieve the delayed generation of the acid and the neutralization of the generated acid for a desired delay period.
The orthoester compositions of the present invention can have any suitable form. For instance, these compositions can be used in a solution form, a gel form, or an emulsion form. In certain applications, a solution form may be useful, e.g., when a faster break of a treatment fluid or a faster degradation of a filter cake, is desired; in other applications, e.g., when a slower break or degradation is desirable, a gel or emulsion form may be used. For the solution form, suitable exemplary solvents include propylene glycol, propylene glycol monomethyl ether, dipropylene glycol monomethyl ether, and ethylene glycol monobutyl ether. In some embodiments, mixtures of solvents and water may be beneficial, for example, to keep the orthoester solubilized. The gel form of the orthoester composition may be gelled with suitable polymers and/or surfactants. For the emulsion form, suitable emulsifiers include emulsifiers like “WS-44,” which is commercially available from Halliburton Energy Services, Duncan, Okla.
In some embodiments of the present invention wherein an orthoester composition of the present invention is used to degrade a filter cake, if desired, chemical components that can degrade a polymeric portion of a filter cake may be used in conjunction with an orthoester composition of the present invention. Suitable examples include compatible oxidizers and/or enzymes that are capable of degrading the polymeric components of the filter cake. These oxidizers or enzymes may be in any suitable form, for example, encapsulated or otherwise contained to create a beneficial release of the oxidizer or enzyme.
In alternative embodiments of the methods of the present invention, an orthoester composition of the present invention may be coated or impregnated onto a particulate that will be placed downhole in a subterranean treatment such as fracturing or gravel packing. When the orthoester ultimately hydrolyzes and generates the acid, the acid may degrade the acid-soluble portion of a filter cake, e.g., at least that portion substantially adjacent to the coated particulates. The generated acid also may act as a breaker for a viscosified treatment fluid, such as a fracturing or gravel pack fluid.
Any particulate suitable for use in conjunction with subterranean applications is suitable for use as particulates in these embodiments of the methods of the present invention. For instance, natural sand, quartz sand, particulate garnet, glass, ground walnut hulls, polymeric pellets, bauxite, ceramics, or the like are all suitable. Suitable sizes range from about 4 to about 100 U.S. mesh, in certain preferred embodiments, the sizes may range from about 10 to about 70 U.S. mesh.
The orthoester compositions of the present invention may be coated onto a particulate material by any means known in the art. For instance, in one embodiment, the particulates may be coated with an orthoester composition “on-the-fly.” The term “on-the-fly” is used herein to refer to an instance where one flowing stream is continuously introduced into another flowing stream so that the streams are combined and mixed while continuing to flow as a single stream as part of an ongoing treatment. Such mixing can also be described as “real-time” mixing. Batch or partial batch mixing processes may also be suitable. The coated particulate as described herein may be used as gravel particles in sand control operations, as proppant particles in fracturing operations, or as any other particulate employed in subterranean operations that may be placed substantially adjacent to a filter cake comprising an acid-soluble component.
Where the orthoester composition is a relatively solid material at ambient temperatures, it may be advantageous to mix the orthoester composition with a solvent to facilitate the coating of the orthoester composition onto the particulates. A variety of solvents known in the art may be suitable. Some such solvents include, but are not limited to, acetone, propylene carbonate, dipropylene glycol methyl ether, methylene chloride, isopropyl alcohol, or combinations thereof.
In some embodiments of the present invention, the particulates are coated with from about 0.1% to about 20% orthoester composition by weight of the particulates, more preferably from about 0.5% to about 10% orthoester composition by weight of the particulates, and most preferably from about 1% to about 8% orthoester composition by weight of the particulate material.
In some embodiments, 100% of the particulates are coated with an orthoester composition of the present invention; in other embodiments, only a portion of the particulates may be coated. Where less than 100% of the particulates are coated with an orthoester composition of the present invention, it may be desirable to use a higher concentration of orthoester composition relative to that portion of the particulates to be coated. It is within the ability of one skilled in the art with the benefit of this disclosure to determine the amount of orthoester composition that will be necessary to sufficiently degrade the filter cake and to coat a portion of particulates with enough orthoester composition to achieve that goal.
Where the coated particulates are used in a sand control operation such as gravel packing, the gravel pack may be formed using any technique known in the art. In one technique, gravel particles (at least a portion of which are partially coated with an orthoester composition of the present invention) are slurried into a treatment fluid and pumped into the well bore having a filter cake deposited therein substantially adjacent to the zone of the subterranean formation that has been fitted with a gravel pack screen. In alternative embodiments, it is possible to not use a screen if desired. The gravel particulates are separated from the slurry as the delivery fluid is forced into the well bore through the screen if a screen is used. The gravel particulates are not able to flow through the mesh of the screen and are left behind, forming a gravel pack. The acid generated by the orthoester composition on the particulates then degrades the acid-soluble portion of the adjacent filter cake.
When the coated particulates are used in a fracturing operation, the proppant pack formed inside a fracture from at least some of the coated particulates of the present invention may be formed using any technique known in the art. In one technique, proppant particulates comprising at least some coated particulates of the present invention are slurried into a fracturing fluid and pumped into a subterranean formation at a pressure sufficient to create or enhance a fracture in the formation. At least a portion of those particulates is then placed in a fracture and forms a proppant pack substantially adjacent to the walls of the fracture. The fracturing fluid also forms a filter cake on the surfaces of the fracture. Once the proppant pack is substantially formed, the orthoester composition produces an acid that at least partially degrades the filter cake on the surfaces of the fracture.
Although this invention has been described in terms of some specific uses of the orthoester compositions of the present invention, the orthoester compositions may be used in other applications, for example, to degrade other acid-soluble components in a subterranean formation like the formation itself, calcium carbonate, acid-soluble components of completion equipment such as plugs, or resins (e.g., thermosetting resins).
To facilitate a better understanding of the present invention, the following examples of preferred embodiments are given. In no way should the following examples be read to limit the scope of the invention.
Six samples were prepared to illustrate the acid generated by the orthoester compositions and its reaction with calcium carbonate. These six samples are shown in Table 1 and were prepared by the following procedure. In a suitable flask, a quantity of water was added. Then to the flask, a quantity of “WS-44” emulsifier was added. The orthoester composition was then added. This was then stirred for 5 minutes to create an emulsion. While continuing to stir, calcium carbonate was added. A sodium hydroxide solution was added. The mixture was heated to a temperature of 135° F. The CO2 gas generation was then monitored to observe the extent of calcium carbonate dissolution with time. Tables 2 through 7 illustrate these results for each sample.
Thus, the present invention is well adapted to carry out the objects and attain the ends and advantages mentioned as well as those, which are inherent therein. While numerous changes may be made by those skilled in the art, such changes are encompassed within the spirit and scope of this invention as defined by the appended claims.
This application is a continuation-in-part of application Ser. No. 10/641,242, entitled Compositions and Methods for Degrading Filter Cake, filed on Aug. 14, 1003, and application Ser. No. 10/650,101, entitled Compositions and Methods for Reducing the Viscosity of a Fluid, filed on Aug. 26, 2003.
Number | Date | Country | |
---|---|---|---|
Parent | 10641242 | Aug 2003 | US |
Child | 10752752 | Jan 2004 | US |
Parent | 10650101 | Aug 2003 | US |
Child | 10752752 | Jan 2004 | US |