Outer cover for an absorbent article

Information

  • Patent Grant
  • 8974432
  • Patent Number
    8,974,432
  • Date Filed
    Friday, July 22, 2011
    12 years ago
  • Date Issued
    Tuesday, March 10, 2015
    9 years ago
Abstract
An outer cover for an absorbent article has an absorbent capacity in addition to the absorbency of an absorbent insert. The outer cover may have two or more layers, at least one of which has liquid absorption capacity. Another layer may be hydrophobic. The outer cover as a whole may be breathable and water-impermeable.
Description
FIELD OF THE INVENTION

This disclosure relates generally to an outer cover for an absorbent article, and more specifically to an outer cover with liquid absorptive capacity.


BACKGROUND OF THE INVENTION

Absorbent articles fitted to the body of a wearer are sometimes used to absorb body exudates, such as urine, feces, or menses. Absorbent articles may be used, for example, by infants who have not been toilet trained, or by children or adults experiencing incontinence due to illness or infirmity, or by menstruating women. Absorbent articles may be disposable or reusable, or a combination of the two. For example, an absorbent article may have a disposable absorbent insert for collecting and containing body fluids, and a reusable outer cover which holds the disposable absorbent insert near the body of the wearer during use.


A disposable absorbent insert may be intended to capture all body exudates; however, some volume of exudates may not be absorbed by the insert, or may not be absorbed immediately. For example, the absorbent capacity of the insert may be exceeded in at least a portion of the insert; or a release of exudates may occur at a rate greater than the maximum rate of absorption of the insert; or the position of the insert relative to the body of the wearer may be such that a small amount of fluid is not directed to the insert, but rather moves beyond the insert and into the outer cover. In such situations, it may be desirable that the outer cover keeps these exudates contained within the absorbent article. Containment may, for example, prevent the soiling of nearby surfaces in the wearer's environment, such as the wearer's clothes, a caregiver's clothes, bedding, furniture, and the like.


One approach to containing such loose substances within the absorbent article is to use a hydrophobic outer cover and secure it tightly to the wearer, particularly around the legs and waist, as by elastic leg bands and waist bands. However, liquid or semi-liquid wastes may pool and collect along the edges of a hydrophobic material, such that any gapping at the leg or waist bands will allow errant wastes to escape. Further, tight closures may be uncomfortable, constrain wearer movement, leave red marks on or abrade the skin, limit the adaptability of a single size of an outer cover to fit a range of wearer shapes and sizes, or have other limitations.


There remains a need for an outer cover for an absorbent article which is comfortable, conformable to a wearer, and contains exudates not absorbed by the absorbent insert within the absorbent article.


SUMMARY OF THE INVENTION

In some aspects, the invention relates to an outer cover for an absorbent article. The outer cover may comprise a first, wearer-facing layer having a wearer-facing surface, and a second, garment-facing layer. The outer cover may have an absorbent capacity between 5 and 100 g, and the wearer-facing surface of the first, wearer-facing layer may have a DAT contact angle at 0.5 second of less than about 75 degrees. The second, garment-facing layer may be hydrophobic. The outer cover as a whole may have a WVTR between 1,200 g/m2/24 hr and 15,000 g/m2/24 hr, or between 3,000 g/m2/24 hr and 10,000 g/m2/24 hr. The wearer-facing surface of the first, wearer-facing layer may have a nonpolar component of surface energy of less than about 3.5 mJ/mm2, or less than about 3.0 mJ/mm2, or less than about 2.5 mJ/mm2. The wearer-facing surface of the first, wearer-facing layer may have a DAT contact angle at 1 second of less than about 70 degrees, or less than about 45 degrees. The first, wearer-facing layer may have a strikethrough time of less than about 15 seconds, or less than about 10 seconds, or between 1 and 15 seconds. The outer cover may comprise a third layer disposed between the first, wearer-facing layer and the second, garment-facing layer. The third layer, if present, may be hydrophobic.


In other aspects, the invention relates to an outer cover for an absorbent article, the outer cover consisting of a single layer or laminate of material. The outer cover may comprise a first, wearer-facing surface and a second, garment-facing surface. The outer cover may have an absorbent capacity between 5 and 100 g. The first, wearer-facing surface may have a DAT contact angle at 0.5 second of less than about 75 degrees. The second, garment-facing surface may be hydrophobic. The outer cover may have a WVTR between 1,200 g/m2/24 hr and 15,000 g/m2/24 hr, or between 3,000 g/m2/24 hr and 10,000 g/m2/24 hr. The outer surface may be coated with a water resistant compound. The water resistant compound, if present, may be selected from the group consisting of polytetrafluoroethylene, fluorocarbon derivatives, hydrophobic silicone polymers, hydrophobic fluorinated polymers, and combinations thereof.


In still other aspects, the invention relates to an absorbent article comprising an absorbent insert and an outer cover, wherein the outer cover may have an absorbent capacity greater than 0 and less than an absorbent capacity of the absorbent insert.





BRIEF DESCRIPTION OF THE DRAWINGS


FIG. 1 is a plan view of an exemplary absorbent article.



FIG. 2 is a schematic view of exemplary fasteners.



FIG. 3 is a perspective view of a portion of an exemplary absorbent article.



FIG. 4 is a front view of a plunger blade used for the upper movable test fixture in the Bending Stiffness Test;



FIG. 5 is a side view of a plunger blade used for the upper movable test fixture in the Bending Stiffness Test;



FIG. 6 is a side view of a lower stationary test fixture in the Bending Stiffness Test.





DETAILED DESCRIPTION OF THE INVENTION

As used herein, “absorbent article” refers to devices which absorb and contain body exudates and, more specifically, refers to devices which are placed against or in proximity to the body of a wearer to absorb and contain various exudates discharged from the body. Exemplary absorbent articles include diapers, training pants, pull-on or pant-type diapers (i.e., a diaper having a pre-formed waist opening and leg openings such as illustrated in U.S. Pat. No. 6,120,487), refastenable diapers, incontinence briefs and undergarments, diaper holders and liners, feminine hygiene garments such as sanitary napkins and panty liners, and the like. An absorbent article may be disposable or reusable.


As used herein, “absorbent insert” refers to a component of an absorbent article used to capture or contain body exudates, and which is removably associated with the absorbent article during use. For example, an absorbent insert may be press-fit into place, or may be releasably attached to some portion of the absorbent article, as by mechanical fasteners, adhesives, cohesives, and the like. An absorbent insert may be disposable or reusable.


As used herein, “disposable” refers to an article or object which is intended to be used once, or for one continuous time period of usage, and then discarded. A disposable article is not intended to be cleaned, repaired, or otherwise prepared for reuse. In contrast, a reusable article is intended to be used at least twice, and may be intended for repeated use over an extended period of time, such as weeks or months. A reusable article may be cleaned, repaired, or otherwise restored prior to reuse.


For example, a reusable article may be used, laundered, and reused. A single article may include disposable components and reusable components. For example, an absorbent article may comprise a reusable outer cover and a disposable absorbent insert.


As used herein, “wearer-facing” or “inner” refers to the side or surface of an absorbent article or a component of an absorbent article which is nearest the body of a wearer, when the absorbent article is applied to the wearer as intended for normal use. In contrast, “garment-facing” or “outer” refers to the side or surface of an absorbent article or a component of an absorbent article opposite the wearer-facing side, and nearest the wearer's clothes, if the wearer is wearing clothes over the absorbent article, when the absorbent article is applied to the wearer as intended for normal use.


As used herein, “hydrophilic” describes surfaces which are wettable by aqueous fluids (e.g., aqueous body fluids) deposited on these surfaces. Hydrophilicity and wettability are typically defined in terms of contact angle on a nonwoven fabric. A surface is said to be wetted by a fluid (i.e., hydrophilic) when the contact angle between the fluid and the surface is less than 90°, as measured at 0.2 seconds using the Dynamic Absorption Test described below. Conversely, a surface is considered to be “hydrophobic” if the contact angle is greater than 90° as measured at 0.2 seconds using the Dynamic Absorption Test described below.


As used herein, “insult” refers to exposure of an article to a body exudate, and may also be referred to as an event or an exposure. An absorbent insert may be changed or discarded after a single insult, for example, after a single act of defecation. An absorbent insert may be changed or discarded after several insults, such as several discrete acts of urination and/or defecation.


As used herein, “outer cover” refers to a component of an absorbent article used to hold the absorbent article against or near a wearer's body. An outer cover may also hold an absorbent insert in place relative to the wearer, or the absorbent article, or both. An outer cover may have one or more layers or components. If the outer cover comprises multiple layers or components, the term “outer cover” refers collectively to all the layers or components which would be assembled to hold an absorbent insert and absorbent article against or near a wearer's body during normal use, i.e., during use according to the manufacturer's instructions.


As shown in FIG. 1, an absorbent article 10 may be formed, in whole or in part, by an outer cover 12 and an absorbent insert 14. Outer cover 12 may serve to hold absorbent article 10 against the body of a wearer, for example, by wrapping around the wearer's legs and torso. Absorbent insert 14 may serve to absorb and contain body exudates, such as urine, feces, or menses, discharged by the wearer into absorbent article 10. Outer cover 12 and absorbent insert 14 may each, independently, be reusable or disposable. For example, absorbent article 10 may have a reusable outer cover 12 and a disposable absorbent insert 14. When disposable absorbent insert 14 is soiled, it may be discarded, and a new disposable absorbent insert 14 may be fitted to reusable outer cover 12. It is also possible to have a disposable outer cover 12 and reusable absorbent insert 14, or absorbent articles 10 wherein the outer cover 12 and absorbent insert 14 are both reusable, or both disposable.


Outer cover 12 may comprise elastic elements, such as elasticized rear waistband 16, elasticized front waistband 18, or elasticized leg bands 20, to help conform absorbent article 10 to a wearer. Outer cover 12 may comprise fasteners 22, which may be permanently or releasably joined to a landing zone 24, to form a waist opening. Fasteners 22 may comprise almost any fastening system, including, but not limited to, adhesives, cohesives, snaps, ties, zippers, buttons, hook-and-loop, hook-and-hook, tab-and-slot, magnets, sewn stitches, or combinations of these fasteners. Landing zone 24, if present, may be adapted to receive fasteners 22. For example, fasteners 22 may comprise hooks and landing zone 24 may comprise loops, or fasteners 22 may comprise and adherent and landing zone 24 may comprise an adherend, or fasteners 22 may comprise button holes and landing zone 24 may comprise one or more buttons. Landing zone 24 may be disposed on the garment-facing surface of absorbent article 10, as shown in FIG. 1. However, in some embodiments, landing zone 24 may be disposed on the wearer-facing surface of absorbent article 10, or on a layer disposed between the garment-facing surface and the wearer-facing surface of absorbent article 10. For example, fasteners 22 may be folded inside absorbent article 10 to contact landing zone 24, or the fastening system may include elements such as magnets, which do not require direct contact between fasteners 22 and landing zone 24 to function.


Outer cover 12 may further comprise one or more connectors 26. Connectors 26 may be adapted to permanently or releasably join absorbent insert 14 to outer cover 12. Connectors 26 may include almost any fastening system, as described above. For examples, connectors 26 may comprise adhesives which adhere the garment-facing surface of absorbent insert 14 to the wearer-facing surface of outer cover 12. Absorbent insert 14 may comprise connectors 28 to facilitate joining absorbent insert 14 to outer cover 12. For example, connectors 28 may comprise hooks and connectors 26 may comprise loops, or connectors 26 and 28 may comprise complementary cohesives. In some embodiments, absorbent insert 14 comprises one or more connectors 28, and outer cover 12 has no connectors. Connectors 28 and 26 may have the same or different shapes and dimensions. In some embodiments, outer cover 12 may have no distinct connectors 26. For example, outer cover 12, or inner surface 40 of outer cover 12, may have a relatively high static coefficient of friction relative to absorbent insert 14, such that absorbent insert 14 does not tend to move against outer cover 12. The static coefficient of friction may be varied by adding coatings or layers having a high coefficient of friction, by mechanically deforming the substrate to create a rougher surface, or by any other means. Static coefficient of friction may be measured as described below, and may vary from 0.3 to 0.4 or 0.5 or higher over inner surface 40 of outer cover 12.


In some embodiments, outer cover 12 comprises two or more connectors 26. A first connector 30 may have a different shape or dimension than at least a second connector 34. In some embodiments, absorbent insert 14 comprises two or more connectors 28. A first connector 32 may have a different shape or dimension than at least a second connector 36. First connector 30 in outer cover 12 may have a shape and size complementary to, or similar to, or the same as, first connector 32 in absorbent insert 14. Second connector 34 in outer cover 12 may have a shape and size complementary to, or similar to, or the same as, second connector 36 in absorbent insert 14. In such an embodiment, the proper orientation of absorbent insert 14 relative to outer cover 12 may be indicated by the different shapes or dimensions of the first and second connectors. For example, if absorbent insert 14 has a front side and a back side, the shape or size of the connectors may indicate that the front of absorbent insert 14 should be placed near the front of outer cover 12. In some embodiments, the position, dimensions, or shapes of the first and second connectors interact such that absorbent insert 14 can only be joined to outer cover 12 in a desired orientation, as shown in FIG. 2, where second connectors 34 and 36 would not substantially interact with first connectors 30 and 32 in a manner that would securely join absorbent insert 14 to outer cover 12. In some embodiments, the first and second connectors are of different types, so that it is not possible to secure absorbent insert 14 to outer cover 12 except in the desired orientation. For example, the first connectors may form a hook-and-loop system, and the second connectors may form a cohesive system.


Absorbent insert 14 may be intended to capture and contain all wastes eliminated by the wearer in the covered region of the body. However, some relatively small quantities of bodily exudates, such as urine, may occasionally evade absorbent insert 14 and contact the wearer-facing surface of outer cover 12. If the wearer-facing surface of outer cover 12 cannot absorb the fluid, the fluid may move along the wearer-facing surface of outer cover 12 and breach the perimeter 38 of absorbent article 10, thereby leaking onto clothing or other surfaces, such as bedding, carpeting, or a caregiver. In some embodiments, outer cover 12 has an absorbent capacity less than the absorbent capacity of absorbent insert 14. In some embodiments, outer cover 12 may have a fluid absorbent capacity between 5 and 100 mL, or between 20 and 60 mL, as measured by the Centrifuge Retention Capacity (CRC) test, described below, when testing the entire outer cover. CRC results may also be reported in a “unitized” or normalized format, wherein the result is reported as the total measured retention capacity of a sample divided by the weight of the dry sample prior to testing. Outer cover 12 may have a unitized CRC greater than 0.5 g/g, or between 0.5 g/g and 1.0 g/g.


Outer cover 12 may be constructed of a unitary element, such as a single layer of material, or a bonded laminate of two or more materials. In some embodiments, as shown in FIG. 3, outer cover 12 may be constructed of two or more discrete layers of material, such as inner, wearer-facing layer 44 and outer, garment-facing layer 46, having similar or different properties. If outer cover 12 is constructed of two or more discrete layers, the two or more discrete layers of material may be joined together at or near the perimeter 38 of absorbent article 10, e.g., in a seam or attachment point of a leg or waistband, or may be joined at one or more discrete locations in the article, such as at locations where a connector 26 or fastener 22 is affixed to inner surface 40 or outer surface 42 of outer cover 12. If outer cover 12 comprises two or more layers, it should be understood that each layer has a wearer-facing surface and a garment-facing surface.


In some embodiments, inner surface 40 of outer cover 12 is absorbent, and any absorbed fluid does not wet through to outer surface 42 of outer cover 12, i.e., the garment-facing surface, under normal wearing conditions. Nonetheless, outer cover 12 may be breathable to prevent over-hydration of the wearer's skin. Over-hydration of the skin may be caused, or exacerbated, by high localized humidity between absorbent article 10 and a wearer's skin. Over-hydrated skin may exhibit erythema (redness), or diaper dermatitis, or may be less resistant to abrasion (i.e., from a lower tensile strength) than skin which is not over-hydrated. Outer cover 12 may have a minimum breathability, or Water Vapor Transmission Rate (WVTR) as measured by the Water Vapor Transmission Rate test described below, to allow sufficient water vapor from urine, sweat and/or other exudates to leave the interior of absorbent article 10, maintaining the skin hydration at a lower level. Outer cover 12 may have a WVTR of at least about 1200 g/m2/24 hr, or a WVTR of at least about 3000 g/m2/24 hr. Higher WVTRs may be helpful, for example, when the ambient conditions are higher in temperature and/or humidity, when the wearer is more active (e.g., perspires more), or when absorbent article 10 has a relatively high load of urine, sweat, or other liquid exudates (e.g., during overnight use, or when the user is a “heavy wetter”). Thus, a WVTR of at least about 1200 g/m2/24 hr may indicate a serviceable outer cover in typical use, while a WVTR of at least about 3000 g/m2/24 hr may indicate a serviceable outer cover under more challenging conditions.


In certain instances, too high a breathability can have undesirable effects, such as moisture condensation, on the garment-facing surface of the article or on clothing. Outer cover 12 may have a WVTR of less than about 15,000 g/m2/24 hr, or even 10,000 g/m2/24 hr, to help prevent this phenomenon. A lower maximum WVTR indicates a serviceable outer cover under challenging conditions, such as lower ambient temperatures, where escaping water vapor may generate more condensation than at relatively higher ambient temperatures.


The outer surface 42 of a single layer outer cover material may be hydrophobic. The hydrophobicity of outer surface 42 may result, for example, from the choice of fiber/yarn chemistry or diameter in the substrate, the manner in which the yarns are woven or knitted, or in coatings or other treatments applied to the yarns, finished material, or both. For example, outer surface 42 may be blended (as with micro or nanofibers), coated, or otherwise treated with water resistant compounds, such as polytetrafluoroethylene (also known as PTFE, or TEFLON); fluorocarbon derivatives (also known as SCOTCHGARD, as described, for example, in U.S. Pat. No. 3,574,791); or a hydrophobic silicone polymer or fluorinated polymer (such as those described, for example, in U.S. Pat. No. 7,626,073), or the like. In outer cover embodiments comprising two or more layers of material, garment-facing layer 46 (i.e., the outer most layer), or either surface thereof, may be hydrophobic or treated to become hydrophobic via any of the treatments or methods described herein. Alternatively, the garment-facing surface of inner layer 44 may be treated to be hydrophobic, or a third, hydrophobic layer may be disposed between inner layer 44 and outer layer 46 of outer cover 12.


The inner layer 44 or inner surface 40 of outer cover 12 may be treated to make it hydrophilic, or to increase its hydrophilicity. For example, inner layer 44 or inner surface 40 may be treated with surfactants or other coatings that confer or improve hydrophilicity. For example, inner layer 44 or inner surface 40 may be treated with a solution comprising nanoparticles, as described in US Patent Application Publication 2009/0048571. The solution may comprise a film-forming polymer, a wetting agent, and from about 0.001% to about 40% by weight of the composition of nanoparticles. The nanoparticles may be selected from the group consisting of alumina, silica, and combinations thereof. The nanoparticles may have a particle size from about 1 to about 750 nanometers. The weight ratio of the film forming polymer to the nanoparticles may be from about 1:1 to about 1:30. Exemplary film-forming polymers include, but are not limited to, polyamines, quaternized polyamines, zwitterionic polymers; polycarboxylates; polyethers; polyhydroxylated polymers; polyphosphonates and polyphosphates; polymeric chelants; ethoxylated or alkoxylated polyamines; polycarboxylated polyamines; water dispersible polyethers; water dispersible polyhydroxylated groups or polymers, including polysaccharides; water dispersible polycarboxylates; water dispersible anionic groups such as carboxylates, sulfonates, sulfates, phosphates, phosphonates and polymers thereof; dispersible polystyrenes containing anionic groups such as carboxylates, sulfonates, sulfates, phosphates, phosphonates and polymers thereof; water dispersible polymers containing groups of amines, quaternaries, amine oxides and combinations thereof; water dispersible zwitterionic groups and polymers thereof; water dispersible amides and polyamides; and water dispersible polymers and copolymers of vinylimidazole and vinylpyrrolidone; polymer and block co-polymer combinations of the above.


As another example, inner layer 44 or inner surface 40 may be treated with hydrophilic monomers and radical polymerization initiators, as described in U.S. Pat. No. 7,521,587. The monomers may contain at least one unsaturated double bond according to the general formula R1R2C═CR3R4, with R1 and R2 preferably being hydrogen atoms. In some embodiments, the hydrophilic monomers comprise a group which can react with an acid or base to form a salt. Examples of suitable monomers include acrylic acid and its derivates (e.g., methacrylic acid, ethylacrylic acid), styrene sulphonic acid and its derivates, vinyl acetate, maleic anhydride and vinyl pyridine. The initiator may be capable of forming reactive radicals upon activation with light. Examples of suitable radical polymerization initiators include benzophenone and its derivates, benzoyl peroxide, or azobisisobutyronitrile (AIBN). The coating solution may further comprise an agent which reduces homopolymerization of the hydrophilic monomers, such as iron-II salts, copper-II-salts, or mixtures thereof. The coating solution may be applied to the fibers, and the coated fibers may be exposed to UV light, such as UV-A light, to form hydrophilic polymers which are chemically grafted to the fibers.


In some embodiments, inner layer 44 or inner surface 40 of outer cover 12 may be treated to increase hydrophilicity, and outer layer 46 or outer surface 42 of outer cover 12 may be treated to increase hydrophobicity. In addition to the exemplary hydrophilic and hydrophobic treatments described herein, virtually any hydrophilic or hydrophobic treatment could be used. Durable treatments may be selected, for example, if outer cover 12 is intended to be reusable, or to reduce the possibility of transferring the coating or treatment to the wearer of outer cover 12.


Inner surface 40 of outer cover 12 may have a Contact Angle at 0.5 second, as measured by the Dynamic Absorption Test disclosed herein, of less than about 90 degrees, or less than about 75 degrees. The Contact Angle at 0.5 second may be in the range of about 45 and about 90 degrees. The outer cover may have a Contact Angle at 1.0 second of less than about 80 degrees, or less than about 45 degrees. In addition to the treatments discussed above, increasing the three-dimensionality of a surface, as discussed below, may lead to a reduction in the contact angle of the material. Increasing the porosity or capillarity of a surface, as may be done, for example, to increase breathability, may also lead to a reduction in the contact angle of the material.


Inner surface 40 of outer cover 12 may have a Strikethrough time, as measured by the method disclosed herein, of less than about 15 seconds, less than about 10 seconds, or between about 1 second and 15 seconds. Low strikethrough times represent faster penetration of fluid into outer cover 12, which reduces free fluid available to escape outer cover 12 and soil the environment.


Inner surface 40 of outer cover 12 may have a nonpolar component of surface energy, as measured by the Surface Free Energy test disclosed herein, of less than about 3.5, less than about 3.0, or less than about 2.5 mJ/mm2. A lower nonpolar component of surface energy may be associated with a lower tendency to stain when contacted by fatty substances. Although urine is typically predominantly aqueous, feces and other exudates may contain fats or fatty substances. Non-aqueous or lipophilic stains are generally difficult to remove from surfaces such as textiles during common water-based washing processes typically employed in domestic laundry facilities, such as laundry facilities in private homes or launderettes. Surfaces which are at least initially more resistant to lipophilic staining may have a relatively low nonpolar surface energy component, for example, a nonpolar surface energy component less than 10 mJ/mm2, or less than 5 mJ/mm2, or less than 3 mJ/mm2


Outer cover 12 may be soft, so as to not abrade the wearer's skin. Perception of softness may involve a complex set of variables. However, for both flexible and resilient surfaces, a surface having a three-dimensional configuration on a micro-scale may be perceived as softer than a more two-dimensional configuration of the same material composition. A three-dimensional configuration may be created, or selected for, with various weaves of woven fabrics. For example, woven fabrics may be created or selected having relatively high warp and weft heights, yarn spacing, etc. Tighter weaves (i.e., lower spacing between yarns) may have a more dominant effect on surface energy.


Outer cover 12 may fit the contours of the wearer's body. Outer cover materials may have a low bending stiffness to enable them to adapt and conform to the wearer's anatomy and move with the wearer's body with relatively low resistance, which may contribute to a comfortable fit whether the wearer is quiescent or active. A conforming fit may also allow the perimeter region of the outer cover, which may include elasticized leg or waist bands, to remain in a desirable orientation and location on the wearer's body. Maintaining a desirable orientation and location may help prevent or reduce leakage of bodily exudates from outer cover 12.


As discussed above, outer cover 12 may be constructed of a unitary element, such as a single layer of material or a bonded laminate of two or more materials. Alternatively, outer cover 12 may be constructed of two or more discrete layers of material, having similar or different properties. If outer cover 12 is constructed of two or more discrete layers of material, the two or more discrete layers of material may be joined together at or near the perimeter of the article, e.g., in a seam or attachment point of a leg or waistband, or may be joined at one or more discrete locations in the article, such as at locations where a fastening element, such as fastener 22 or connector 26, is affixed to the inner surface 40 or outer surface 42 of outer cover 12. Regardless of the number of layers, or “stack up”, the bending stiffness of the stack up of outer cover 12 material may be less than about 0.20 N, or 0.19 N, in the Bending Stiffness test described herein. If outer cover 12 includes more than one discrete layer (i.e., separable from another layer of the outer cover over a sufficient area to enable the Bending Stiffness test to be performed, the Bending Stiffness of at least one of the layers may be less than about 0.10 N or less than about 0.08 N. In some embodiments, each layer may have a Bending Stiffness of less than about 0.10 N or 0.08 N.


The addition of a fastening element to the wearer-facing surface of the outer cover may require, in some embodiments, a higher Bending Stiffness to create additional support to carry the loading force transferred from insert 14 to the outer cover material. The Bending Stiffness of the “as used” stack up of outer cover material to which an insert-to-outer cover material is affixed may be less than about 0.30 N.


In some embodiments, outer cover 12 may comprise a different layer structure in different regions. For example, outer cover 12 may have a longitudinal centerline 48. Outer cover 12 may have three portions of approximately equal lengths along longitudinal centerline 48. Rear portion 50, for example, may occupy approximately one-third of the length of outer cover 12 from the laterally extending rear longitudinal edge 56, front portion 54 may occupy approximately one-third of the length of outer cover 12 from the laterally extending front longitudinal edge 58, and central portion 52 may occupy approximately one-third of the length of outer cover 12 between rear portion 50 and front portion 54.


The rear portion 50, center portion 52, and front portion 54 of outer cover 12 may desirably have different properties. For example, regions of outer cover 12 corresponding to the wearer's waist, hips, and buttocks regions, generally in rear portion 50 and front portion 54, may be subjected to tensile and bending/torsional stresses during application and/or wearing of absorbent article 10. In contrast, center portion 52 may be subject to stresses different in direction and magnitude related to the mass of exudates contained by the diaper as it is soiled. Center portion 52 may also be more likely to be soiled by exudates during use, including wearing absorbent article 10 and changing absorbent insert 14. Accordingly, it may be desirable, for example, for center portion 52 to extend less than rear portion 50 and/or front portion 54 under similar tensile forces. This could allow rear portion 50 and/or front portion 54 to comfortably fit the waist and hips of a range of users, or of a single user over a period in which the user grows or gains weight, while providing additional support for absorbent insert 14 in center portion 52, such that a heavily soiled absorbent insert 14 does not cause outer cover 12 to sag to a degree that gaps are created along the legs. Gaps along the legs could make it more likely that exudates would leak from absorbent article 12.


In some embodiments, different portions of the outer cover may have different properties due to different layers of materials. The layers may be different in the number of layer(s), the kinds of layers (e.g., material, basis weight, texture, treatment, etc.), or both. For example, rear portion 50 and center portion 52 may comprise the same material, such as the material used in Example 1, but there may be only one layer of the material in rear portion 50 and two, or more, layers of the material in center portion 52. This would provide lower extension under tension in center portion 52 and increased resistance to penetration of wearer exudates through center portion 52 to the wearer's clothing or surroundings. In addition, one or both of the layers in center portion 52 may be modified as described above, for example, by hydrophobic treatments.


In some embodiments, it may be desirable to provide greater extension under tension in center portion 52 than in the front portion 54 and/or rear portion 50. This could, for example, allow center portion 52 to expand so as not to mechanically constrain the absorption of exudates into absorbent insert 14, and limit the extension of front portion 54 and/or rear portion 50 to provide better unload forces for sustained fit around the wearer's waist and hips.


In some embodiments, one or more portion of outer cover 12 may have three or more layers. For example, in addition to rear portion 50, center portion 52, and front portion 54, outer cover 12 may have a leg portion 60. Leg portion 60 may run more or less parallel to perimeter 38 in center portion 52, and may extend a distance from perimeter 38 which is greater than 0 mm, but less than approximately one-third the width of outer cover 12 at its narrowest point in center portion 52, on each longitudinally-extending lateral side 62 of outer cover 12. If perimeter 38 is curvilinear in center portion 52, leg portion 60 may have generally the same curvature as perimeter 38. Outer cover 12 may comprise three or more layers in rear portion 50. Leg portion 60, if present, may comprise three or more layers of material, to provide some stiffness and help hold leg portion 60 against the wearer's body to contain exudates. In some embodiments, rear portion 50 may comprise two layers of fabric and an anchoring band, which may be a different fabric or an elastic band having greater unload forces than the other layers of fabric. In other embodiments, landing zone 24 may comprise three or more layers to provide some stiffness to landing zone 24, which may make it easier to press and attach fasteners 22 to landing zone 24.


One or more portions of outer cover 12 may comprise alternating numbers of layers, longitudinally or laterally or both, to distribute forces within outer cover 12 or provide an appearance of three-dimensionality.


In some embodiments, outer cover 12 comprises two layers in leg portion 60 and one layer in center portion 52, to enhance resistance to gapping at the legs and allow absorbent insert 14 to swell in center portion 52. It should be understood that if center portion 52 differs from leg portion 60, center portion 52 will itself vary laterally, since leg portion 60 is a sub-portion of center portion 52.


In some embodiments, outer cover 12 comprises a central portion 64 of rear waistband 16 and/or front waistband 18 which has different layers than ear portions 62 of rear waistband 16 and/or front waistband 18. Central portion 64 may have a lateral width roughly corresponding to one-third the width of outer cover 12 along laterally-extending longitudinal edge 56 or 58. If laterally-extending longitudinal edge 56 or 58 is rounded or otherwise has no distinct edge, central portion 64 is considered that portion of the waistband corresponding to the width of outer cover 12 at the laterally narrowest point of longitudinal central portion 52. Ear portions 62 are those portions of the outer cover along laterally-extending longitudinal edge 56 or 58 which are laterally outboard of lateral central portion 64. Ear portions 62 and lateral central portion 64 may extend longitudinally from longitudinal end edge 56 along all of rear portion 50 or from longitudinal end edge 58 along all of front portion 54. Ear portions 62 may comprise fewer layers than lateral central portion 64. For example, ear portions 62 may comprise a single layer of material, and lateral central portion 64 may comprise two layers. Such a construction may allow ear portions 62 to stretch easily, thereby facilitating application of the product to a wearer, while central portion 64 may provide higher unload forces, thereby improving the sustained fit of the product over time.


Of course, it should be understood that the front portion 54 and rear portion 50 may be, but need not be, of like construction with regard to the materials, treatment of the materials, or layers of materials used. Although different constructions are described herein as various embodiments, combinations and permutations of the different constructions are expressly contemplated.


EXAMPLES

















Exam-
Exam-
Exam-
Exam-
Exam-


Property
ple 1
ple 2
ple 3
ple 4
ple 5




















Strikethrough (s)
8.86
49.0
17.8
198
204


for all layers of







Outer Cover using







regular 0.9% saline







Surface Energy







(mJ/mm2)







polar
0.89
0.87
4.71
0.092
0.47


Non-polar
1.47
3.96
26.9
27.2
28.9


DAT contact angle







(degrees)*







0.5 sec
66.5
92.5
126.9
97.7
96.7


  1 sec
25.9
85.5
126.9
97.5
96.4


Absorbent capacity (g)







OC or insert (g)
44.4
28.1
18.2
37.3
24.0


Unitized Capacity (g/g)







whole OC
0.63
0.46
0.30
0.70
0.72


OC Material only
1.13
1.48
0.30
0.52
0.70


Mass of whole OC (g)
70.5
61.1
60.6
53.3
33.3


Bending stiffness
0.183
0.355
0.381
0.261
0.206


peak force**







(Newtons)





*Measured on the wearer-facing surface of the wearer-facing layer of the outer cover.


**For each type of outer cover, ten samples were tested, using all layers of the Outer Cover (OC), and the average was reported. The outer cover bending stiffness peak force was measured using the Bending Stiffness Test, disclosed herein. Also, for the Test Article, the bending stiffness peak force of the outer layer material was measured using the Bending Stiffness Test, and was found to be 0.070 Newtons. Further, for the Test Article, the bending stiffness peak force of the inner liner material was measured using the Bending Stiffness Test, and was found to be 0.056 Newtons.






Example 1 is an outer cover configured according to embodiments of the present disclosure, with an outer layer material and inner liner material both made of 93% Modal and 7% Spandex, available as code E.n.n-14 from Koshtex, Los Angeles, Calif., United States, outer cover hooks made of 100% nylon, available as sewable hooks from Perfectek Plus, Huntington Beach, Calif., United States, outer cover landing zone, available as code 960E from Aplix, Paris, France, and insert landing zone made of 100% nylon, available as standard sew on material from Touchtape, St. Augustine, Fla., United States.


Example 2 is a gDiaper™ reusable diaper cover purchased from www.gdiapers.com in April 2010. The SKU number is 31041 and the size is Large (26-36 pounds). The manufacturer is gDiapers, Inc. of Portland, Oreg.


Example 3 is a Gro Baby™ reusable diaper cover purchased from www.thenaturalbabyco.com in April 2010. The outer cover is only available in one size. The manufacturer is GroVia™ (formerly Gro Baby™), of Bozeman, Mont.


Example 4 is a Bummis™ SuperBrite reusable diaper cover, size L, purchased from www.thenaturalbabyco.com in April 2010, and manufactured by Bummis, Inc., Montreal, Quebec, Canada.


Example 5 is a Diaperaps™ reusable diaper cover, size large, purchased from www.babysorganicnursery.com in April 2010, manufactured by Diaperaps: Baby's Organic Nursery, Granada Hills, Calif.


Modified Liquid Strike-Though


Liquid strike-through of the outer cover is measured using a Lister Strike Through instrument (available from Lenzing Technik, Austria), or any apparatus compliant with the Harmonized Test Method WSP 70.3 (08). The instrument is calibrated and operated in accordance with the manufacturer's instructions except where specified below. The test fluid was 0.9% w/v sodium chloride prepared in distilled water.


Precondition samples at 23° C.±2° C. and 50%±2% relative humidity for 2 hours prior to testing. The outer cover article is opened and placed with the wearer-facing surface facing downward. Using scissors, remove the leg elastics, if present, such that the article can be laid flat. Select a sampling site along the longitudinal axis of the cover that is equal-distant between the distal edge of the back waist and the midpoint of the cover's total length. If structures such as seams, snaps, labels, etc. are present at this site, it is permissible to shift the sampling region to an adjacent area to avoid them. With a hydraulic press and cutting die (100 mm square±0.1 mm and 8 mm deep), cut a specimen centered on this mark through all the layers of the article, with the specimen's cut edges parallel and perpendicular to the longitudinal and lateral axis of the article. The specimen can be tested with all layers as one composite or as individual layers.


The specimen is placed under the strike-through plate with the wearer-facing surface facing upward, and its edges parallel and perpendicular to the plate (for this experiment no absorbent paper is placed under the specimen). The plate is aligned underneath the delivery funnel such that the funnel is centered over the plate's cavity and is 30 mm±1 mm above the top of the plate's surface. Add 5.00 mL±0.01 mL of the test fluid into the funnel, and then open the valve to deliver the flow into the plate cavity. The test fluid will complete the electrical circuit of the plate electrodes and start the timer. The timer will stop when the liquid has penetrated into the specimen. Record the strike-through time to the nearest 0.01 second.


Repeat the analysis on three equivalent specimens from separate outer covers. Average the three values and report to the nearest 0.01 sec.


Surface Energy


The surface energy of a surface is derived from contact angle measurements, which can be converted to surface energy by various accepted models that would be known to one of skill in the art. One such model, used in the present disclosure, is the Fowkes equation, as described in Fowkes, F. M.: Industrial and Engineering Chemistry, vol. 56, number 12, p. 40 (1964) which is herein incorporated by reference:

γ1v(1+cos θ)=2(γ1vdγsvd)1/2+2(γ1vpγsvp)1/2

where:

    • θ the contact angle;
    • γ1v the surface tension of the liquid;
    • γ1vd the dispersive component of the surface tension of the liquid being deposited on the specimen's surface;
    • γsvd the dispersive component of the surface energy of the specimen's surface;
    • γ1vp the polar component of the surface tension of the liquid being deposited on the specimen's surface;
    • γsvp the polar component of the surface energy of the specimen's surface;


Sessile drop contact angle is measured using a FTA 200 dynamic contact angle analyzer with FTA 200 software, version 2.1, build 340 (available from First Ten Angstroms, Portsmouth, Va.), or equivalent. Purified distilled water, processed through a Milli-Q water system (Millipore Corporation, Billerica, Mass.) and 99% diiodomethane (Sigma-Aldrich, Saint Louis, Mo.) are used as the test fluids. All measurements were performed at constant temperature (25° C.±1° C.) and humidity (33%±2%).


Precondition samples at 25° C.±1° C. and 33%±2% relative humidity for 2 hours prior to testing. The outer cover article is opened and placed with the wearer-facing surface facing upward. Using scissors, remove the leg elastics, if present, such that the article can be laid flat. Select a sampling site along the longitudinal axis of the cover that is equal-distant between the distal edge of the back waist and the midpoint of the cover's total length. If structures such as seams, snaps, labels, etc. are present at this site, it is permissible to shift the sampling region to an adjacent area to avoid them. Using scissors excise a 1 cm by 3 cm specimen of the wearer-facing surface from the selected site. The specimen is adhesively mounted flat on a glass microscope slide such that no ridges are present and with the wearer-facing surface facing upward.


Using the FTA 200, 7 μL of purified water is dangled from the end of a blunt tip, 27 gauge stainless steel needle. The surface of the specimen is slowly raised until it makes contact with the drop. A video stream collected at a rate of 120 images/s is optically triggered at first contact between drop and specimen and collects images for the first 1 minute while the drop detaches and subsequently equilibrates with the surface of the specimen. Preferably, the contact angle is measured at 0.2 seconds after drop contact with the specimen surface. If significant penetration of the placed test fluid occurs within that 0.2 seconds, i.e., greater than 2.5%, contact angle is alternatively determined at 0.02 seconds. Contact angle is measured using a non-spherical tracing of the drop profile as automatically determined by the FTA 200 software and reported to the nearest 0.01 degrees.


The above procedure is next repeated using 3 μL of diiodomethane in place of the purified water. Contact angle using diiodomethane is reported to the nearest 0.01 degrees.


The surface energy of the baby-facing surface of the specimen is calculated using the Fowkes equation with the constants listed in Table 1 and recorded to the nearest 0.001 mJ/m2.









TABLE 1







Solvents used to determine surface energy of outer wrap









Surface Energy



Component (mJ/m2)












Solvent
Nonpolar
Polar
Total















Water
21.8
51.0
72.8



Diiodomethane
50.8
0
50.8










Dynamic Absorption Test


The Dynamic Absorption Test measures the absorption of a test fluid on to a specimen's surface by measuring the change in contact angle of the test fluid as it makes contact with, and absorbs into the surface. Sessile drop contact angle is measured using a FTA 200 dynamic contact angle analyzer with FTA 200 software, version 2.1, build 340 (available from First Ten Angstroms, Portsmouth, Va.), or equivalent. All measurements are performed at constant temperature (28° C.±1° C.) and humidity (33%±2%). For these experiments, the test fluid was 0.9% w/v sodium chloride (99.9% purity) prepared in purified distilled water, processed through a Milli-Q water system (Millipore Corporation, Billerica, Mass.).


Precondition samples at 28° C.±1° C. and 33%±2% relative humidity for 2 hours prior to testing. The outer cover article is opened and placed with the wearer-facing surface facing upward. Using scissors, remove the leg elastics, if present, such that the article can be laid flat. Select a sampling site along the longitudinal axis of the cover that is equal-distant between the distal edge of the back waist and the midpoint of the cover's total length. If structures such as seams, snaps, labels, etc. are present at this site, it is permissible to shift the sampling region to an adjacent area to avoid them. Using scissors, excise a 1 cm by 3 cm specimen of the wearer-facing surface from the selected site. The specimen is adhesively mounted flat on a glass microscope slide such that no ridges are present and with the wearer-facing surface facing upward.


Using the FTA 200, 7 μL test fluid is dangled from the end of a blunt tip, 27 gauge stainless steel needle. The surface of the specimen is slowly raised until it makes contact with the drop. A video stream collected at a rate of 1 image/0.1 second is optically triggered at first contact between drop and specimen and collects images for the first 3 seconds while the drop detaches and subsequently equilibrates with the surface of the specimen. Contact angle is measured on each image using a non-spherical tracing of the drop profile as automatically determined by the FTA 200 software and reported to the nearest 0.01 degrees.


Centrifuge Retention Capacity (CRC) Test


The Centrifuge Retention Capacity (CRC) is a measure of the fluid retention capacity (absorbent capacity) of a specimen submerged in 0.9% NaCl saline solution for 30 minutes and then subjected to centrifugation. The test is a based on the Worldwide Strategic Partners Standard Test Method WSP 241.2 (09), Gravimetric Determination of Fluid Retention Capacity in Saline Solution after Centrifugation.


For analysis, specimens are placed into a bag constructed from heat-sealable, water-permeable, non-apertured nonwoven material. Specifications for the bag material are given in WSP 241.2 (09). Measure the length (L) and width (W) of the specimen to be tested. Cut a piece of the bag material that is 2×L+50 mm by W+25 mm. Fold the bag material in half across its width and heat-seal two of the open edges approximately 3 to 5 mm from the edges. The finished bag is L+25 mm by W+25 mm. In addition to the bags for samples, prepare three bags of the same dimensions to be used as blanks.


Outer Cover Material Sample Preparation:


The outer cover article is opened and placed with the wearer-facing surface facing downward. Using scissors remove the leg elastics, if present, such that the article can be laid flat. Select a sampling site along the longitudinal axis of the cover that is equal-distant between the distal edge of the back waist and the midpoint of the cover's total length. If structures such as seams, snaps, labels, etc. are present at this site, it is permissible to shift the sampling region to an adjacent area to avoid them. With a hydraulic press and cutting die (76.2 mm square±0.1 mm and 8 mm deep), cut a specimen centered on this mark through all the layers of the article, with the specimen's cut edges parallel and perpendicular to the longitudinal and lateral axis of the article. Obtain and record the dry mass of the specimen to the nearest 0.001 grams. Place all layers of the specimen into an appropriately sized bag and heat seal the remaining open edge. Prepare three replicates of each specimen for testing.


Whole Absorbent Insert Sample Preparation:


Precondition samples at about 23° C.±2° C. and about 50%±2% relative humidity for 2 hours prior to testing. The absorbent insert is unfolded and placed with the wearer-facing surface facing upward. Using scissors cut any elastic along the longitudinal edges of the article at an interval of approximately 2 cm, such that the article can be laid flat. Lay the absorbent insert on a piece of aluminum foil and cut the absorbent insert along the longitudinal and lateral axis resulting in four individual specimens. On a calibrated balance, tare the weight of an appropriately sized bag. Place the specimen, and any material that fell onto the foil during cutting, into the tared bag and heat seal the remaining open edge. Obtain and record the dry mass of the specimen to the nearest 0.001 grams. Repeat this procedure to obtain the dry mass of the three remaining specimens. Three replicate absorbent inserts are prepared for testing.


Whole Outer Cover Sample Preparation:


Obtain and record the dry mass of the entire outer cover to the nearest 0.001 grams. Three replicate outer covers are prepared for testing.


Test Procedure:


Obtain a pan large enough to hold several bags or specimens, and fill it with 0.9% saline solution to a level such that the bag or specimen can be completely submerged. Lay the bags or specimens to be tested onto the surface of the saline, and allow them to become wet for 1 minute before submerging. A weight placed onto the edge of the bag may be used to ensure that the sample remains submerged while allowing the solution to be freely absorbed by the specimen. After 30 minutes remove the bag or specimen from the saline solution, and immediately transfer it into the basket of a suitable centrifuge capable of subjecting the specimens to a 250 G centrifugal acceleration (such as a Clay Adams Dynac Centrifuge available from Block Scientific, Bohemia, N.Y.). Orient the specimens in the centrifuge such that the wearer-facing surface is facing outward, unless the wearer-facing surface is hydrophobic, in which case it should be oriented inward. Position the bags or specimens so that similarly weighted samples are opposite each other for proper balancing. Centrifuge the bags or specimens for 3 minutes±10 seconds at 250 G. The bags or specimens are then removed and immediately weighed. Record the wet mass of the specimen and bag, blank bag, or specimen without a bag to the nearest 0.001 grams.


Calculate the average of the three wet blank bag masses after centrifugation (mb); this value is disregarded if the specimen was tested without a bag. For each specimen (i=1, 2, and 3), calculate the centrifuge retention capacity (wi), expressed as a mass fraction (g/g) using the following equation:

wi=((mwi−mb)−msi)/msi


Where msi is the mass, expressed in grams, of the dry specimen and mwi is the mass, expressed in grams, of the wet specimen and bag or specimen without a bag. For the absorbent inserts cut and tested as four separate specimens. Sum up the four individual masses of the dry specimens to get msi, sum up the four individual masses of the wet specimens and bags to get mwi, and sum up four of the average wet blank bag masses after centrifugation to get mb. Use these values to calculate a total centrifuge retention capacity (wi) value. Calculate and report the average centrifuge retention capacity for the three replicates to the nearest 0.001 (g/g).


Water Vapor Transmission Rate


Water Vapor Transmission rate (WVTR) is measured according to EDANA/INDA Worldwide Strategic Partners Method WSP 70.4 (08) using a Permatran-W model 100K (MOCON, Minnesota, Minn.). The test method is run as per the WSP standard test, using a test apparatus temperature of 37.8 C, a nitrogen flow rate of 120 SCCM, and the standard mode with 2 cycles and 5 minute exam time. Each cell is individually adjusted to a relative humidity (RH) of 60%±1.5%. The standard reference film (S/N 1008WK089 from MOCON) should be run prior to testing the samples in order to ensure that the equipment is running properly. The standard reference film results should be within ±10% of the values reported by MOCON.


Using scissors or a die cut a specimen 35 mm in diameter. If the outer cover is multilayered the specimen is run as the composite sample. The side of the outer cover which normally faces the skin is oriented toward the water for testing. Report the WVTR as g/m2/24 hr to the nearest 1 g/m2/24 hr.


Coefficient of Friction


The static coefficient of friction can be measured using ASTM Method D 1894-01 with the following particulars. The test is performed on a constant rate of extension tensile tester with computer interface (a suitable instrument is the MTS Alliance using Testworks 4 Software, as available from MTS Systems Corp., Eden Prairie, Minn.) fitted with a coefficient of friction fixture and sled as described in D 1894-01 (a suitable fixture is the Coefficient of Friction Fixture and Sled available from Instron Corp., Canton, Mass.). The apparatus is configured as depicted in FIG. 1c of ASTM 1894-01 using a stainless steel plane with a grind surface of 320 granulation as the target surface. A load cell is selected such that the measured forces are within 10% to 90% of the range of the cell. The tensile tester is programmed for a crosshead speed of 127 mm/min, and a total travel of 130 mm. Data are collected at a rate of 100 Hz.


The test specimen is cut into a square 6.35 cm by 6.35 cm with its sides parallel and perpendicular to the longitudinal axis of the outer cover. The specimen is mounted onto the foam rubber side of the sled using double sided adhesive tape (tape should be wide enough to cover 100% of the sled's surface). The specimen is oriented on the sled such that the skin facing surface of the outer cover will face toward the target surface and the longitudinal axis of the outer cover is parallel to the pull direction of the sled. The mass of the sled with mounted sample is recorded to 0.1 gram. The surface of the stainless steel plane is cleaned with isopropanol between each analysis. To measure the static coefficient of friction against an absorbent insert, the target surface is an 18 gsm matte polypropylene film from Clopay Plastics Products Company of Mason, Ohio.


The Static COF is calculated as follows:

Static COF=AS/B


AS=maximum peak force in grams force (gf) for the initial peak


B=mass of sled in grams


Bending Stiffness Test


Peak Bending Force and Total Stiffness are measured using a constant rate of extension tensile tester with computer interface (a suitable instrument is an MTS Alliance under TestWorks 4 software, as available from MTS Systems Corp., Eden Prairie, Minn.) using a load cell for which the forces measured are within 10% and 90% of the limit of the cell. A plunger blade 600, shown in FIG. 4 (front view) and FIG. 5 (side view), is used for the upper movable test fixture. Base support platforms 700, shown in FIG. 6, are used as the lower stationary test fixture. All testing is performed in a conditioned room maintained at about 23° C.±2° C. and about 50%±2% relative humidity.


Components of the plunger 600 are made of a light weight material such as aluminum to maximize the available load cell capacity. The shaft 601 is machined to fit the tensile tester and has a locking collar 602 to stabilize the plunger and maintain alignment orthogonal to base support platforms 704. The blade 603, is 115 mm long 608 by 65 mm high 607 by 3.25 mm wide 609, and has a material contact edge with a continuous radius of 1.625 mm. The bracket 604 is fitted with set screws 605 that are used to level the blade and a main set screw 606 to firmly hold it in place after adjustment.


The bottom fixture 700 is attached to the tensile tester with the shaft 701 and locking collar 702. Two horizontally movable support platforms 704 are mounted on a rail 703. Each test surface 705 is 85 mm wide 706 by 115 mm long (into plane of drawing) and made of polished stainless steel so as to have a minimal coefficient of friction. Each platform has a digital position monitor 708 which reads the individual platform positions, and set screws 707 to lock their position after adjustment. The two platforms 704 are square at the gap edge and the plate edges should be parallel front to back. The two platforms form a gap 709 with an adjustable gap width 710.


Accurately (±0.02 mm) align the plunger blade 603 so that it is orthogonal to the top surface of the support platforms 704 and exhibits no skew relative to their gap edges. Using the position monitors 708, accurately set the gap 710 to 13.25±0.02 mm between the two gap edges of the support platforms 704, with the plunger blade 603 accurately (±0.02 mm) centered in the gap. Set the gauge length from the bottom of the plunger blade 603 to the top surface of the support platform 704 to 15 mm. Program the tensile tester to perform a compression test, collecting force and extension data at an acquisition rate of 200 Hz as the crosshead lowers at a rate of 500 mm/min for a total distance of 35 mm.


Precondition samples at about 23° C.±2° C. and about 50%±2% relative humidity for 2 hours prior to testing. The outer cover article is opened and placed with the wearer-facing surface facing downward. Using scissors remove the leg elastics, such that the article can be laid flat. Identify and mark the center of a sampling region which is representative of the material making up the majority of the article, ensuring that it is free of seams, snaps, labels, etc. The sampling region may often be located toward the back/crotch region of the article. With a hydraulic press and cutting die (76.2 mm square±0.1 mm and 8 mm deep), cut a specimen centered on this mark through all the layers of the article, with the specimen's cut edges parallel and perpendicular to the longitudinal and lateral axis of the article.


Place the all layers of the specimen flat onto the surface of the support platform 704 over the gap 709 with the wearer-facing surface facing upward. Arrange the specimen 1009 under the blade 603 such that about ⅓ of the specimen is to the right of the blade and ⅔ to the left. The specimen is placed such that the direction corresponding to the lateral axis of the absorptive article it was harvested from is parallel to the length of the blade. Zero the load cell; start the tensile tester and the data acquisition. Program the software to calculate the maximum Peak Bending Force (N) from the constructed force (N) verses extension (m) curve, and record as “Lateral face-up”.


Remove the specimen from the gap 709, keeping the wearer-facing side up. Rotate the specimen 90° clockwise, and arrange the specimen under the blade 603 such that about ⅓ of the specimen is to the right of the blade and ⅔ to the left, exposing a fresh area of the specimen for testing. Zero the load cell; start the tensile tester and the data acquisition. Record the maximum Peak Bending Force (N) as “Longitudinal face-up”.


Remove the specimen from the gap 709, keeping the wearer-facing side up. Rotate the specimen 90° counter-clockwise, and turn the specimen over from left to right, so that the wearer-facing surface is facing downward. Arrange the specimen under the blade 603 such that about ⅓ of the specimen is to the right of the blade and ⅔ to the left, exposing a fresh area of the specimen for testing. Zero the load cell; start the tensile tester and the data acquisition. Record the maximum Peak Bending Force (N) as “Lateral face-down”.


Remove the specimen from the gap 709, keeping the wearer-facing side down. Rotate the specimen 90° counter-clockwise, and arrange the specimen under the blade 603 such that about ⅓ of the specimen is to the right of the blade and ⅔ to the left, exposing a fresh area of the specimen for testing. Zero the load cell; start the tensile tester and the data acquisition. Record the maximum Peak Bending Force (N) as “Longitudinal face-down”.


Calculate the Total Stiffness for a specimen by summing the “Lateral face-up”, “Longitudinal face-up”, “Lateral face-down” and “Longitudinal face-down” forces. Report the Total Stiffness to the nearest 0.001 N. Repeat the test and record the results for 10 samples. Calculate and report the average Total Stiffness.


The dimensions and values disclosed herein are not to be understood as being strictly limited to the exact numerical values recited. Instead, unless otherwise specified, each such dimension is intended to mean both the recited value and a functionally equivalent range surrounding that value. For example, a dimension disclosed as “40 mm” is intended to mean “about 40 mm.”


Every document cited herein, including any cross referenced or related patent or application, is hereby incorporated herein by reference in its entirety unless expressly excluded or otherwise limited. The citation of any document is not an admission that it is prior art with respect to any invention disclosed or claimed herein or that it alone, or in any combination with any other reference or references, teaches, suggests or discloses any such invention. Further, to the extent that any meaning or definition of a term in this document conflicts with any meaning or definition of the same term in a document incorporated by reference, the meaning or definition assigned to that term in this document shall govern.


While particular embodiments of the present invention have been illustrated and described, it would be obvious to those skilled in the art that various other changes and modifications can be made without departing from the spirit and scope of the invention. It is therefore intended to cover in the appended claims all such changes and modifications that are within the scope of this invention.

Claims
  • 1. A diaper comprising an outer cover, the outer cover comprising: a front waistband and a rear waistband opposite the front waistband;a landing zone adjacent to the front waistband, wherein the landing zone extends perpendicularly across a longitudinal center line of the outer cover;a fastener configured to permanently or releasably join to the landing zone to form a waist opening;a first connector disposed on the rear portion of the outer cover;a second connector disposed on the front portion of the outer cover, wherein the first connector and the second connector are adapted to releasably join an absorbent insert to the outer cover, and wherein the first connector is different from the second connector to indicate a proper orientation of the absorbent insert;a first, wearer-facing layer having a wearer-facing surface; anda second, garment-facing layer;wherein the outer cover has an absorbent capacity between 5 and 100 g and the wearer-facing surface of the first, wearer-facing layer has a DAT contact angle at 0.5 second of less than about 75 degrees,wherein the first, wearer-facing layer and the second, garment-facing layer are both made of Modal and Spandex,wherein the first, wearer-facing layer and the second, garment-facing layer are joined to at least one of the front waistband and the rear waistband, andwherein each of the first, wearer-facing layer and the second, garment-facing layer have a bending stiffness less than 0.10N.
  • 2. The outer cover of claim 1, wherein the second, garment-facing layer is hydrophobic.
  • 3. The outer cover of claim 1, wherein the outer cover as a whole has a WVTR between 1,200 g/m2/24 hr and 15,000 g/m2/24 hr.
  • 4. The outer cover of claim 3, wherein the outer cover as a whole has a WVTR between 3,000 g/m2/24 hr and 10,000 g/m2/24 hr.
  • 5. The outer cover of claim 1, wherein the wearer-facing surface of the first, wearer-facing layer has a nonpolar component of surface energy of less than about 3.5 mJ/mm2.
  • 6. The outer cover of claim 5, wherein the wearer-facing surface has a nonpolar component of surface energy of less than about 3.0 mJ/mm2.
  • 7. The outer cover of claim 6, wherein the wearer-facing surface has a nonpolar component of surface energy of less than about 2.5 mJ/mm2.
  • 8. The outer cover of claim 1, wherein the wearer-facing surface of the first, wearer-facing layer has a DAT contact angle at 1 second of less than about 70 degrees.
  • 9. The outer cover of claim 8, wherein the wearer-facing surface of the first, wearer-facing layer has a DAT contact angle at 1 second of less than about 45 degrees.
  • 10. The outer cover of claim 1, wherein the first, wearer-facing layer has a strikethrough time of less than about 15 seconds.
  • 11. The outer cover of claim 1, wherein the first, wearer-facing layer has a strikethrough time of less than about 10 seconds.
  • 12. The outer cover of claim 1, wherein the first, wearer-facing layer has a strikethrough time between 1 and 15 seconds.
  • 13. The outer cover of claim 1, further comprising a third layer disposed between the first, wearer-facing layer and the second, garment-facing layer, wherein the third layer is hydrophobic.
  • 14. A diaper comprising an outer cover, the outer cover comprising a single layer or laminate of material, wherein the outer cover comprises: a first, wearer facing surface;a second, garment facing surface opposite the first, wearer facing surface;a front waistband and a rear waistband opposite the front waistband;a landing zone disposed on the wearer-facing surface of the outer cover, wherein the landing zone extends perpendicularly across a longitudinal center line of the outer cover;a fastener configured to permanently or releasably join to the landing zone to form a waist opening;a legband attached to a portion of a perimeter of the outer cover and intermediate the front waistband and the rear waistband;a first connector adjacent to the front waistband and a second connector adjacent to the rear waistband, wherein the first and second connectors are adapted to permanently or releasably join an absorbent insert to the outer cover, and wherein the first connector has at least one of a different shape and a different dimension than the second connector to indicate a desired orientation of the absorbent insert;wherein the outer cover has an absorbent capacity between 5 and 100 g and the first, wearer-facing surface has a DAT contact angle at 0.5 second of less than about 75 degrees,wherein the outer cover is made of Modal and Spandex.
  • 15. The outer cover of claim 14, wherein the second, garment-facing surface is hydrophobic.
  • 16. The outer cover of claim 14, wherein the outer cover has a WVTR between 1,200 g/m2/24 hr and 15,000 g/m2/24 hr.
  • 17. The outer cover of claim 16, wherein the outer cover has a WVTR between 3,000 g/m2/24 hr and 10,000 g/m2/24 hr.
  • 18. The outer cover of claim 15, wherein the second, garment-facing surface is coated with a water resistant compound.
  • 19. The outer cover of claim 18, wherein the water resistant compound is selected from the group consisting of polytetrafluoroethylene, fluorocarbon derivatives, hydrophobic silicone polymers, hydrophobic fluorinated polymers, and combinations thereof.
CROSS REFERENCE TO RELATED APPLICATIONS

This application claims the benefit of U.S. Provisional Application No. 61/366,670, filed Jul. 22, 2010, and U.S. Provisional Application No. 61/484,782, filed May 11, 2011, both of which are hereby incorporated by reference in their entireties.

US Referenced Citations (327)
Number Name Date Kind
2530647 Buehler Nov 1950 A
2688328 Marcus Sep 1954 A
2793642 Andruhovici May 1957 A
3077193 Mann Feb 1963 A
3162196 Salk Dec 1964 A
3496259 Guenther Feb 1970 A
3560292 Butter Feb 1971 A
3574791 Patsy et al. Apr 1971 A
3719736 Woodruff Mar 1973 A
3735424 Maggio et al. May 1973 A
3860003 Buell Jan 1975 A
3911173 Sprague, Jr. Oct 1975 A
3926189 Taylor Dec 1975 A
3929135 Thompson Dec 1975 A
3955575 Okuda May 1976 A
4022210 Glassman May 1977 A
4072150 Glassman Feb 1978 A
4081301 Buell Mar 1978 A
4116892 Schwarz Sep 1978 A
4223059 Schwarz Sep 1980 A
4265245 Glassman May 1981 A
4284454 Joa Aug 1981 A
4324246 Mullane et al. Apr 1982 A
4326302 Lowe et al. Apr 1982 A
4338939 Daville Jul 1982 A
4342314 Radel et al. Aug 1982 A
4352356 Tong Oct 1982 A
4397646 Daniels et al. Aug 1983 A
4438167 Schwarz Mar 1984 A
4463045 Ahr et al. Jul 1984 A
4475912 Coates Oct 1984 A
4496360 Joffe et al. Jan 1985 A
4573986 Minetola et al. Mar 1986 A
4578073 Dysart et al. Mar 1986 A
4579556 Mcfarland Apr 1986 A
4582550 Sigl Apr 1986 A
4597760 Buell Jul 1986 A
4597761 Buell Jul 1986 A
4609518 Curro et al. Sep 1986 A
4610678 Weisman et al. Sep 1986 A
4615695 Cooper Oct 1986 A
4629643 Curro et al. Dec 1986 A
4643726 Gegelys Feb 1987 A
4650483 Joffe Mar 1987 A
4657539 Hasse Apr 1987 A
4661102 Shikata et al. Apr 1987 A
4673402 Weisman et al. Jun 1987 A
4695278 Lawson Sep 1987 A
4701170 Wilson et al. Oct 1987 A
4704114 Wilson et al. Nov 1987 A
4710187 Boland et al. Dec 1987 A
4743239 Cole May 1988 A
4747846 Boland et al. May 1988 A
4756709 Stevens Jul 1988 A
4770656 Proxmire et al. Sep 1988 A
4773906 Krushel Sep 1988 A
4785996 Ziecker et al. Nov 1988 A
4795452 Blaney et al. Jan 1989 A
4795454 Dragoo Jan 1989 A
4808176 Kielpikowski Feb 1989 A
4808177 Desmarais et al. Feb 1989 A
4808178 Aziz et al. Feb 1989 A
4816026 Richardson Mar 1989 A
4821342 Troyer Apr 1989 A
4834735 Alemany et al. May 1989 A
4834736 Boland et al. May 1989 A
4834737 Khan May 1989 A
4834738 Kielpikowski et al. May 1989 A
4842666 Werenicz Jun 1989 A
4872871 Proxmire et al. Oct 1989 A
4880423 Green Nov 1989 A
4888231 Angstadt Dec 1989 A
4892536 Desmarais et al. Jan 1990 A
4892598 Stevens et al. Jan 1990 A
4906243 Dravland Mar 1990 A
4908247 Baird et al. Mar 1990 A
4909803 Aziz et al. Mar 1990 A
4936840 Proxmire Jun 1990 A
4955880 Rodriquez Sep 1990 A
4961736 McCloud Oct 1990 A
4961737 Orlando et al. Oct 1990 A
4964857 Osborn Oct 1990 A
4968311 Chickering et al. Nov 1990 A
4968312 Khan Nov 1990 A
4978046 Hagmann et al. Dec 1990 A
4981480 Gaudet et al. Jan 1991 A
4988344 Reising et al. Jan 1991 A
4988345 Reising Jan 1991 A
4990147 Freeland Feb 1991 A
5006394 Baird Apr 1991 A
5019068 Perez et al. May 1991 A
5021051 Hiuke Jun 1991 A
5032120 Freeland et al. Jul 1991 A
5037416 Allen et al. Aug 1991 A
5069672 Wippler et al. Dec 1991 A
5087253 Cooper Feb 1992 A
5108385 Snyder Apr 1992 A
5127108 Weiss Jul 1992 A
5137537 Herron et al. Aug 1992 A
5141870 Bedbrook et al. Aug 1992 A
5147345 Young et al. Sep 1992 A
5155867 Norvell Oct 1992 A
5156793 Buell et al. Oct 1992 A
5167897 Weber et al. Dec 1992 A
5185011 Strasser Feb 1993 A
5202173 Wu et al. Apr 1993 A
5207663 McQueen May 1993 A
5210882 Moretz et al. May 1993 A
5217447 Gagnon Jun 1993 A
5234423 Alemany et al. Aug 1993 A
5254111 Cancio et al. Oct 1993 A
5260345 Desmarais et al. Nov 1993 A
5261901 Guay Nov 1993 A
5269775 Freeland et al. Dec 1993 A
5291617 Moretz et al. Mar 1994 A
5296184 Wu et al. Mar 1994 A
5306267 Hahn et al. Apr 1994 A
5342338 Roe Aug 1994 A
5354597 Capik et al. Oct 1994 A
5360422 Brownlee et al. Nov 1994 A
5368584 Clear et al. Nov 1994 A
5368585 Dokken Nov 1994 A
5387207 Dyer et al. Feb 1995 A
5401266 Runeman et al. Mar 1995 A
5405342 Roessler et al. Apr 1995 A
5415650 Sigl May 1995 A
5435014 Moretz et al. Jul 1995 A
5458591 Roessler et al. Oct 1995 A
5476457 Roessler et al. Dec 1995 A
5514121 Roe et al. May 1996 A
5518801 Chappell et al. May 1996 A
5554142 Dreier et al. Sep 1996 A
5562648 Peterson Oct 1996 A
5571096 Dobrin et al. Nov 1996 A
5607760 Roe Mar 1997 A
5609587 Roe Mar 1997 A
5613959 Roessler et al. Mar 1997 A
5624425 Gray et al. Apr 1997 A
5625222 Yoneda et al. Apr 1997 A
5635191 Roe et al. Jun 1997 A
H1670 Aziz et al. Jul 1997 H
5643588 Roe et al. Jul 1997 A
5667503 Roe et al. Sep 1997 A
5671615 Kj.ae butted.rgaard et al. Sep 1997 A
5716349 Taylor et al. Feb 1998 A
H1732 Johnson Jun 1998 H
5769838 Buell et al. Jun 1998 A
5772649 Siudzinski Jun 1998 A
5776121 Roe et al. Jul 1998 A
5795347 Roe et al. Aug 1998 A
5795348 Roe et al. Aug 1998 A
5807371 Toyoda et al. Sep 1998 A
5814037 Coates Sep 1998 A
5827261 Osborn et al. Oct 1998 A
5843065 Wyant Dec 1998 A
5843267 Cashaw et al. Dec 1998 A
H1788 Christon et al. Feb 1999 H
5865823 Curro Feb 1999 A
5906603 Roe et al. May 1999 A
5911713 Yamada et al. Jun 1999 A
5938648 Lavon et al. Aug 1999 A
5941864 Roe Aug 1999 A
5947946 Fisher et al. Sep 1999 A
5968025 Roe et al. Oct 1999 A
6007528 Osborn Dec 1999 A
6010491 Roe et al. Jan 2000 A
6120487 Ashton Sep 2000 A
6229061 Dragoo et al. May 2001 B1
6251097 Kline et al. Jun 2001 B1
6258308 Brady et al. Jul 2001 B1
6278037 Schmidt et al. Aug 2001 B1
6287169 Willms et al. Sep 2001 B1
6291039 Combe et al. Sep 2001 B1
6307119 Cammarota et al. Oct 2001 B1
6368444 Jameson et al. Apr 2002 B1
6414215 Roe Jul 2002 B1
6420627 Ohnishi et al. Jul 2002 B1
6423043 Gustafsson Jul 2002 B1
6432098 Kline et al. Aug 2002 B1
6468257 Ono et al. Oct 2002 B1
6482191 Roe et al. Nov 2002 B1
6547773 Kleinschmidt et al. Apr 2003 B2
6562016 Shinkai May 2003 B2
6575951 Ono et al. Jun 2003 B1
6579273 Dupuy Jun 2003 B2
6605071 Gray et al. Aug 2003 B1
6610901 McMahon-Ayerst et al. Aug 2003 B2
6623466 Richardson Sep 2003 B1
6669618 Reising et al. Dec 2003 B2
6680422 Roe Jan 2004 B2
6716441 Osborne et al. Apr 2004 B1
6764477 Chen et al. Jul 2004 B1
6764478 Ashton et al. Jul 2004 B2
6786895 Schmitz Sep 2004 B1
6794023 Melik et al. Sep 2004 B1
6807685 Hasegawa et al. Oct 2004 B1
6811643 McAmish et al. Nov 2004 B2
6817992 Sassak et al. Nov 2004 B1
6821612 Melik et al. Nov 2004 B1
6843949 Brady et al. Jan 2005 B2
6893388 Reising et al. May 2005 B2
6980872 Kano et al. Dec 2005 B2
7037569 Curro et al. May 2006 B2
7101359 Kline et al. Sep 2006 B2
7166095 Coates Jan 2007 B1
7250549 Richlen et al. Jul 2007 B2
7264615 Sherrod et al. Sep 2007 B2
7344526 Yang et al. Mar 2008 B2
7387620 Watanabe et al. Jun 2008 B2
7407468 Reising et al. Aug 2008 B2
7431716 Tracy Oct 2008 B2
7458961 Carstens Dec 2008 B2
7462173 Carstens Dec 2008 B2
7481801 Carstens Jan 2009 B2
7491196 Frank et al. Feb 2009 B2
7521587 Busam et al. Apr 2009 B2
7537587 Carstens May 2009 B2
7576019 Bond et al. Aug 2009 B2
7626073 Catalan Dec 2009 B2
7629501 Labit et al. Dec 2009 B2
7666175 Trennepohl Feb 2010 B2
7695463 LaVon et al. Apr 2010 B2
7771406 Mueller et al. Aug 2010 B2
7771408 Mueller et al. Aug 2010 B2
7776771 Autran et al. Aug 2010 B2
7785309 Van Gompel et al. Aug 2010 B2
7820875 Roe et al. Oct 2010 B2
7833211 Mansfield Nov 2010 B2
7914507 Magee Mar 2011 B1
7993322 Brud et al. Aug 2011 B2
8118801 Macura et al. Feb 2012 B2
8158043 Gibson et al. Apr 2012 B2
20020010452 Dupuy Jan 2002 A1
20020035747 Kusibojoska et al. Mar 2002 A1
20020128619 Carlbark et al. Sep 2002 A1
20030091807 Desai et al. May 2003 A1
20030114805 Rainville et al. Jun 2003 A1
20030125701 Widlund Jul 2003 A1
20030163104 Tears et al. Aug 2003 A1
20030233082 Kline et al. Dec 2003 A1
20040023771 Reising et al. Feb 2004 A1
20040127867 Odorzynski et al. Jul 2004 A1
20050033258 Suzuki et al. Feb 2005 A1
20050096624 Hoshino et al. May 2005 A1
20050131382 Brud et al. Jun 2005 A1
20050148974 Datta et al. Jul 2005 A1
20050164587 Melik et al. Jul 2005 A1
20050177123 Catalan Aug 2005 A1
20050215965 Schmidt et al. Sep 2005 A1
20050215968 Henderson Sep 2005 A1
20050215970 Kline et al. Sep 2005 A1
20050215971 Roe et al. Sep 2005 A1
20050234411 Ashton et al. Oct 2005 A1
20060035055 Schneider et al. Feb 2006 A1
20060047260 Ashton et al. Mar 2006 A1
20060058766 Mueller et al. Mar 2006 A1
20060069372 Chakavarty et al. Mar 2006 A1
20060087053 O'Donnell et al. Apr 2006 A1
20060107505 Desai et al. May 2006 A1
20060129114 Mason et al. Jun 2006 A1
20060129116 Hughes et al. Jun 2006 A1
20060178652 Miller Aug 2006 A1
20060189956 Catalan Aug 2006 A1
20060229582 LaVon Oct 2006 A1
20060247599 Mullen et al. Nov 2006 A1
20060264865 Carstens Nov 2006 A1
20060264867 Carstens Nov 2006 A1
20060264868 Carstens Nov 2006 A1
20060264869 Carstens Nov 2006 A1
20060264870 Carstens Nov 2006 A1
20060264871 Carstens Nov 2006 A1
20060264872 Carstens Nov 2006 A1
20060264873 Carstens Nov 2006 A1
20060264874 Carstens Nov 2006 A1
20060264877 Carstens Nov 2006 A1
20060264878 Carstens Nov 2006 A1
20060264879 Carstens Nov 2006 A1
20060264880 Carstens Nov 2006 A1
20060264881 Carstens Nov 2006 A1
20060264882 Carstens Nov 2006 A1
20060264883 Carstens Nov 2006 A1
20060264884 Carstens Nov 2006 A1
20060264885 Carstens Nov 2006 A1
20060282056 McDonald Dec 2006 A1
20060293637 La Von et al. Dec 2006 A1
20070005038 Mansfield et al. Jan 2007 A1
20070032772 Ehrnsperger et al. Feb 2007 A1
20070142798 Goodlander et al. Jun 2007 A1
20070142816 Carstens Jun 2007 A1
20070191806 Mueller et al. Aug 2007 A1
20070239130 Trennepohl Oct 2007 A1
20080033388 Mueller et al. Feb 2008 A1
20080114320 Beck et al. May 2008 A1
20080114327 Barge May 2008 A1
20080119813 Carstens May 2008 A1
20080119816 Carstens May 2008 A1
20080125737 Modgeddi et al. May 2008 A1
20080224351 Curro et al. Sep 2008 A1
20080287983 Smith et al. Nov 2008 A1
20080312617 Hundorf et al. Dec 2008 A1
20080312618 Hundorf et al. Dec 2008 A1
20080312619 Ashton et al. Dec 2008 A1
20080312620 Ashton et al. Dec 2008 A1
20080312621 Hundorf et al. Dec 2008 A1
20080312622 Hundorf et al. Dec 2008 A1
20080312623 Hundorf et al. Dec 2008 A1
20080312624 Hundorf et al. Dec 2008 A1
20080312625 Hundorf et al. Dec 2008 A1
20080312628 Hundorf et al. Dec 2008 A1
20090048571 Spitzmueller et al. Feb 2009 A1
20090127742 Qureshi et al. May 2009 A1
20090133446 Burrow et al. May 2009 A1
20090317584 Ivanoff et al. Dec 2009 A1
20100005570 Rachman Jan 2010 A1
20100179495 Roe et al. Jul 2010 A1
20100179496 Roe et al. Jul 2010 A1
20100179498 Roe Jul 2010 A1
20100179499 Roe Jul 2010 A1
20100179500 Roe et al. Jul 2010 A1
20100179501 Roe et al. Jul 2010 A1
20100179502 Roe Jul 2010 A1
20100179503 Roe Jul 2010 A1
20100201024 Gibson et al. Aug 2010 A1
20100249736 Png et al. Sep 2010 A1
20110172628 Roe et al. Jul 2011 A1
20120022481 Roe et al. Jan 2012 A1
20120049404 Gibson et al. Mar 2012 A1
Foreign Referenced Citations (79)
Number Date Country
642 386 Oct 1993 AU
2 103 537 Feb 1995 CA
2 221 209 Nov 1996 CA
2 365 577 Jun 2003 CA
1505531 Jun 2004 CN
1285727 Nov 2006 CN
103 03 903 Nov 2003 DE
0 023 804 Feb 1981 EP
0 187 726 Jul 1986 EP
0 319 314 Jun 1989 EP
0 811 362 Dec 1997 EP
0 549 988 Jun 1998 EP
0 796 069 Aug 2000 EP
0 763 353 Jun 2002 EP
2 106 775 Oct 2009 EP
2532337 Mar 1984 FR
2606257 May 1988 FR
0 112 638 Jan 1918 GB
2 440 314 Jan 2008 GB
55-37849 Sep 1978 JP
57-138908 Aug 1982 JP
57-181003 Nov 1982 JP
57-184864 Dec 1982 JP
59-5656 Jan 1984 JP
59-5657 Jan 1984 JP
59-147214 Sep 1984 JP
59-147215 Sep 1984 JP
60-87139 Jun 1985 JP
60-91191 Jun 1985 JP
61-98628 Jun 1986 JP
61-168103 Oct 1986 JP
62-110903 Jul 1987 JP
63-196701 Aug 1988 JP
03-091325 Jan 1990 JP
04-77922 Nov 1990 JP
06-178795 Jan 1993 JP
06-63077 Mar 1994 JP
30-73695 Sep 2000 JP
2001-353183 Dec 2001 JP
2002-95698 Apr 2002 JP
2002-325786 Nov 2002 JP
2003-038564 Feb 2003 JP
2003-190213 Jul 2003 JP
2005-6827 Jan 2005 JP
2005-111119 Apr 2005 JP
31-09189 May 2005 JP
2007-244506 Mar 2006 JP
2007-68654 Mar 2007 JP
2008-055002 Mar 2008 JP
WO 9008524 Aug 1990 WO
WO 9116871 Nov 1991 WO
WO 9201431 Feb 1992 WO
WO 9215444 Sep 1992 WO
WO 9415563 Jul 1994 WO
WO 9415663 Jul 1994 WO
WO 9510992 Apr 1995 WO
WO 9516746 Jun 1995 WO
WO 9617572 Jun 1996 WO
WO 9624319 Aug 1996 WO
WO 9632912 Oct 1996 WO
WO 9724095 Jul 1997 WO
WO 0065348 Nov 2000 WO
WO 0134080 May 2001 WO
WO 02066086 Aug 2002 WO
WO 2004060229 Jul 2004 WO
WO 2005039469 May 2005 WO
WO 2005052052 Jun 2005 WO
WO 2005096855 Oct 2005 WO
WO 2005097031 Oct 2005 WO
WO 2008030984 Mar 2008 WO
WO 2008120959 Oct 2008 WO
WO 2008142634 Nov 2008 WO
WO 2010053006 May 2010 WO
WO 2010111717 Sep 2010 WO
WO 2010113071 Oct 2010 WO
WO 2010134169 Nov 2010 WO
WO 2010135510 Nov 2010 WO
WO 2011047252 Apr 2011 WO
WO 2011047264 Apr 2011 WO
Non-Patent Literature Citations (16)
Entry
PCT International Search Report dated Dec. 22, 2011, 10 pages.
PCT International Search Report and Written Opinion dated Mar. 27, 2011, 26 pages.
www.gdiapers.com—Web pages dated Nov. 23, 2009.
www.fuzzibunz.com—Web pages dated Nov. 23, 2009.
www.greenmountaindiapers.com—Web pages dated Nov. 23, 2009.
www.bumgenius.com—Web pages dated Nov. 23, 2009.
www.thirstiesbaby.com—Web pages dated Nov. 23, 2009.
www.crickettsdiaper.com—Web pages dated Nov. 23, 2009.
Archived web page from www.bummis.com, Aug. 8, 2005, obtained via www.waybackmachine.org.
“Green Life; Earth-Friendly Disposable Diaper Lets Parents Flush Away the Guilt”, The Oregonian (Apr. 7 2005).
“Crazy for Cloth: The Benefits of Cotton Diapers”, Mothering Magazine (Jan. 1, 2003).
“Not Your Grandma's Diapers”, E: The Environmental Magazine (Mar.-Apr. 2006).
“Y2K Babyware: Your Green Guide to Carefree Diapering for Your Millennium Bundle of Joy”. The Gazette (Montreal, Quebec) (Oct. 5, 2000).
“The Evolution of Diapers: Cloth Meets Cute for Some Mothers (and Grandmothers), The Changes in Cloth Diapers Have Made Them all the Rage. Learning the Lingo Navigating Cloth” Omaha World Herald (Mar. 22, 2004).
37 photographs (obtained from Marketing Technology Service, Inc.) of a product believed to be a product of Kao Corp. and sold in Japan in 1986 (translations provided by Applicants.
Data Sheet, p. V-17, from “Baby Diaper Design Update—1987”; publication of Marketing Technology Service, Inc., product believed to be a product of Kao Corp. sold. in Japan in 1986 or 1987.
Related Publications (1)
Number Date Country
20120022481 A1 Jan 2012 US
Provisional Applications (2)
Number Date Country
61366670 Jul 2010 US
61484782 May 2011 US