This application claims a priority to Chinese Patent Application No. 201610191220.6 filed on Mar. 30, 2016, the disclosures of which are incorporated in their entirety by reference herein.
The present disclosure relates to the technology of sealing cell devices, and in particular to a panel.
A cell sealing technology refers to seal a cell formed by oppositely arranging two substrates at a periphery thereof by a sealant. At present, the vast majority of display panels are formed by oppositely arranging an array substrate and a packaging substrate to form a cell. In the related art, the display panel is generally sealed by a single ring of sealant, and then a stress of a laser sintering process performed onto the single ring of sealant is in only one direction, such that a mechanical support ability of the display panel is reduced. In additions, it is found in an environmental reliability test that a damage of a single point of the single ring of sealant may be easily to be spread peripherally, such that the components in the display panel may be aged and malfunctioned rapidly, therefore the service life and the mechanical support ability may not be guaranteed.
The object of the present disclosure is to solve the issue that mechanical support strength of a cell device sealed by a single ring of sealant is low and a service life thereof is short.
To achieve the object, a panel is provided by the present disclosure, including a cell defined by a first substrate and a second substrate and a functional component between the first and second substrates. There exist at least two rings of sealant configured to seal the functional component, and the rings of the sealant are spaced from each other.
Optionally, the sealant is glass sealant.
Optionally, the rings of the glass sealant are cured by laser sintering processes performed in different directions.
Optionally, a water-resistive and oxygen-resistive material is further arranged between the adjacent two rings of the sealant.
Optionally, the water-resistive and oxygen-resistive material is a desiccant.
Optionally, the water-resistive and oxygen-resistive material is spaced from each of the adjacent two rings of the sealant.
Optionally, the panel is a display panel. The panel further includes a display region enclosed by the rings of the sealant and a spacer between the display region and the rings of the sealant.
Optionally, the spacer includes a spacer body made of a photopolymer material or a photolysis material and a supporting portion within the spacer body.
Optionally, the supporting portion is harder than the spacer body.
Optionally, the supporting portion is made of silicon or silicon oxide, and the spacer body is made of an ultraviolet-curing adhesive or a photoresist.
Optionally, the supporting portion is spherical.
According to the panel provided by the present disclosure, supposing that the region of the sealant of the panel in some embodiments of the present disclosure is identical to that in the related art, the single ring of sealant is divided into a plurality of rings, and thus a total contact area of the sealant and both the first and second substrates may be reduced, thereby reducing a stress action and increasing a mechanical support strength. In addition, a ring of sealant at an inner side may also be functioned to protect the inner component in the case that a ring of sealant at an outer side is broken.
In order to make the objects, the technical solutions and the advantages of the present disclosure more apparent, the present disclosure will be described hereinafter in conjunction with the drawings and embodiments.
In order to solve the issues in the related art, a panel is provided by the present disclosure. As shown in
There exist at least two rings of sealant 4 between the first substrate 1 and the second substrate 2 (two rings of sealant 4 are shown in
Supposing that a region of the sealant of the panel in some embodiments of the present disclosure is identical to that in the related art, the single ring of sealant is divided into a plurality of rings, and thus a total contact area of the sealant and both the first and the second substrates may be reduced, thereby reducing a stress action and increasing a mechanical support strength. In addition, a ring of sealant at an inner side may also be functioned to protect the inner component in the case that a ring of sealant at an outer side is broken.
In some embodiments of the present disclosure, the sealant may be a glass sealant cured by a laser sintering process. In order to make the stresses of the glass sealant onto the first and the second substrates uniform, optionally laser sintering processes performed onto the rings of the glass sealant are in different directions, thereby avoiding a direct superposition of the stresses of the cured glass sealant which may reduce the mechanical support strength of the display panel.
It can be seen that, in compared with the packaging structure with a single ring of sealant, each ring of the sealant is narrowed in the packaging structure with multiple rings of sealant, and a laser spot may be reduced, thereby reducing a heating area of the glass sealant, significantly reducing the stress between the glass sealants, and reducing a reject ratio during a cutting process.
In addition, in order to prevent the component from being oxidized, as shown in
Of course, the glass sealant 4 is cured by the laser sintering process, so the water-resistive and oxygen-resistive material 5 may be spaced from each of the adjacent two rings of the sealant 4 by a predetermined distance H, thereby preventing chemical properties of the water-resistive and oxygen-resistive material 5 from being adversely influenced due to the high temperature.
In addition, in some embodiments of the present disclosure, the panel is a display panel, and then the display effect may be adversely influenced in the case that the distance between the first and the second substrates cannot be kept. The sealant is arranged between at the edge of the display panel, so it is difficult to support the first and the second substrates only by the sealant. Once a pressure is applied onto the display panel, a distance between the first and the second substrates at a center portion of the cell may be larger than that at the edges thereof, and then Newton ring phenomenon may occur at the edges of the displayed image, thereby seriously influencing the user's viewing experience. In view of this, as shown in
In the practical application, the spacer 6 in the display panel with a relative small distance between the two substrates may be formed by a stretchy photopolymer material (e.g., an ultraviolet-curing adhesive) or a stretchy photolysis material (e.g., photoresist), so as to buffer the impact onto the display panel.
However, for the display panel with a relative large distance between the two substrates such as the display panel with a 3D display function, the spacer formed by the photopolymer material or the photolysis material need to be thicker, such that a structural strength of the spacer may be reduced and then the spacer is easy to be subsided or deformed. In view of this, as shown in
It can be seen that, as shown in
Furthermore, in order to make the spacer have higher support strength, optionally, the supporting portion is harder than the spacer body. For example, when the spacer 61 is made of ultraviolet-curing adhesive or a photoresist, the supporting portion 62 may be made of silicon or silicon oxide.
The above are merely the preferred embodiments of the present disclosure. A person skilled in the art may make further modifications and improvements without departing from the principle/spirit of the present disclosure, and these modifications and improvements shall also fall within the scope of the present disclosure. For example, the spacer in some embodiments of the present disclosure may include one or more supporting portions, and the shapes of the supporting portions are not limited to be spherical as shown in
Number | Date | Country | Kind |
---|---|---|---|
201610191220.6 | Mar 2016 | CN | national |