Claims
- 1. In a process for the partial oxidation and desulfurization of sulfur and silicate-containing comminuted solid carbonaceous fuel including, basis solid fuel, 0.2 to 6.0 wt. % sulfur and 0.1 to 30 wt. % of silicate compounds including iron silicate the improvement comprising: (1) introducing into the reaction zone of a free-flow unobstructed vertical down-flowing refractory lined partial oxidation gas generator a feed mixture comprising said solid carbonaceous fuel and supplemental calcium-containing material entrained in a gaseous medium selected from the group consisting of steam, nitrogen, CO.sub.2, recycle synthesis gas, free-oxygen containing gas, and mixtures thereof; and with or without a temperature moderator; (2) reacting in said reaction zone said feed mixture from (1) with a controlled amount of free-oxygen containing gas so that an equilibrium oxygen concentration is provided in the gas phase in the reaction zone with partial pressure which is less than about 10.sup.-12 atmosphere, the O/C atomic ratio is in the range of about 0.3 to 1.1, the H.sub.2 O/solid carbonaceous fuel weight ratio is in the range of about 0.03 to 0.70, the total moles of calcium in the reaction zone is at least equal to about 1.0 times the moles of sulfur in the solid carbonaceous fuel, and about 70 to 98 wt. % of the carbon in said solid carbonaceous fuel is converted into carbon oxides, thereby producing a hot raw product gas mixture comprising H.sub.2, CO, CO.sub.2, less than about 0.05 mole % of the H.sub.2 S and COS, at least one gas selected from the group consisting of H.sub.2 O, N.sub.2, CH.sub.4, and A, and entrained fly-ash in admixture with calcium sulfide and particulate carbon; wherein the mole ratio in the reaction zone for H.sub.2 O/H.sub.2 is in the range of about 0.1 to 0.7, wherein the partial oxidation and desulfurization reactions take place at a temperature which is at least about 400.degree. F. below the softening temperature o the ash in the solid fuel, and a pressure in the range of about 2 to 250 atmospheres; and wherein substantially no elemental iron is produced and there is substantially no formation of additional calcium silicates in the gas generator from said supplemental calcium-containing compound and the silicates from the said solid carbonaceous fuel, and at least about 90 wt. % of the sulfur in the solid carbonaceous fuel in the reaction zone is converted into said calcium sulfide particulate matter which leaves the reaction zone entrained in the hot raw product gas mixture from (1) along with said fly-ash and particulate carbon; and (3) cooling and cleaning the hot raw product gas mixture from (2) without direct contact with water.
- 2. The process of claim 1 wherein said sulfur and silicate-containing solid carbonaceous fuel is selected from the group consisting of coal coke made from coal; petroleum coke; oil shale; tar sands, pitch; and mixtures thereof.
- 3. The process of claim 1 wherein said calcium-containing material is selected from the group consisting of calcium oxide, calcium hydroxide, calcium carbonate, calcium acetate, calcium formate, calcium hydride, calcium nitrate, calcium chloride, and mixtures thereof.
- 4. The process of claim 1 wherein the hot raw product gas mixture in (2) is cooled and cleaned by contacting said hot raw product gas mixture with a liquid hydrocarbonaceous fuel cooling and scrubbing agent thereby producing a slurry comprising calcium sulfide, fly-ash and particulate carbon in liquid hydrocarbonaceous fuel.
- 5. The process of claim 4 provided with the steps of steam stripping said slurry comprising calcium-sulfide, fly-ash and particulate carbon in liquid hydrocarbonaceous fuel and and separating H.sub.2 S, and recycling the sulfur-depleted slurry to the front end of the process for use in preparation of fresh feed mixture to the partial oxidation gas generator.
- 6. The process of claim 5 provided with the steps of recovering sulfur from the mixture of steam and H.sub.2 S.
- 7. The process of claim 1 wherein the temperature in said reaction zone is below about 2175.degree. F.
- 8. The process of claim 2 wherein said coal is selected from the group consisting of subbituminous, bituminous anthracite, lignite, and mixtures thereof.
Parent Case Info
This is a continuation-in-part of copending application Ser. No. 07/062,018, filed June 15, 1987, now U.S. Pat. No. 4,801,438.
US Referenced Citations (15)
Continuation in Parts (1)
|
Number |
Date |
Country |
Parent |
62018 |
Jun 1987 |
|