The present invention generally relates to vertical cavity surface emitting lasers (VCSELs) and, more particularly to, a VCSEL and a method of making the same which allows the VCSEL array to be packed in a denser way, thereby increasing the die counts formed on a wafer and reducing the die cost accordingly.
Semiconductor lasers are being used in many imaging applications which require high power illumination such as structured light sources for 3D imaging, Laser Detection and Ranging (LADAR), Time of Flight (TOF) 3D imaging, aviation defense, and fusion research, among others. Vertical Cavity Surface Emitting Lasers (VCSELs), are commonly used in many semiconductor laser applications due to the low power applications and high frequency superiority and manufacturing advantages over other type of semiconductor laser devices.
A VCSEL is a semiconductor micro-laser diode that emits light in a generally cylindrical beam. The beam is emitted vertically from the surface of the substrate on which it is fabricated. Because the beams in VCSELs emit vertically from the surface of the substrate, they can be tested on-wafer, before they are separated into individual devices. This reduces the fabrication cost of the devices. It also allows VCSELs to be built not only in one-dimensional, but also in two-dimensional arrays.
VCSELs generally have larger output apertures compared to most edge-emitting lasers. This may allow VCSELs to produce a lower divergence angle of the output beam, and makes possible high coupling efficiency with optical fibers. VCSELs also have high reflectivity mirrors, compared to most edge-emitting lasers, which may reduce the threshold current of VCSELs, resulting in low power consumption. The low threshold current also permits high intrinsic modulation bandwidths in VCSELs. The wavelength of VCSELs may also be tuned, within the gain band of the active region, by adjusting the thickness of the reflector layers.
In one type of VCSEL structure, a mesa/pillar type structure is formed with a relatively small oxidation aperture area, which enables it for high speed operations. Unfortunately, due to the structure of the required oxide layers, it is difficult to reduce the size of the VCSEL mesa. This limits the size/density of a VCSEL array, which limits the number of VCSEL devices that may be made on a single wafer, and thus increases die cost.
Therefore, it would be desirable to provide a homeopathic treatment and method that overcome the above problems.
In accordance with one embodiment, a backside Vertical Cavity Surface Emitting Laser (VCSEL) is disclosed. The VCSEL has a substrate. A first mirror device is formed on the substrate. An active region is formed on the first mirror device. A second mirror device is formed on the active region. A pillar is formed by directional Inductive Coupled Plasma-Reactive Ion Etcher (ICP-RIE). The pillar exposes a portion of the first mirror device, the active region and the second mirror device. A first metal contact is formed over a top section of the pillar. A second metal contact is formed on the substrate. An opening is formed in the second metal contact and aligned with the pillar.
In accordance with one embodiment, a method of forming a backside Vertical Cavity Surface Emitting Laser (VCSEL) device is disclosed. The method comprises: forming a first mirror device on a substrate; forming an active region on the first mirror device; forming a second mirror device on the active region; forming a pillar by directional Inductive Coupled Plasma-Reactive Ion Etcher (ICP-RIE), the pillar exposing a portion of the first mirror device, the active region and the second mirror device; applying a first metal contact over a top section of the pillar, and applying a second metal contact on the substrate, wherein an opening is formed in the second metal contact, and the opening aligned with the pillar.
In accordance with one embodiment, a backside Vertical Cavity Surface Emitting Laser (VCSEL) array is disclosed. The VCSEL array has a substrate. A first mirror device is formed on the substrate. An active region is formed on the first mirror device. A second mirror device is formed on the active region. A plurality of pillars is formed by directional Inductive Coupled Plasma-Reactive Ion Etcher (ICP-RIE). Each pillar exposes a portion of the first mirror device, the active region and the second mirror device. A first metal contact is formed over a top section of each of the pillars. A second metal contact is formed on the substrate. A plurality of openings is formed in the second metal contact, wherein each opening is aligned with a corresponding pillar.
The present application is further detailed with respect to the following drawings. These figures are not intended to limit the scope of the present application but rather illustrate certain attributes thereof. The same reference numbers will be used throughout the drawings to refer to the same or like parts.
The description set forth below in connection with the appended drawings is intended as a description of presently preferred embodiments of the disclosure and is not intended to represent the only forms in which the present disclosure may be constructed and/or utilized. The description sets forth the functions and the sequence of steps for constructing and operating the disclosure in connection with the illustrated embodiments. It is to be understood, however, that the same or equivalent functions and sequences may be accomplished by different embodiments that are also intended to be encompassed within the spirit and scope of this disclosure.
Embodiments of the exemplary VCSEL and method of forming the same disclose a VCSEL having a pillar/mesa (hereinafter pillar) formed without the need of any oxide layer for narrowing the internal optical aperture definition and formation. Metal contacts at the top of Inductively Coupled Plasma (ICP)/Reactive Ion Etching (RIE) etched pillars do not need to form a hollow ring (i.e., an open circle in the middle) to emit the laser light from the center opening. This may eliminate the need of a metal contact ring for extended pillar size and allow the VCSEL array to be packed in the densest way, hence increasing the die count on a wafer and reducing the die cost accordingly.
Referring to
Referring to
An active region 18 may be formed between the pair of DBRs 14 and 16. The active region 18 may be formed of one or more quantum wells for laser light generation. A buried layer 20 may be formed between the active region 18 and the DBR 16. The buried region 20 may be selectively oxidized to form oxide apertures 22 and 24.
One or more pillars 26 may then be formed by etching through the DBR 16 down to the active region 18 and to the BDR 14. Reactive ion etching may be used to form the free-standing pillars 26 that confine both the light and electrical current in the lateral direction. However, this type of device suffers increasing optical loss due to optical scattering at the surfaces of the pillar 26 as the pillar 26 diameter is reduced. A top metal contact ring 28 may then be formed on the top of the pillar 26. The metal contact ring 28 will need to have a center open 30 to emit light therethrough. A bottom metal contact layer 32 may be formed on the substrate 12.
Referring to
The VCSEL device 40 is formed on a substrate 42. The substrate 42 may be gallium arsenide (GaAs) substrate 42 or similar material. A pair of Distributed Braggs Reflectors (BDR) 44 and 46 may be formed on the substrate 42 and runs parallel to the substrate 42. The BDRs 44 and 46 may be formed of a plurality of layers. The DBRs 44 and 46 may be formed by disposing multiple layers of alternating materials with varying optical impedances. In general, the multiple alternate between high and low optical impedances.
An active region 48 may be formed between the pair of DBRs 44 and 46. The active region 48 may be formed of one or more quantum wells for laser light generation.
One or more pillars 50 may then be formed. In the present embodiment, a highly directional ICP (Inductive Coupled Plasma) reactive ion etcher (RIE) may be used to etch highly anisotropic pillars 50. By using ICP-RIE, the pillars 50 may have a cylinder type of cross-sectional profile having close to straight side walls. In accordance with one embodiment, the pillars 50 may have a profile in the 5-50 um diameter range. Etching by using ICP-RIE is important since if wet chemical isotropic etchant is used, the side walls of the pillars 50 will be tapered which will present issues when small diameter VCSELs are to be fabricated. Thus, the pillars 50 should be etched by ICP-RIE with an anisotropic straight wall profile.
A top metal contact 52 may then be deposited and cover the top of the pillar 50. The metal contact 52 does not have to be in a ring configuration to emit light therethrough. In accordance with one embodiment, the top metal contact 52 may be use as the pillar ICP-RIE etch mask so there will be no need to deposit the top metal contact after the ICP-RIE pillar etch is performed. This will greatly simplify the manufacturing process of the VCSEL array with the current invention.
After the top metal contact 52 and pillars 50 are formed, the wafer upon which the VCSEL device 40 is formed upon may be turned around to form a backside metal contact 54. The backside metal contact 54 may be formed with an opening 56 to allow the laser light to be emitted from the back of the VCSEL device 40. The opening 56 may be aligned with the pillar 50 to allow the laser light to be emitted from the back of the VCSEL device 40.
Referring to
To flip-chip mount the VCSEL device 40, solder tips may be placed on the metal contact 52 formed on the pillars 50. In accordance with one embodiment, the solder tips may be done by electric-chemical plating a thin layer of solder 54 such as Au—Sn on top of the metal contact 42 of the pillar 50. The wafer upon which the VCSEL device 40 is formed upon may be turned upside down so that the solder 54 meets and join metal pad 56 of a package or heat sinking substrate 58. In accordance with one embodiment, the solder 54 meets and joins the metal pad 56 through a furnace-based solder re-flow process.
The VCSEL device 40 allows for additional design features such as lithographically formed focusing or diffraction or structure lens to be placed on the backside of the wafer where the backside metal opening is that emits the laser light. This feature will provide the VCSEL users to align, direct, focus, and adjust the laser lights coming out of the pillars 50 with different lens designs.
Referring to
To flip-chip mount the array 70 of VCSEL devices 40, solder tip may be placed on the metal contact 52 formed on each pillar 50. In accordance with one embodiment, the solder tips may be done by electric-chemical plating a thin layer of solder 54 such as Au—Sn on top of the metal contact 42 of the pillar 50. The wafer upon which the VCSEL device 40 is formed upon may be turned upside down so that the solder 54 meets and join metal pad 56 of a package or heat sinking substrate 58. In accordance with one embodiment, the solder 54 meets and joins the metal pad 56 through a furnace-based solder re-flow process.
It is necessary that the solder 54 be placed on the metal contact 52 formed on each pillar 50 to ensure good thermal contact of every VCSEL device 40, and to avoid any air voids. Air voids formed underneath a large area array may cause uneven thermal contact and create localized heated spots.
Referring to
In typical prior art VCSEL designs, there are two thick DBR layers, each of 3-5 micron in thickness, sandwiched the active region (i.e., Quantum Well (QW) action region). In the prior art designs, the AlGaAs oxidation layer which is close to the active region must be exposed by the pillar etch so subsequent oxidation process can be performed. Since the AlGaAs oxidation layer is in between the two DBR layers, the pillar must be formed deep enough to penetrate through one side of DBR layers to expose the AlGaAs oxidation layer. However, in the current invention since no dedicated oxidation layer is required to define the optical aperture, a shallow pillar etch may be adequate and applicable.
Referring to
The VCSEL device and method of manufacturing eliminates the need for dedicated internal oxide aperture as well as the front side contact metal opening thus the size of the VCSEL pillar 50 can be reduced as shown in
In practice “da” may typically be around 5-10 um, the same range for “dc” and “dgap”, so for simplicity purpose let's assume all three distances da, dc, and dgap are 10 um in length. Thus, the unit cell of one-dimensional distance is 40 um for the prior art, and only 20 um under the current design. Since 3D sensing VCSEL array is typically 2D array in nature, the die size and density advantage of the current design will be ( 20/40)×( 20/40)=0.25, meaning a minimum of 4× increase of the total die counts in the same wafer area with the current invention. The die size and die count advantage will greatly decrease the die cost without compromising or giving up any performance spec. This is in fact in addition to the advantage of assembly and packaging simplification and better thermal arrangement with the Flip-chip configuration when the solder tip is place at each and every VCSEL pillar.
The VCSEL design of the current invention has offered multiple advantages over the prior art designs namely; (1) flip-chip configurable, (2) better thermal arrangement, (3) denser array for the same power output, (4) one step reflow assembly and packaging process, (5) lithographically based lens formation at the backside opening, (6) lower pillar or mesa height, and (6) dielectric DBR feasible to replace one epi-based DBR for more design flexibility and lower cost.
While embodiments of the disclosure have been described in terms of various specific embodiments, those skilled in the art will recognize that the embodiments of the disclosure may be practiced with modifications within the spirit and scope of the claims
This patent application is related to U.S. Provisional Application No. 62/615,069 filed Jan. 9, 2018, entitled “PILLAR CONFINED BACKSIDE ILLUMINATING VCSEL FOR 3D SENSING ARRAY” in the names of Yi-Ching Pao, Majid Riaziat, Ta-Chung Wu, Wilson Kyi and James Pao, and which is incorporated herein by reference in its entirety. The present patent application claims the benefit under 35 U.S.C. § 119(e).
Number | Date | Country | |
---|---|---|---|