This invention relates to a piston and a method of manufacturing a piston for use in magneto-rheological fluid systems.
Suspension dampers, such as shock absorbers, have been used for many years to control the ride quality of automotive vehicles. In many vehicles, it is desirable to control suspension stiffness. Recently, magneto-rheological fluids have become available for use in vehicle suspension dampers. Magneto-rheological fluids permit the viscosity of the damping fluid to be changed in response to an applied magnetic field. Ride stiffness may thereby be controlled by controlling current in an electric coil within the damper. In magneto-rheological suspension systems, a magnetic field is generated and is applied to the magneto-rheological damping fluid, thereby permitting the viscosity of the fluid to be modified depending upon ride conditions. Accordingly, the stiffness of the suspension system may be easily controlled.
Magneto-rheological suspension systems require a piston rod and a suspension piston in which a coil is mounted. The coil circumscribes the piston rod, and the fluid is communicated through passages circumscribing the piston rod between the coil and the piston ring or skirt. The piston includes a piston skirt or ring, which is held in place by a piston plate which is mounted on the piston rod and supports the piston ring. Accordingly, in order that the magnetic field be applied to the magneto-rheological fluid communicated through the passages, the portion of the piston rod extending through the coil and the piston skirt or ring must be made of a magnetically soft material exhibiting high magnetic permeability and high saturation magnetization. The piston plate, which extends between the piston ring and the piston rod, is desirably a magnetic insulator exhibiting low magnetic permeability and serves only to hold the other components in place. Accordingly, the rod and piston ring define a magnetic circuit in which the electrodes are the piston rod and piston ring. This magnetic circuit is energized by the coil and the magnetic field is generated by electrical current flowing through the coil.
Since the piston ring must be made of a material having high magnetic permeability and the piston plate is desirably a magnetic insulator having extremely low magnetic permeability, it is desirable to manufacture the piston ring and rod out of low carbon soft magnetic steel, while the plate is desirably made out of non-magnetic stainless steel. Because the plate and piston ring are made out of materials having different properties, joining the plate to the ring has been difficult. Conventional welding and brazing techniques have proven to be unreliable. Welding dissimilar materials of the type used in the piston ring and plate disclosed herein is inherently difficult and often results in inconsistent and cracked or failed welds.
According to the invention, the ring is clamped in two nearly semi-circular electrodes whose inner diameter matches the outer diameter of the ring closely. The semi-circular electrodes are connected together electrically and connected to one of the terminals of a power supply of a resistance welding machine. The plate is supported on a deflectable pin that extends coaxially through the ring so that the plate is supported coaxial with the ring. The plate is engaged by another electrode which is connected to the other terminal of the power supply of the resistance welding machine. The ring is urged against the ring with a predetermined weld force. Electrical current is then caused to flow through the ring and the plate. The magnitude of the current is adjusted so that the portions of the ring and the plate which engage one another are heated to a temperature causing the portions in both components engaging one another to become pliable or plastic. When this occurs, the plate is forced into the piston, thereby causing the plasticized material at the interface to mix with one another, thereby forming a solid state bond between the components. Because of the intermingling of the portions of the components, the strength of the bond is greater than the strength of either of the components. Although the invention has been specifically described with respect to a magneto-rheological suspension damper, the piston of the present invention may be used in other types of magneto-rheological fluid systems.
Referring now to the drawings, a suspension damper generally indicated by the numeral 10 is designed to operate with a magneto-rheological damping fluid to control suspension stiffness. Magneto-rheological fluids are commercially available and generally comprise a synthetic hydrocarbon or silicone based fluid in which magnetically soft particles (such as iron microspheres) are suspended. In the absence of a magnetic field, the particles exhibit a random orientation within the fluid. Fluid viscosity is relatively low. When a magnetic coil generates a magnetic field in the vicinity of the fluid, the applied magnetic field aligns the magnetic particles into fibrous structures, thereby changing the fluid viscosity to a much higher value. By controlling current in the electromagnetic coil, the strength of the applied magnetic field may be varied, thus permitting gradations in the viscosity of the fluid. Referring to the damper 10 of
The skirt or piston ring 16 includes an outer diameter surface 28 and inner diameter surface 30, which is stepped to defined a larger diameter portion 32 and a smaller diameter portion 34 with a shoulder 36 therebetween. Piston plate 18 is provided with a central opening 38 through which piston rod 20 extends and is attached. Plate 18 also defines an outer circumferential surface 40, which is less than the smaller diameter portion 34 of skirt 16 and cooperates with inner circumferential surface 30 to define the passages 26 therebetween. Segments of the outer circumferential surface 40 extend between radially outwardly projecting portions 42 of the plate 18. As can be seen on
Referring now to
As also shown in
Due to interference of the projections 42 of the plate 18, the plate 18 does not enter the ring 12 with the application of the weld force alone (but instead engages the end face 54), as indicated by FIG. 5. When an appropriate weld current is applied for a short period typically not exceeding one second, the heat and pressure make the plate 18 move into the ring 12, without significant melting at the weld interface, as shown in FIG. 6. The portions 42 of the plate 18 and the portions of the skirt engaged by projections 42 become plastic and intermingle with one another, forming a solid state weld. The clamping electrodes 44, 46 are then moved away to release the completed assembly, as shown in FIG. 7.
This is a division of application Ser. No. 09/775,192 filed on Feb. 1, 2001 now U.S. Pat. No. 6,525,289.
Number | Name | Date | Kind |
---|---|---|---|
4106171 | Basiulis | Aug 1978 | A |
4673067 | Munning et al. | Jun 1987 | A |
5277281 | Carlson et al. | Jan 1994 | A |
5878851 | Carlson et al. | Mar 1999 | A |
6260675 | Muhlenkamp | Jul 2001 | B1 |
6279700 | Lisenker et al. | Aug 2001 | B1 |
6311810 | Hopkins et al. | Nov 2001 | B1 |
6318519 | Kruckemeyer et al. | Nov 2001 | B1 |
6318520 | Lisenker et al. | Nov 2001 | B1 |
6382369 | Lisenker | May 2002 | B1 |
6390252 | Namuduri et al. | May 2002 | B1 |
6419058 | Oliver et al. | Jul 2002 | B1 |
6471018 | Gordaninejad et al. | Oct 2002 | B1 |
6481546 | Oliver et al. | Nov 2002 | B2 |
6497308 | Lisenker | Dec 2002 | B2 |
6497309 | Lisenker | Dec 2002 | B1 |
6525289 | Ananthanarayanan et al. | Feb 2003 | B2 |
6612409 | Lun et al. | Sep 2003 | B2 |
6637560 | Oliver et al. | Oct 2003 | B2 |
Number | Date | Country |
---|---|---|
3304903 | Aug 1984 | DE |
Number | Date | Country | |
---|---|---|---|
20030085201 A1 | May 2003 | US |
Number | Date | Country | |
---|---|---|---|
Parent | 09775192 | Feb 2001 | US |
Child | 10325191 | US |