Claims
- 1. A method for scoring and breaking plastic sheet material and comprising:
- a. placing the sheet on a generally flat surface at a first location, and providing the intended line of cut over a raised bead in said table,
- b. scoring the upper surface of the sheet opposite the bead,
- c. deflecting said sheet on both sides of the resulting score line through a critical bend angle in the range between 4.degree. and 6.degree. as measured from the plane defined by the initially flat upper surface of the plastic sheet,
- d. further deflecting said sheet past said critical bend angle at a second location and only after said first mentioned deflecting step, and
- e. heating said scoring tool to a temperature in the range between 750.degree. and 1500.degree. F prior to said scoring step.
- 2. The method of claim 1 wherein said further deflecting step is accomplished by bending said sheet about a table edge or the like.
- 3. The method of claim 1 wherein said scoring, deflecting, and further deflecting steps are accomplished at longitudinally spaced locations along said score line, said longitudinal spacing being at least as great as the lateral spacing of the force applying areas from said score line.
- 4. A method for scoring and breaking plastic sheet material comprising the successive steps of:
- a. placing the sheet on a generally flat surface, and providing the intended line of score over a raised bead in said table,
- b. passing a scoring tool across the upper surface of the sheet opposite the bead to provide a relatively shallow V-shaped score line,
- c. passing a sheet bending device across the upper surface of the sheet while the lower surface remains on the bead to deflect the sheet downwardly on both sides of the score line through deflection angles in the range between 4.degree. and 6.degree. as measured from the plane of the initially flat upper surface of the sheet, to produce a deepened fissure in the sheet,
- d. removing the sheet from its position over the bead and exerting a bending moment at least at one end of the sheet to project the fissure through the sheet, and to facilitate
- e. running the break along the deepened fissure produced by the step (d) in a manner not unlike that of breaking glass following a single scoring step.
- 5. The method of claim 4 wherein said step (d) is accomplished by bending said sheet about a table edge or the like beyond said 4.degree. to 6.degree. of step (c) above.
- 6. The method of claim 4 wherein said method is further characterized by heating the scoring tool prior to said scoring step.
CROSS REFERENCE TO RELATED APPLICATION
This application is a continuation-in-part of my copending application bearing the same title filed Jan. 30, 1974, under Ser. No. 437,982, and now abandoned.
US Referenced Citations (2)
Continuation in Parts (1)
|
Number |
Date |
Country |
Parent |
437982 |
Jan 1974 |
|