Claims
- 1. A method for preparing an improved polymer polyblend composition which comprises blending a liquid polymer of a conjugated diene monomer with the polymerization product of
- (A) 13 to 97 parts by weight of at least one monoalkenyl aromatic monomer,
- (B) 0 to 85 parts by weight of at least one monoalkenyl nitrile monomer, and
- (C) 2 to 36 parts by weight of a diene rubber, wherein said liquid polymer is blended with said polyblend in an amount of about 0.2 to 20 parts by weight, said polymer containing groups selected from the group consisting of hydroxyl, carboxy, mercaptan, xanthate, hydrogen, aralkyl and phenyl or mixtures thereof, said groups being present at the terminal position only of said liquid polymer, the total polyblend being 100 parts by weight.
- 2. A method of claim 1, wherein said monoalkenyl aromatic monomer is styrene, aralkylstyrene, alphalkystyrene, alpha-arhalostyrene and mixtures of the same.
- 3. A method of claim 1, wherein said monoalkenyl aromatic monomer is styrene.
- 4. A method of claim 1, wherein said monoalkenyl nitrile monomer is acrylonitrile or methacrylonitrile and mixtures of the same.
- 5. A method of claim 1, wherein the monoalkenyl nitrile monomer is acrylonitrile.
- 6. A method of claim 1, wherein said diene rubber is polybutadiene, butadiene-styrene copolymer, butadiene-acrylonitrile copolymer of polypentenamer or mixtures thereof, wherein said polybutadiene rubber has a cis isomer content of about 30 percent to 98 percent and a Tg range of from about -50.degree. C. to -105.degree. C., said butadiene copolymer rubbers having a Tg range of from about -20.degree. C. to -70.degree. C.
- 7. A method of claim 1, wherein said diene rubber is polybutadiene.
- 8. A method of claim 1, wherein said liquid polymer of a conjugated diene monomer is a polybutadiene, a butadiene-styrene copolymer or a butadiene-acrylonitrile copolymer and mixtures of the same.
- 9. A method of claim 1, wherein said liquid polymer is a polybutadiene having a molecular weight of from about 1,000 to 10,000.
- 10. A method of claim 1, wherein said liquid polymer is a polybutadiene containing terminal aralkyl groups.
- 11. A method of claim 1, wherein said liquid polymer is a polybutadiene containing terminal hydrogen.
- 12. A method of claim 1, which comprises blending a liquid polymer of a conjugated diene monomer with the polymerization product of
- (A) 13 to 97 parts by weight of styrene,
- (B) 0 to 98 parts by weight of acrylonitrile,
- (C) 2 to 36 parts by weight of polybutadiene rubber, wherein said liquid polymer of a conjugated monomer has a molecular weight of about 500 to 10,000 and is blended with said polyblend in an amount of about 0.2 to 20 parts by weight, the total polyblend being 100 parts by weight.
Parent Case Info
This application is a continuation-in-part of application Ser. No. 515,933, filed Oct. 18, 1974, now abandoned.
US Referenced Citations (9)
Continuation in Parts (1)
|
Number |
Date |
Country |
Parent |
515933 |
Oct 1974 |
|