Claims
- 1. The method of polymerizing 2-pyrrolidone comprising contacting a substantially anhydrous mixture of monomeric 2-pyrrolidone, a catalyst embodying an alkali metal salt of 2-pyrrolidone the alkali metal being selected from the group consisting of rubidium and cesium, with an activator consisting of sulfur dioxide at a temperature of from 20.degree. to 60.degree. C. whereby a white polymer of 2-pyrrolidone is formed having thermal characteristics suitable for melt extrusion.
- 2. The method of claim 1 wherein the temperature of polymerization is from 38.degree. to 42.degree. C.
RELATED APPLICATIONS
This application is a division of Application Ser. No. 039,773 filed May 17, 1979, which in turn is a continuation-in-part of Application Ser. No. 899,066, filed Apr. 24, 1978, now abandoned.
US Referenced Citations (10)
Non-Patent Literature Citations (1)
Entry |
Die Makromolekulare Chemie, 161, p. 64, (1972). |
Divisions (1)
|
Number |
Date |
Country |
Parent |
39773 |
May 1979 |
|
Continuation in Parts (1)
|
Number |
Date |
Country |
Parent |
899066 |
Apr 1978 |
|